Shwetabh Gupta
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Shwetabh Gupta has a total of 4 co-authors. Here are the top co-authors by number of shared publications:
- Gururaj Parande
Department of Mechanical Engineering, National University of Singapore, 9 Engineering Drive 1, Singapore 117575, Singapore
3 shared publications - Manoj Gupta
Department of Mechanical Engineering, National University of Singapore, 9 Engineering, Drive 1, Singapore 117575, Singapore
3 shared publications - Khin Sandar Tun
Department of Mechanical Engineering, National University of Singapore, Singapore 117576, Singapore
1 shared publication - Michael Johanes
Department of Mechanical Engineering, National University of Singapore, 9 Engineering, Drive 1, Singapore 117575, Singapore
1 shared publication
Latest Publications
- Open Access
An Investigation into the Effect of Length Scale of Reinforcement on the Cryogenic Response of a Mg/2wt.%CeO2 Composite
The present study attempted for the first time an investigation on the effect of deep cryogenic treatment in liquid nitrogen (LN) on magnesium–cerium oxide (Mg/2wt.%CeO2) composites containing equal amounts of different length scales (micron and nanosize) cerium oxide (CeO2) particles. The disintegrated melt deposition method was used to synthesize Mg-2CeO2 micro- and nanocomposites, followed by hot extrusion as the secondary processing. Further liquid nitrogen treatment was performed at a cryogenic temperature of −196 °C. The combined effects of cryogenic treatment and reinforcement length scale on physical, mechanical, and thermal behaviors were studied. The results indicate that LN-treated micro- and nanocomposite samples exhibit, in common, a reduction in porosity, similar grain size, and a limited effect on the original texture of the matrix. However, microhardness, 0.2% Compressive Yield Strength (CYS), failure strain, and energy absorbed increased for both micro- and nanocomposite samples. Overall, results clearly indicate the capability of deep cryogenic treatment with LN to positively diversify the properties of both micro- and nanocomposite samples.
Open AccessAn Investigation into the Effect of Length Scale of Reinforcement on the Cryogenic Response of a Mg/2wt.%CeO2 Composite
The present study attempted for the first time an investigation on the effect of deep cryogenic treatment in liquid nitrogen (LN) on magnesium–cerium oxide (Mg/2wt.%CeO2) composites containing equal amounts of different length scales (micron and nanosize) cerium oxide (CeO2) particles. The disintegrated melt deposition method was used to synthesize Mg-2CeO2 micro- and nanocomposites, followed by hot extrusion as the secondary processing. Further liquid nitrogen treatment was performed at a cryogenic temperature of −196 °C. The combined effects of cryogenic treatment and reinforcement length scale on physical, mechanical, and thermal behaviors were studied. The results indicate that LN-treated micro- and nanocomposite samples exhibit, in common, a reduction in porosity, similar grain size, and a limited effect on the original texture of the matrix. However, microhardness, 0.2% Compressive Yield Strength (CYS), failure strain, and energy absorbed increased for both micro- and nanocomposite samples. Overall, results clearly indicate the capability of deep cryogenic treatment with LN to positively diversify the properties of both micro- and nanocomposite samples.
- Open Access
- 23 January 2024
- Published by MDPI AG in Technologies
- Vol. 12 (2) , 14
Comparison of Shallow (−20 °C) and Deep Cryogenic Treatment (−196 °C) to Enhance the Properties of a Mg/2wt.%CeO2 Nanocomposite
Magnesium and its composites have been used in various applications owing to their high specific strength properties and low density. However, the application is limited to room-temperature conditions owing to the lack of research available on the ability of magnesium alloys to perform in sub-zero conditions. The present study attempted, for the first time, the effects of two cryogenic temperatures (−20 °C/253 K and −196 °C/77 K) on the physical, thermal, and mechanical properties of a Mg/2wt.%CeO2 nanocomposite. The materials were synthesized using the disintegrated melt deposition method followed by hot extrusion. The results revealed that the shallow cryogenically treated (refrigerated at −20 °C) samples display a reduction in porosity, lower ignition resistance, similar microhardness, compressive yield, and ultimate strength and failure strain when compared to deep cryogenically treated samples in liquid nitrogen at −196 °C. Although deep cryogenically treated samples showed an overall edge, the extent of the increase in properties may not be justified, as samples exposed at −20 °C display very similar mechanical properties, thus reducing the overall cost of the cryogenic process. The results were compared with the data available in the open literature, and the mechanisms behind the improvement of the properties were evaluated.
- 23 January 2024
- Published by MDPI AG in Technologies
- Vol. 12 (2) , 14
Open AccessComparison of Shallow (−20 °C) and Deep Cryogenic Treatment (−196 °C) to Enhance the Properties of a Mg/2wt.%CeO2 Nanocomposite
Magnesium and its composites have been used in various applications owing to their high specific strength properties and low density. However, the application is limited to room-temperature conditions owing to the lack of research available on the ability of magnesium alloys to perform in sub-zero conditions. The present study attempted, for the first time, the effects of two cryogenic temperatures (−20 °C/253 K and −196 °C/77 K) on the physical, thermal, and mechanical properties of a Mg/2wt.%CeO2 nanocomposite. The materials were synthesized using the disintegrated melt deposition method followed by hot extrusion. The results revealed that the shallow cryogenically treated (refrigerated at −20 °C) samples display a reduction in porosity, lower ignition resistance, similar microhardness, compressive yield, and ultimate strength and failure strain when compared to deep cryogenically treated samples in liquid nitrogen at −196 °C. Although deep cryogenically treated samples showed an overall edge, the extent of the increase in properties may not be justified, as samples exposed at −20 °C display very similar mechanical properties, thus reducing the overall cost of the cryogenic process. The results were compared with the data available in the open literature, and the mechanisms behind the improvement of the properties were evaluated.
- Open Access
Enhancing the Physical, Thermal, and Mechanical Responses of a Mg/2wt.%CeO2 Nanocomposite Using Deep Cryogenic Treatment
Deep cryogenic treatment has shown promise as a facile method of increasing the characteristics of many materials including alloys of iron, aluminum, and magnesium. However, there have not been any prior studies on its effect on the microstructure and thermal and mechanical properties of magnesium-based nanocomposites. In this study, a Mg/2wt.%CeO2 nanocomposite was processed using disintegrated melt deposition processing coupled with hot extrusion, followed by cryogenic treatment in liquid nitrogen for 24 h. The characterization results show increases in density (reduction in porosity), ignition temperature, compressive yield strength, compressive ductility, and microhardness. This study, for the first time, shows the significant relevance of deep cryogenic treatment in enhancing an array of properties of a magnesium-based nanocomposite that may be catalytic in improving its application spectrum.
Open AccessEnhancing the Physical, Thermal, and Mechanical Responses of a Mg/2wt.%CeO2 Nanocomposite Using Deep Cryogenic Treatment
Deep cryogenic treatment has shown promise as a facile method of increasing the characteristics of many materials including alloys of iron, aluminum, and magnesium. However, there have not been any prior studies on its effect on the microstructure and thermal and mechanical properties of magnesium-based nanocomposites. In this study, a Mg/2wt.%CeO2 nanocomposite was processed using disintegrated melt deposition processing coupled with hot extrusion, followed by cryogenic treatment in liquid nitrogen for 24 h. The characterization results show increases in density (reduction in porosity), ignition temperature, compressive yield strength, compressive ductility, and microhardness. This study, for the first time, shows the significant relevance of deep cryogenic treatment in enhancing an array of properties of a magnesium-based nanocomposite that may be catalytic in improving its application spectrum.