Ying Wang
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Ying Wang has a total of 78 co-authors. Here are the top co-authors by number of shared publications:
Zhenwen Yang
Tianjin Key Lab of Advanced Joining Technology School of Materials Science and Engineering Tianjin University Tianjin China
9 shared publicationsShiyu Niu
Tianjin Key Lab of Advanced Joining Technology School of Materials Science and Engineering Tianjin University Tianjin China
7 shared publications- Zhenwen Yang
Tianjin Key Lab of Advanced Joining Technology School of Materials Science and Engineering Tianjin University Tianjin China
5 shared publications Ying Han
Tianjin Key Lab of Advanced Joining Technology School of Materials Science and Engineering Tianjin University Tianjin China
3 shared publicationsBen Liu
Guizhou Space Appliance Co., Ltd Guiyang China
2 shared publicationsDongpo Wang
Tianjin Key Lab of Advanced Joining Technology School of Materials Science and Engineering Tianjin University Tianjin 300350 China
2 shared publications
Latest Publications
- Open Access
- 25 September 2026
- Published by Wiley in Advanced Engineering Materials
- Vol. 28 (21) , e71224
Effect of Micro‐Alloying Elements on the Interfacial Behavior and Properties of Diffusion‐Bonded Zirconium Alloys
Zirconium alloys are widely used as nuclear fuel cladding materials; however, achieving joints with both high strength and corrosion resistance remains challenging. In this work, diffusion bonding of Zr–Hf, Zr–Sn, and Zr–Sn–Nb alloys was systematically studied (760–840 °C, 10 MPa) to elucidate the roles of alloying elements in interfacial evolution and joint performance. Our findings show that micro‐alloying affects bonding through two coupled mechanisms: grain‐size‐dependent diffusion promotes interfacial void closure, particularly at the early bonding stage and at lower temperatures, while alloying‐element‐controlled reactions determine the type and distribution of interfacial precipitates, where Nb‐induced Zener pinning stabilizes a fine‐grained structure (~10 μm) and promotes rapid interface healing. After sufficient interfacial void closure has been achieved, alloying‐element‐controlled interfacial reactions mainly determine the type and distribution of interfacial precipitates, with Fe initiating reactions and Nb suppressing brittle Zr(Fe, Cr) 2 while promoting Zr(Fe, Nb) 2 formation. These mechanisms collectively determine joint properties. The Zr–Sn–Nb joint achieves the highest strength (356 MPa) but reduced corrosion resistance. In contrast, the Zr–Sn joint exhibits the best corrosion resistance while maintaining relatively high shear strength. This work provides insight into alloying–microstructure–interface relationships in zirconium alloy bonding.
- 25 September 2026
- Published by Wiley in Advanced Engineering Materials
- Vol. 28 (21) , e71224
Open AccessEffect of Micro‐Alloying Elements on the Interfacial Behavior and Properties of Diffusion‐Bonded Zirconium Alloys
Zirconium alloys are widely used as nuclear fuel cladding materials; however, achieving joints with both high strength and corrosion resistance remains challenging. In this work, diffusion bonding of Zr–Hf, Zr–Sn, and Zr–Sn–Nb alloys was systematically studied (760–840 °C, 10 MPa) to elucidate the roles of alloying elements in interfacial evolution and joint performance. Our findings show that micro‐alloying affects bonding through two coupled mechanisms: grain‐size‐dependent diffusion promotes interfacial void closure, particularly at the early bonding stage and at lower temperatures, while alloying‐element‐controlled reactions determine the type and distribution of interfacial precipitates, where Nb‐induced Zener pinning stabilizes a fine‐grained structure (~10 μm) and promotes rapid interface healing. After sufficient interfacial void closure has been achieved, alloying‐element‐controlled interfacial reactions mainly determine the type and distribution of interfacial precipitates, with Fe initiating reactions and Nb suppressing brittle Zr(Fe, Cr) 2 while promoting Zr(Fe, Nb) 2 formation. These mechanisms collectively determine joint properties. The Zr–Sn–Nb joint achieves the highest strength (356 MPa) but reduced corrosion resistance. In contrast, the Zr–Sn joint exhibits the best corrosion resistance while maintaining relatively high shear strength. This work provides insight into alloying–microstructure–interface relationships in zirconium alloy bonding.
- Open Access
- 29 June 2026
- Published by Elsevier in SSRN Electronic Journal
High-strength Diffusion Bonding of Zr-4 Alloy via Hydrogen-Enabled Plastic Deformation Induced Dynamic Recrystallization
Plasticity plays a key role in diffusion bonding process, while the fundamental mechanism by which plasticity affects the diffusion bonding process remains unclear, hindering the further advancement of the diffusion bonding technology. In this work, Zr-4 alloys with various plasticity were obtained through hydrogenation first and subsequently diffusion bonded at identical temperature and pressure. The high-temperature plasticity of the Zr-4 alloy were improved after hydrogenation, accompanied by increased interface bonding ratios and shear strengths of the diffusion-bonded joints. Meanwhile, EBSD images proved that a ~110% increase in recrystallization happened with the increase of the hydrogen content. MD simulation was conducted and the results further confirmed that hydrogen-induced generation of β-Zr with better plasticity indeed exhibited lower compressive yield strength than α-Zr at diffusion-bonded temperatures. Therefore, the β-Zr underwent rapid dynamic recrystallization within only 0.5ns, while α-Zr failed to recrystallize even after 2 ns at the same load. A notable stress-strain curve fluctuation was detected for the hydrogenated Zr-4 samples tested at 700℃, further indicating that an in-situ dynamic recrystallization indeed happened during the diffusion bonding process. The strong recrystallization finally facilitated the formation and growth of grains at the bonding interface. This work revealed that improving the intrinsic plasticity of the Zr-4 substracts via hydrogen-induced phase transformation, without changing the temperature and pressure, effectively enhanced the dynamic recrystallization of the substracts, thereby improving interface bonding ratio and overall mechanical performance of diffusion-bonded joints, providing new insights on improving the diffusion bonding quality in addition to the common process parameter optimizations.
- 29 June 2026
- Published by Elsevier in SSRN Electronic Journal
Open AccessHigh-strength Diffusion Bonding of Zr-4 Alloy via Hydrogen-Enabled Plastic Deformation Induced Dynamic Recrystallization
Plasticity plays a key role in diffusion bonding process, while the fundamental mechanism by which plasticity affects the diffusion bonding process remains unclear, hindering the further advancement of the diffusion bonding technology. In this work, Zr-4 alloys with various plasticity were obtained through hydrogenation first and subsequently diffusion bonded at identical temperature and pressure. The high-temperature plasticity of the Zr-4 alloy were improved after hydrogenation, accompanied by increased interface bonding ratios and shear strengths of the diffusion-bonded joints. Meanwhile, EBSD images proved that a ~110% increase in recrystallization happened with the increase of the hydrogen content. MD simulation was conducted and the results further confirmed that hydrogen-induced generation of β-Zr with better plasticity indeed exhibited lower compressive yield strength than α-Zr at diffusion-bonded temperatures. Therefore, the β-Zr underwent rapid dynamic recrystallization within only 0.5ns, while α-Zr failed to recrystallize even after 2 ns at the same load. A notable stress-strain curve fluctuation was detected for the hydrogenated Zr-4 samples tested at 700℃, further indicating that an in-situ dynamic recrystallization indeed happened during the diffusion bonding process. The strong recrystallization finally facilitated the formation and growth of grains at the bonding interface. This work revealed that improving the intrinsic plasticity of the Zr-4 substracts via hydrogen-induced phase transformation, without changing the temperature and pressure, effectively enhanced the dynamic recrystallization of the substracts, thereby improving interface bonding ratio and overall mechanical performance of diffusion-bonded joints, providing new insights on improving the diffusion bonding quality in addition to the common process parameter optimizations.
- 25 February 2026
- Published by Springer Nature in Journal of Materials Engineering and Performance
- Vol. 35 (20) , 19600-19615
Effect of Post-weld Heat Treatment on the Microstructure and Mechanical Properties of the Heat-Affected Zone of Alloy 617
- 25 February 2026
- Published by Springer Nature in Journal of Materials Engineering and Performance
- Vol. 35 (20) , 19600-19615
Effect of Post-weld Heat Treatment on the Microstructure and Mechanical Properties of the Heat-Affected Zone of Alloy 617
- 19 December 2025
- Published by Wiley in Advanced Engineering Materials
- Vol. 28 (3)
Effect of Hydrogenation on the Microstructure and Mechanical Properties of Low‐Temperature Diffusion Bonding Joints of Zirconium Alloy
To address the limitations of high‐temperature diffusion bonding in zirconium alloys, the effect of controlled hydrogenation is investigated on bonding behavior, microstructure evolution, and joint performance. Zirconium alloy with 0, 200, and 2000 ppm hydrogen are prepared for diffusion bonding at 700–800 °C under 15 MPa for 30–120 min. At 200 ppm hydrogen, hydrides decomposed during bonding and reprecipitated along the interface upon cooling, eliminating interfacial voids and preserving finely dispersed second‐phase particles around equiaxed α ‐Zr grains with minimal coarsening. At 2000 ppm hydrogen, incomplete hydride decomposition resulted in residual hydrides, while β ‐Zr at grain boundaries softened the interfacial grains without extensive recrystallization, maintaining grain sizes below 7 μm. Hydrogenation lowered the required bonding temperature, where joints bonded at 700 °C with 200 ppm hydrogen achieved shear strengths of 220 MPa, comparable to un‐hydrogenated joints bonded at 750 °C. Similarly, 2000 ppm hydrogen enabled comparable strength at 720 °C to that of un‐hydrogenated joints bonded at 780 °C. Molecular dynamics simulations confirmed that hydrogen‐induced hydrogen‐vacancy clusters enhanced atomic diffusion, while finite‐element modeling demonstrated that hydrogen‐induced softening lowered local stress concentrations and promoted void closure during bonding. These multiscale insights clarify the mechanisms where hydrogen enhances diffusion bonding efficiency and joint properties in zirconium alloys.
- 19 December 2025
- Published by Wiley in Advanced Engineering Materials
- Vol. 28 (3)
Effect of Hydrogenation on the Microstructure and Mechanical Properties of Low‐Temperature Diffusion Bonding Joints of Zirconium Alloy
To address the limitations of high‐temperature diffusion bonding in zirconium alloys, the effect of controlled hydrogenation is investigated on bonding behavior, microstructure evolution, and joint performance. Zirconium alloy with 0, 200, and 2000 ppm hydrogen are prepared for diffusion bonding at 700–800 °C under 15 MPa for 30–120 min. At 200 ppm hydrogen, hydrides decomposed during bonding and reprecipitated along the interface upon cooling, eliminating interfacial voids and preserving finely dispersed second‐phase particles around equiaxed α ‐Zr grains with minimal coarsening. At 2000 ppm hydrogen, incomplete hydride decomposition resulted in residual hydrides, while β ‐Zr at grain boundaries softened the interfacial grains without extensive recrystallization, maintaining grain sizes below 7 μm. Hydrogenation lowered the required bonding temperature, where joints bonded at 700 °C with 200 ppm hydrogen achieved shear strengths of 220 MPa, comparable to un‐hydrogenated joints bonded at 750 °C. Similarly, 2000 ppm hydrogen enabled comparable strength at 720 °C to that of un‐hydrogenated joints bonded at 780 °C. Molecular dynamics simulations confirmed that hydrogen‐induced hydrogen‐vacancy clusters enhanced atomic diffusion, while finite‐element modeling demonstrated that hydrogen‐induced softening lowered local stress concentrations and promoted void closure during bonding. These multiscale insights clarify the mechanisms where hydrogen enhances diffusion bonding efficiency and joint properties in zirconium alloys.
- 7 July 2025
- Published by Springer Nature in Journal of Materials Engineering and Performance
- Vol. 35 (2) , 1448-1459
Study on the Microstructure and Properties of Additive Manufacturing Al-Mg-Sc Alloy with CMT-PADV + Arc Weaving Process
- 7 July 2025
- Published by Springer Nature in Journal of Materials Engineering and Performance
- Vol. 35 (2) , 1448-1459
Study on the Microstructure and Properties of Additive Manufacturing Al-Mg-Sc Alloy with CMT-PADV + Arc Weaving Process
- Top Cited PapersOpen Access
- 1 January 2025
- Published by Tsinghua University Press in Journal of Advanced Ceramics
- Vol. 14 (1)
Excellent high-temperature strength of (HfZrTiTaNb)C high-entropy carbide diffusion-bonded joint via in-situ alloying of Ni/Nb/Ni composite interlayer
To obtain high-entropy carbide (HEC) joints with excellent high-temperature performance, a (HfZrTiTaNb)C HEC joint featuring a direct diffusion-bonded interface with Nb-based interlayer was successfully fabricated at relatively low temperatures of 1150-1250 °C for 60 min under 10 MPa. Starting from a modified Ni/Nb/Ni composite interlayer with a Nb content of > 64 at.%, an alloyed Nb2Ni layer was constructed in situ by accelerating the directional diffusion of Ni atoms from the high-entropy interface into the remaining pure Nb through the Ni-Nb eutectic liquid. Moreover, the excess liquid phase was squeezed out of the bonding region, ensuring the absence of Ni-based compounds. Leveraging the intrinsic interfacial stability and sluggish diffusion effect, the HEC with its original lattice structure was capable of developing diffusion bonding with the Nb2Ni layer, instead of interacting with the liquid phase. The high reliability of the HEC/Nb2Ni bonded interface was confirmed by the coherence of (13) HEC // (141) Nb2Ni and calculated lattice misfit of 0.044. The HEC joint had high room-temperature strength of 174 MPa due to a homogenous Nb2Ni layer that exhibited nanohardness (15.2 ± 1.5 GPa) and elastic modulus (219.9 ± 17.5 GPa). Further, the strength of the HEC joint did not decrease at 1000 °C, enhancing ~ 49% over that of HEC/Ni/HEC diffusion-bonded joints with stringent requirements on surface flatness. This suggested the HEC/Nb2Ni interface had excellent resistance to high-temperature softening, even though it was invariably the initial failure location. This work is informative for designing bonding structures and preparing HEC components.
- 1 January 2025
- Published by Tsinghua University Press in Journal of Advanced Ceramics
- Vol. 14 (1)
Top Cited PapersOpen AccessExcellent high-temperature strength of (HfZrTiTaNb)C high-entropy carbide diffusion-bonded joint via in-situ alloying of Ni/Nb/Ni composite interlayer
To obtain high-entropy carbide (HEC) joints with excellent high-temperature performance, a (HfZrTiTaNb)C HEC joint featuring a direct diffusion-bonded interface with Nb-based interlayer was successfully fabricated at relatively low temperatures of 1150-1250 °C for 60 min under 10 MPa. Starting from a modified Ni/Nb/Ni composite interlayer with a Nb content of > 64 at.%, an alloyed Nb2Ni layer was constructed in situ by accelerating the directional diffusion of Ni atoms from the high-entropy interface into the remaining pure Nb through the Ni-Nb eutectic liquid. Moreover, the excess liquid phase was squeezed out of the bonding region, ensuring the absence of Ni-based compounds. Leveraging the intrinsic interfacial stability and sluggish diffusion effect, the HEC with its original lattice structure was capable of developing diffusion bonding with the Nb2Ni layer, instead of interacting with the liquid phase. The high reliability of the HEC/Nb2Ni bonded interface was confirmed by the coherence of (13) HEC // (141) Nb2Ni and calculated lattice misfit of 0.044. The HEC joint had high room-temperature strength of 174 MPa due to a homogenous Nb2Ni layer that exhibited nanohardness (15.2 ± 1.5 GPa) and elastic modulus (219.9 ± 17.5 GPa). Further, the strength of the HEC joint did not decrease at 1000 °C, enhancing ~ 49% over that of HEC/Ni/HEC diffusion-bonded joints with stringent requirements on surface flatness. This suggested the HEC/Nb2Ni interface had excellent resistance to high-temperature softening, even though it was invariably the initial failure location. This work is informative for designing bonding structures and preparing HEC components.
- 28 August 2024
- Published by Wiley in Advanced Engineering Materials
- Vol. 26 (21)
Joint Microstructure and Performance of Brazing Si 3 N 4 ‐MoSi 2 Composites to Nb with AgCuTi and AgCuTi+MoSi 2p Active Fillers
MoSi 2 particle (MoSi 2p ), the component of Si 3 N 4 ‐MoSi 2 composites, is added into an AgCuTi filler to strengthen the interface bonding without bringing new elements into the Nb/Si 3 N 4 ‐MoSi 2 brazed joint. In this new brazing system, microstructure evolution and strength of Nb/Si 3 N 4 ‐MoSi 2 joints as a function of brazing temperature and holding time, as well as MoSi 2p content, are investigated. With an AgCuTi filler, the reaction of active Ti and Si 3 N 4 ‐MoSi 2 forms a composite layer consisting of Mo 5 Si 3 , TiN, and Ti 5 Si 3 at the interface. The extensive growth of the layer is observed from 1.9 μm at 860 °C to 5.0 μm at 920 °C, and from 1.3 μm for 5 min to 4.6 μm for 20 min as the chemical reactions between Ti and Si 3 N 4 ‐MoSi 2 are more sufficient. Adding 6 wt% MoSi 2p to the filler, the joints exhibit a peak shear strength of 154 MPa, an increase of 20% over that of a commercial AgCuTi filler, with the fracture path changing from the Si 3 N 4 ‐MoSi 2 to the brazing seam. The enhancement of the joint is attributed to the reinforcement of the seam by in situ reaction of the dispersed MoSi 2p with Ti, refining the microstructure and reducing the thickness of the Mo 5 Si 3 +TiN+Ti 5 Si 3 reaction layer.
- 28 August 2024
- Published by Wiley in Advanced Engineering Materials
- Vol. 26 (21)
Joint Microstructure and Performance of Brazing Si 3 N 4 ‐MoSi 2 Composites to Nb with AgCuTi and AgCuTi+MoSi 2p Active Fillers
MoSi 2 particle (MoSi 2p ), the component of Si 3 N 4 ‐MoSi 2 composites, is added into an AgCuTi filler to strengthen the interface bonding without bringing new elements into the Nb/Si 3 N 4 ‐MoSi 2 brazed joint. In this new brazing system, microstructure evolution and strength of Nb/Si 3 N 4 ‐MoSi 2 joints as a function of brazing temperature and holding time, as well as MoSi 2p content, are investigated. With an AgCuTi filler, the reaction of active Ti and Si 3 N 4 ‐MoSi 2 forms a composite layer consisting of Mo 5 Si 3 , TiN, and Ti 5 Si 3 at the interface. The extensive growth of the layer is observed from 1.9 μm at 860 °C to 5.0 μm at 920 °C, and from 1.3 μm for 5 min to 4.6 μm for 20 min as the chemical reactions between Ti and Si 3 N 4 ‐MoSi 2 are more sufficient. Adding 6 wt% MoSi 2p to the filler, the joints exhibit a peak shear strength of 154 MPa, an increase of 20% over that of a commercial AgCuTi filler, with the fracture path changing from the Si 3 N 4 ‐MoSi 2 to the brazing seam. The enhancement of the joint is attributed to the reinforcement of the seam by in situ reaction of the dispersed MoSi 2p with Ti, refining the microstructure and reducing the thickness of the Mo 5 Si 3 +TiN+Ti 5 Si 3 reaction layer.
- 22 June 2024
- Published by Wiley in International Journal of Applied Ceramic Technology
- Vol. 21 (6) , 4228-4240
Microstructure and mechanical properties of Al 2 O 3 ceramic and copper joints brazed with AgCuInTi brazing alloy
Reliable metallurgical bonding between Al 2 O 3 ceramic and copper was achieved by vacuum brazing using Ag–23Cu–14.5In–3.3Ti (wt.%) alloy. The representative interfacial structure of the joint was Al 2 O 3 /Ti 3 (Cu,Al) 3 O + γ‐TiO/Ag‐based solid solution + (Cu,Ag) 7 In 3 + Ag–Cu eutectic + Cu‐based solid solution/copper. The interface microstructure evolved with process parameters, including the formation of γ‐TiO and Ti 3 (Cu,Al) 3 O, as evidenced by microstructural analysis and etched surface morphology. The relationship between fracture path and shear strength was established by observing the fracture morphology and performing shear strength tests on joints with various process parameters, utilizing the degree of the Ag‐based solid solution loss and the thickness of the reaction layer as evaluative factors. When brazed at 760 or 780°C for 20 min using a 100 µm brazing alloy foil, the brazed joints demonstrated a peak shear strength of 215 ± 25 MPa, and the fracture predominantly occurred in the Al 2 O 3 matrix and Ti 3 (Cu,Al) 3 O layer.
- 22 June 2024
- Published by Wiley in International Journal of Applied Ceramic Technology
- Vol. 21 (6) , 4228-4240
Microstructure and mechanical properties of Al 2 O 3 ceramic and copper joints brazed with AgCuInTi brazing alloy
Reliable metallurgical bonding between Al 2 O 3 ceramic and copper was achieved by vacuum brazing using Ag–23Cu–14.5In–3.3Ti (wt.%) alloy. The representative interfacial structure of the joint was Al 2 O 3 /Ti 3 (Cu,Al) 3 O + γ‐TiO/Ag‐based solid solution + (Cu,Ag) 7 In 3 + Ag–Cu eutectic + Cu‐based solid solution/copper. The interface microstructure evolved with process parameters, including the formation of γ‐TiO and Ti 3 (Cu,Al) 3 O, as evidenced by microstructural analysis and etched surface morphology. The relationship between fracture path and shear strength was established by observing the fracture morphology and performing shear strength tests on joints with various process parameters, utilizing the degree of the Ag‐based solid solution loss and the thickness of the reaction layer as evaluative factors. When brazed at 760 or 780°C for 20 min using a 100 µm brazing alloy foil, the brazed joints demonstrated a peak shear strength of 215 ± 25 MPa, and the fracture predominantly occurred in the Al 2 O 3 matrix and Ti 3 (Cu,Al) 3 O layer.