Marzieh Neshandar Asli
Research Subjects
Marzieh Neshandar Asli has a total of 4 co-authors. Here are the top co-authors by number of shared publications:
- Hamid Neshandar Asli
Department of Prosthodontics, Dental Sciences Research Center, School of Dentistry Guilan University of Medical Sciences Rasht Iran
1 shared publication - Mehran Falahchai1 shared publication
- Navid Belyani1 shared publication
- Samiye Rahimabadi
Guilan University of Medical Sciences, Iran
1 shared publication
Latest Publications
- 30 December 2022
- Published by Facultad de Odontologia, Universidad de Concepcion in Journal of Oral Research
- Vol. 11 (6) , 1-10
Effect of different mechanical surface treatments on flexural strength of repaired denture base
Aim: To assess the effect of different mechanical surface treatments on flexural strength of repaired denture base. Material and Methods: Sixty bar-shaped specimens of heat-polymerized acrylic resin were fabricated, and divided into six groups (n=10). All specimens, except the positive control group (group PC), were sectioned into halves to create a 1-mm clearance. A negative control group with no surface treatment (group NC) was also considered. Other groups underwent different surface treatments: group Laser; treated with erbium: yttrium-aluminum-garnet (Er:YAG) laser, group APA; airborne-particle abrasion (APA), group APA plus Laser; a combination of laser and APA, and group Bur; bur grinding. After measuring surface roughness (Ra) with a profilometer, all sectioned specimens were repaired by auto-polymerizing acrylic resin, and thermocycled afterward. Three-point bending test was performed by a universal testing machine. Data were statistically analyzed (α=0.05). Results: The mean surface roughness of all experimental groups were significantly higher than that of group NC (pandlt;0.05). The mean flexural strength of all groups was significantly lower than that of group PC (pandlt;0.05). Group B had significantly higher flexural strength than the other surface-treated groups (pandlt;0.05). Group Laser had significantly higher flexural strength than groups APA (p=0.043) and APA plus Laser (p=0.023). No significant difference was found between groups APA and APA plus Laser (p=0.684). Conclusion: All surface treatments increased the surface roughness and flexural strength compared with the untreated group. The highest flexural strength was observed in specimens treated by bur grinding and then laser, however, it was still significantly lower than intact specimens.
- 30 December 2022
- Published by Facultad de Odontologia, Universidad de Concepcion in Journal of Oral Research
- Vol. 11 (6) , 1-10
Effect of different mechanical surface treatments on flexural strength of repaired denture base
Aim: To assess the effect of different mechanical surface treatments on flexural strength of repaired denture base. Material and Methods: Sixty bar-shaped specimens of heat-polymerized acrylic resin were fabricated, and divided into six groups (n=10). All specimens, except the positive control group (group PC), were sectioned into halves to create a 1-mm clearance. A negative control group with no surface treatment (group NC) was also considered. Other groups underwent different surface treatments: group Laser; treated with erbium: yttrium-aluminum-garnet (Er:YAG) laser, group APA; airborne-particle abrasion (APA), group APA plus Laser; a combination of laser and APA, and group Bur; bur grinding. After measuring surface roughness (Ra) with a profilometer, all sectioned specimens were repaired by auto-polymerizing acrylic resin, and thermocycled afterward. Three-point bending test was performed by a universal testing machine. Data were statistically analyzed (α=0.05). Results: The mean surface roughness of all experimental groups were significantly higher than that of group NC (pandlt;0.05). The mean flexural strength of all groups was significantly lower than that of group PC (pandlt;0.05). Group B had significantly higher flexural strength than the other surface-treated groups (pandlt;0.05). Group Laser had significantly higher flexural strength than groups APA (p=0.043) and APA plus Laser (p=0.023). No significant difference was found between groups APA and APA plus Laser (p=0.684). Conclusion: All surface treatments increased the surface roughness and flexural strength compared with the untreated group. The highest flexural strength was observed in specimens treated by bur grinding and then laser, however, it was still significantly lower than intact specimens.