Nabeel M S Kaawash
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Research Interests
Nabeel M S Kaawash has a total of 20 co-authors. Here are the top co-authors by number of shared publications:
- Kashinath Arjun Bogle
Thin film and Devices Laboratory School of Physical Sciences Swami Ramanand Teerth Marathwada University Nanded 431606 India
3 shared publications Hamdan A.S. Al-Shamiri
2 shared publications- Abdulaziz Almalki
Department of Physics, College of Science in Yanbu, Taibah University, Yanbu governorate, Saudi Arabia
1 shared publication Aeshah Salem
1 shared publicationAl-Arique Hakim Q.N.M.
Department of Chemistry, Faculty of Applied Science, Taiz University, Taiz – 6803, Yemen
1 shared publication- Alqadasy Sameerah S.S.
Department of Physics, Dr. Rafiq Zakaria College for Women, Dr. Babasahieb Ambedkar Marathwada University, Aurangabad – 341 004, Maharashtra, India
1 shared publication
Latest Publications
- Open Access
- 6 September 2024
- Published by JACS Directory in Journal of Advanced Chemical Sciences
- Vol. 10 (2) , 803-807
Synthesis of Ag-Doped Lanthanum Nanoparticles using Simple Wet Chemical Process in Alkaline Medium; and Characterization of Optical, Morphological and Structural Properties
The manufacturing of doped semiconductor Ag2O.La2O3 (Ag-La) nanoparticles (NPs) in an alkaline medium at 60–70 °C is described in this paper, utilising a straightforward wet chemical procedure. Numerous tools are used to characterise Ag-La NPs, such as ultraviolet/visible spectroscopy (UV/Vis.), field emission scanning electron microscopy (FE-SEM), Fourier transform infrared spectroscopy (FTIR), and powder X-ray diffractometer (XRD). An X-ray diffraction analysis revealed that the Ag-doped Nps are polycrystalline in nature and crystallise in a hexagonal phase with crystallites oriented in various directions. The morphology of the particles shows layers of aggregation of different sized and shaped nanosheets. Studies on their optical properties, however, have revealed that absorption takes place in the 270–291 nm range and that the transmission value, which ranges from 30 to 64%, is influenced by the temperature during annealing. An increase in annealing temperature results in a corresponding drop in band gap energy, from 4.27 to 4.10 eV.
- 6 September 2024
- Published by JACS Directory in Journal of Advanced Chemical Sciences
- Vol. 10 (2) , 803-807
Open AccessSynthesis of Ag-Doped Lanthanum Nanoparticles using Simple Wet Chemical Process in Alkaline Medium; and Characterization of Optical, Morphological and Structural Properties
The manufacturing of doped semiconductor Ag2O.La2O3 (Ag-La) nanoparticles (NPs) in an alkaline medium at 60–70 °C is described in this paper, utilising a straightforward wet chemical procedure. Numerous tools are used to characterise Ag-La NPs, such as ultraviolet/visible spectroscopy (UV/Vis.), field emission scanning electron microscopy (FE-SEM), Fourier transform infrared spectroscopy (FTIR), and powder X-ray diffractometer (XRD). An X-ray diffraction analysis revealed that the Ag-doped Nps are polycrystalline in nature and crystallise in a hexagonal phase with crystallites oriented in various directions. The morphology of the particles shows layers of aggregation of different sized and shaped nanosheets. Studies on their optical properties, however, have revealed that absorption takes place in the 270–291 nm range and that the transmission value, which ranges from 30 to 64%, is influenced by the temperature during annealing. An increase in annealing temperature results in a corresponding drop in band gap energy, from 4.27 to 4.10 eV.
- 24 May 2024
- Published by IOP Publishing in Physica Scripta
- Vol. 99 (6) , 0659a3
Effect of boron-doping and annealing on the structure, morphological and optical properties of ZnO films prepared by spray pyrolysis method
This study investigates the influence of boron doping from boric acid (H3BO3) on the structural, morphological, and optical properties of ZnO thin films deposited on glass substrates via spray pyrolysis at a deposition temperature of 250 °C. Subsequently, they undergo annealing in air at varying temperatures (200, 300, and 400 °C) for 45 min. The research reveals a significant dependence of all investigated properties on both annealing temperature and boron doping. Both pristine ZnO and boron-doped ZnO (BZO) films exhibit a polycrystalline hexagonal wurtzite structure. At the highest annealing temperature (400 °C), both films demonstrate high optical transmittance exceeding 70%, with crystallite diameters ranging from 25.8 to 28.5 nm for ZnO and 15.96 to 24.80 nm for BZO. Additionally, both films exhibit pronounced absorbance up to 400 nm. Scanning electron microscopy (SEM) analysis confirms a uniformly thick film surface. As the annealing temperature increases, the crystallite size grows, particle morphology evolves, and the overall film thickness increases. Fourier transform infrared (FTIR) spectroscopy validates the successful incorporation of boron atoms into the ZnO lattice structure. No contaminant peaks are observed in the FTIR spectra, indicating film purity. Furthermore, the study finds that BZO films possess a narrower optical band gap compared to pristine ZnO films. The band gap of the as-deposited and annealed BZO films is measured to be 3.04 eV and 2.9 eV, respectively, which is lower than the 3.23 eV band gap observed for the ZnO film. In general, the band gap exhibits a decreasing trend with increasing annealing temperature.
- 24 May 2024
- Published by IOP Publishing in Physica Scripta
- Vol. 99 (6) , 0659a3
Effect of boron-doping and annealing on the structure, morphological and optical properties of ZnO films prepared by spray pyrolysis method
This study investigates the influence of boron doping from boric acid (H3BO3) on the structural, morphological, and optical properties of ZnO thin films deposited on glass substrates via spray pyrolysis at a deposition temperature of 250 °C. Subsequently, they undergo annealing in air at varying temperatures (200, 300, and 400 °C) for 45 min. The research reveals a significant dependence of all investigated properties on both annealing temperature and boron doping. Both pristine ZnO and boron-doped ZnO (BZO) films exhibit a polycrystalline hexagonal wurtzite structure. At the highest annealing temperature (400 °C), both films demonstrate high optical transmittance exceeding 70%, with crystallite diameters ranging from 25.8 to 28.5 nm for ZnO and 15.96 to 24.80 nm for BZO. Additionally, both films exhibit pronounced absorbance up to 400 nm. Scanning electron microscopy (SEM) analysis confirms a uniformly thick film surface. As the annealing temperature increases, the crystallite size grows, particle morphology evolves, and the overall film thickness increases. Fourier transform infrared (FTIR) spectroscopy validates the successful incorporation of boron atoms into the ZnO lattice structure. No contaminant peaks are observed in the FTIR spectra, indicating film purity. Furthermore, the study finds that BZO films possess a narrower optical band gap compared to pristine ZnO films. The band gap of the as-deposited and annealed BZO films is measured to be 3.04 eV and 2.9 eV, respectively, which is lower than the 3.23 eV band gap observed for the ZnO film. In general, the band gap exhibits a decreasing trend with increasing annealing temperature.
- 25 March 2024
- Published by Elsevier in Optical Materials
- Vol. 150
Study the characterization of ZnO and AZO films prepared by spray pyrolysis and the effect of annealing temperature
- 25 March 2024
- Published by Elsevier in Optical Materials
- Vol. 150
Study the characterization of ZnO and AZO films prepared by spray pyrolysis and the effect of annealing temperature
- 25 April 2023
- Published by Elsevier in Materials Today: Proceedings
- Vol. 92, 732-736
Analysis of current-voltage curves of ZnO thin films under dark and optical stimulus
- 25 April 2023
- Published by Elsevier in Materials Today: Proceedings
- Vol. 92, 732-736
Analysis of current-voltage curves of ZnO thin films under dark and optical stimulus