Zheying Wu
Research Subjects
Zheying Wu has a total of 7 co-authors. Here are the top co-authors by number of shared publications:
- Jie Gu
Shanghai Bao Steel Packaging Co., Ltd., Shanghai 200949, China
2 shared publications - Jinyang Chen
School of Environmental and Chemical Engineering, Shanghai University, 99 Shangda Road, Shanghai 200444, China
2 shared publications - Jingying Cui
Chemical Engineering and Technology, Shanghai University, Shanghai 200444, China
1 shared publication - Menghan Hong
Chemical Engineering and Technology, Shanghai University, Shanghai 200444, China
1 shared publication - Mingjie Fan
Chemical Engineering and Technology, Shanghai University, Shanghai 200444, China
1 shared publication - Xiaomin Hong
Chemical Engineering and Technology, Shanghai University, Shanghai 200444, China
1 shared publication
Latest Publications
- Open Access
Corrosion Behavior of 3104 Aluminum Cans When Used as Packaging for Chinese Liquor
Aluminum cans are commonly used for packaging soft drinks and low-alcohol beverages due to their good recyclability. To enhance the economic cycle and expand the packaging of liquors, the feasibility of commercial 3104 aluminum cans for packaging Chinese liquor was studied. The aluminum’s migration into alcoholic solutions was studied using inductively coupled plasma emission spectroscopy (ICP-OES). Electrochemical impedance spectroscopy (EIS) was used to study the corrosion process of epoxy coatings on the aluminum cans. Scanning electron microscopy (SEM), energy dispersive X-ray spectroscopy (EDS), infrared attenuated total reflection (IR-ATR), and X-ray diffraction (XRD) were used to determine the inner coatings and adhering surfaces of the cans and the corrosion process. The results showed that the maximum aluminum migration in Chinese liquor was 4.3572 mg/kg at 60 °C for 30 days. The epoxy coating was corroded enough to decrease the coating impedance and expose the metal substrate after 25 days. Permeation and aging degradation of coatings are the main factors to consider when packaging liquor.
Open AccessCorrosion Behavior of 3104 Aluminum Cans When Used as Packaging for Chinese Liquor
Aluminum cans are commonly used for packaging soft drinks and low-alcohol beverages due to their good recyclability. To enhance the economic cycle and expand the packaging of liquors, the feasibility of commercial 3104 aluminum cans for packaging Chinese liquor was studied. The aluminum’s migration into alcoholic solutions was studied using inductively coupled plasma emission spectroscopy (ICP-OES). Electrochemical impedance spectroscopy (EIS) was used to study the corrosion process of epoxy coatings on the aluminum cans. Scanning electron microscopy (SEM), energy dispersive X-ray spectroscopy (EDS), infrared attenuated total reflection (IR-ATR), and X-ray diffraction (XRD) were used to determine the inner coatings and adhering surfaces of the cans and the corrosion process. The results showed that the maximum aluminum migration in Chinese liquor was 4.3572 mg/kg at 60 °C for 30 days. The epoxy coating was corroded enough to decrease the coating impedance and expose the metal substrate after 25 days. Permeation and aging degradation of coatings are the main factors to consider when packaging liquor.
- Open Access
Migration of TiO2 from PET/TiO2 Composite Films Used for Polymer-Laminated Steel Cans in Acidic Solution
Nano-TiO2 is widely used as a commercial food contact material (FCM), which poses potential risks to food. Therefore, the migration of TiO2 is crucial for the safety of FCM. Since PET/TiO2 composite films are food contact layers used for producing polymer-laminated steel cans and the majority of beverages contained in cans are acidic, it is necessary to study the migration of TiO2 from PET/TiO2 composite films in acidic solutions. The migration of TiO2 in 4% (v/v) acetic acid was studied through the ICP-OES method. The corrosion process that occurred during the migration process was studied using electrochemical impedance spectroscopy (EIS). The morphology of Ti nanoparticles and films was measured by SEM, TEM, and dynamic light scattering (DLS) techniques. The results indicate that, at a temperature of 60 °C, the maximum migration concentration of TiO2 is 0.32 mg/kg. The TiO2 particles released during the migration process are unstable and tend to aggregate in the simulated material, with most of the Ti being present in the form of particles. Therefore, the migration of TiO2 does not follow the Fick law of diffusion but rather conforms to the Weibull model based on the non-Fick law of diffusion.
Open AccessMigration of TiO2 from PET/TiO2 Composite Films Used for Polymer-Laminated Steel Cans in Acidic Solution
Nano-TiO2 is widely used as a commercial food contact material (FCM), which poses potential risks to food. Therefore, the migration of TiO2 is crucial for the safety of FCM. Since PET/TiO2 composite films are food contact layers used for producing polymer-laminated steel cans and the majority of beverages contained in cans are acidic, it is necessary to study the migration of TiO2 from PET/TiO2 composite films in acidic solutions. The migration of TiO2 in 4% (v/v) acetic acid was studied through the ICP-OES method. The corrosion process that occurred during the migration process was studied using electrochemical impedance spectroscopy (EIS). The morphology of Ti nanoparticles and films was measured by SEM, TEM, and dynamic light scattering (DLS) techniques. The results indicate that, at a temperature of 60 °C, the maximum migration concentration of TiO2 is 0.32 mg/kg. The TiO2 particles released during the migration process are unstable and tend to aggregate in the simulated material, with most of the Ti being present in the form of particles. Therefore, the migration of TiO2 does not follow the Fick law of diffusion but rather conforms to the Weibull model based on the non-Fick law of diffusion.