Isabella Mombrini
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Isabella Mombrini has a total of 33 co-authors. Here are the top co-authors by number of shared publications:
- Paul Robert Shearing
University of Oxford
2 shared publications - Rhodri Jervis
Electrochemical Innovation Lab, Department of Chemical Engineering, University College London, London, UK
2 shared publications A. Jnawali
Electrochemical Innovation Laboratory, Department of Chemical Engineering, University College of London, London, UK
1 shared publicationA. Llewellyn
Electrochemical Innovation Laboratory, Department of Chemical Engineering, University College of London, London, UK
1 shared publication- Adam M. Boyce
University College Dublin
1 shared publication - Alice V. Llewellyn
Electrochemical Innovation Lab, Department of Chemical Engineering, University College London, London, UK
1 shared publication
Latest Publications
- Open Access
- 7 April 2026
- Published by Royal Society of Chemistry (RSC) in EES Batteries
- Vol. 2 (3) , 911-923
Understanding energy–power trade-off in the structure of Li-ion battery cathodes by localized operando XRD
Structured Li-ion electrodes improve Li ion mass transport by providing low-tortuosity routes through the electrode. We apply a localized XRD technique (multi-channel collimator) to understand how structuring affects transport through the electrode.
- 7 April 2026
- Published by Royal Society of Chemistry (RSC) in EES Batteries
- Vol. 2 (3) , 911-923
Open AccessUnderstanding energy–power trade-off in the structure of Li-ion battery cathodes by localized operando XRD
Structured Li-ion electrodes improve Li ion mass transport by providing low-tortuosity routes through the electrode. We apply a localized XRD technique (multi-channel collimator) to understand how structuring affects transport through the electrode.
- 17 May 2023
- Published by Springer Nature in Nature
- Vol. 617 (7961) , 507-512
Mapping internal temperatures during high-rate battery applications
Electric vehicles demand high charge and discharge rates creating potentially dangerous temperature rises. Lithium-ion cells are sealed during their manufacture, making internal temperatures challenging to probe1. Tracking current collector expansion using X-ray diffraction (XRD) permits non-destructive internal temperature measurements2; however, cylindrical cells are known to experience complex internal strain3,4. Here, we characterize the state of charge, mechanical strain and temperature within lithium-ion 18650 cells operated at high rates (above 3C) by means of two advanced synchrotron XRD methods: first, as entire cross-sectional temperature maps during open-circuit cooling and second, single-point temperatures during charge–discharge cycling. We observed that a 20-minute discharge on an energy-optimized cell (3.5 Ah) resulted in internal temperatures above 70 °C, whereas a faster 12-minute discharge on a power-optimized cell (1.5 Ah) resulted in substantially lower temperatures (below 50 °C). However, when comparing the two cells under the same electrical current, the peak temperatures were similar, for example, a 6 A discharge resulted in 40 °C peak temperatures for both cell types. We observe that the operando temperature rise is due to heat accumulation, strongly influenced by the charging protocol, for example, constant current and/or constant voltage; mechanisms that worsen with cycling because degradation increases the cell resistance. Design mitigations for temperature-related battery issues should now be explored using this new methodology to provide opportunities for improved thermal management during high-rate electric vehicle applications.
- 17 May 2023
- Published by Springer Nature in Nature
- Vol. 617 (7961) , 507-512
Mapping internal temperatures during high-rate battery applications
Electric vehicles demand high charge and discharge rates creating potentially dangerous temperature rises. Lithium-ion cells are sealed during their manufacture, making internal temperatures challenging to probe1. Tracking current collector expansion using X-ray diffraction (XRD) permits non-destructive internal temperature measurements2; however, cylindrical cells are known to experience complex internal strain3,4. Here, we characterize the state of charge, mechanical strain and temperature within lithium-ion 18650 cells operated at high rates (above 3C) by means of two advanced synchrotron XRD methods: first, as entire cross-sectional temperature maps during open-circuit cooling and second, single-point temperatures during charge–discharge cycling. We observed that a 20-minute discharge on an energy-optimized cell (3.5 Ah) resulted in internal temperatures above 70 °C, whereas a faster 12-minute discharge on a power-optimized cell (1.5 Ah) resulted in substantially lower temperatures (below 50 °C). However, when comparing the two cells under the same electrical current, the peak temperatures were similar, for example, a 6 A discharge resulted in 40 °C peak temperatures for both cell types. We observe that the operando temperature rise is due to heat accumulation, strongly influenced by the charging protocol, for example, constant current and/or constant voltage; mechanisms that worsen with cycling because degradation increases the cell resistance. Design mitigations for temperature-related battery issues should now be explored using this new methodology to provide opportunities for improved thermal management during high-rate electric vehicle applications.
- Open Access
- 4 April 2023
- Published by Royal Society of Chemistry (RSC) in Journal of Materials Chemistry A
- Vol. 11 (17) , 9521-9529
Cellulose nanofiber-reinforced solid polymer electrolytes with high ionic conductivity for lithium batteries
Lithium–metal electrodes are promising for developing next-generation lithium-based batteries with high energy densities. However, their implementation is severely limited by dendritic growth during battery cycling, which eventually short-circuits the battery. Replacing conventional liquid electrolytes with solid polymer electrolytes (SPEs) can suppress dendritic growth. Unfortunately, in SPEs the high stiffness required for suppressing dendrites comes at the expense of efficient lithium-ion transport. Some polymer-based composite electrolytes, however, enable the decoupling of stiffness and ionic conductivity. This study introduces a composite SPE comprised of a relatively soft poly(ethylene oxide-co-epichlorohydrin) (EO-co-EPI) statistical copolymer with high ionic conductivity and cellulose nanofibers (CNFs), a filler with extraordinary stiffness sourced from abundant cellulose. CNF-reinforcement of EO-co-EPI increases the storage modulus up to three orders of magnitude while essentially maintaining the SPE's high ionic conductivity. The composite SPE exhibits good cycling ability and electrochemical stability, demonstrating its utility in lithium metal batteries.
- 4 April 2023
- Published by Royal Society of Chemistry (RSC) in Journal of Materials Chemistry A
- Vol. 11 (17) , 9521-9529
Open AccessCellulose nanofiber-reinforced solid polymer electrolytes with high ionic conductivity for lithium batteries
Lithium–metal electrodes are promising for developing next-generation lithium-based batteries with high energy densities. However, their implementation is severely limited by dendritic growth during battery cycling, which eventually short-circuits the battery. Replacing conventional liquid electrolytes with solid polymer electrolytes (SPEs) can suppress dendritic growth. Unfortunately, in SPEs the high stiffness required for suppressing dendrites comes at the expense of efficient lithium-ion transport. Some polymer-based composite electrolytes, however, enable the decoupling of stiffness and ionic conductivity. This study introduces a composite SPE comprised of a relatively soft poly(ethylene oxide-co-epichlorohydrin) (EO-co-EPI) statistical copolymer with high ionic conductivity and cellulose nanofibers (CNFs), a filler with extraordinary stiffness sourced from abundant cellulose. CNF-reinforcement of EO-co-EPI increases the storage modulus up to three orders of magnitude while essentially maintaining the SPE's high ionic conductivity. The composite SPE exhibits good cycling ability and electrochemical stability, demonstrating its utility in lithium metal batteries.