Latest Publications

  • Open Access

    Femtosecond Laser Bessel Beam Generation via Holographic Beam Shaping for High-Quality Silicon Wafer Dicing

    by Yaofei Ma, Shufeng Sun, Jin Wang, Fengyun Zhang, Tao Wei, Xuecheng Gao, Bingkun Xia, Pingping Wang

    To overcome the limitations of conventional wafer dicing methods, this paper proposes a femtosecond laser cutting technique based on holographic Bessel beam modulation. By loading axicon phase holograms onto a spatial light modulator (SLM), Gaussian beams are flexibly converted into Bessel beams with tunable parameters to improve cutting depth and surface quality. At a laser power of 1.8 W, compared with Gaussian beam cutting (average depth 6.1 μm, cross-sectional roughness 1.122 μm), Bessel beam cutting increases the depth to 21.3 μm (71.4% improvement) and reduces roughness to 0.468 μm (58.3% reduction). Moreover, oxidation and recast layer formation are significantly suppressed, ensuring smooth edges and wafer stability. This holographic SLM-based approach simplifies the optical system while enabling real-time beam regulation, offering a flexible and efficient method for high-quality silicon wafer dicing and broader semiconductor applications.

  • Open Access

    Study on the microstructure and properties of laser-cladded AlCoCrFeNiCu0.5-xNbₓ high-entropy alloy coatings

    by Mingsai Zhang, Shufeng Sun, Jin Wang, Fengyun Zhang, Yadi Wang

    In this study, the high-entropy alloy AlCoCrFeNiCu0.5 − xNbx (x = 0, 0.1, 0.2, 0.3, 0.4, 0.5) is selected as the research subject. Coatings with varying Cu/Nb ratios are fabricated by laser cladding. The phase composition, microstructure, microhardness, tribological behavior, and corrosion resistance are systematically investigated. The results reveal that when x = 0.2, the coating exhibits a dual-phase structure consisting of FCC and Laves phases. A large cellular structure forms and maintains good microstructural continuity. The coating shows a low friction coefficient of 0.327, and no significant spalling is observed on the worn surface. In both 3.5% NaCl and 0.5 M H₂SO₄ solutions, the coating exhibits the most positive corrosion potential, the lowest corrosion current density, and the highest polarization resistance, indicating excellent electrochemical stability.


  • Open Access

    Application of ultrafast laser beam shaping in micro-optical elements

    by Zhihao Qu, Shufeng Sun, Jin Wang, Mingming Jiang, Fengyun Zhang, Xi Wang, Jing Shao, Guanglei Liang, Pingping Wang

    The manufacturing and application of micro-optical elements are constantly evolving toward miniaturization, integration, and intelligence and have important applications in holographic displays, optical imaging, laser processing, information processing, and other fields. Ultrafast lasers, with their ultrashort pulse width, extremely high peak power, high processing resolution, small thermal influence zone, and nondestructive material processing advantages, have become an important processing method for preparing micro-optical elements. However, the laser output from the laser usually has a Gaussian distribution, with limitations in spatial and temporal energy and shape distribution, making it difficult to meet the requirements of processing efficiency and quality, which poses new challenges to ultrafast laser manufacturing technology. Therefore, by shaping the ultrafast laser beam and regulating nonlinear optical effects, the optimization and adjustment of the beam shape can be achieved, thus improving the quality and efficiency of micro-optical element processing. Ultrafast laser beam shaping technology provides a new method for the manufacture of micro-optical elements. This article first introduces the commonly used manufacturing methods for micro-optical elements. Second, from the perspective of the temporal domain, spatial domain, and spatiotemporal domain, the basic principles, methods, and existing problems of ultrafast laser beam shaping are summarized. Then, the application of these shaping technologies in the preparation of micro-optical elements is elaborated. Finally, the challenges and future development prospects of ultrafast laser beam shaping technology are discussed.


  • Non‐damage deep etching of SiC by hybrid laser‐high temperature chemical processing

    by Xi Wang, Bing Han, Martin Ehrhardt, Fengyun Zhang, Jin Wang, Pingping Wang, Peter Pavol Monka, Shufeng Sun

    SiC is considered as preferred material for micro‐electro‐mechanical system in the future. The excellent mechanical property and chemical stability make it difficult to perform deep etching. The hybrid laser‐high temperature chemical etching is investigated to realize non‐damage deep etching of SiC. The influences of defocus, laser pulse interval, laser intensity, and pulse number on etching depth are researched. The optimized laser parameter for SiC non‐damage deep etching is laser intensity of 10 × 10 9 W/cm 2 with a pulse interval of 10 ms. In order to analyze the interaction mechanism, the temperature field and laser‐induced liquid jet in the liquid environment are calculated numerically. It is concluded that the material removal mechanism consists of laser heating vaporization during laser pulse, mechanical effect of laser‐induced liquid jet impact between two adjacent laser pulses and chemical etching in laser‐induced local high‐temperature environment. The chemical reaction between SiC and mixture of HF, and HNO 3 solution produces gases and fluosilicic acid and effectively reduces the roughness of the modified layer making the surface smoother, and also removes the microcracks on the side wall of the etched region.


  • Performance comparison of laser-etched microstructures on K9 glass and PMMA light guide plate

    by Li Liu, Jin Wang, Xi Wang, Feng-Yun Zhang, Ping-Ping Wang, Yun-Long Zhang, Shu-Feng Sun


  • THERMAL CONDUCTIVITY AND THERMAL AGING PERFORMANCE OF Sn WITH 0.7 wt.% Cu and VARIOUS GRAPHENE ADDITIONS

    by Caixia Sun, Fengyun Zhang, Hongxia Zhang, Nianlong Zhang, Shouying Li, Jingjie Dai, Hailong Zhang

    The effect of graphene content (0.08, 0.16 and 0.33[Formula: see text]wt.%) on the thermal conductivity and thermal aging performance of an Sn based composite material with 0.7[Formula: see text]wt.% Cu and various graphene additions was investigated via X-ray diffraction (XRD), scanning electron microscope (SEM) and accelerated thermal aging test. The XRD results showed that the graphene diffraction intensity was weak (approximately 10∘) due to little content and distribution of the graphene on the surface of the composite materials. After thermal aging testing the diffraction intensity on some crystal planes of the composite materials was enhanced, proving that preferential growth occurs on the crystal plane. SEM results showed that before aging testing no whiskers were generated on the surface of the composite materials. After the accelerated thermal aging at 100∘C for 24[Formula: see text]h, whisker growth became apparent in the composite materials. All the whiskers were located in the grains rather than on the grain boundaries of the composite materials. The highest thermal conductivity was obtained at 0.16[Formula: see text]wt.% graphene addition (indicated as 0.16[Formula: see text]wt.% graphene–0.7[Formula: see text]wt.% Cu/Sn). After the accelerated thermal aging at 100∘C for 24[Formula: see text]h, the bamboo-shaped whiskers with a low aspect ratio grew in large quantities on the surface of the 0.16[Formula: see text]wt.% graphene–0.7[Formula: see text]wt.% Cu/Sn composite material, while when the aging was at 100∘C for 366[Formula: see text]h the thermal conductivity decreased from 67[Formula: see text]W[Formula: see text][Formula: see text][Formula: see text][Formula: see text] to 52[Formula: see text]W[Formula: see text][Formula: see text][Formula: see text][Formula: see text]. When the graphene addition was 0.33[Formula: see text]wt.% (indicated as 0.33[Formula: see text]wt.% graphene–0.7[Formula: see text]wt.% Cu/Sn) the thermal conductivity maintains a value above 59[Formula: see text]W[Formula: see text][Formula: see text][Formula: see text][Formula: see text] after the accelerated thermal aging.