Sadettin Sahin
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Sadettin Sahin has a total of 4 co-authors. Here are the top co-authors by number of shared publications:
- Cihangir Tevfik Sezgin
Kastamonu Vocational School, Mechanical and Metal Technology, Kastamonu University, Kastamonu, Turkey
1 shared publication - Fatih Hayat
Karabük Üniversitesi
1 shared publication - Muharrem Pul
Kırıkkale Vocational School, Kırıkkale University
1 shared publication - Şahlı Başkurt
Karabük Üniversitesi
1 shared publication
Latest Publications
- Open Access
- 30 December 2024
- Published by Prensip Publishing in Journal of Advanced Applied Sciences
- Vol. 3 (2) , 85-90
Behaviour of 32 CrMoV12-10 Steel Towards Boronizing Variables
During the shooting in gun barrels; there are many forces that affect each other such as external swelling caused by the explosion, excessive wear caused by the bullet core rubbing inside the barrel, high temperature caused by friction and gunpowder temperature, thermal expansion caused by temperature, chemical corrosion caused by gunpowder gases. It is expected that the barrel steel will show optimum resistance against all these effects. The most harmful of these is the wear force. The barrel, whose inner diameter expands due to wear, becomes unusable after a certain number of shots. In order to increase the effective number of shots, different hardening applications are made to the inner surfaces of the barrels of very different steel qualities. One of the commonly used barrel steels is 32CrMoV12-10 steel and hard chrome plating of the inner surface of the barrel. In this study, the boronizing behavior of 32CrMoV12-10 steel was investigated as an alternative coating technique. The changes in the type, layer thickness and hardness values of boron compounds formed on the surface as a function of temperature and time were investigated. Boriding processes were carried out with a holding time of 2, 4 and 6 hours by setting the boriding temperature to 900oC. Typical columnar structures were observed at depths of 73, 100 and 133 μm in SEM microscope images. XRD (X-Ray Diffraction) analysis revealed that these were FeB, Fe2B, MnB and CrB compounds and that boride depth and hardness increased as the holding time increased. In microhardness tests conducted in this area, hardness values up to 2500 HV were obtained.
- 30 December 2024
- Published by Prensip Publishing in Journal of Advanced Applied Sciences
- Vol. 3 (2) , 85-90
Open AccessBehaviour of 32 CrMoV12-10 Steel Towards Boronizing Variables
During the shooting in gun barrels; there are many forces that affect each other such as external swelling caused by the explosion, excessive wear caused by the bullet core rubbing inside the barrel, high temperature caused by friction and gunpowder temperature, thermal expansion caused by temperature, chemical corrosion caused by gunpowder gases. It is expected that the barrel steel will show optimum resistance against all these effects. The most harmful of these is the wear force. The barrel, whose inner diameter expands due to wear, becomes unusable after a certain number of shots. In order to increase the effective number of shots, different hardening applications are made to the inner surfaces of the barrels of very different steel qualities. One of the commonly used barrel steels is 32CrMoV12-10 steel and hard chrome plating of the inner surface of the barrel. In this study, the boronizing behavior of 32CrMoV12-10 steel was investigated as an alternative coating technique. The changes in the type, layer thickness and hardness values of boron compounds formed on the surface as a function of temperature and time were investigated. Boriding processes were carried out with a holding time of 2, 4 and 6 hours by setting the boriding temperature to 900oC. Typical columnar structures were observed at depths of 73, 100 and 133 μm in SEM microscope images. XRD (X-Ray Diffraction) analysis revealed that these were FeB, Fe2B, MnB and CrB compounds and that boride depth and hardness increased as the holding time increased. In microhardness tests conducted in this area, hardness values up to 2500 HV were obtained.
- 30 December 2024
- Published by Manufacturing Technologies and Applications in İmalat Teknolojileri ve Uygulamaları
- Vol. 5 (3) , 203-213
Influences of Heat Treatment Parameters on Microstructure And Mechanical Behavior of TWIP Steel
In this study, the effects of different heat treatment temperatures and times on the mechanical properties and microstructure of Twinning Induced Plasticity (TWIP) steel were examined. TWIP steel slabs produced by casting were shaped into plates by hot and cold rolling processes, respectively. The heat treatments were carried out at 600, 700, 800, and 900 °C for 20, 60, and 150 min. As a result of the experiments, M3C carbide precipitates were formed instead of twinning in the tempered sheets at 600 °C and 700 °C, and twinning occurred at 800 °C and 900 °C. The microstructure analysis and mechanical test results demonstrate that the carbide precipitates prevent twinning plane formation. The Vickers hardness and tensile test results showed the intense presence of carbides at 600 °C and 700 °C and twinning at 800 °C and 900 °C. As the annealing temperature and time increased, a decrease in hardness and tensile strength was observed. Elongation increased. However, as a result of annealing at 600 °C for 20 minutes, an increase in elongation and tensile strength was observed compared to the untreated sample.
- 30 December 2024
- Published by Manufacturing Technologies and Applications in İmalat Teknolojileri ve Uygulamaları
- Vol. 5 (3) , 203-213
Influences of Heat Treatment Parameters on Microstructure And Mechanical Behavior of TWIP Steel
In this study, the effects of different heat treatment temperatures and times on the mechanical properties and microstructure of Twinning Induced Plasticity (TWIP) steel were examined. TWIP steel slabs produced by casting were shaped into plates by hot and cold rolling processes, respectively. The heat treatments were carried out at 600, 700, 800, and 900 °C for 20, 60, and 150 min. As a result of the experiments, M3C carbide precipitates were formed instead of twinning in the tempered sheets at 600 °C and 700 °C, and twinning occurred at 800 °C and 900 °C. The microstructure analysis and mechanical test results demonstrate that the carbide precipitates prevent twinning plane formation. The Vickers hardness and tensile test results showed the intense presence of carbides at 600 °C and 700 °C and twinning at 800 °C and 900 °C. As the annealing temperature and time increased, a decrease in hardness and tensile strength was observed. Elongation increased. However, as a result of annealing at 600 °C for 20 minutes, an increase in elongation and tensile strength was observed compared to the untreated sample.
- 30 October 2021
- Published by Bandirma Onyedi Eylul University in Mühendislik Bilimleri ve Araştırmaları Dergisi
- Vol. 3 (2) , 152-160
Vortex Yöntemiyle Üretilen FeB takviyeli AA1050 Kompozitlerde FeB Miktarının Mekanik Özelliklere Etkisi
Bu çalışmada %99,5 ticari saflıktaki alüminyum malzeme içine vortex yöntemiyle %2, %4 ve %8 oranında FeB (ferrobor) takviye edilerek kompozit numuneler üretilmiştir. Daha sonra üretilen kompozit numunelere, mikroyapının sıkıştırılması amacıyla sıcak presleme işlemi uygulanmıştır. Mikroyapı analizleri için SEM görüntüleri çekilmiş ve bazı mekanik özellikleri belirlemek üzere sertlik ölçümleri, çekme testleri ve abrasif aşınma deneyleri gerçekleştirilmiştir. SEM görüntülerinden FeB takviye miktarının artmasıyla kompozit yapıdaki topaklanma gözenek miktarının arttığı anlaşılmıştır. Kompozit yapı içindeki FeB oranını artmasıyla sertlik, çekme dayanımı ve abrasif aşınma dayanımı değerleri önce artmış daha sonra azalmıştır. Her üç mekanik deneyde de kompozit yapı benzer davranış sergilemiştir. Bu tür kompozit yapılarda FeB takviye oranın belli bir orana kadar mekanik dayanımı arttırdığı ancak daha yüksek oranlara çıkıldığında ise mekanik dayanımı azaltıcı etki yaptığı sonucuna varılmıştır.
- 30 October 2021
- Published by Bandirma Onyedi Eylul University in Mühendislik Bilimleri ve Araştırmaları Dergisi
- Vol. 3 (2) , 152-160
Vortex Yöntemiyle Üretilen FeB takviyeli AA1050 Kompozitlerde FeB Miktarının Mekanik Özelliklere Etkisi
Bu çalışmada %99,5 ticari saflıktaki alüminyum malzeme içine vortex yöntemiyle %2, %4 ve %8 oranında FeB (ferrobor) takviye edilerek kompozit numuneler üretilmiştir. Daha sonra üretilen kompozit numunelere, mikroyapının sıkıştırılması amacıyla sıcak presleme işlemi uygulanmıştır. Mikroyapı analizleri için SEM görüntüleri çekilmiş ve bazı mekanik özellikleri belirlemek üzere sertlik ölçümleri, çekme testleri ve abrasif aşınma deneyleri gerçekleştirilmiştir. SEM görüntülerinden FeB takviye miktarının artmasıyla kompozit yapıdaki topaklanma gözenek miktarının arttığı anlaşılmıştır. Kompozit yapı içindeki FeB oranını artmasıyla sertlik, çekme dayanımı ve abrasif aşınma dayanımı değerleri önce artmış daha sonra azalmıştır. Her üç mekanik deneyde de kompozit yapı benzer davranış sergilemiştir. Bu tür kompozit yapılarda FeB takviye oranın belli bir orana kadar mekanik dayanımı arttırdığı ancak daha yüksek oranlara çıkıldığında ise mekanik dayanımı azaltıcı etki yaptığı sonucuna varılmıştır.