Uğur Şen
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Uğur Şen has a total of 22 co-authors. Here are the top co-authors by number of shared publications:
- Şaduman Şen
Sakarya Üniversitesi
6 shared publications - Bülent Kılınç
Sakarya Uygulamali Bilimler Universitesi
3 shared publications Ebru Akcan
2 shared publications- Engin Kocaman
Department of Aerospace Engineering, Faculty of Engineering, Zonguldak Bülent Ecevit University, Zonguldak, Turkey
2 shared publications - Uğursoy Olgun
Department of Chemistry, Faculty of Arts and Sciences, Sakarya University, Sakarya, Turkey
2 shared publications A. Sukran Demirkıran
1 shared publication
Latest Publications
- Open Access
- 27 March 2026
- Published by Afyon Kocatepe Universitesi Fen Ve Muhendislik Bilimleri Dergisi in Afyon Kocatepe University Journal of Sciences and Engineering
- Vol. 26 (2) , 421-430
Investigation of The Effect of W Addition to FeB Hard Surface Alloy
In this study, the effect of W addition to Fe-B based hard surfacing filler alloy was investigated. For this purpose, electric arc electrode was produced by adding 5% and 10% W to Fe17B3 hard surfacing filler compound and hard surfacing alloy welding was applied on AISI 1010 steel substrate. It was observed that hard boride phases were formed in situ in the microstructure formed after the welding process. As a result of XRD analysis, α-Fe and Fe2B phases were detected in Fe-B based coating. It was determined that FeWB phase was also present together with α-Fe and Fe2B phase in Fe-W-B based coatings. As a result of hardness measurements, micro hardness of Fe-B based composition was determined as 303-341 HV while surface hardness was 28 HRC. When 5% and 10% W element was added to the coating compound, hardness values increased and micro hardness values of 470-699 HV and 642-756 HV were reached, respectively. SEM images showed that the wear microstructures were adhesive, abrasive, fatigue and oxidative in character. The friction coefficient values obtained from the wear tests of the coatings were determined to be between 0.55-0.8. Wear rates were measured between 0.8x10-5 - 1.15x10-5 mm3/m.
- 27 March 2026
- Published by Afyon Kocatepe Universitesi Fen Ve Muhendislik Bilimleri Dergisi in Afyon Kocatepe University Journal of Sciences and Engineering
- Vol. 26 (2) , 421-430
Open AccessInvestigation of The Effect of W Addition to FeB Hard Surface Alloy
In this study, the effect of W addition to Fe-B based hard surfacing filler alloy was investigated. For this purpose, electric arc electrode was produced by adding 5% and 10% W to Fe17B3 hard surfacing filler compound and hard surfacing alloy welding was applied on AISI 1010 steel substrate. It was observed that hard boride phases were formed in situ in the microstructure formed after the welding process. As a result of XRD analysis, α-Fe and Fe2B phases were detected in Fe-B based coating. It was determined that FeWB phase was also present together with α-Fe and Fe2B phase in Fe-W-B based coatings. As a result of hardness measurements, micro hardness of Fe-B based composition was determined as 303-341 HV while surface hardness was 28 HRC. When 5% and 10% W element was added to the coating compound, hardness values increased and micro hardness values of 470-699 HV and 642-756 HV were reached, respectively. SEM images showed that the wear microstructures were adhesive, abrasive, fatigue and oxidative in character. The friction coefficient values obtained from the wear tests of the coatings were determined to be between 0.55-0.8. Wear rates were measured between 0.8x10-5 - 1.15x10-5 mm3/m.
- Open Access
- 16 August 2024
- Published by MDPI AG in Biomimetics
- Vol. 9 (8) , 498
Examination of Various Abutment Designs Behavior Depending on Load Using Finite Element Analysis
Studies on dental implant abutments’ geometric design and material selection offer significant innovations and results. These studies aim to improve the abutments’ functionality and aesthetic performance, minimize microcavities’ formation, and ensure implant-supported prostheses’ longevity. For example, CAD-CAM fabricated custom abutments have been found to produce a better marginal fit and fewer microgaps than standard abutments. In an in vitro study, transepithelial abutments offered lower microgap values than titanium-based abutments and provided a better fit at the implant–abutment interface. It is known that studies to improve mechanical and biological performance with Polyether Ether Ketone (PEEK) material have been addressed. New materials such as PEEK and zirconia have offered significant advantages in biocompatibility and aesthetics. Along with those studies, different abutment designs are also important. Abutment geometry is optimized to improve stress distribution and minimize peri-implant bone loss. In implant and abutment connections with different angles, mechanical life performances may vary depending on static and dynamic load. These studies emphasize the importance of material research on different types of connections to improve dental implants’ durability, homogeneous load distribution, and reliability. The abutment parts used in implant treatment are insufficient to distribute the load homogeneously against chewing pressure due to their materials and geometry. Non-uniform load distribution damages the abutment and the prosthetic crown, accelerating the wear process. This study aimed to create different abutment designs to improve dental implants’ biomechanical performance and longevity. This study aimed to increase the mechanical durability of the implant–abutment connection by reducing stress concentrations in response to masticatory compression on the abutment in different directions and forces and to guarantee the long-term success of the implant system by providing a more homogeneous stress distribution. It aimed to apply different forces in the axial direction to these models in a simulation environment and to calculate and compare the deformation and stress load distribution. As a method, three-dimensional models of the parts used in implant treatments and forming the implant system were designed. Different abutment designs were created with these models. Taking the current material values used in implant treatments as a reference, finite element analysis (FEA) was performed by applying different axial loads to each implant system model in the ANSYS software (version 24.1). Comparative analysis graphs were prepared and interpreted for the stress values obtained after the applied load. This study evaluated the mechanical performance of different abutment models (A, B, C, D, and E) under a 100 N load using the Kruskal–Wallis test. The Kruskal–Wallis test showed significant differences between the groups (p < 0.001). The greatest difference was observed between models E and A (q′ = 6.215), with a significant difference also found between models C and A (q′ = 3.219, p < 0.005). Regarding stress values, the highest stress on the abutment was observed in Model B (97.4 MPa), while the lowest stress was observed in Model E (9.6 MPa). The crown exhibited the highest stress in Model B (22.7 MPa) and the lowest in Model E (17.3 MPa). The implant stress was highest in Model C (14.8 MPa) and lowest in Model B (11.3 MPa). The stress values for the cortical bone and cancellous bone were quite similar across the models, showing no significant differences. These findings indicate that the abutment design and material selection significantly impact mechanical performance. Among the implant systems created with five different abutment models, in which the existing abutment geometry was also compared, homogeneous and axial distribution of the load on the abutment was achieved, especially with viscoelastic and surface area increased abutment designs. Clinically, the inadequacy and limited mounting surface or geometry of the abutments used in today’s implant treatment applications have led to different design searches. It was concluded that the designs in this study, which are considered alternatives to existing abutment models, contribute positively to the mechanical life of the abutment material, considering the von Mises stresses and directions. This study brings a new perspective to today’s practices and offers an alternative to treatment practices.
- 16 August 2024
- Published by MDPI AG in Biomimetics
- Vol. 9 (8) , 498
Open AccessExamination of Various Abutment Designs Behavior Depending on Load Using Finite Element Analysis
Studies on dental implant abutments’ geometric design and material selection offer significant innovations and results. These studies aim to improve the abutments’ functionality and aesthetic performance, minimize microcavities’ formation, and ensure implant-supported prostheses’ longevity. For example, CAD-CAM fabricated custom abutments have been found to produce a better marginal fit and fewer microgaps than standard abutments. In an in vitro study, transepithelial abutments offered lower microgap values than titanium-based abutments and provided a better fit at the implant–abutment interface. It is known that studies to improve mechanical and biological performance with Polyether Ether Ketone (PEEK) material have been addressed. New materials such as PEEK and zirconia have offered significant advantages in biocompatibility and aesthetics. Along with those studies, different abutment designs are also important. Abutment geometry is optimized to improve stress distribution and minimize peri-implant bone loss. In implant and abutment connections with different angles, mechanical life performances may vary depending on static and dynamic load. These studies emphasize the importance of material research on different types of connections to improve dental implants’ durability, homogeneous load distribution, and reliability. The abutment parts used in implant treatment are insufficient to distribute the load homogeneously against chewing pressure due to their materials and geometry. Non-uniform load distribution damages the abutment and the prosthetic crown, accelerating the wear process. This study aimed to create different abutment designs to improve dental implants’ biomechanical performance and longevity. This study aimed to increase the mechanical durability of the implant–abutment connection by reducing stress concentrations in response to masticatory compression on the abutment in different directions and forces and to guarantee the long-term success of the implant system by providing a more homogeneous stress distribution. It aimed to apply different forces in the axial direction to these models in a simulation environment and to calculate and compare the deformation and stress load distribution. As a method, three-dimensional models of the parts used in implant treatments and forming the implant system were designed. Different abutment designs were created with these models. Taking the current material values used in implant treatments as a reference, finite element analysis (FEA) was performed by applying different axial loads to each implant system model in the ANSYS software (version 24.1). Comparative analysis graphs were prepared and interpreted for the stress values obtained after the applied load. This study evaluated the mechanical performance of different abutment models (A, B, C, D, and E) under a 100 N load using the Kruskal–Wallis test. The Kruskal–Wallis test showed significant differences between the groups (p < 0.001). The greatest difference was observed between models E and A (q′ = 6.215), with a significant difference also found between models C and A (q′ = 3.219, p < 0.005). Regarding stress values, the highest stress on the abutment was observed in Model B (97.4 MPa), while the lowest stress was observed in Model E (9.6 MPa). The crown exhibited the highest stress in Model B (22.7 MPa) and the lowest in Model E (17.3 MPa). The implant stress was highest in Model C (14.8 MPa) and lowest in Model B (11.3 MPa). The stress values for the cortical bone and cancellous bone were quite similar across the models, showing no significant differences. These findings indicate that the abutment design and material selection significantly impact mechanical performance. Among the implant systems created with five different abutment models, in which the existing abutment geometry was also compared, homogeneous and axial distribution of the load on the abutment was achieved, especially with viscoelastic and surface area increased abutment designs. Clinically, the inadequacy and limited mounting surface or geometry of the abutments used in today’s implant treatment applications have led to different design searches. It was concluded that the designs in this study, which are considered alternatives to existing abutment models, contribute positively to the mechanical life of the abutment material, considering the von Mises stresses and directions. This study brings a new perspective to today’s practices and offers an alternative to treatment practices.
- Open Access
- 1 January 2022
- Published by National Library of Serbia in Journal of Mining and Metallurgy, Section B: Metallurgy
- Vol. 58 (1) , 29-41
Effect of titanium content on the microstructure and wear behavior of Fe(13-x)TixB7 (x=0-5) hardfacing alloy
In this study, the effects of titanium addition on microstructure, hardness, and wear rate of Fe(13-x)TixB7 (x = 0, 1, 2, 3 and 5) based hard surface alloy layers formed by gas tungsten arc (GTA) welding method were investigated. As a result of the microstructure studies and phase analysis, it was determined that the structures of the coating layers consisted of ?-Fe, ?Fe+Fe2B eutectic, ?-Fe+Fe2Ti eutectic and hard TiB2 phases. In the hard surface alloy layer, as the amount of titanium was increased, the TiB2 phase density formed in the system increased and it was observed that rod-like and long sharpedged phases formed from the equiaxed structure. As a result of wear tests performed at different loads, it was determined that the addition of titanium reduces the wear rates in the coating layers. In addition, scanning electron microscopy (SEM) images of the worn surfaces showed that the wear mechanisms were adhesive and oxidative.
- 1 January 2022
- Published by National Library of Serbia in Journal of Mining and Metallurgy, Section B: Metallurgy
- Vol. 58 (1) , 29-41
Open AccessEffect of titanium content on the microstructure and wear behavior of Fe(13-x)TixB7 (x=0-5) hardfacing alloy
In this study, the effects of titanium addition on microstructure, hardness, and wear rate of Fe(13-x)TixB7 (x = 0, 1, 2, 3 and 5) based hard surface alloy layers formed by gas tungsten arc (GTA) welding method were investigated. As a result of the microstructure studies and phase analysis, it was determined that the structures of the coating layers consisted of ?-Fe, ?Fe+Fe2B eutectic, ?-Fe+Fe2Ti eutectic and hard TiB2 phases. In the hard surface alloy layer, as the amount of titanium was increased, the TiB2 phase density formed in the system increased and it was observed that rod-like and long sharpedged phases formed from the equiaxed structure. As a result of wear tests performed at different loads, it was determined that the addition of titanium reduces the wear rates in the coating layers. In addition, scanning electron microscopy (SEM) images of the worn surfaces showed that the wear mechanisms were adhesive and oxidative.
- 1 December 2020
- Published by Journal of the Faculty of Engineering and Architecture of Gazi University in Gazi Üniversitesi Mühendislik-Mimarlık Fakültesi Dergisi
- Vol. 36 (1) , 177-190
Krom içeriğinin Fe(18-x)CrxB2 (X=3,4,5) sert dolgu elektrotunda mikroyapı, aşınma ve korozyon davranışı üzerindeki etkisi
Bu çalışmada, Fe(18-X)CrXB2 (X=3,4,5) bileşimine sahip örtülü elektrotlar üretilmiş ve AISI 1010 çeliği üzerine elektrik ark kaynak yöntemi kullanılarak kaplama işlemi gerçekleştirilmiştir. Nihai mikroyapılarda in-situ olarak oluşan ötektik borür fazlarının varlığı gözlemlenmiştir. Bununla birlikte, ötektik altı faz dağılımı gösteren bileşimlerde, başlıca α(Fe-Cr), tetragonal (Fe,Cr)2B, ortorombik (Fe,Cr)2B ve eser miktarda (Fe,Cr)3(C,B) fazlarının varlığı tespit edilmiştir. Alümina bilyeye karşı gerçekleştirilen ileri-geri aşınma testinde, kaplama tabakalarının sürtünme katsayısı değerleri artan yük ile birlikte azaldığı ve 0,844-0,65 arasında değiştiği tespit edilmiştir. Bununla birlikte, sürtünme katsayısının değişimi krom oranından bağımsız olarak hareket ettiği gözlemlenmiştir. Aşınma oranının ise artan krom miktarı ile azaldığı buna karşın artan yük ile arttığı gözlemlenmiştir. Aşınma oranının, en düşük değeri 3N yükte Fe13Cr5B2 bileşimine sahip elektrot için 2,32x10-5 (mm3/m); en yüksek değeri ise 9N yükte Fe15Cr3B2 bileşimine sahip elektrot için 8,16x10-5 (mm3/m) olduğu tespit edilmiştir. Fe(18-X)CrXB2 (X=3,4,5) bileşimine sahip elektrotlar ile kaplanmış yüzey alaşım tabakalarına potansiyodinamik polorizasyon testi uygulanmıştır. Potansiyodinamik polorizasyon testine göre korozyon direncinin artan krom miktarı ile arttığı görülmüştür. Korozyon testine göre, Ikor değerinin artan krom miktarına göre azalarak sırasıyla 1,7x10-4 µA/cm2 ve 6,5x10-5 µA/cm2 ve 3,4 x10-5 µA/cm2 olarak ölçülmüştür. Ekor değerinin ise artan krom miktarı ile arttığı ve sırasıyla -0,119 mV, -0,179 mV ve -0,239 mV değerine ulaştığı tespit edilmiştir.
- 1 December 2020
- Published by Journal of the Faculty of Engineering and Architecture of Gazi University in Gazi Üniversitesi Mühendislik-Mimarlık Fakültesi Dergisi
- Vol. 36 (1) , 177-190
Krom içeriğinin Fe(18-x)CrxB2 (X=3,4,5) sert dolgu elektrotunda mikroyapı, aşınma ve korozyon davranışı üzerindeki etkisi
Bu çalışmada, Fe(18-X)CrXB2 (X=3,4,5) bileşimine sahip örtülü elektrotlar üretilmiş ve AISI 1010 çeliği üzerine elektrik ark kaynak yöntemi kullanılarak kaplama işlemi gerçekleştirilmiştir. Nihai mikroyapılarda in-situ olarak oluşan ötektik borür fazlarının varlığı gözlemlenmiştir. Bununla birlikte, ötektik altı faz dağılımı gösteren bileşimlerde, başlıca α(Fe-Cr), tetragonal (Fe,Cr)2B, ortorombik (Fe,Cr)2B ve eser miktarda (Fe,Cr)3(C,B) fazlarının varlığı tespit edilmiştir. Alümina bilyeye karşı gerçekleştirilen ileri-geri aşınma testinde, kaplama tabakalarının sürtünme katsayısı değerleri artan yük ile birlikte azaldığı ve 0,844-0,65 arasında değiştiği tespit edilmiştir. Bununla birlikte, sürtünme katsayısının değişimi krom oranından bağımsız olarak hareket ettiği gözlemlenmiştir. Aşınma oranının ise artan krom miktarı ile azaldığı buna karşın artan yük ile arttığı gözlemlenmiştir. Aşınma oranının, en düşük değeri 3N yükte Fe13Cr5B2 bileşimine sahip elektrot için 2,32x10-5 (mm3/m); en yüksek değeri ise 9N yükte Fe15Cr3B2 bileşimine sahip elektrot için 8,16x10-5 (mm3/m) olduğu tespit edilmiştir. Fe(18-X)CrXB2 (X=3,4,5) bileşimine sahip elektrotlar ile kaplanmış yüzey alaşım tabakalarına potansiyodinamik polorizasyon testi uygulanmıştır. Potansiyodinamik polorizasyon testine göre korozyon direncinin artan krom miktarı ile arttığı görülmüştür. Korozyon testine göre, Ikor değerinin artan krom miktarına göre azalarak sırasıyla 1,7x10-4 µA/cm2 ve 6,5x10-5 µA/cm2 ve 3,4 x10-5 µA/cm2 olarak ölçülmüştür. Ekor değerinin ise artan krom miktarı ile arttığı ve sırasıyla -0,119 mV, -0,179 mV ve -0,239 mV değerine ulaştığı tespit edilmiştir.
- 1 April 2017
- Published by Sakarya University Journal of Science in Sakarya University Journal of Science
- Vol. 21 (2) , 1
Nano dolgulu polimer esaslı hidrofobik kaplamanın yüzey özelliklerinin incelenmesi
Tr en Bu çalışmada ETİAL 171 numaralı alüminyum alaşımlı yüzeylere Trimethoxymethylsilane (MTMS), TetraethylorthoSilicate (TEOS), asetik asit ve saf suyun mol oranları sırasıyla 1:0,04:0,34:1,59 olacak şekilde sol-gel yöntemi kullanılarak kaplanmıştır. Kaplamalar titanyumdioksit (TiO2) nano toz katkısı kullanılarak üretilmiştir. Üretilen kaplamaların yüzey analizleri optik mikroskop, ıslatma açısı, kalınlık ölçümü cihazları kullanılarak ve cross-cut test kiti ile yapışma adezyonu belirlenmiştir. Islatma açısı 145,5° olan hidrofobik özelliklere sahip kaplama üretilmiştir. In this study ETIAL 171 to aluminum alloy surfaces were coated using the sol-gel process the molar ratio of Trimethoxymethylsilane (MTMS), TetraethylorthoSilicate (TEOS), acetic acid and pure water 1: 0.04: 0.34: 1.59. Coatings are manufactured using nano-additive powders titanium dioxide (TiO2). Optical microscope, contact angle, thickness measurement, cross cut test kit devices were used for tests. Coatings produced with hydrophobic properties.
- 1 April 2017
- Published by Sakarya University Journal of Science in Sakarya University Journal of Science
- Vol. 21 (2) , 1
Nano dolgulu polimer esaslı hidrofobik kaplamanın yüzey özelliklerinin incelenmesi
Tr en Bu çalışmada ETİAL 171 numaralı alüminyum alaşımlı yüzeylere Trimethoxymethylsilane (MTMS), TetraethylorthoSilicate (TEOS), asetik asit ve saf suyun mol oranları sırasıyla 1:0,04:0,34:1,59 olacak şekilde sol-gel yöntemi kullanılarak kaplanmıştır. Kaplamalar titanyumdioksit (TiO2) nano toz katkısı kullanılarak üretilmiştir. Üretilen kaplamaların yüzey analizleri optik mikroskop, ıslatma açısı, kalınlık ölçümü cihazları kullanılarak ve cross-cut test kiti ile yapışma adezyonu belirlenmiştir. Islatma açısı 145,5° olan hidrofobik özelliklere sahip kaplama üretilmiştir. In this study ETIAL 171 to aluminum alloy surfaces were coated using the sol-gel process the molar ratio of Trimethoxymethylsilane (MTMS), TetraethylorthoSilicate (TEOS), acetic acid and pure water 1: 0.04: 0.34: 1.59. Coatings are manufactured using nano-additive powders titanium dioxide (TiO2). Optical microscope, contact angle, thickness measurement, cross cut test kit devices were used for tests. Coatings produced with hydrophobic properties.
- Open Access
- 2 May 2016
- Published by Sakarya University Journal of Science in Sakarya University Journal of Science
- Vol. 21 (1)
NANO DOLGULU POLİMER ESASLI HİDROFOBİK KAPLAMANIN YÜZEY ÖZELLİKLERİNİN İNCELENMESİ
- 2 May 2016
- Published by Sakarya University Journal of Science in Sakarya University Journal of Science
- Vol. 21 (1)
Open AccessNANO DOLGULU POLİMER ESASLI HİDROFOBİK KAPLAMANIN YÜZEY ÖZELLİKLERİNİN İNCELENMESİ
- 4 April 2014
- Published by Springer Nature
- p. 143-149
Microstructural Examinations of Fe-W-B Base Hard-Faced Steel
- 4 April 2014
- Published by Springer Nature
- p. 143-149
Microstructural Examinations of Fe-W-B Base Hard-Faced Steel
- 1 October 2013
- Published by Elsevier in Surface and Coatings Technology
- Vol. 232, 703-709
The effect of bond coat composition on oxidation behavior of basalt base glass and glass–ceramics
- 1 October 2013
- Published by Elsevier in Surface and Coatings Technology
- Vol. 232, 703-709
The effect of bond coat composition on oxidation behavior of basalt base glass and glass–ceramics
- 1 July 2004
- Published by Elsevier in Materials Chemistry and Physics
- Vol. 86 (1) , 189-194
Kinetics of niobium carbide coating produced on AISI 1040 steel by thermo-reactive deposition technique
- 1 July 2004
- Published by Elsevier in Materials Chemistry and Physics
- Vol. 86 (1) , 189-194
Kinetics of niobium carbide coating produced on AISI 1040 steel by thermo-reactive deposition technique