Sida Ma
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Sida Ma has a total of 14 co-authors. Here are the top co-authors by number of shared publications:
- Hui Chen
School of Material Science and Engineering, Southwest Jiaotong University, Chengdu, China
2 shared publications - Pu Xie
Department of Aeronutics and Astronautics, Stanford University, Stanford, CA 94305, USA
2 shared publications - Zhenlin Zhang
Southwest Jiaotong University
2 shared publications - Aiping Wu
Department of Mechanical Engineering, Tsinghua University, Beijing 100084, China
1 shared publication - Geng Zhi
Second Institute of China Aerospace Science and Technology Corporation, Beijing Institute of Radio Measurement, Beijing 100854, China
1 shared publication - Guo Li
School of Materials Science and Engineering, SouthWest Jiaotong University, Chengdu 610031, China
1 shared publication
Latest Publications
- Open Access
Study on the Forming Process and Properties of AlSi60 Alloy by Selective Laser Melting
Hypereutectic Al-Si alloys, which have a silicon content ranging from 12% to 70%, are a new generation of casing materials for chip packaging. They have broad applications in aerospace, weaponry, and civilian communications. Selective Laser Melting (SLM) offers significant advantages in achieving near-net shaping of complex casings. This paper presents a study on the formation defects, microstructure, and room temperature tensile properties of AlSi60 alloy prepared by SLM. The results indicate that the primary forming defects in the SLM AlSi60 alloy are balling, lack of fusion, and porosity. These defects are mainly influenced by the volumetric energy density. Samples of good quality can be produced within the range of 150 J/mm3 to 250 J/mm3. However, the same volumetric energy density can result in differences in sample quality due to various combinations of process parameters. Therefore, it has been determined that a well-formed AlSi60 alloy can be obtained within a laser power range of 300 W–350 W, scanning speed of 400 mm/s–800 mm/s, and hatch spacing of 0.09 mm–0.13 mm, with a density close to 98%. The microstructure of the SLM AlSi60 alloy consists of primary Si phases with irregular shapes and sharp edges measuring 5–10 μm, eutectic Si particles of 0.5 μm, and α-Al phases, with eutectic Si dispersed within the α-Al. The SLM AlSi60 alloy exhibits fine and evenly distributed primary Si phases with an average hardness of 203 HV. No significant anisotropy in hardness values was observed in the X and Y directions. The tensile strength of the alloy reached an average of 219 MPa, with an average elongation of 2.99%. During the tensile process, cracks initiated by the primary Si phases rapidly expanded, exhibiting minor ductile fracture characteristics in the Al phases. Due to the high volume fraction of Si phases, the tensile test was dominated by brittle fracture. The tensile curve only exhibited the elastic stage.
Open AccessStudy on the Forming Process and Properties of AlSi60 Alloy by Selective Laser Melting
Hypereutectic Al-Si alloys, which have a silicon content ranging from 12% to 70%, are a new generation of casing materials for chip packaging. They have broad applications in aerospace, weaponry, and civilian communications. Selective Laser Melting (SLM) offers significant advantages in achieving near-net shaping of complex casings. This paper presents a study on the formation defects, microstructure, and room temperature tensile properties of AlSi60 alloy prepared by SLM. The results indicate that the primary forming defects in the SLM AlSi60 alloy are balling, lack of fusion, and porosity. These defects are mainly influenced by the volumetric energy density. Samples of good quality can be produced within the range of 150 J/mm3 to 250 J/mm3. However, the same volumetric energy density can result in differences in sample quality due to various combinations of process parameters. Therefore, it has been determined that a well-formed AlSi60 alloy can be obtained within a laser power range of 300 W–350 W, scanning speed of 400 mm/s–800 mm/s, and hatch spacing of 0.09 mm–0.13 mm, with a density close to 98%. The microstructure of the SLM AlSi60 alloy consists of primary Si phases with irregular shapes and sharp edges measuring 5–10 μm, eutectic Si particles of 0.5 μm, and α-Al phases, with eutectic Si dispersed within the α-Al. The SLM AlSi60 alloy exhibits fine and evenly distributed primary Si phases with an average hardness of 203 HV. No significant anisotropy in hardness values was observed in the X and Y directions. The tensile strength of the alloy reached an average of 219 MPa, with an average elongation of 2.99%. During the tensile process, cracks initiated by the primary Si phases rapidly expanded, exhibiting minor ductile fracture characteristics in the Al phases. Due to the high volume fraction of Si phases, the tensile test was dominated by brittle fracture. The tensile curve only exhibited the elastic stage.
- Open Access
Key Parameters and Optimal Design of a Split Induction Coil for T-Shaped Pipe Brazing
The heat exchanger made up of several T-shaped joints is a critical component in energy equipment. A split induction coil was designed for T-shaped aluminum pipe brazing, and the Taguchi method was combined with multi-physical simulation to solve the multi-factor optimization of the split coil. The results showed that the multi-physical simulation model had high precision. The melting of filler metal was almost consistent with the spatial distribution of the temperature field, and the average simulation error was approximately 5.753 °C. The optimal coil parameters were obtained with a turn number of 3.5, a turn space of 7 mm, a heating distance of 15.6 mm, a coil diameter of 8 mm, and a coil length of 9 mm. Three well-formed T-shaped joints could be obtained at one time via the optimal split coil. During the induction brazing, the skin effects and the proximity effects induced a high magnetic field intensity around the joint, which had a significant relationship with the coil length and coil diameter. The high magnetic field intensity promoted a high eddy current density in this place, and as a result, the high Joule heat could be generated around the joint. In addition, the significant decrease in the heating rate at high temperatures promoted the homogenization of the temperature and the melting and filling of the filler metal as well as avoided local overheating.
Open AccessKey Parameters and Optimal Design of a Split Induction Coil for T-Shaped Pipe Brazing
The heat exchanger made up of several T-shaped joints is a critical component in energy equipment. A split induction coil was designed for T-shaped aluminum pipe brazing, and the Taguchi method was combined with multi-physical simulation to solve the multi-factor optimization of the split coil. The results showed that the multi-physical simulation model had high precision. The melting of filler metal was almost consistent with the spatial distribution of the temperature field, and the average simulation error was approximately 5.753 °C. The optimal coil parameters were obtained with a turn number of 3.5, a turn space of 7 mm, a heating distance of 15.6 mm, a coil diameter of 8 mm, and a coil length of 9 mm. Three well-formed T-shaped joints could be obtained at one time via the optimal split coil. During the induction brazing, the skin effects and the proximity effects induced a high magnetic field intensity around the joint, which had a significant relationship with the coil length and coil diameter. The high magnetic field intensity promoted a high eddy current density in this place, and as a result, the high Joule heat could be generated around the joint. In addition, the significant decrease in the heating rate at high temperatures promoted the homogenization of the temperature and the melting and filling of the filler metal as well as avoided local overheating.