Hojun Moon
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Hojun Moon has a total of 40 co-authors. Here are the top co-authors by number of shared publications:
- Misook Kang
Department of Chemistry, College of Natural Sciences, Yeungnam University, 280 Daehak-ro, Gyeongsan, Gyeongbuk 38541, Republic of Korea
5 shared publications - Jeeyoung Yoo
School of Energy Engineering Kyungpook National University Daegu Republic of Korea
2 shared publications - Jemin Lee
School of Energy Engineering Kyungpook National University Daegu Republic of Korea
2 shared publications Buseong Kim
Department of Chemistry College of Natural Sciences Yeungnam University Gyeongsan Gyeongbuk Republic of Korea
1 shared publicationByung Hyun Park
1 shared publication- Chunli Liu
Department of Physics and Oxide Research Center, Hankuk University of Foreign Studies, Yongin 17035, Republic of Korea
1 shared publication
Latest Publications
- Open Access
- 29 September 2026
- Published by Wiley in Advanced Functional Materials
- Vol. 36 (90) , e78762
Engineering a Fluorinated AlPO 4 Interface: Toward High Initial Coulombic Efficiency and Stable Oxygen Redox in Li‐Rich Layered Oxide Cathodes
Li‐rich layered oxides (LLOs) are promising high‐energy‐density cathode candidates; however, their practical application is hindered by severe voltage decay originating from irreversible layered‐to‐spinel phase transformation and interfacial degradation under high‐voltage operation (>4.5 V). Herein, we report a fluorinated AlPO 4 (AlPO 4 ‐F) surface architecture for LLO cathodes designed to simultaneously stabilize the oxygen framework and modify the interfacial charge environment. Electrostatic force microscopy, zeta‐potential measurements, and density functional theory calculations reveal that fluorination induces localized charge redistribution and a more negative surface potential, accompanied by enhanced Li affinity at the cathode surface. In situ Raman spectroscopy and in situ X‐ray diffraction further demonstrate improved structural reversibility, suppressed c‐axis contraction, and mitigated phase‐transition behavior during electrochemical cycling. As a result, the fluorinated AlPO 4 ‐coated cathode (LLO‐APF) delivers an initial Coulombic efficiency of 95.9% and stable cycling over 244 cycles at 1 C, compared with 57 cycles for pristine LLO under identical conditions, while limiting voltage decay to 0.23 V. These results suggest that fluorinated phosphate interfaces can provide a multifunctional platform for simultaneously regulating interfacial stability, Li + transport behavior, and structural reversibility in high‐capacity anionic‐redox cathode systems.
- 29 September 2026
- Published by Wiley in Advanced Functional Materials
- Vol. 36 (90) , e78762
Open AccessEngineering a Fluorinated AlPO 4 Interface: Toward High Initial Coulombic Efficiency and Stable Oxygen Redox in Li‐Rich Layered Oxide Cathodes
Li‐rich layered oxides (LLOs) are promising high‐energy‐density cathode candidates; however, their practical application is hindered by severe voltage decay originating from irreversible layered‐to‐spinel phase transformation and interfacial degradation under high‐voltage operation (>4.5 V). Herein, we report a fluorinated AlPO 4 (AlPO 4 ‐F) surface architecture for LLO cathodes designed to simultaneously stabilize the oxygen framework and modify the interfacial charge environment. Electrostatic force microscopy, zeta‐potential measurements, and density functional theory calculations reveal that fluorination induces localized charge redistribution and a more negative surface potential, accompanied by enhanced Li affinity at the cathode surface. In situ Raman spectroscopy and in situ X‐ray diffraction further demonstrate improved structural reversibility, suppressed c‐axis contraction, and mitigated phase‐transition behavior during electrochemical cycling. As a result, the fluorinated AlPO 4 ‐coated cathode (LLO‐APF) delivers an initial Coulombic efficiency of 95.9% and stable cycling over 244 cycles at 1 C, compared with 57 cycles for pristine LLO under identical conditions, while limiting voltage decay to 0.23 V. These results suggest that fluorinated phosphate interfaces can provide a multifunctional platform for simultaneously regulating interfacial stability, Li + transport behavior, and structural reversibility in high‐capacity anionic‐redox cathode systems.