QXQingfang Xu

Qingfang Xu

*This is an algorithmically generated author record based on publicly available information.

Current Organizations / Institutes

The organizations/institutes from the scholar's latest article


Qingfang Xu has a total of 45 co-authors. Here are the top co-authors by number of shared publications:


Latest Publications

  • Open Access

    Deposition Temperature-Driven Structural Evolution and Wet-Oxygen Corrosion Behavior of a-SiOC Coatings on Optical Fibers

    by Rong Tu, Haodong He, Jiangxin Yang, Qingfang Xu, Chitengfei Zhang, Tenghua Gao, Song Zhang, Takashi Goto, Lianmeng Zhang

    Optical fiber sensors deployed in harsh industrial fields, e.g., high-temperature wet-oxygen, face severe challenges in signal attenuation and mechanical degradation. While amorphous silicon oxycarbide (a-SiOC) coatings offer a promising solution due to their adjustable thermo-mechanical properties, balancing their structural density with environmental stability remains a critical technical bottleneck. In this study, a-SiOC coatings were deposited on optical fibers using hexamethyldisilane (HMDS) and trace oxygen via radio-frequency capacitively coupled plasma-enhanced chemical vapor deposition (PECVD). A systematic investigation was conducted to determine the impact of deposition temperature (70–420 °C) on the precursor dissociation kinetics, microstructural evolution, and corrosion resistance of the coatings. An elevation in temperature promotes the elimination of organic terminal groups (–CH3, –H) and enhances surface diffusion, driving the coating from a loose, carbon-rich “polymer-like” structure (dominated by Si–C bonds) to a dense, inorganic “silica-like” skeleton (dominated by Si–O–Si bonds). High-temperature corrosion tests in a wet-oxygen environment (500–900 °C) demonstrate that the failure mechanism is highly dependent on deposition temperature. Coatings deposited at low temperatures suffer catastrophic cracking due to pronounced oxidative shrinkage and the release of volatile species, whereas coatings deposited at 420 °C exhibit microcracking caused by severe carbon phase separation and stress concentration within the rigid inorganic network. In the present system, 350 °C is identified as the optimal deposition temperature, as it achieves the best balance of network densification and structural flexibility, while exhibiting the best mechanical performance.

  • Open Access

    One-Step LCVD Fabrication of Binder-Free Porous Graphene@SiC Heterostructures for Lithium-Ion Battery Anodes

    by Song Zhang, Feiyang Ji, Wei Huang, Chitengfei Zhang, Chongjie Wang, Cuicui Li, Qingfang Xu, Rong Tu

    The potential of silicon carbide (SiC) as a promising high-capacity and stable anode material is hindered by poor electronic conductivity and slow lithium diffusion kinetics. Here, we report a one-step laser chemical vapor deposition (LCVD) process to directly synthesize porous graphene@SiC heterostructures on carbon fiber substrates. This in situ method yields an integral, binder-free electrode architecture that enhances mechanical robustness against pulverization. A critical feature of this heterostructure is the built-in electric field at the graphene–SiC interface, which is revealed by theoretical calculations to significantly accelerate charge transport and lithium-ion diffusion. The resulting anode delivers a high reversible capacity of 668 mAh·g−1 after 100 cycles at 0.1 A·g−1. More remarkably, a unique multi-stage activation mechanism is discovered, leading to an unprecedented capacity rebound to 735 mAh·g−1 after cycling at rates up to 5 A·g−1. This activation process is observed to accelerate with increasing current density in the 0.1–2 A·g−1 range. Furthermore, post-cycling analysis via XRD, TEM, and XPS confirms both the structural durability of the electrode and a reversible lithium intercalation mechanism, providing a critical foundation for the future design of high-performance LIB anodes.


  • Oxygen Vacancy-Induced Room-Temperature Ferromagnetism in a Layered Aluminosilicate Material

    by Hongyun Ji, Jian Peng, Meijun Yang, Qingfang Xu, Tenghua Gao, Rong Tu, Song Zhang, Lianmeng Zhang

    Defect engineering has been utilized to induce ferromagnetism in various nonmagnetic van der Waals (vdW) crystals, which are vital for fundamental research and applications. Herein, oxygen vacancies were successfully created in montmorillonite, a layered aluminosilicate, by acetic acid treatment and annealing in an argon atmosphere. This treatment facilitated the transition from paramagnetism to room-temperature ferromagnetism with a Curie temperature of 330 K. As the annealing temperature increased, in-plane stretching along the [002] crystallographic direction was found to reduce the formation energy of oxygen defects, thereby promoting the creation of oxygen vacancies. By controlling the concentration of oxygen vacancies, precise regulation of the material's ferromagnetic properties was achieved. This work presents a novel room-temperature ferromagnetic material and advances the study of oxygen vacancy-induced ferromagnetism in vdW materials.


  • Laser chemical vapor deposition of nitrogen-doped SiC electrode for electrochemical detection of uric acid

    by Cuicui Li, Qingfang Xu, Jiawei Zhu, Tingting Luo, Meijun Yang, Honglian Dai, Marina L. Kosinova, Song Zhang, Rong Tu


  • Graphene/SiC composite porous electrodes for high-performance micro-supercapacitors

    by Song Zhang, Ming Zhang, Chongjie Wang, Pengjian Lu, Bingjian Guo, Bao-Wen Li, Rong Tu, Qingfang Xu, Chuanbin Wang, Lianmeng Zhang


  • SiC/Graphene Film by Laser CVD as an Implantable Sensor Material for Dopamine Detection

    by Cuicui Li, Yilun Cai, Jinrong Hu, Jiawei Liu, Honglian Dai, Qingfang Xu, Chitengfei Zhang, Xian Zhang, Kai Liu, Marina L. Kosinova, et al.

    Implantable electrochemical sensor holds great promise in the real-time monitoring of dopamine (DA) to regulate body function. However, the real application of these sensors is limited by the weak current signal of DA in the human body and the poor compatibility of the on-chip microelectronic devices. In this work, a SiC/graphene composite film was fabricated using laser chemical vapor deposition (LCVD) and employed as a DA sensor. The graphene in the porous nanoforest-like SiC framework offered efficient channels for electronic transmission, leading to an enhanced electron transfer rate and consequently an increased current response for DA detection. The three-dimensional (3D) porous network also facilitated the exposure of more catalytic active sites toward DA oxidation. Besides, the wide distribution of graphene in the nanoforest-like SiC films reduced the interfacial resistance of the charge transfer. The SiC/graphene composite film exhibited excellent electrocatalytic activity toward DA oxidation with a low detection limit of 0.11 μM and a high sensitivity of 0.86 μA·μM-1·cm-2. The film electrode also showed a wide linear response for DA in 0.5-78 μM, along with good selectivity, repeatability, and reproducibility. Furthermore, the cell counting kit-8 (CCK-8) and live-dead assays revealed that the film is also biocompatible for biomedical applications. Therefore, the nanoforest-like SiC/graphene composite film via the CVD process enables a promising candidate for an integrated miniature DA biosensor with high detection performance.


  • Open Access

    Epitaxial Growth of SiC Films on 4H-SiC Substrate by High-Frequency Induction-Heated Halide Chemical Vapor Deposition

    by Rong Tu, Chengyin Liu, Qingfang Xu, Kai Liu, Qizhong Li, Xian Zhang, Marina L. Kosinova, Takashi Goto, Song Zhang

    SiC epitaxial wafers offer enormous potential for a wide range of telecom technologies due to their excellent properties. The experimental process was simulated by software, and the contour of gas flow velocity and raw material mass fraction inside the chamber were obtained. SiC films were epitaxially grown on 4H-SiC single crystalline substrates at different temperatures for one batch, using SiCl4, CH4, and H2 as precursors. With increasing temperature, the crystal phase changed from 4H-SiC at 1773 K to a mixture of 4H- and 3C-SiC, and then a mixture of 3C-SiC and graphite at higher than 1923 K. The film was mainly (004)-oriented 4H-SiC and (111)-oriented 3C-SiC.