Maïté Lacante
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Maïté Lacante has a total of 24 co-authors. Here are the top co-authors by number of shared publications:
- Brice Delsaute
BATir Department (LGC), Université libre de Bruxelles (ULB), 1050 Brussels, Belgium
7 shared publications - Stéphanie Staquet
BATir Department (LGC), Université libre de Bruxelles (ULB), 1050 Brussels, Belgium
7 shared publications Brice Delsaute
2 shared publicationsStéphanie Staquet
2 shared publications- Babak Vafaei
University of Miami
1 shared publication Dimitrios G. Aggelis
1 shared publication
Latest Publications
- Open Access
- 10 April 2026
- Published by Elsevier in Developments in the Built Environment
- Vol. 26
Volume changes and acoustic emission study of alkali-activated slag pastes in free and sealed conditions
- 10 April 2026
- Published by Elsevier in Developments in the Built Environment
- Vol. 26
Open AccessVolume changes and acoustic emission study of alkali-activated slag pastes in free and sealed conditions
- 2 January 2026
- Published by Springer Nature
- p. 349-428
Autogenous Shrinkage of Alkali-Activated Materials
- 2 January 2026
- Published by Springer Nature
- p. 349-428
Autogenous Shrinkage of Alkali-Activated Materials
- Open Access
Volume Changes of Alkali-Activated Slag-Based Mortars and Concretes in Sealed and Free Conditions
The goal of this paper is to assess the evolution of the autogenous strains as well as the thermal strains (thanks to the assessment of the coefficient of thermal expansion) of alkali-activated slag-based materials at early age. The effect of the sand and the coarse aggregates on the paste and mortar scale to upscale to mortar and concrete, respectively, has been investigated as a function of the age of the material. The restraint imposed by the sand on the paste seemed more significant than that of the coarse aggregate on the mortar. In addition, the long-term autogenous strains have been monitored on the mortar scale. These results revealed a separation into groups based on the solution concentration. Different testing methods were also compared. Thermal and autogenous strains were monitored with a customized testing device where the thermal variations are controlled. These devices were the horizontal corrugated tubes method (for tests on paste and mortar scales) and the vertical corrugated tubes method (for tests on mortar and concrete scales). Depending on the compositions (lower concentration), good correlations can be obtained between the two testing methods. Moreover, the autogenous strain of two different specimen sizes was also assessed manually (initially for the long-term), but early-age comparison showed good correlation for lower solution-to-binder ratios. On the concrete scale, a correlation based on the modified equations from the standards was established between the compressive strength and the tensile strength, obtained from the splitting tensile test.
Open AccessVolume Changes of Alkali-Activated Slag-Based Mortars and Concretes in Sealed and Free Conditions
The goal of this paper is to assess the evolution of the autogenous strains as well as the thermal strains (thanks to the assessment of the coefficient of thermal expansion) of alkali-activated slag-based materials at early age. The effect of the sand and the coarse aggregates on the paste and mortar scale to upscale to mortar and concrete, respectively, has been investigated as a function of the age of the material. The restraint imposed by the sand on the paste seemed more significant than that of the coarse aggregate on the mortar. In addition, the long-term autogenous strains have been monitored on the mortar scale. These results revealed a separation into groups based on the solution concentration. Different testing methods were also compared. Thermal and autogenous strains were monitored with a customized testing device where the thermal variations are controlled. These devices were the horizontal corrugated tubes method (for tests on paste and mortar scales) and the vertical corrugated tubes method (for tests on mortar and concrete scales). Depending on the compositions (lower concentration), good correlations can be obtained between the two testing methods. Moreover, the autogenous strain of two different specimen sizes was also assessed manually (initially for the long-term), but early-age comparison showed good correlation for lower solution-to-binder ratios. On the concrete scale, a correlation based on the modified equations from the standards was established between the compressive strength and the tensile strength, obtained from the splitting tensile test.
- Open Access
Mitigation of Volume Changes of Alkali-Activated Materials by Using Limestone Filler
As autogenous and thermal strains are significantly high in alkali-activated pastes, it becomes necessary to investigate ways to reduce these. This research studies how the volume changes of pastes made from slag activated by alkalis can be mitigated by substituting part of the slag with limestone filler and how this impacts the properties of the material, including autogenous strains, thermal strains, heat flow, compressive strength, and workability. The first part investigates how the different substitution rates impact the compressive strength and workability. The substitution rates of 15% and 30% emerged as the most optimal with a maximal reduction in the compressive strength of 23%. Five compositions were consequently investigated in the second part of the study. Isothermal calorimetry revealed that the limestone filler was probably not entirely inert and showed the effect of dilution, which is linked to the increase in the solution-to-binder ratio when the substitution rate increases. The autogenous shrinkage decreased when substituting 15% of the slag, while higher autogenous shrinkage was obtained when 30% was substituted. In addition, its rate of development was reduced. Finally, the coefficient of thermal expansion was generally slightly reduced and delayed when slag was substituted.
Open AccessMitigation of Volume Changes of Alkali-Activated Materials by Using Limestone Filler
As autogenous and thermal strains are significantly high in alkali-activated pastes, it becomes necessary to investigate ways to reduce these. This research studies how the volume changes of pastes made from slag activated by alkalis can be mitigated by substituting part of the slag with limestone filler and how this impacts the properties of the material, including autogenous strains, thermal strains, heat flow, compressive strength, and workability. The first part investigates how the different substitution rates impact the compressive strength and workability. The substitution rates of 15% and 30% emerged as the most optimal with a maximal reduction in the compressive strength of 23%. Five compositions were consequently investigated in the second part of the study. Isothermal calorimetry revealed that the limestone filler was probably not entirely inert and showed the effect of dilution, which is linked to the increase in the solution-to-binder ratio when the substitution rate increases. The autogenous shrinkage decreased when substituting 15% of the slag, while higher autogenous shrinkage was obtained when 30% was substituted. In addition, its rate of development was reduced. Finally, the coefficient of thermal expansion was generally slightly reduced and delayed when slag was substituted.
- Open Access
Mitigation of Volume Changes in Alkali-Activated Slag by Using Metakaolin
This research investigates whether metakaolin can be used as a partial substitution for slag to mitigate significant volume changes in alkali-activated slags. Its effect on compressive strength and workability (as well as on isothermal calorimetry, autogenous strain, and coefficient of thermal expansion (CTE)) were found to depend on both the type and concentration of the alkaline activator. When using 8 M and 10 M sodium hydroxide (NaOH), increasing the substitution rate increased the compressive strength. With sodium silicate (Na2SiO3), compressive strength decreased as the substitution increased. Isothermal calorimetry revealed metakaolin’s dilution effect at 10% substitution. With 8 M NaOH, a third reaction peak appeared, whose magnitude increased with the substitution rate, while the second peak decreased. The swelling was increased at 10% substitution, followed by constant shrinkage in case of NaOH-activation. Shrinkage was mitigated with Na2SiO3-activation. Higher substitutions with 8 M NaOH resulted in a significant increase in the shrinkage rate and CTE, occurring when the third reaction peak appeared. A 10% substitution delayed the CTE increase but resulted in higher later-age values (dilution effect). The 20% substitution led to a similar final CTE value at 300 h, while 30% substitution resulted in a decrease in CTE after the initial increase.
Open AccessMitigation of Volume Changes in Alkali-Activated Slag by Using Metakaolin
This research investigates whether metakaolin can be used as a partial substitution for slag to mitigate significant volume changes in alkali-activated slags. Its effect on compressive strength and workability (as well as on isothermal calorimetry, autogenous strain, and coefficient of thermal expansion (CTE)) were found to depend on both the type and concentration of the alkaline activator. When using 8 M and 10 M sodium hydroxide (NaOH), increasing the substitution rate increased the compressive strength. With sodium silicate (Na2SiO3), compressive strength decreased as the substitution increased. Isothermal calorimetry revealed metakaolin’s dilution effect at 10% substitution. With 8 M NaOH, a third reaction peak appeared, whose magnitude increased with the substitution rate, while the second peak decreased. The swelling was increased at 10% substitution, followed by constant shrinkage in case of NaOH-activation. Shrinkage was mitigated with Na2SiO3-activation. Higher substitutions with 8 M NaOH resulted in a significant increase in the shrinkage rate and CTE, occurring when the third reaction peak appeared. A 10% substitution delayed the CTE increase but resulted in higher later-age values (dilution effect). The 20% substitution led to a similar final CTE value at 300 h, while 30% substitution resulted in a decrease in CTE after the initial increase.
- Open Access
Effect of Curing Temperature on Volume Changes of Alkali-Activated Slag Pastes
This study investigates the influence of curing temperature (explored at 10 °C, 20 °C, and 30 °C) on the volume changes of alkali-activated slag (AAS) pastes with the aim of expanding existing knowledge on alkali-activated materials (AAMs). The focus was on autogenous and thermal strains, internal relative humidity (IRH), heat flow and cumulative heat, setting times, and workability. The results indicate that increasing the curing temperature to 30 °C reduces autogenous shrinkage, likely due to changes in the elastic modulus and viscoelastic properties, while promoting swelling, especially for higher molarities. The coefficient of thermal expansion (CTE), related to thermal strains, is higher when the curing temperature is increased, but its development is delayed. The IRH is influenced more by the activating solution’s molarity than by curing temperature, although temperature does affect the initial IRH. The study also revealed that higher curing temperatures accelerate chemical reactions and reduce setting times. The initial workability was significantly affected by the solution-to-binder ratio, while higher temperatures decreased workability, especially at higher molarities. These findings contribute to the understanding of how curing temperature influences the durability of AAS pastes, offering insights into optimized construction practices under varying environmental conditions.
Open AccessEffect of Curing Temperature on Volume Changes of Alkali-Activated Slag Pastes
This study investigates the influence of curing temperature (explored at 10 °C, 20 °C, and 30 °C) on the volume changes of alkali-activated slag (AAS) pastes with the aim of expanding existing knowledge on alkali-activated materials (AAMs). The focus was on autogenous and thermal strains, internal relative humidity (IRH), heat flow and cumulative heat, setting times, and workability. The results indicate that increasing the curing temperature to 30 °C reduces autogenous shrinkage, likely due to changes in the elastic modulus and viscoelastic properties, while promoting swelling, especially for higher molarities. The coefficient of thermal expansion (CTE), related to thermal strains, is higher when the curing temperature is increased, but its development is delayed. The IRH is influenced more by the activating solution’s molarity than by curing temperature, although temperature does affect the initial IRH. The study also revealed that higher curing temperatures accelerate chemical reactions and reduce setting times. The initial workability was significantly affected by the solution-to-binder ratio, while higher temperatures decreased workability, especially at higher molarities. These findings contribute to the understanding of how curing temperature influences the durability of AAS pastes, offering insights into optimized construction practices under varying environmental conditions.
- Open Access
Effect of Solution-to-Binder Ratio and Molarity on Volume Changes in Slag Binder Activated by Sodium Hydroxide at Early Age
This research investigates the impact of solution concentration and solution-to-binder ratio (S/B) on the volume changes in alkali-activated slags with sodium hydroxide at 20 °C. Autogenous and thermal strains are monitored with a customized testing device in which thermal variations are controlled. Consequently, both the autogenous strain and coefficient of thermal expansion (CTE) are determined. Heat flow and internal relative humidity (IRH) are also monitored in parallel, making this research a multifaceted study. The magnitudes of autogenous strain and CTE are higher than those of ordinary Portland cement paste. Decreasing the solution concentration or S/B generally decreases the autogenous strain (swelling and shrinkage) and the CTE. The shrinkage amounted to 87 to 1981 µm/m, while the swelling reached between 27 and 295 µm/m and was only present in half of the compositions. The amplitude of the CTE, which increases up to 55 µm/m/°C for some compositions while the CTE of OPC remains between 20 and 25 µm/m/°C, can be explained by the high CTE of the solution in comparison with water. The IRH of paste cannot explain the autogenous strain’s development alone. Increasing S/B eliminates the self-desiccation-related decrease.
Open AccessEffect of Solution-to-Binder Ratio and Molarity on Volume Changes in Slag Binder Activated by Sodium Hydroxide at Early Age
This research investigates the impact of solution concentration and solution-to-binder ratio (S/B) on the volume changes in alkali-activated slags with sodium hydroxide at 20 °C. Autogenous and thermal strains are monitored with a customized testing device in which thermal variations are controlled. Consequently, both the autogenous strain and coefficient of thermal expansion (CTE) are determined. Heat flow and internal relative humidity (IRH) are also monitored in parallel, making this research a multifaceted study. The magnitudes of autogenous strain and CTE are higher than those of ordinary Portland cement paste. Decreasing the solution concentration or S/B generally decreases the autogenous strain (swelling and shrinkage) and the CTE. The shrinkage amounted to 87 to 1981 µm/m, while the swelling reached between 27 and 295 µm/m and was only present in half of the compositions. The amplitude of the CTE, which increases up to 55 µm/m/°C for some compositions while the CTE of OPC remains between 20 and 25 µm/m/°C, can be explained by the high CTE of the solution in comparison with water. The IRH of paste cannot explain the autogenous strain’s development alone. Increasing S/B eliminates the self-desiccation-related decrease.
- 9 June 2023
- Published by Springer Nature
- p. 350-361
Effect of Internal and External Factors on the Volume Changes of Slag Binder Activated by Sodium Hydroxide at Early-Age
- 9 June 2023
- Published by Springer Nature
- p. 350-361
Effect of Internal and External Factors on the Volume Changes of Slag Binder Activated by Sodium Hydroxide at Early-Age
- Open Access
- 6 December 2022
- Published by Frontiers Media SA in Frontiers in Built Environment
- Vol. 8
Development of early age autogenous and thermal strains of alkali-activated slag-fly ash pastes
Replacing ordinary Portland cement-based materials with alkali-activated industrial wastes is often limited because of significant volume changes occurring in these materials at early age. This experimental study aims to quantify the extent of the volume changes and explore the underlying mechanisms of pastes composed of slag and fly ash (ratio 50:50) which are activated by sodium hydroxide and sodium silicate. Eight compositions were tested, with silica modulus (Ms) varying between 1.04 and 1.58 and with solution-to-binder ratios (S/B) varying between 0.47 and 0.70. Specimen length changes in sealed conditions are monitored by applying repeated thermal variations in an adapted AutoShrink device and are accompanied by isothermal calorimetry, uniaxial compressive strength, and internal relative humidity (IRH) tests. This way, the temporal evolutions of autogenous strains, the coefficient of thermal expansion (CTE), the heat release, the apparent activation energy (Ea), the IRH and the strength are determined and compared to each other. Both the measured autogenous shrinkage and CTEs are rather large; they amount to 4,000–5,000 μm/m and roughly 40 μm/m/°C, respectively, at material ages of 2 weeks. An increase in S/B leads to a decrease in autogenous shrinkage and an increase in CTE. An increase in the Ms causes a decrease in both the autogenous shrinkage and the CTE. Most strikingly, autogenous shrinkage evolves linearly with the cumulative heat released by the binders. The IRH remains continuously above 94% during the first 2 weeks. The apparent activation energy amounts to roughly 74 kJ/mol and is virtually unaffected by S/B and Ms.
- 6 December 2022
- Published by Frontiers Media SA in Frontiers in Built Environment
- Vol. 8
Open AccessDevelopment of early age autogenous and thermal strains of alkali-activated slag-fly ash pastes
Replacing ordinary Portland cement-based materials with alkali-activated industrial wastes is often limited because of significant volume changes occurring in these materials at early age. This experimental study aims to quantify the extent of the volume changes and explore the underlying mechanisms of pastes composed of slag and fly ash (ratio 50:50) which are activated by sodium hydroxide and sodium silicate. Eight compositions were tested, with silica modulus (Ms) varying between 1.04 and 1.58 and with solution-to-binder ratios (S/B) varying between 0.47 and 0.70. Specimen length changes in sealed conditions are monitored by applying repeated thermal variations in an adapted AutoShrink device and are accompanied by isothermal calorimetry, uniaxial compressive strength, and internal relative humidity (IRH) tests. This way, the temporal evolutions of autogenous strains, the coefficient of thermal expansion (CTE), the heat release, the apparent activation energy (Ea), the IRH and the strength are determined and compared to each other. Both the measured autogenous shrinkage and CTEs are rather large; they amount to 4,000–5,000 μm/m and roughly 40 μm/m/°C, respectively, at material ages of 2 weeks. An increase in S/B leads to a decrease in autogenous shrinkage and an increase in CTE. An increase in the Ms causes a decrease in both the autogenous shrinkage and the CTE. Most strikingly, autogenous shrinkage evolves linearly with the cumulative heat released by the binders. The IRH remains continuously above 94% during the first 2 weeks. The apparent activation energy amounts to roughly 74 kJ/mol and is virtually unaffected by S/B and Ms.