Jihan Farouk Younis
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Jihan Farouk Younis has a total of 4 co-authors. Here are the top co-authors by number of shared publications:
- Ashraf Mokhtar
Fixed prosthodontics department, Dentistry, Cairo University, Cairo, Egypt
1 shared publication - Mohamad Kheir Jihad Kheir
Department fixed prosthodontics, Misr International University
1 shared publication - Mostafa Hassan Hafez
Post graduate student, Misr International University, Cairo, Egypt
1 shared publication - Tarek Salah Morsi
Department of Fixed Prosthodontics, Ain-Shams University, Egypt
1 shared publication
Latest Publications
- Open Access
- 1 December 2023
- Published by Egyptian Knowledge Bank in Journal of Fundamental and Clinical Research
- Vol. 3 (2) , 190-206
Effect of Fabrication Technique and Margin Design on the Marginal Fit of Interim Fixed Dental Prosthesis (An In-Vitro Study)
Background: There is limited evidence available regarding the effectiveness of various digital manufacturing techniques for producing interim prosthesis with different finish line designs. Aim: The objective was to evaluate the influence of CAM techniques, 3D printed and milled on the vertical margin gap of interim fixed dental prosthesis using two finish line designs. Materials and Methods: Two prepared abutment teeth were designed with finish line designs (shoulder and knife-edge) to receive a 3-unit interim prosthesis (polymethyl methacrylate and microfilled hybrid resin). The reference models were 3D printed (n=28), and an optical impression was performed to design FDPs on CAD software. Group A milled with shoulder finish line. Group B milled with knife-edge finish line. Group C 3D-printed with shoulder finish line. Group D 3D-printed with knife-edge finish line. Samples were cemented with long-term temporary cement. Vertical marginal fit was assessed using stereo-optical microscope before and after thermocycling Results: Marginal gaps in both techniques were influenced by thermocycling. The knife-edge finish line showed a higher gap when milled. Overall gap distance for 3D-printed knife-edge and shoulder finish line before (20-74.8 µm, 17.8-91µm) and after thermocycling (34-103µm, 33-112µm). Overall gap distance for milled knife-edge and milled finish lines before (43-111.8 µm, 17.2-93µm) and after thermocycling (62-141 µm, 27-103µm). Conclusion: Thermocycling showed a negative effect on vertical marginal adaptation in both techniques. Vertical marginal gap of the interim restorations fabricated by the two techniques was within the acceptable clinical range of ≤120μm.
- 1 December 2023
- Published by Egyptian Knowledge Bank in Journal of Fundamental and Clinical Research
- Vol. 3 (2) , 190-206
Open AccessEffect of Fabrication Technique and Margin Design on the Marginal Fit of Interim Fixed Dental Prosthesis (An In-Vitro Study)
Background: There is limited evidence available regarding the effectiveness of various digital manufacturing techniques for producing interim prosthesis with different finish line designs. Aim: The objective was to evaluate the influence of CAM techniques, 3D printed and milled on the vertical margin gap of interim fixed dental prosthesis using two finish line designs. Materials and Methods: Two prepared abutment teeth were designed with finish line designs (shoulder and knife-edge) to receive a 3-unit interim prosthesis (polymethyl methacrylate and microfilled hybrid resin). The reference models were 3D printed (n=28), and an optical impression was performed to design FDPs on CAD software. Group A milled with shoulder finish line. Group B milled with knife-edge finish line. Group C 3D-printed with shoulder finish line. Group D 3D-printed with knife-edge finish line. Samples were cemented with long-term temporary cement. Vertical marginal fit was assessed using stereo-optical microscope before and after thermocycling Results: Marginal gaps in both techniques were influenced by thermocycling. The knife-edge finish line showed a higher gap when milled. Overall gap distance for 3D-printed knife-edge and shoulder finish line before (20-74.8 µm, 17.8-91µm) and after thermocycling (34-103µm, 33-112µm). Overall gap distance for milled knife-edge and milled finish lines before (43-111.8 µm, 17.2-93µm) and after thermocycling (62-141 µm, 27-103µm). Conclusion: Thermocycling showed a negative effect on vertical marginal adaptation in both techniques. Vertical marginal gap of the interim restorations fabricated by the two techniques was within the acceptable clinical range of ≤120μm.
- Open Access
- 1 June 2023
- Published by Egyptian Knowledge Bank in Journal of Fundamental and Clinical Research
- Vol. 3 (1) , 50-62
Fracture Resistance of Implant Supported Three Units Fixed Partial Dentures Fabricated from Zirconia and PEEK “In-vitro study”
Background: Selection of prosthetic material is a critical factor affecting implant supported restorations long term success. It influences the transmission of stresses during function that transferred to each prosthetic component. PEEK -poly ether ether ketone-is a quite new polymeric material used for dental applications, it has been introduced for its promising shock absorbing and stress distribution qualities. However, there are limited data available in literature concerning fracture strength of PEEK restorations as implant superstructure. Aim of study: To evaluate fracture resistance of three units implant supported fixed partial dentures fabricated from PEEK and monolithic zirconia. Materials and methods: An in-vitro model was fabricated while two implants were embedded in an epoxy resin block simulating a case of missing mandibular first premolar and first molar. A total of 14 Monolithic zirconia and PEEK three unit fixed partial dentures were CAD/CAM (computer aided designing/computer aided manufacturing) fabricated and divided into two equal groups (n=7). Load till fracture was applied with a crosshead speed of 0.5 mm/min using a universal testing machine and fracture resistance was recorded in Newtons(N). Mode of failure was assessed using digital microscope. Results. The mean fracture resistance for zirconia was 979N while PEEK was 920N. Kolmogorov-Smirnov and Shapiro-Wilk tests showed that there was no statistically significant difference between both groups. Conclusion: PEEK superstructures are considered a new alternative that can rely on regarding its load bearing capacity and fracture strength. PEEK shock absorbing makes it such an innovative approach can substitute other commonly used materials.
- 1 June 2023
- Published by Egyptian Knowledge Bank in Journal of Fundamental and Clinical Research
- Vol. 3 (1) , 50-62
Open AccessFracture Resistance of Implant Supported Three Units Fixed Partial Dentures Fabricated from Zirconia and PEEK “In-vitro study”
Background: Selection of prosthetic material is a critical factor affecting implant supported restorations long term success. It influences the transmission of stresses during function that transferred to each prosthetic component. PEEK -poly ether ether ketone-is a quite new polymeric material used for dental applications, it has been introduced for its promising shock absorbing and stress distribution qualities. However, there are limited data available in literature concerning fracture strength of PEEK restorations as implant superstructure. Aim of study: To evaluate fracture resistance of three units implant supported fixed partial dentures fabricated from PEEK and monolithic zirconia. Materials and methods: An in-vitro model was fabricated while two implants were embedded in an epoxy resin block simulating a case of missing mandibular first premolar and first molar. A total of 14 Monolithic zirconia and PEEK three unit fixed partial dentures were CAD/CAM (computer aided designing/computer aided manufacturing) fabricated and divided into two equal groups (n=7). Load till fracture was applied with a crosshead speed of 0.5 mm/min using a universal testing machine and fracture resistance was recorded in Newtons(N). Mode of failure was assessed using digital microscope. Results. The mean fracture resistance for zirconia was 979N while PEEK was 920N. Kolmogorov-Smirnov and Shapiro-Wilk tests showed that there was no statistically significant difference between both groups. Conclusion: PEEK superstructures are considered a new alternative that can rely on regarding its load bearing capacity and fracture strength. PEEK shock absorbing makes it such an innovative approach can substitute other commonly used materials.