Dan Li
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Dan Li has a total of 20 co-authors. Here are the top co-authors by number of shared publications:
Chenyao Cai
School of Materials Science and Engineering, Inner Mongolia University of Technology Hohhot China
1 shared publicationDan Li
1 shared publication- Edwin Ernest Nyakilla
Peking University Ordos Research Institute of Energy, Inner Mongolia Autonomous Region, Ordos City 017010, China
1 shared publication Feifei Huang
1 shared publicationHaiping Qi
Inner Mongolia Autonomous Region Ecological Environment Inspection Technical Support Center Hohhot China
1 shared publication- Hongliang Hao
Ordos Research Institute of Energy, Peking University, Ordos 017010, China
1 shared publication
Latest Publications
- 5 November 2026
- Published by Wiley in Polymer Composites
Graphene Oxide With an Interfacial Buffer Layer for Epoxy Resin Modification
Graphene oxide (GO) can simultaneously strengthen and toughen epoxy resin (EP), but sheet restacking and limited interfacial compatibility restrict its effectiveness. In this study, a flexible‐chain hyperbranched epoxy resin (F‐HBEP) was synthesized via a one‐step A 2 + B 3 reaction in the presence of GO to obtain F‐HBEP‐modified GO (FGO). GO was added before polymerization and remained in the reaction medium throughout synthesis. Flexible aliphatic segments derived from 1,4‐butanediol were incorporated into the hyperbranched structure to provide an interfacial buffer layer. Spectroscopic, structural, and thermal analyses supported GO surface modification with F‐HBEP and indicated increased interlayer spacing and suppressed ordered restacking. At an FGO loading of 0.5 wt.%, the tensile strength, flexural strength, and impact toughness of the composite increased by 58.1%, 50.9%, and 192.1%, respectively, relative to neat EP. The composites also exhibited a higher glassy storage modulus, a broader loss response, while maintaining initial thermal stability. Fractographic observations indicated improved interfacial contact, rougher fracture surfaces, and more tortuous crack paths. These improvements were attributed to load transfer and crack deflection by GO, combined with stress buffering and energy dissipation by the flexible F‐HBEP interfacial layer. This work provides a feasible polymerization‐stage route for tailoring the overall mechanical performance and maintaining the initial thermal stability of epoxy nanocomposites.
- 5 November 2026
- Published by Wiley in Polymer Composites
Graphene Oxide With an Interfacial Buffer Layer for Epoxy Resin Modification
Graphene oxide (GO) can simultaneously strengthen and toughen epoxy resin (EP), but sheet restacking and limited interfacial compatibility restrict its effectiveness. In this study, a flexible‐chain hyperbranched epoxy resin (F‐HBEP) was synthesized via a one‐step A 2 + B 3 reaction in the presence of GO to obtain F‐HBEP‐modified GO (FGO). GO was added before polymerization and remained in the reaction medium throughout synthesis. Flexible aliphatic segments derived from 1,4‐butanediol were incorporated into the hyperbranched structure to provide an interfacial buffer layer. Spectroscopic, structural, and thermal analyses supported GO surface modification with F‐HBEP and indicated increased interlayer spacing and suppressed ordered restacking. At an FGO loading of 0.5 wt.%, the tensile strength, flexural strength, and impact toughness of the composite increased by 58.1%, 50.9%, and 192.1%, respectively, relative to neat EP. The composites also exhibited a higher glassy storage modulus, a broader loss response, while maintaining initial thermal stability. Fractographic observations indicated improved interfacial contact, rougher fracture surfaces, and more tortuous crack paths. These improvements were attributed to load transfer and crack deflection by GO, combined with stress buffering and energy dissipation by the flexible F‐HBEP interfacial layer. This work provides a feasible polymerization‐stage route for tailoring the overall mechanical performance and maintaining the initial thermal stability of epoxy nanocomposites.
- Open Access
Evolution of the Corrosion Products around MnS Embedded in AISI 304 Stainless Steel in NaCl Solution
The characterization and evolution of corrosion products deposited on/around MnSs, a typical kind of inclusive particle embedded in AISI 304 stainless steel, was analyzed using a quasi-in-situ method in a 3.5 wt.% NaCl solution. On/around the MnS inclusion, a corrosion product layer with spinel Fe3−xCrxO4 as the main component was formed, with a thickness of several hundred nanometers. Below the layer, there was a cavity layer in which part of the MnS remained, forming secondary pitting along the MnS/matrix boundary. The mechanism of corrosion product deposition and evolution accompanied by MnS dissolution, as well as the characteristics of the corrosion products, are discussed.
Open AccessEvolution of the Corrosion Products around MnS Embedded in AISI 304 Stainless Steel in NaCl Solution
The characterization and evolution of corrosion products deposited on/around MnSs, a typical kind of inclusive particle embedded in AISI 304 stainless steel, was analyzed using a quasi-in-situ method in a 3.5 wt.% NaCl solution. On/around the MnS inclusion, a corrosion product layer with spinel Fe3−xCrxO4 as the main component was formed, with a thickness of several hundred nanometers. Below the layer, there was a cavity layer in which part of the MnS remained, forming secondary pitting along the MnS/matrix boundary. The mechanism of corrosion product deposition and evolution accompanied by MnS dissolution, as well as the characteristics of the corrosion products, are discussed.
- Open Access
Localized Corrosion of Stainless Steel Triggered by Typical Inclusions in NaCl Solution: Oxy-Sulfide and MnS
The localized corrosion behavior of stainless steel (SS) induced by typical inclusion such as MnS and oxy-sulfide in NaCl solution was investigated by immersion tests and microelectrochemical tests. Oxy-sulfide consists of an internal polygonal oxide part and an external sulfide part. The surface Volta potential of the sulfide part is always lower than that of the surrounding matrix, as in the case of individual MnS, while the potential of the oxide part is indistinguishable from that of the surrounding matrix. Sulfides are soluble, while oxides are almost insoluble. Oxy-sulfide exhibits a complex electrochemical behavior in the passive region, which can be attributed to its complex composition and multi-interface coupling effects. It was found that both MnS and oxy-sulfide increase the susceptibility of the local area to pitting corrosion.
Open AccessLocalized Corrosion of Stainless Steel Triggered by Typical Inclusions in NaCl Solution: Oxy-Sulfide and MnS
The localized corrosion behavior of stainless steel (SS) induced by typical inclusion such as MnS and oxy-sulfide in NaCl solution was investigated by immersion tests and microelectrochemical tests. Oxy-sulfide consists of an internal polygonal oxide part and an external sulfide part. The surface Volta potential of the sulfide part is always lower than that of the surrounding matrix, as in the case of individual MnS, while the potential of the oxide part is indistinguishable from that of the surrounding matrix. Sulfides are soluble, while oxides are almost insoluble. Oxy-sulfide exhibits a complex electrochemical behavior in the passive region, which can be attributed to its complex composition and multi-interface coupling effects. It was found that both MnS and oxy-sulfide increase the susceptibility of the local area to pitting corrosion.
- Open Access
- 22 March 2022
- Published by Elsevier in SSRN Electronic Journal
Evolution of the Corrosion Products Around Mns Embedded in 304 Stainless Steel in Nacl Solution
A quasi in-situ approach was carried out aiming at analyzing the evolution rule of corrosion products around MnS of stainless steel in 3.5 wt.% NaCl solution. The characteristics of the corrosion product film, which is mainly composed of spinel Fe 3-x Cr x O 4 , were analyzed. Thickness of the film increases over the immersion time, and its value reaches hundreds of nanometers at 60 h. An enclosed zone was formed underneath the film where MnS severely dissolved and pits were formed. Accordingly, the evolution model of corrosion product deposition accompanied by the MnS dissolution was proposed in detail.
- 22 March 2022
- Published by Elsevier in SSRN Electronic Journal
Open AccessEvolution of the Corrosion Products Around Mns Embedded in 304 Stainless Steel in Nacl Solution
A quasi in-situ approach was carried out aiming at analyzing the evolution rule of corrosion products around MnS of stainless steel in 3.5 wt.% NaCl solution. The characteristics of the corrosion product film, which is mainly composed of spinel Fe 3-x Cr x O 4 , were analyzed. Thickness of the film increases over the immersion time, and its value reaches hundreds of nanometers at 60 h. An enclosed zone was formed underneath the film where MnS severely dissolved and pits were formed. Accordingly, the evolution model of corrosion product deposition accompanied by the MnS dissolution was proposed in detail.