Wangchang Li
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Wangchang Li has a total of 69 co-authors. Here are the top co-authors by number of shared publications:
- Shenglei Che
College of Materials Science and Engineering, Zhejiang University of Technology, Hangzhou 310014, China
19 shared publications - Yao Ying
College of Materials Science and Engineering, Zhejiang University of Technology, Hangzhou 310014, China
12 shared publications - Jing Yu
College of Materials Science and Engineering, Zhejiang University of Technology, Hangzhou 310014, China
11 shared publications - Jingwu Zheng
Zhejiang University of Technology
10 shared publications - Liang Qiao
College of Materials Science and Engineering Zhejiang University of Technology Hangzhou China
9 shared publications Jingwu Zheng
College of Materials Science and Engineering Zhejiang University of Technology Hangzhou 310014 China
8 shared publications
Latest Publications
- Open Access
- 6 December 2024
- Published by MDPI AG in Journal of Composites Science
- Vol. 8 (12) , 514
Investigation of the Impact of SmFeN Doping on the Anisotropic NdFeB/SmFeN Composite Magnets
By incorporating various types of permanent magnetic powders, composite magnets with cost-effectiveness and a wide range of magnetic properties can be achieved. In this study, the anisotropic composite magnets were fabricated using the hot press forming method, which involved blending neodymium iron boron (NdFeB) powder and samarium iron nitrogen (SmFeN) powder. The experiment demonstrated that the magnet density reaches its maximum point when the doping level of SmFeN reaches 20 wt.%, aligning remarkably well with the corresponding theoretical value of 19.22 wt.% achieved through a cubic stacking arrangement. In the absence of an applied magnetic field or under a sufficiently high oriented magnetic field (3 T), the remanence variation pattern in composite magnets doped with different amounts of SmFeN aligns consistently with the density pattern, yielding a maximum value of 20%. However, in the actual solidification process, the orientation field is insufficient (e.g., 1.5 T), necessitating a doping amount that exceeds the value corresponding to peak density by 28% to achieve optimal remanence. This observation suggests that the incorporation of a higher proportion of small-sized and relatively low coercivity SmFeN magnetic powder can effectively facilitate the rotational alignment of neighboring large-sized NdFeB magnetic powder under weak magnetic fields, thereby inducing a synergistic effect.
- 6 December 2024
- Published by MDPI AG in Journal of Composites Science
- Vol. 8 (12) , 514
Open AccessInvestigation of the Impact of SmFeN Doping on the Anisotropic NdFeB/SmFeN Composite Magnets
By incorporating various types of permanent magnetic powders, composite magnets with cost-effectiveness and a wide range of magnetic properties can be achieved. In this study, the anisotropic composite magnets were fabricated using the hot press forming method, which involved blending neodymium iron boron (NdFeB) powder and samarium iron nitrogen (SmFeN) powder. The experiment demonstrated that the magnet density reaches its maximum point when the doping level of SmFeN reaches 20 wt.%, aligning remarkably well with the corresponding theoretical value of 19.22 wt.% achieved through a cubic stacking arrangement. In the absence of an applied magnetic field or under a sufficiently high oriented magnetic field (3 T), the remanence variation pattern in composite magnets doped with different amounts of SmFeN aligns consistently with the density pattern, yielding a maximum value of 20%. However, in the actual solidification process, the orientation field is insufficient (e.g., 1.5 T), necessitating a doping amount that exceeds the value corresponding to peak density by 28% to achieve optimal remanence. This observation suggests that the incorporation of a higher proportion of small-sized and relatively low coercivity SmFeN magnetic powder can effectively facilitate the rotational alignment of neighboring large-sized NdFeB magnetic powder under weak magnetic fields, thereby inducing a synergistic effect.
- 26 December 2023
- Published by Wiley in Small Methods
- Vol. 8 (7) , e2301258
Scalable and Flexible Multi‐Layer Prismatic Photonic Metamaterial Film for Efficient Daytime Radiative Cooling
To maintain a comfortable indoor living environment in low latitude or tropical regions, humans consume significant amounts of electrical energy in air conditioning, leading to substantial CO2 emissions. Passive daytime radiative cooling (PDRC) allows objects to cool down during the daytime without any energy consumption by dissipating heat through the atmospheric transparency window (8−13 µm) to outer space, which has garnered significant attention. However, the practical applications of common PDRC materials are hindered by their poor optical selectivity and high‐reflective silver backing. Additionally, the availability of artificial photon emitters with complex structures and excellent performance is also limited by their high cost. Herein, a novel multilayer prismatic photonic metamaterial film without any silver reflector, easily scalable and produced by a roll‐to‐roll method is demonstrated, which exhibits ≈96.4% sunlight reflectance (0.3−2.5 µm) and ≈97.2% emissivity in mid‐infrared (IR) (8−13 µm). At an average solar intensity of ≈920 W m−2, it is on average 6.8 °C below ambient temperature during the day and theoretically yields a radiative cooling power of 88.9 W m−2. Furthermore, the film exhibits excellent hydrophobicity, superior flexibility, and robust mechanical strength, providing an attractive and viable pathway for practical applications addressing the pressing challenges of climate and energy issues.
- 26 December 2023
- Published by Wiley in Small Methods
- Vol. 8 (7) , e2301258
Scalable and Flexible Multi‐Layer Prismatic Photonic Metamaterial Film for Efficient Daytime Radiative Cooling
To maintain a comfortable indoor living environment in low latitude or tropical regions, humans consume significant amounts of electrical energy in air conditioning, leading to substantial CO2 emissions. Passive daytime radiative cooling (PDRC) allows objects to cool down during the daytime without any energy consumption by dissipating heat through the atmospheric transparency window (8−13 µm) to outer space, which has garnered significant attention. However, the practical applications of common PDRC materials are hindered by their poor optical selectivity and high‐reflective silver backing. Additionally, the availability of artificial photon emitters with complex structures and excellent performance is also limited by their high cost. Herein, a novel multilayer prismatic photonic metamaterial film without any silver reflector, easily scalable and produced by a roll‐to‐roll method is demonstrated, which exhibits ≈96.4% sunlight reflectance (0.3−2.5 µm) and ≈97.2% emissivity in mid‐infrared (IR) (8−13 µm). At an average solar intensity of ≈920 W m−2, it is on average 6.8 °C below ambient temperature during the day and theoretically yields a radiative cooling power of 88.9 W m−2. Furthermore, the film exhibits excellent hydrophobicity, superior flexibility, and robust mechanical strength, providing an attractive and viable pathway for practical applications addressing the pressing challenges of climate and energy issues.
- Open Access
Preparation of Densified Fine-Grain High-Frequency MnZn Ferrite Using the Cold Sintering Process
The densified MnZn ferrite ceramics were prepared using the cold sintering process under pressure, with an acetate ethanol solution used as the transient solvent. The effects of the transient solvent, the pressure and annealing temperature on the density, and the micromorphology and magnetic properties of the sintered MnZn ferrites were studied. The densified MnZn ferrite was obtained using the cold sintering process and its relative density reached up to 85.4%. The transient solvent and high pressure are essential to the cold sintering process for MnZn ferrite. The annealing treatment is indispensable in obtaining the sample with the higher density. The relative density was further increased to 97.2% for the sample annealed at 950 °C for 6 h. The increase in the annealing temperature reduces the power loss at high frequencies.
Open AccessPreparation of Densified Fine-Grain High-Frequency MnZn Ferrite Using the Cold Sintering Process
The densified MnZn ferrite ceramics were prepared using the cold sintering process under pressure, with an acetate ethanol solution used as the transient solvent. The effects of the transient solvent, the pressure and annealing temperature on the density, and the micromorphology and magnetic properties of the sintered MnZn ferrites were studied. The densified MnZn ferrite was obtained using the cold sintering process and its relative density reached up to 85.4%. The transient solvent and high pressure are essential to the cold sintering process for MnZn ferrite. The annealing treatment is indispensable in obtaining the sample with the higher density. The relative density was further increased to 97.2% for the sample annealed at 950 °C for 6 h. The increase in the annealing temperature reduces the power loss at high frequencies.
- Open Access
Low Core Losses of Fe-Based Soft Magnetic Composites with an Zn-O-Si Insulating Layer Obtained by Coupling Synergistic Photodecomposition
The major method used to reduce the magnetic loss of soft magnetic composites (SMCs) is to coat the magnetic powder with an insulating layer, but the permeability is usually sacrificed in the process. In order to achieve a better balance between low losses and high permeability, a novel photodecomposition method was used in this study to create a ZnO insulating layer. The effect of the concentration of diethyl zinc on the formation of a ZnO insulating film by photodecomposition was studied. The ZnO film was best formed with a diethyl zinc n-hexane solution at a concentration of around 0.40 mol/L. Combined with conventional coupling treatment processes, a thin and dense insulating layer was coated on the surface of iron powder in situ. Treating the iron powder before coating by photodecomposition led to a synergistic effect, significantly reduced core loss, and the effective permeability only decreased slightly. An iron-based soft magnetic composite with a loss value of 124 kW/m3 and an effective permeability of 107 was obtained at the frequency of 100 kHz and a magnetic field intensity of 20 mT.
Open AccessLow Core Losses of Fe-Based Soft Magnetic Composites with an Zn-O-Si Insulating Layer Obtained by Coupling Synergistic Photodecomposition
The major method used to reduce the magnetic loss of soft magnetic composites (SMCs) is to coat the magnetic powder with an insulating layer, but the permeability is usually sacrificed in the process. In order to achieve a better balance between low losses and high permeability, a novel photodecomposition method was used in this study to create a ZnO insulating layer. The effect of the concentration of diethyl zinc on the formation of a ZnO insulating film by photodecomposition was studied. The ZnO film was best formed with a diethyl zinc n-hexane solution at a concentration of around 0.40 mol/L. Combined with conventional coupling treatment processes, a thin and dense insulating layer was coated on the surface of iron powder in situ. Treating the iron powder before coating by photodecomposition led to a synergistic effect, significantly reduced core loss, and the effective permeability only decreased slightly. An iron-based soft magnetic composite with a loss value of 124 kW/m3 and an effective permeability of 107 was obtained at the frequency of 100 kHz and a magnetic field intensity of 20 mT.
- Open Access
- 7 November 2022
- Published by MDPI AG in Magnetochemistry
- Vol. 8 (11) , 149
Magnetic Properties and Microstructure of Ce-Cu-Al Low Melting Alloy Bonding Sm2Fe17N3 Magnet Fabricated by the Hot-Pressing Method
Sm2Fe17N3 compounds, having excellent intrinsic magnetic properties, are prone to decomposition at high temperatures; thus, a low melting point metal binder is the key to prepare high performance bulk magnets at low temperatures. In this paper, a new low melting point alloy Ce72Cu28-xAlx was used as the binders, and high-performance Ce-based alloy bonding Sm2Fe17N3 magnets were realized by the hot-pressing method. The experimental results demonstrated that the content of Al in the Ce-based alloys had an important influence on the performance of the magnets. High performance Sm-Fe-N bonded magnets with remanence of 10.19 KGs and maximum magnetic energy product of 21.06 MGOe were achieved by using 5 wt.% Ce72Cu22Al6 alloy as a binder. At the same time, it was found that the Ce72Cu28-xAlx alloy has a lower density and better bonding effect than the common Zn binder. Its bonding magnets still have higher performance even with extremely high oxygen content. Therefore, Ce72Cu28-xAlx alloy with low melting point is a promising new rare earth-based alloy binder. If the oxygen content of the alloy powders could be reduced, higher performance Sm2Fe17N3 bonded magnets can be prepared.
- 7 November 2022
- Published by MDPI AG in Magnetochemistry
- Vol. 8 (11) , 149
Open AccessMagnetic Properties and Microstructure of Ce-Cu-Al Low Melting Alloy Bonding Sm2Fe17N3 Magnet Fabricated by the Hot-Pressing Method
Sm2Fe17N3 compounds, having excellent intrinsic magnetic properties, are prone to decomposition at high temperatures; thus, a low melting point metal binder is the key to prepare high performance bulk magnets at low temperatures. In this paper, a new low melting point alloy Ce72Cu28-xAlx was used as the binders, and high-performance Ce-based alloy bonding Sm2Fe17N3 magnets were realized by the hot-pressing method. The experimental results demonstrated that the content of Al in the Ce-based alloys had an important influence on the performance of the magnets. High performance Sm-Fe-N bonded magnets with remanence of 10.19 KGs and maximum magnetic energy product of 21.06 MGOe were achieved by using 5 wt.% Ce72Cu22Al6 alloy as a binder. At the same time, it was found that the Ce72Cu28-xAlx alloy has a lower density and better bonding effect than the common Zn binder. Its bonding magnets still have higher performance even with extremely high oxygen content. Therefore, Ce72Cu28-xAlx alloy with low melting point is a promising new rare earth-based alloy binder. If the oxygen content of the alloy powders could be reduced, higher performance Sm2Fe17N3 bonded magnets can be prepared.
- Open Access
Injection Molding and Sintering of ZrO2 Ceramic Powder Modified by a Zirconate Coupling Agent
Ceramic injection molding is a near-net shape-processing technique, producing ceramic components with low tooling costs and complex shapes. In this paper, ZrO2 ceramics with high loading content in the green part were prepared by powder modification using zirconate coupling agent, injection molding and sintering, which benefited decreasing the usage of binders and deformation of ceramics. The rheological characteristics of feedstocks, densities, microstructures and mechanical properties of green and sintered parts with the different coupling media and sintering temperatures were studied. The results showed that the addition of a zirconate coupling agent with ethanol medium obviously increased the flowability of feedstocks and benefited achieving the green parts with high powder loading (86.5 wt.%) and bending strength (12.9 MPa) and the final unbroken ceramics. In addition, the sintering temperatures from 1500–1575 °C had no significant effects on the density, hardness, and surface morphology of the ceramic samples. However, the bending strength increased and some large grains with transgranular fracture occurred on the fractural surface at the sintering temperature of 1575 °C.
Open AccessInjection Molding and Sintering of ZrO2 Ceramic Powder Modified by a Zirconate Coupling Agent
Ceramic injection molding is a near-net shape-processing technique, producing ceramic components with low tooling costs and complex shapes. In this paper, ZrO2 ceramics with high loading content in the green part were prepared by powder modification using zirconate coupling agent, injection molding and sintering, which benefited decreasing the usage of binders and deformation of ceramics. The rheological characteristics of feedstocks, densities, microstructures and mechanical properties of green and sintered parts with the different coupling media and sintering temperatures were studied. The results showed that the addition of a zirconate coupling agent with ethanol medium obviously increased the flowability of feedstocks and benefited achieving the green parts with high powder loading (86.5 wt.%) and bending strength (12.9 MPa) and the final unbroken ceramics. In addition, the sintering temperatures from 1500–1575 °C had no significant effects on the density, hardness, and surface morphology of the ceramic samples. However, the bending strength increased and some large grains with transgranular fracture occurred on the fractural surface at the sintering temperature of 1575 °C.
- 18 July 2022
- Published by Springer Nature in Journal of Materials Science
- Vol. 57 (28) , 13481-13495
Monomolecular cross-linked highly dense cubic FeCo nanocomposite for high-frequency application
- 18 July 2022
- Published by Springer Nature in Journal of Materials Science
- Vol. 57 (28) , 13481-13495
Monomolecular cross-linked highly dense cubic FeCo nanocomposite for high-frequency application
- Open Access
Carbothermal Reduction Synthesis of Aluminum Nitride from Al(OH)3/C/PVB Slurries Prepared by Three-Roll Mixing
Polyvinyl butyral (PVB) was used in the Al(OH)3/carbon black/ethanol slurries by the three-roll mixing to prepare AlN powder using the carbothermal reduction–nitridation (CRN) process in the experiments. The effects of PVB addition on the synthesis of AlN powder were studied by viscosity, tap density, XRD, SEM and TG measurements. The results showed that the PVB layer covering on the surface of Al(OH)3 particles reduced the viscosity of Al(OH)3/carbon/ethanol slurry and increased the dispersion homogeneity of Al(OH)3/carbon raw powder. The tap densities of the Al(OH)3/carbon mixtures after three-roll milling could be increased with the increase in PVB addition. In the CRN process, most of the PVB covering Al(OH)3 particles evaporated and supplied the passage for nitrogen removal to the particles. Based on the experimental data, the role of PVB on the mixing and CRN process was discussed.
Open AccessCarbothermal Reduction Synthesis of Aluminum Nitride from Al(OH)3/C/PVB Slurries Prepared by Three-Roll Mixing
Polyvinyl butyral (PVB) was used in the Al(OH)3/carbon black/ethanol slurries by the three-roll mixing to prepare AlN powder using the carbothermal reduction–nitridation (CRN) process in the experiments. The effects of PVB addition on the synthesis of AlN powder were studied by viscosity, tap density, XRD, SEM and TG measurements. The results showed that the PVB layer covering on the surface of Al(OH)3 particles reduced the viscosity of Al(OH)3/carbon/ethanol slurry and increased the dispersion homogeneity of Al(OH)3/carbon raw powder. The tap densities of the Al(OH)3/carbon mixtures after three-roll milling could be increased with the increase in PVB addition. In the CRN process, most of the PVB covering Al(OH)3 particles evaporated and supplied the passage for nitrogen removal to the particles. Based on the experimental data, the role of PVB on the mixing and CRN process was discussed.
- 28 July 2020
- Published by Springer Nature in Journal of Superconductivity and Novel Magnetism
- Vol. 33 (11) , 3563-3570
Preparation, Microstructure, and Magnetic Properties of Electrodeposited Nanocrystalline L10 FePt Films
- 28 July 2020
- Published by Springer Nature in Journal of Superconductivity and Novel Magnetism
- Vol. 33 (11) , 3563-3570
Preparation, Microstructure, and Magnetic Properties of Electrodeposited Nanocrystalline L10 FePt Films
- Open Access
- 1 May 2020
- Published by AIP Publishing in AIP Advances
- Vol. 10 (5) , 055119
Preparation of submicron-sized Sm2Fe17N3 fine powder by ultrasonic spray pyrolysis-hydrogen reduction (USP-HR) and subsequent reduction–diffusion process
A new reduction–diffusion method for preparing submicron-sized Sm2Fe17N3 was developed. First, submicron-sized α-Fe/Sm2O3 composite precursors with good dispersibility were prepared directly by ultrasonic spray pyrolysis and hydrogen reduction (USP-HR). Then, the precursor was successfully converted into Sm2Fe17N3 powder by Ca reduction–diffusion and nitridation. The results displayed that the precursor prepared by USP-HR was a monodisperse homogeneous composite of spherical particles of α-Fe and Sm2O3. α-Fe and Sm2O3 exist in an intercalated structure in the composite spherical particles. This creates conditions for the preparation of ultrafine Sm2Fe17N3 particles with uniform sizes and dispersity. The results show that Sm2Fe17N3 is a single-phase, composed of submicron-sized particles with no other impurity phases. The physical property measurement system shows that the coercivity of 0.616 ± 0.347 µm particles reaches 14.7 kOe.
- 1 May 2020
- Published by AIP Publishing in AIP Advances
- Vol. 10 (5) , 055119
Open AccessPreparation of submicron-sized Sm2Fe17N3 fine powder by ultrasonic spray pyrolysis-hydrogen reduction (USP-HR) and subsequent reduction–diffusion process
A new reduction–diffusion method for preparing submicron-sized Sm2Fe17N3 was developed. First, submicron-sized α-Fe/Sm2O3 composite precursors with good dispersibility were prepared directly by ultrasonic spray pyrolysis and hydrogen reduction (USP-HR). Then, the precursor was successfully converted into Sm2Fe17N3 powder by Ca reduction–diffusion and nitridation. The results displayed that the precursor prepared by USP-HR was a monodisperse homogeneous composite of spherical particles of α-Fe and Sm2O3. α-Fe and Sm2O3 exist in an intercalated structure in the composite spherical particles. This creates conditions for the preparation of ultrafine Sm2Fe17N3 particles with uniform sizes and dispersity. The results show that Sm2Fe17N3 is a single-phase, composed of submicron-sized particles with no other impurity phases. The physical property measurement system shows that the coercivity of 0.616 ± 0.347 µm particles reaches 14.7 kOe.