Qi Jiao
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Research Interests
Qi Jiao has a total of 6 co-authors. Here are the top co-authors by number of shared publications:
- Dongsheng Wang
Science and Technology on Advanced High Temperature Structural Materials Laboratory, Beijing Institute of Aeronautical Materials, Beijing 100095, China
1 shared publication - Jie Li
School of Materials Science & Engineering, Chang’an University, Xi’an 710061, China
1 shared publication - Shuxin Niu
Science and Technology on Advanced High Temperature Structural Materials Laboratory, Beijing Institute of Aeronautical Materials, Beijing 100095, China
1 shared publication - Xin Li
Science and Technology on Advanced High Temperature Structural Materials Laboratory, Beijing Institute of Aeronautical Materials, Beijing 100095, China
1 shared publication - Xinlong Guo
Science and Technology on Advanced High Temperature Structural Materials Laboratory, Beijing Institute of Aeronautical Materials, Beijing 100095, China
1 shared publication - Xiqing Xu
School of Materials Science and Engineering, Chang’an University, Xi’an 710061, China
1 shared publication
Latest Publications
- Open Access
Microstructure and Crystallization Kinetics of Silica-Based Ceramic Cores with Enhanced High-Temperature Property
Silica-based ceramic cores play key roles in the casting of aeroengine blades, but they are highly limited by the poor high-temperature mechanical property. Here, fused mullite (FM) and sintered mullite (SM) powders were modified in silica-based ceramic cores, and the microstructure evolution and crystallization kinetics of ceramic cores depending on mullite types were studied. The ceramic cores with FM showed a dense microstructure and superior mechanical properties compared to those with SM. The ceramic cores with 10 wt.% of FM showed a crystallization activation energy of 1119.5 kJ/mol and a crystallization exponent of 1.74, and the values of 938.4 kJ/mol and 1.86 as SM were employed; the decreased crystallization activation energy and the elevated crystallization exponent by SM suggested that the excess impurities of alkali oxides and alkaline-earth oxides significantly promoted the crystallization of cristobalite. Even though the ceramic cores with mullite powders decreased slightly in the room-temperature mechanical property, their high-temperature flexure strength and creep deformation resistance were enhanced. The ceramic cores with 10 wt.% of FM showed excellent comprehensive performance, with linear shrinkage of 0.69%, room-temperature strength of 18.9 MPa, and high-temperature strength of 15.5 MPa, which satisfied the demands for hollow-blade casting.
Open AccessMicrostructure and Crystallization Kinetics of Silica-Based Ceramic Cores with Enhanced High-Temperature Property
Silica-based ceramic cores play key roles in the casting of aeroengine blades, but they are highly limited by the poor high-temperature mechanical property. Here, fused mullite (FM) and sintered mullite (SM) powders were modified in silica-based ceramic cores, and the microstructure evolution and crystallization kinetics of ceramic cores depending on mullite types were studied. The ceramic cores with FM showed a dense microstructure and superior mechanical properties compared to those with SM. The ceramic cores with 10 wt.% of FM showed a crystallization activation energy of 1119.5 kJ/mol and a crystallization exponent of 1.74, and the values of 938.4 kJ/mol and 1.86 as SM were employed; the decreased crystallization activation energy and the elevated crystallization exponent by SM suggested that the excess impurities of alkali oxides and alkaline-earth oxides significantly promoted the crystallization of cristobalite. Even though the ceramic cores with mullite powders decreased slightly in the room-temperature mechanical property, their high-temperature flexure strength and creep deformation resistance were enhanced. The ceramic cores with 10 wt.% of FM showed excellent comprehensive performance, with linear shrinkage of 0.69%, room-temperature strength of 18.9 MPa, and high-temperature strength of 15.5 MPa, which satisfied the demands for hollow-blade casting.