Stelian Stan
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Stelian Stan has a total of 38 co-authors. Here are the top co-authors by number of shared publications:
- Iulian Riposan
Materials Science and Engineering Faculty, National University of Science and Technology Politehnica Bucharest, 060042 Bucharest, Romania
19 shared publications - Iuliana Stan
Materials Science and Engineering Faculty, National University of Science and Technology Politehnica Bucharest, 060042 Bucharest, Romania
11 shared publications - Denisa Anca
Materials Science and Engineering Faculty, National University of Science and Technology Politehnica Bucharest, 060042 Bucharest, Romania
9 shared publications - Mihai Chisamera
Materials Science and Engineering Faculty, National University of Science and Technology Politehnica Bucharest, 060042 Bucharest, Romania
8 shared publications - Eduard Stefan
Materials Science and Engineering Faculty, National University of Science and Technology POLITEHNICA Bucharest, 313 Splaiul Independentei, Sector 6, 060042 Bucharest, Romania
3 shared publications Mihai Chisamera
Politehnica University of Bucharest, Bucharest, Romania
3 shared publications
Latest Publications
- Open Access
Solidification Patterns of Ductile and Grey Cast Irons Produced from the Same Base Iron Melt: Thermal (Cooling-Curve) Analysis
The cast iron foundry industry has undergone important changes in melting operations, with induction furnaces becoming a major source of molten iron. In many foundries, grey (GI) and ductile (DI) irons are produced simultaneously, including from the same base iron prepared in the same melting furnace. The response of a common base iron to the specific metallurgical treatments required for GI and DI production may differ and can be evaluated by thermal (cooling curve) analysis (TCCA). Experiments were conducted to evaluate, by TCCA, the effects of inoculation on near-eutectic DI (4.10–4.15% CE) and medium-strength GI (3.7–3.8% CE) produced from the same base iron melts, with a limited Mn content and less than 0.02% S. Based on the average values from four melts, inoculation decreased the austenite liquidus temperature by 7.2 °C in DI and 1.8 °C in GI, increased the eutectic undercooling temperature by 16 °C in DI and 2.2 °C in GI, and produced a substantially larger increase in the end-of-solidification temperature in DI. Eutectic recalescence increased by approximately 72% in both irons, while the first-derivative minimum at the end of solidification became more negative after inoculation. The results indicate that the common base iron is suitable for DI production under the specified compositional constraints for ferritic–pearlitic and pearlitic matrices. In contrast, the high degree of undercooling during solidification of the resulting GI increased susceptibility to free-carbide formation and undercooled graphite. Under the present conditions, inoculation had only a limited ability to reduce undercooling during the eutectic reaction and at the end of solidification and to promote sufficient graphitization in GI. Based on previous research on low-sulphur GI, possible improvements are recommended, including stronger inoculation, preconditioning with oxide-forming elements, a more effective inoculation technique, and/or improved graphite nucleation through an increase in the (%Mn) × (%S) factor.
Open AccessSolidification Patterns of Ductile and Grey Cast Irons Produced from the Same Base Iron Melt: Thermal (Cooling-Curve) Analysis
The cast iron foundry industry has undergone important changes in melting operations, with induction furnaces becoming a major source of molten iron. In many foundries, grey (GI) and ductile (DI) irons are produced simultaneously, including from the same base iron prepared in the same melting furnace. The response of a common base iron to the specific metallurgical treatments required for GI and DI production may differ and can be evaluated by thermal (cooling curve) analysis (TCCA). Experiments were conducted to evaluate, by TCCA, the effects of inoculation on near-eutectic DI (4.10–4.15% CE) and medium-strength GI (3.7–3.8% CE) produced from the same base iron melts, with a limited Mn content and less than 0.02% S. Based on the average values from four melts, inoculation decreased the austenite liquidus temperature by 7.2 °C in DI and 1.8 °C in GI, increased the eutectic undercooling temperature by 16 °C in DI and 2.2 °C in GI, and produced a substantially larger increase in the end-of-solidification temperature in DI. Eutectic recalescence increased by approximately 72% in both irons, while the first-derivative minimum at the end of solidification became more negative after inoculation. The results indicate that the common base iron is suitable for DI production under the specified compositional constraints for ferritic–pearlitic and pearlitic matrices. In contrast, the high degree of undercooling during solidification of the resulting GI increased susceptibility to free-carbide formation and undercooled graphite. Under the present conditions, inoculation had only a limited ability to reduce undercooling during the eutectic reaction and at the end of solidification and to promote sufficient graphitization in GI. Based on previous research on low-sulphur GI, possible improvements are recommended, including stronger inoculation, preconditioning with oxide-forming elements, a more effective inoculation technique, and/or improved graphite nucleation through an increase in the (%Mn) × (%S) factor.
- Open Access
- 29 September 2026
- Published by MDPI AG in Sustainability
- Vol. 18 (19) , 9947
From Risk Assessment to Sustainable Supply-Chain Resilience: Evaluating EU Rare-Earth Policy Outcomes, 2011–2023
Rare-earth elements (REEs) constrain the deployment of wind generation and electric mobility, on which EU climate targets depend. The EU accordingly developed five criticality assessments between 2011 and 2023, led by the European Commission’s DG GROW and supported by JRC methodological work. This article asks whether assessment capacity has been converted into industrial capacity. Combining EU, USGS and IEA indicators with documented capacity evidence, we classify each assessment cycle on two ordinal scales: policy response and structural outcome, interpreted separately. Exposure remained high: China’s share of global REE processing stayed within an 87–95% band, the end-of-life recycling input rate remained below 1%, and EU separation, magnet production and recycling capacity showed no sustained net expansion during the paired period. Between 2011 and 2020, policy responses became more formalised, while an early recycling-capacity gain was reversed, and no sustained structural improvement remained. The 2023 cycle is reported on the response side only, while 2024–2025 developments are treated as a post-period update. Japan, an illustrative contrast, absorbed the same 2010 shock under a different policy configuration. The EU case indicates an implementation constraint rather than a knowledge deficit, bearing directly on the feasibility of EU climate and circular-economy targets.
- 29 September 2026
- Published by MDPI AG in Sustainability
- Vol. 18 (19) , 9947
Open AccessFrom Risk Assessment to Sustainable Supply-Chain Resilience: Evaluating EU Rare-Earth Policy Outcomes, 2011–2023
Rare-earth elements (REEs) constrain the deployment of wind generation and electric mobility, on which EU climate targets depend. The EU accordingly developed five criticality assessments between 2011 and 2023, led by the European Commission’s DG GROW and supported by JRC methodological work. This article asks whether assessment capacity has been converted into industrial capacity. Combining EU, USGS and IEA indicators with documented capacity evidence, we classify each assessment cycle on two ordinal scales: policy response and structural outcome, interpreted separately. Exposure remained high: China’s share of global REE processing stayed within an 87–95% band, the end-of-life recycling input rate remained below 1%, and EU separation, magnet production and recycling capacity showed no sustained net expansion during the paired period. Between 2011 and 2020, policy responses became more formalised, while an early recycling-capacity gain was reversed, and no sustained structural improvement remained. The 2023 cycle is reported on the response side only, while 2024–2025 developments are treated as a post-period update. Japan, an illustrative contrast, absorbed the same 2010 shock under a different policy configuration. The EU case indicates an implementation constraint rather than a knowledge deficit, bearing directly on the feasibility of EU climate and circular-economy targets.
- Open Access
- 14 August 2026
- Published by MDPI AG in Applied Sciences
- Vol. 16 (16) , 8101
Influence of Bimodal Pore Architecture on Broadband Acoustic Absorption and Mass Reduction in AlSi Open-Cell Structures
Lightweight materials capable of simultaneously providing noise and mass reduction are increasingly required in aerospace applications. This paper investigates the acoustic performance of a novel hierarchical bimodal architecture in open-cell AlSi porous structures, integrating μm-sized macro-pores (200–400 μm) and mm-sized macro-pores (2–2.5 mm) at 60% porosity. The bimodal specimen was produced through replication casting, and its porosity was evaluated using gravimetric measurements and image-based surface analysis, while acoustic performance was experimentally characterized using the two-microphone impedance tube method in accordance with ISO 10534-2:2023, covering a frequency range from 500 to 6500 Hz. The resulting frequency-averaged sound absorption coefficients (αFA) were 0.518, 0.72 and 0.844 for the μm-sized macro-porous, mm-sized macro-porous and bimodal structures, respectively. Furthermore, the proposed architecture improved the mass-to-acoustic efficiency ratio η by 125% compared to the μm-sized macro-pores structure and approximately 28.5% relative to the mm-sized macro-pore sample. Based on these values, bimodal architecture is considered to be the most acoustic efficient lightweight solution, among all specimens studied, demonstrating that hierarchical pore architectures can effectively enhance acoustic absorption, while maintaining low structural weight, highlighting the potential of bimodal open-cell AlSi structures for lightweight aerospace noise-control applications.
- 14 August 2026
- Published by MDPI AG in Applied Sciences
- Vol. 16 (16) , 8101
Open AccessInfluence of Bimodal Pore Architecture on Broadband Acoustic Absorption and Mass Reduction in AlSi Open-Cell Structures
Lightweight materials capable of simultaneously providing noise and mass reduction are increasingly required in aerospace applications. This paper investigates the acoustic performance of a novel hierarchical bimodal architecture in open-cell AlSi porous structures, integrating μm-sized macro-pores (200–400 μm) and mm-sized macro-pores (2–2.5 mm) at 60% porosity. The bimodal specimen was produced through replication casting, and its porosity was evaluated using gravimetric measurements and image-based surface analysis, while acoustic performance was experimentally characterized using the two-microphone impedance tube method in accordance with ISO 10534-2:2023, covering a frequency range from 500 to 6500 Hz. The resulting frequency-averaged sound absorption coefficients (αFA) were 0.518, 0.72 and 0.844 for the μm-sized macro-porous, mm-sized macro-porous and bimodal structures, respectively. Furthermore, the proposed architecture improved the mass-to-acoustic efficiency ratio η by 125% compared to the μm-sized macro-pores structure and approximately 28.5% relative to the mm-sized macro-pore sample. Based on these values, bimodal architecture is considered to be the most acoustic efficient lightweight solution, among all specimens studied, demonstrating that hierarchical pore architectures can effectively enhance acoustic absorption, while maintaining low structural weight, highlighting the potential of bimodal open-cell AlSi structures for lightweight aerospace noise-control applications.
- Open Access
Slightly Irregular Spheroidal Graphite (Type-V, ISO): Typical Graphite Morphology for High-Si/SiMo Ductile Cast Irons
The present paper reviews original data obtained by the authors from recent separate publications with additional unpublished data, specifically concerning the specific graphite morphology in Si/SiMo alloyed ductile irons (2.5–5.5% Si, 0.01–2.3% Mo) with alloying grade, cooling rate, and inoculation as influencing factors. Different formulas used for nodularity evaluation, including different forms of graphite participating in different proportion and two graphite shape factors: Roundness (RSF, involving maximum Ferret) and Sphericity (SSF, involving real perimeter). Slightly irregular spheroidal graphite morphology (Form V, ISO 945) characterized by RSF = 0.59–0.75 was found to be typical for Si and SiMo ductile irons in all of the test conditions, such as Si level (4.2–5.25% Si), Si–Mo system (4.1–4.8% Si + 1.6–2.3% Mo), mould type (green sand, resin sand, metal mould, external metallic chill), un-inoculation and inoculation, and inoculating element type. Increasing Si content negatively affects the compactness degree of spheroidal graphite particles (transition from VI to V form) and nodularity. Metal mould versus sand mould solidification of 4.5% Si ductile iron increases nodule count, graphite shape factors (RSF = 0.68–0.7 versus 0.59–0.64) and nodularity (67% to 76%). An external metallic chill in a resin sand mould promoted directional solidification and showed a nodularity decrease for increasing Si, for all the nodularity formulas and for the cooling rate range. Inoculating elements influenced the shape factors in thin wall castings, where Ca–Ba was better than simple Ca and Ca–RE could promote graphite at higher real perimeter and with lower shape factors. The correlation of the aspect of structure, graphite parameters and nodularity led to the conclusion that the nodularity formula according to ISO/WD 945-4-2015 (100% total area of Form VI and 90% of Form V), with SSF instead of RSF, appears to be better in High-Si/SiMo DI (especially for more than 4% Si), because it takes into account the presence of slightly irregular spheroidal graphite (with high real perimeter) at a high rate.
Open AccessSlightly Irregular Spheroidal Graphite (Type-V, ISO): Typical Graphite Morphology for High-Si/SiMo Ductile Cast Irons
The present paper reviews original data obtained by the authors from recent separate publications with additional unpublished data, specifically concerning the specific graphite morphology in Si/SiMo alloyed ductile irons (2.5–5.5% Si, 0.01–2.3% Mo) with alloying grade, cooling rate, and inoculation as influencing factors. Different formulas used for nodularity evaluation, including different forms of graphite participating in different proportion and two graphite shape factors: Roundness (RSF, involving maximum Ferret) and Sphericity (SSF, involving real perimeter). Slightly irregular spheroidal graphite morphology (Form V, ISO 945) characterized by RSF = 0.59–0.75 was found to be typical for Si and SiMo ductile irons in all of the test conditions, such as Si level (4.2–5.25% Si), Si–Mo system (4.1–4.8% Si + 1.6–2.3% Mo), mould type (green sand, resin sand, metal mould, external metallic chill), un-inoculation and inoculation, and inoculating element type. Increasing Si content negatively affects the compactness degree of spheroidal graphite particles (transition from VI to V form) and nodularity. Metal mould versus sand mould solidification of 4.5% Si ductile iron increases nodule count, graphite shape factors (RSF = 0.68–0.7 versus 0.59–0.64) and nodularity (67% to 76%). An external metallic chill in a resin sand mould promoted directional solidification and showed a nodularity decrease for increasing Si, for all the nodularity formulas and for the cooling rate range. Inoculating elements influenced the shape factors in thin wall castings, where Ca–Ba was better than simple Ca and Ca–RE could promote graphite at higher real perimeter and with lower shape factors. The correlation of the aspect of structure, graphite parameters and nodularity led to the conclusion that the nodularity formula according to ISO/WD 945-4-2015 (100% total area of Form VI and 90% of Form V), with SSF instead of RSF, appears to be better in High-Si/SiMo DI (especially for more than 4% Si), because it takes into account the presence of slightly irregular spheroidal graphite (with high real perimeter) at a high rate.
- Open Access
Influence of Pore Size on the Acoustic Absorption Properties of Open-Cell AlSi Porous Cylinders
Airframe noise generated at wing trailing edges and high-lift devices, such as flaps, remains a major challenge during landing, with significant contributions in the low-frequency band of 500–1500 Hz. While solid surfaces reflect this acoustic energy, metallic porous materials can effectively absorb it through viscous and thermal dissipation within their internal pore structure. To address this, the present study examines the acoustic absorption characteristics of open-cell AlSi porous cylinders featuring controlled pore diameters between 0.3 mm and 2.25 mm. Measurements were conducted in an acoustic impedance tube according to the ISO 10534-2:2023 standard, using six cylindrical samples (28 mm diameter, 70 mm length). Two sets of measurements were performed for each sample (front and rear faces), and the average values were used. The findings indicate that the normal-incidence sound absorption coefficient α rises as pore size increases, reaching 0.93–0.97 at low frequencies of 500–700 Hz for the samples with the largest pores (1.8–2.25 mm). These results indicate that open-cell AlSi alloys offer strong low-frequencies sound absorption, positioning them as promising options for aeroacoustic noise mitigation, including applications such as porous trailing edge and hybrid flap designs.
Open AccessInfluence of Pore Size on the Acoustic Absorption Properties of Open-Cell AlSi Porous Cylinders
Airframe noise generated at wing trailing edges and high-lift devices, such as flaps, remains a major challenge during landing, with significant contributions in the low-frequency band of 500–1500 Hz. While solid surfaces reflect this acoustic energy, metallic porous materials can effectively absorb it through viscous and thermal dissipation within their internal pore structure. To address this, the present study examines the acoustic absorption characteristics of open-cell AlSi porous cylinders featuring controlled pore diameters between 0.3 mm and 2.25 mm. Measurements were conducted in an acoustic impedance tube according to the ISO 10534-2:2023 standard, using six cylindrical samples (28 mm diameter, 70 mm length). Two sets of measurements were performed for each sample (front and rear faces), and the average values were used. The findings indicate that the normal-incidence sound absorption coefficient α rises as pore size increases, reaching 0.93–0.97 at low frequencies of 500–700 Hz for the samples with the largest pores (1.8–2.25 mm). These results indicate that open-cell AlSi alloys offer strong low-frequencies sound absorption, positioning them as promising options for aeroacoustic noise mitigation, including applications such as porous trailing edge and hybrid flap designs.
- 7 January 2023
- Published by Springer Nature in International Journal of Metalcasting
- Vol. 17 (4) , 2389-2412
Structure Characteristics of High-Si Ductile Cast Irons
- 7 January 2023
- Published by Springer Nature in International Journal of Metalcasting
- Vol. 17 (4) , 2389-2412
Structure Characteristics of High-Si Ductile Cast Irons
- 28 December 2022
- Published by Springer Nature in Journal of Thermal Analysis and Calorimetry
- Vol. 148 (5) , 1805-1817
Solidification pattern of 4.5%Si ductile iron in metal mould versus sand mould castings
- 28 December 2022
- Published by Springer Nature in Journal of Thermal Analysis and Calorimetry
- Vol. 148 (5) , 1805-1817
Solidification pattern of 4.5%Si ductile iron in metal mould versus sand mould castings
- Open Access
Graphite Nodularity Evaluation in High-Si Ductile Cast Irons
Ferritic high-Si ductile cast irons replace an unstable mixed ferrite-pearlite matrix with a unique combination of high elongation, strength and hardness (ideal for automotive drive train components) and resistance to oxidation and corrosion at high temperatures (automotive exhaust and turbocharger systems). The present paper analyses the graphite parameters of 4.5%Si, un-inoculated ductile cast iron (4.7%CE, 0.035%Mgres) as an effect of the casting section size. The structure is characterized by 10.5–11.2% graphite and 464–975 nodules/mm2, at more than 70% ferrite and no carbides, including at 3 mm wall thickness. The lower the wall thickness is, the higher the nodule count is and, consequently, the higher the ferrite amount is. The Roundness Graphite Shape Factor (RSF = 0.65–0.68) illustrates the presence of Slightly Irregular Spheroidal Graphite (Form V ISO 945). There is a big difference between the graphite nodularity evaluated according to ISO 16112:2017 [CGI] (NG1 = 79–86%) and according to ISO 945-4-2019 (DI) (NG2 = 65.2–74.6%), both of them based on RSF. Graphite Nodularity (NG3), calculated with the ISO 945-4-2019 [DI] formula, but replacing RSF with SSF, Sphericity Graphite Shape Factor, has an intermediary position. The higher the imposed minimum RSF or SSF is, the lower the Graphite Nodularity (NG4, NG5): 80–90% for min. 0.50 (minimum Form IV or Intermediate Graphite), 60–80% for min. 0.60–0.65 (minimum Form V graphite) and 35–70% for min. 0.80 (minimum Form VI graphite). The SSF is more representative than the RSF for Si-alloyed ductile cast iron, so it is recommended to use a graphite nodularity calculus considering SSF instead of the RSF formula (stipulated by ISO 945-4-2019), with SSF replacing RSF.
Open AccessGraphite Nodularity Evaluation in High-Si Ductile Cast Irons
Ferritic high-Si ductile cast irons replace an unstable mixed ferrite-pearlite matrix with a unique combination of high elongation, strength and hardness (ideal for automotive drive train components) and resistance to oxidation and corrosion at high temperatures (automotive exhaust and turbocharger systems). The present paper analyses the graphite parameters of 4.5%Si, un-inoculated ductile cast iron (4.7%CE, 0.035%Mgres) as an effect of the casting section size. The structure is characterized by 10.5–11.2% graphite and 464–975 nodules/mm2, at more than 70% ferrite and no carbides, including at 3 mm wall thickness. The lower the wall thickness is, the higher the nodule count is and, consequently, the higher the ferrite amount is. The Roundness Graphite Shape Factor (RSF = 0.65–0.68) illustrates the presence of Slightly Irregular Spheroidal Graphite (Form V ISO 945). There is a big difference between the graphite nodularity evaluated according to ISO 16112:2017 [CGI] (NG1 = 79–86%) and according to ISO 945-4-2019 (DI) (NG2 = 65.2–74.6%), both of them based on RSF. Graphite Nodularity (NG3), calculated with the ISO 945-4-2019 [DI] formula, but replacing RSF with SSF, Sphericity Graphite Shape Factor, has an intermediary position. The higher the imposed minimum RSF or SSF is, the lower the Graphite Nodularity (NG4, NG5): 80–90% for min. 0.50 (minimum Form IV or Intermediate Graphite), 60–80% for min. 0.60–0.65 (minimum Form V graphite) and 35–70% for min. 0.80 (minimum Form VI graphite). The SSF is more representative than the RSF for Si-alloyed ductile cast iron, so it is recommended to use a graphite nodularity calculus considering SSF instead of the RSF formula (stipulated by ISO 945-4-2019), with SSF replacing RSF.
- Open Access
Graphite Compactness Degree and Nodularity of High-Si Ductile Iron Produced via Permanent Mold versus Sand Mold Casting
In recent years, high-Si ductile cast irons (3–6% Si) have begun to be used more and more in the automotive and maritime industries, but also in wind energy technology and mechanical engineering. Si-alloyed ferrite has high strength, hardness and oxidation and corrosion resistance, but it has low ductility, toughness and thermal conductivity, with graphite as an important influencing factor. In this study, 4.5% Si uninoculated ductile iron solidified in thin wall castings (up to 15 mm section size) via a permanent (metal) mold versus a sand mold, was evaluated. Solidification in a metal mold led to small size, higher graphite particles (less dependent on the section size). The graphite particles’ real perimeter was 3–5% higher than the convex perimeter, while the values of these parameters were 41–43% higher in the sand mold. Increasing the casting section size led to an increased graphite perimeter, with it being much higher for sand mold. The graphite particles’ shape factors, involving the maximum and minimum size, were at a lower level for metal mold solidification, while by involving the difference between Pr and Pc, is higher for the metal mold. The shape factor, including the graphite area and maximum size, had higher values in the metal mold, sustaining a higher compactness degree of graphite particles and a higher nodularity regarding metal mold solidification (75.5% versus 67.4%). The higher was due to the graphite compactness degree level (shape factor increasing from 0.50 up to 0.80), while the lower was due to the graphite nodularity for both the metal mold (39.1% versus 88.5%) and the sand mold (32.3% versus 83.1%). The difference between the metal mold and sand mold as the average graphite nodularity increased favored the metal mold.
Open AccessGraphite Compactness Degree and Nodularity of High-Si Ductile Iron Produced via Permanent Mold versus Sand Mold Casting
In recent years, high-Si ductile cast irons (3–6% Si) have begun to be used more and more in the automotive and maritime industries, but also in wind energy technology and mechanical engineering. Si-alloyed ferrite has high strength, hardness and oxidation and corrosion resistance, but it has low ductility, toughness and thermal conductivity, with graphite as an important influencing factor. In this study, 4.5% Si uninoculated ductile iron solidified in thin wall castings (up to 15 mm section size) via a permanent (metal) mold versus a sand mold, was evaluated. Solidification in a metal mold led to small size, higher graphite particles (less dependent on the section size). The graphite particles’ real perimeter was 3–5% higher than the convex perimeter, while the values of these parameters were 41–43% higher in the sand mold. Increasing the casting section size led to an increased graphite perimeter, with it being much higher for sand mold. The graphite particles’ shape factors, involving the maximum and minimum size, were at a lower level for metal mold solidification, while by involving the difference between Pr and Pc, is higher for the metal mold. The shape factor, including the graphite area and maximum size, had higher values in the metal mold, sustaining a higher compactness degree of graphite particles and a higher nodularity regarding metal mold solidification (75.5% versus 67.4%). The higher was due to the graphite compactness degree level (shape factor increasing from 0.50 up to 0.80), while the lower was due to the graphite nodularity for both the metal mold (39.1% versus 88.5%) and the sand mold (32.3% versus 83.1%). The difference between the metal mold and sand mold as the average graphite nodularity increased favored the metal mold.