Ya. D. Zelyakh
Ya. D. Zelyakh has a total of 5 co-authors. Here are the top co-authors by number of shared publications:
- Gennady I. Maltsev
Institute of Metallurgy of the Ural Branch of the RAS
2 shared publications - Konstantin L. Timofeev
JSC «Uralelectromed»; UMMC Technical University
2 shared publications - Roman S. Voinkov
JSC “Uralelectromed”; Technical University UMMC
2 shared publications Я. Д. Зелях
АО «Уралэлектромедь
2 shared publications- V. A. Shunin
JSC «Uralelectromed
1 shared publication
Latest Publications
- 27 March 2024
- Published by National University of Science and Technology MISiS in Izvestiya Vuzov. Tsvetnaya Metallurgiya (Proceedings of Higher Schools. Nonferrous Metallurgy)
- No. 1,p. 5-13
Purification of process solutions from mercury by sorption
At JSC «Uralelectromed», selenium-containing raw materials and industrial products are processed, resulting in solutions containing a mixture of mercury with concentrations as follows (g/dm3): 157–210 Se; 0.004–0.02 Hg; 0.15–0.20 Te; 2–3 As; 0.15–0.20 Sb; and 45–50 S. To produce branded selenium, the mercury concentration in the solution must be kept below 0.001 g/dm3. Various methods, such ashydrometallurgical and electrochemical processes, are known for mercury purification from solutions. JSC «Uralelectromed» has selected sorption technology for mercury removal using the weak-base macroporous anionite Lewatit MP-68 (Germany), which allows for control over the degree of solution purification. In pursuit of import substitution for the Western European sorbent Lewatit MP-68, we investigated several pre-selected industrial sorbents for extracting mercury anionic complexes produced in Russia (AM-2B, AN-31, AV 17-8, VP-3Ap), China (Seplite MA 940 and LSC 710), and India (Tulsion CH-95 and CH-97). Initially, in static mode, we determined the distribution coefficient (Cd), the degree of element extraction (ε), the static exchange capacity of the resins (SEC, g/dm3), and the mercury/selenium separation coefficient (DHg/Se) which led to the selection of the best samples: AV 17-8, Seplite MA 940, AM-2B, and CH-97, with SEC values of 0.95–0.97 g/dm3 (SEC = 0.98 g/dm3 of resin Lewatit MP-68). Subsequently, in dynamic mode, we ranked the ionites by decreasing dynamic exchange capacity (DEC / TDEC): AV 17-8 ≥ Lewatit MP-68 > AM-2B > Seplite MA 940 > Tulsion CH-97. Resins AV 17-8, Seplite MA 940, and AM-2B demonstrated similar dynamic sorption characteristics; under comparable conditions, mercury breakthrough occurred after processing at least 950 specific volumes of the initial solution. In contrast, with Lewatit MP-68 ionite, mercury breakthrough occurred after no more than 750 specific volumes, indicating the need to increase the number of sorption steps in the solution purification cascade. Considering the totality of ion-exchange properties, for further industrial testing, it is recommended to use the domestically produced resin AV 17-8 instead of the foreign sorbent Lewatit MP-68 in the sorption purification process of selenic acid to remove mercury, thereby ensuring the production of branded selenium.
- 27 March 2024
- Published by National University of Science and Technology MISiS in Izvestiya Vuzov. Tsvetnaya Metallurgiya (Proceedings of Higher Schools. Nonferrous Metallurgy)
- No. 1,p. 5-13
Purification of process solutions from mercury by sorption
At JSC «Uralelectromed», selenium-containing raw materials and industrial products are processed, resulting in solutions containing a mixture of mercury with concentrations as follows (g/dm3): 157–210 Se; 0.004–0.02 Hg; 0.15–0.20 Te; 2–3 As; 0.15–0.20 Sb; and 45–50 S. To produce branded selenium, the mercury concentration in the solution must be kept below 0.001 g/dm3. Various methods, such ashydrometallurgical and electrochemical processes, are known for mercury purification from solutions. JSC «Uralelectromed» has selected sorption technology for mercury removal using the weak-base macroporous anionite Lewatit MP-68 (Germany), which allows for control over the degree of solution purification. In pursuit of import substitution for the Western European sorbent Lewatit MP-68, we investigated several pre-selected industrial sorbents for extracting mercury anionic complexes produced in Russia (AM-2B, AN-31, AV 17-8, VP-3Ap), China (Seplite MA 940 and LSC 710), and India (Tulsion CH-95 and CH-97). Initially, in static mode, we determined the distribution coefficient (Cd), the degree of element extraction (ε), the static exchange capacity of the resins (SEC, g/dm3), and the mercury/selenium separation coefficient (DHg/Se) which led to the selection of the best samples: AV 17-8, Seplite MA 940, AM-2B, and CH-97, with SEC values of 0.95–0.97 g/dm3 (SEC = 0.98 g/dm3 of resin Lewatit MP-68). Subsequently, in dynamic mode, we ranked the ionites by decreasing dynamic exchange capacity (DEC / TDEC): AV 17-8 ≥ Lewatit MP-68 > AM-2B > Seplite MA 940 > Tulsion CH-97. Resins AV 17-8, Seplite MA 940, and AM-2B demonstrated similar dynamic sorption characteristics; under comparable conditions, mercury breakthrough occurred after processing at least 950 specific volumes of the initial solution. In contrast, with Lewatit MP-68 ionite, mercury breakthrough occurred after no more than 750 specific volumes, indicating the need to increase the number of sorption steps in the solution purification cascade. Considering the totality of ion-exchange properties, for further industrial testing, it is recommended to use the domestically produced resin AV 17-8 instead of the foreign sorbent Lewatit MP-68 in the sorption purification process of selenic acid to remove mercury, thereby ensuring the production of branded selenium.
- Open Access
- 17 June 2023
- Published by National University of Science and Technology MISiS in Izvestiya Vuzov. Tsvetnaya Metallurgiya (Proceedings of Higher Schools. Nonferrous Metallurgy)
- No. 3,p. 27-37
Preparation of rhodium concentrate from gold cementate
This article describes studies on improving reprocessing technology gold production cementate (GPC) formed in refining section of chemical metallurgical shop at JSC Uralelektromed, in order to increase the extraction rate of targeted metals into marketable products, diversification of production, achievement of economic effect due to increasing content of precious metals (PM) in individual concentrates. The optimization of GPC reprocessing technology includes intensification of leaching of initial material and filtration of produced pulp, in order to increase the extraction of gold and platinum group metals (PGM) into solution and decrease the circulated PM. This would allow individual products (crude PM) to be obtained with minimum material loss and labor consumption. It is possible to increase rhodium content in concentrate and to reduce its circulation by preliminary oxidating annealing at the temperature above 500 °C. At this temperature hardly soluble trioxide Rh2O3 is formed on rhodium surface, insoluble in aqua regia, thus allowing it to deposit in the form of individual product. The influence of temperature and composition of gaseous phase was established upon oxidizing annealing of initial raw stuff (t = 500÷750 °C) on the composition of rhodium trioxide concentrate (15÷45 % Rh2O3). Reprocessing flowchart of gold production cementate was developed and tested on commercial scale, allowing for the simultaneous production of several products: deposited gold (Au ≥ 98 %), deposited silver (Ag ≥ 98 %), PGM concentrate (Pt ≥ 45 % and Pd ≥ 15 %), rhodium concentrate (Rh = 15÷45 %).
- 17 June 2023
- Published by National University of Science and Technology MISiS in Izvestiya Vuzov. Tsvetnaya Metallurgiya (Proceedings of Higher Schools. Nonferrous Metallurgy)
- No. 3,p. 27-37
Open AccessPreparation of rhodium concentrate from gold cementate
This article describes studies on improving reprocessing technology gold production cementate (GPC) formed in refining section of chemical metallurgical shop at JSC Uralelektromed, in order to increase the extraction rate of targeted metals into marketable products, diversification of production, achievement of economic effect due to increasing content of precious metals (PM) in individual concentrates. The optimization of GPC reprocessing technology includes intensification of leaching of initial material and filtration of produced pulp, in order to increase the extraction of gold and platinum group metals (PGM) into solution and decrease the circulated PM. This would allow individual products (crude PM) to be obtained with minimum material loss and labor consumption. It is possible to increase rhodium content in concentrate and to reduce its circulation by preliminary oxidating annealing at the temperature above 500 °C. At this temperature hardly soluble trioxide Rh2O3 is formed on rhodium surface, insoluble in aqua regia, thus allowing it to deposit in the form of individual product. The influence of temperature and composition of gaseous phase was established upon oxidizing annealing of initial raw stuff (t = 500÷750 °C) on the composition of rhodium trioxide concentrate (15÷45 % Rh2O3). Reprocessing flowchart of gold production cementate was developed and tested on commercial scale, allowing for the simultaneous production of several products: deposited gold (Au ≥ 98 %), deposited silver (Ag ≥ 98 %), PGM concentrate (Pt ≥ 45 % and Pd ≥ 15 %), rhodium concentrate (Rh = 15÷45 %).