Shadyar Farhangfar
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Shadyar Farhangfar has a total of 12 co-authors. Here are the top co-authors by number of shared publications:
- Kornelius Nielsch
Leibniz Institute for Solid State and Materials Research
2 shared publications - Jaeyoung Lee
School of Materials Science and Engineering, Gwangju Institute of Science and Technology, Gwangju 61005, Republic of Korea
1 shared publication - Jong-Min Lee
Department of Energy Science and Engineering Daegu Gyeongbuk Institute of Science and Technology (DGIST) Daegu Republic of Korea
1 shared publication K. Nielsch
Institute of Applied Physics University of Hamburg Jungiusstr. 11 D-20355 Hamburg Germany
1 shared publicationM Pelletier
Institute of Physical Chemistry|UniVersity of Hamburg
1 shared publicationM. Pelletier
Institute of Physical Chemistry University of Hamburg Bundesstr. 45 D-20146 Hamburg Germany
1 shared publication
Latest Publications
- 27 August 2009
- Published by Royal Society of Chemistry (RSC) in Journal of Materials Chemistry
- Vol. 19 (38) , 7050-7054
A novel approach for fabrication of bismuth-silicon dioxide core-shell structures by atomic layer deposition
Bismuth (Bi) nanowires were grown electrochemically into the pores of anodic aluminium oxide (AAO) templates. The diameter of the pores in the AAO membranes has been precisely tuned down to 30 nm by atomic layer deposition (ALD) of silicon dioxide onto the pore walls. Bi nanowires with diameters of 30, 50, and 200 nm were subsequently deposited by potentiostatic electrochemical deposition. The fabricated Bi nanowires showed a highly preferential growth orientation along the (110) direction. High resolution transmission electron microscopy (HRTEM) and selected area electron diffraction (SAED) investigations further confirmed the existence of a preferred growth orientation and polycrystalline nature of the nanowires. Using Fourier transform infrared (FT-IR) spectroscopy, optical absorption of nanowires was investigated as a function of wire diameter. The absorption edge energy, ∼87 meV, of narrower 30 nm diameter semiconducting nanowires decreased with increasing the wire diameter and led ultimately to the observation of semimetallic behavior in the 200 nm thick wires. In the electrical measurements, a metallic contact to an array of 50 nm diameter nanowires was made and the resistance of the array was measured in the temperature range 130–300 K. The semiconducting bandgap energy, ∼67 meV, was obtained by comparison of the experimental data to a simple theoretical model.
- 27 August 2009
- Published by Royal Society of Chemistry (RSC) in Journal of Materials Chemistry
- Vol. 19 (38) , 7050-7054
A novel approach for fabrication of bismuth-silicon dioxide core-shell structures by atomic layer deposition
Bismuth (Bi) nanowires were grown electrochemically into the pores of anodic aluminium oxide (AAO) templates. The diameter of the pores in the AAO membranes has been precisely tuned down to 30 nm by atomic layer deposition (ALD) of silicon dioxide onto the pore walls. Bi nanowires with diameters of 30, 50, and 200 nm were subsequently deposited by potentiostatic electrochemical deposition. The fabricated Bi nanowires showed a highly preferential growth orientation along the (110) direction. High resolution transmission electron microscopy (HRTEM) and selected area electron diffraction (SAED) investigations further confirmed the existence of a preferred growth orientation and polycrystalline nature of the nanowires. Using Fourier transform infrared (FT-IR) spectroscopy, optical absorption of nanowires was investigated as a function of wire diameter. The absorption edge energy, ∼87 meV, of narrower 30 nm diameter semiconducting nanowires decreased with increasing the wire diameter and led ultimately to the observation of semimetallic behavior in the 200 nm thick wires. In the electrical measurements, a metallic contact to an array of 50 nm diameter nanowires was made and the resistance of the array was measured in the temperature range 130–300 K. The semiconducting bandgap energy, ∼67 meV, was obtained by comparison of the experimental data to a simple theoretical model.
- Open Access
Atomic layer deposition of ZnS nanotubes
We report on growth of high-aspect-ratio ($\gtrsim300$) zinc sulfide nanotubes with variable, precisely tunable, wall thicknesses and tube diameters into highly ordered pores of anodic alumina templates by atomic layer deposition (ALD) at temperatures as low as 75 $^{\circ}$C. Various characterization techniques are employed to gain information on the composition, morphology, and crystal structure of the synthesized samples. Besides practical applications, the ALD-grown tubes could be envisaged as model systems for the study of a certain class of size-dependent quantum and classical phenomena.
Open AccessAtomic layer deposition of ZnS nanotubes
We report on growth of high-aspect-ratio ($\gtrsim300$) zinc sulfide nanotubes with variable, precisely tunable, wall thicknesses and tube diameters into highly ordered pores of anodic alumina templates by atomic layer deposition (ALD) at temperatures as low as 75 $^{\circ}$C. Various characterization techniques are employed to gain information on the composition, morphology, and crystal structure of the synthesized samples. Besides practical applications, the ALD-grown tubes could be envisaged as model systems for the study of a certain class of size-dependent quantum and classical phenomena.
- 21 July 2009
- Published by IOP Publishing in Nanotechnology
- Vol. 20 (32) , 325602
Atomic layer deposition of ZnS nanotubes
We report on the growth of high-aspect-ratio (approximately > 300) zinc sulfide nanotubes with variable, precisely tunable, wall thicknesses and tube diameters into highly ordered pores of anodic alumina templates by atomic layer deposition (ALD) at temperatures as low as 75 degrees C. Various characterization techniques are employed to gain information on the composition, morphology and crystal structure of the synthesized samples. Besides practical applications, the ALD-grown tubes could be envisaged as model systems for the study of a certain class of size-dependent quantum and classical phenomena.
- 21 July 2009
- Published by IOP Publishing in Nanotechnology
- Vol. 20 (32) , 325602
Atomic layer deposition of ZnS nanotubes
We report on the growth of high-aspect-ratio (approximately > 300) zinc sulfide nanotubes with variable, precisely tunable, wall thicknesses and tube diameters into highly ordered pores of anodic alumina templates by atomic layer deposition (ALD) at temperatures as low as 75 degrees C. Various characterization techniques are employed to gain information on the composition, morphology and crystal structure of the synthesized samples. Besides practical applications, the ALD-grown tubes could be envisaged as model systems for the study of a certain class of size-dependent quantum and classical phenomena.