SBSomaye Bahrani

Somaye Bahrani

*This is an algorithmically generated author record based on publicly available information.

Current Organizations / Institutes

The organizations/institutes from the scholar's latest article


Somaye Bahrani has a total of 3 co-authors. Here are the top co-authors by number of shared publications:

  • F. Sharafeddin

    Professor, Biomaterials Research Center, Department of Operative Dentistry, School of Dentistry, Shiraz University of Medical Sciences, Shiraz, Iran

    1 shared publication
  • Farahnaz Sharafeddin

    Department of Operative Dentistry, Biomaterials Research Center, School of Dentistry, Shiraz University of Medical Sciences, Shiraz, Iran

    1 shared publication
  • Z. Jowkar

    Assistant professor, Oral and Dental Disease Research Center, Department of Operative Dentistry, School of Dentistry, Shiraz University of Medical Sciences, Shiraz, Iran

    1 shared publication

Latest Publications

  • Open Access

    Comparison between the effect of adding microhydroxyapatite and chitosan on surface roughness and Microhardness of resin modified and conventional glass ionomer cements

    by F. Sharafeddin, Z. Jowkar, S. Bahrani

    This study aimed to compare the effect of chitosan (CH) and hydroxyapatite (HP) on the surface roughness and microhardness of a conventional glass ionomer cement (CGIC) and a resin modified glass ionomer cement (RMGIC). 60 disk-shaped specimens (2mm x 6mm) were prepared in 6 groups; group I: CGIC, group II: RMGIC, group III: CGIC + 15% volume CH solution in liquid, group IV: CGIC +10% weight micro-HP in powder, group V: RMGIC + 15% volume CH, group VI: RMGIC + 10% weight micro-HP. After storage in deionized water at room temperature for 24 hours, the surface roughness and microhardness of the specimens were measured using a surface profilometer and Vickers microhardness (VHN) tester, respectively. Data were analyzed using two-way ANOVA, Tukey HSD test and paired t-test (P<0.05). The microhardness values of RMGIC and CGIC decreased significantly with the addition of micro-HP (P<0.001). None of the CH-containing GICs showed significant changes in microhardness (P = 0.552). The VHN values of CGIC were higher than RMGIC, regardless of the added substance (P<0.001). The surface roughness (Ra) values (μm) of both RMGIC and CGIC decreased significantly with the addition of CH (P = 0.004). The incorporation of micro-HP into GICs did not have a significant effect on surface roughness values (P = 0.700). The RMGIC showed less Ra values compared to the CGIC regardless of the added substance (P<0.001). The lowest and highest Ra values were observed in RMGIC + CH and CGIC + micro-HP groups, respectively. The addition of CH to GIC and RMGIC reduced the surface roughness and did not have an adverse effect on the microhardness. Mixing GIC and RMGIC with micro-HP resulted in microhardness reduction and did not affect the surface roughness. Key words:Glass ionomer, hydroxyapatite, chitosan, hardness, surface roughness


  • Open Access

    Effect of Hydroxyapatite on Surface Roughness of Zirconomer, and Conventional and Resin-Modified Glass Ionomers

    by Farahnaz Sharafeddin, Somaye Bahrani

    Objectives: Glass ionomer cements (GICs) are among the most popular dental restorative materials, but their use is limited due to their clinical disadvantages. Many efforts have been made to improve the properties of these materials by adding various fillers. Incorporation of hydroxyapatite (HA) into the GICs is considered to improve the physical properties of restorations, and may prevent treatment failure. This study aimed to evaluate the surface roughness (Ra) of a conventional glass ionomer cement (CGIC), a resin-modified glass ionomer (RMGI) and a Zirconomer with and without micro-hydroxyapatite (µHA). Materials and Methods: This experimental study was conducted on 6 groups (n=10) including CGIC, CGIC + µHA, RMGI, RMGI + µHA, Zirconomer, and Zirconomer + µHA. A total of 60 disc-shaped samples (6 mm × 2 mm) were prepared in plastic molds and were stored in distilled water for 24 h. After polishing of the specimens, their Ra was measured by a profilometer in micrometers (µm). The data were analyzed using two and one-way ANOVA, Tukey's HSD test, and independent t-test. Results: Incorporation of µHA resulted in statistically significant differences in Ra between the study groups (P<0.05). Following the incorporation of µHA, the Ra significantly decreased in CGIC (P=0.013) and Zirconomer (P=0.003). However, addition of µHA to RMGI resulted in a significant increase in its Ra (P<0.001). Conclusion: Addition of µHA decreased the Ra of Zirconomer and CGIC, and increased the surface roughness of RMGI samples.