Yan Zhang
School of Materials Science and Engineering, Nanjing Institute of Technology, Nanjing 211167 China
3 shared publicationsCanhui Wu
School of Material Science and Engineering, Nanjing Institute of Technology, Nanjing 211167, China
2 shared publicationsChangsheng Wang
Key Laboratory of Advanced Structural Materials and Application Technology of Jiangsu Province, 1Hongjing venue, Nanjing 211167, PR China
1 shared publicationHenghui Zhan
School of Material Science and Engineering, Nanjing Institute of Technology, Nanjing 211167, China
1 shared publicationJiahao Qian
Key Laboratory of Advanced Structural Materials and Application Technology of Jiangsu Province, 1Hongjing venue, Nanjing 211167, PR China
1 shared publicationQianyi Lu
School of Material Science and Engineering, Nanjing Institute of Technology, Nanjing 211167, China
1 shared publication
Latest Publications
- Open Access
- 17 October 2024
- Published by IOS Press
- p. 192-201
Effects of Solution Temperature on Microstructure and Properties of Zn-2Cu-0.8Mg Alloy
Zn-2Cu-0.8Mg zinc alloy was prepared by metal mold casting. The effects of solution temperature on the microstructure, corrosion behavior and mechanical properties of zinc alloy were studied. The results show that the microstructure of zinc alloy is mainly composed of η-Zn, Mg2Zn11 and a small amount of CuZn5 compounds. As the solution temperature increases, η-Zn content increases, the grain size increases, from dendrite to equiaxed crystal to coarsening; The tensile strength and elongation of the solid solution alloy are higher than those of the as cast alloy, and decrease with the increase of solution temperature. The alloy after 320°C solution treatment has the maximum values of mechanical properties, which are 396 MPa and 1.18% respectively, 1.3 and 1.8 times of those of as cast alloy; Fracture analysis shows that the fracture mode of zinc alloy is mainly cleavage fracture. The electrochemical test shows that the corrosion resistance of zinc alloy increases with the increase of solution temperature, and the self-corrosion current density of the alloy after 380°C solution treatment is the lowest, 14.965μA.cm-2. The corrosion rate is the lowest, 0.022mm/y.
- 17 October 2024
- Published by IOS Press
- p. 192-201
Open AccessEffects of Solution Temperature on Microstructure and Properties of Zn-2Cu-0.8Mg Alloy
Zn-2Cu-0.8Mg zinc alloy was prepared by metal mold casting. The effects of solution temperature on the microstructure, corrosion behavior and mechanical properties of zinc alloy were studied. The results show that the microstructure of zinc alloy is mainly composed of η-Zn, Mg2Zn11 and a small amount of CuZn5 compounds. As the solution temperature increases, η-Zn content increases, the grain size increases, from dendrite to equiaxed crystal to coarsening; The tensile strength and elongation of the solid solution alloy are higher than those of the as cast alloy, and decrease with the increase of solution temperature. The alloy after 320°C solution treatment has the maximum values of mechanical properties, which are 396 MPa and 1.18% respectively, 1.3 and 1.8 times of those of as cast alloy; Fracture analysis shows that the fracture mode of zinc alloy is mainly cleavage fracture. The electrochemical test shows that the corrosion resistance of zinc alloy increases with the increase of solution temperature, and the self-corrosion current density of the alloy after 380°C solution treatment is the lowest, 14.965μA.cm-2. The corrosion rate is the lowest, 0.022mm/y.
- Open Access
- 1 February 2021
- Published by IOP Publishing in IOP Conference Series: Earth and Environmental Science
- Vol. 675 (1) , 012059
Effect of Mg content on microstructure and properties of Zn-Al-Cu Alloy
Zn-Cu-Al-xMg (x=0,0.25,0.5) zinc alloy was prepared by metal mould casting. The effects of Mg addition on the structure, electrical conductivity and mechanical properties of Zn-Al-Cu alloy were studied. The results show that without Mg addition, the alloy consists of Zn solid solution(ƞ phase) containing of Cu and Al and layered α+η eutectic structure. With the addition of Mg, the η phase grains were refined, the layered eutectic structure disappeared, and the intermetallic compound Mg2Zn11 appeared, and its content increased with the increase of Mg content. The hardness of the alloy increases with the increase of Mg content. When the content of Mg is 0.5wt.%, the hardness reaches the maximum value of 151HV. Tensile strength and electrical conductivity first increase and then decrease. When the addition of Mg is 0.25wt.%, the maximum tensile strength and electrical conductivity are 270 MPa and 26.4% IACS, respectively. The wear mechanism of zinc alloy is a mixture of adhesive wear and abrasive wear, and the adhesive wear is dominant.
- 1 February 2021
- Published by IOP Publishing in IOP Conference Series: Earth and Environmental Science
- Vol. 675 (1) , 012059
Open AccessEffect of Mg content on microstructure and properties of Zn-Al-Cu Alloy
Zn-Cu-Al-xMg (x=0,0.25,0.5) zinc alloy was prepared by metal mould casting. The effects of Mg addition on the structure, electrical conductivity and mechanical properties of Zn-Al-Cu alloy were studied. The results show that without Mg addition, the alloy consists of Zn solid solution(ƞ phase) containing of Cu and Al and layered α+η eutectic structure. With the addition of Mg, the η phase grains were refined, the layered eutectic structure disappeared, and the intermetallic compound Mg2Zn11 appeared, and its content increased with the increase of Mg content. The hardness of the alloy increases with the increase of Mg content. When the content of Mg is 0.5wt.%, the hardness reaches the maximum value of 151HV. Tensile strength and electrical conductivity first increase and then decrease. When the addition of Mg is 0.25wt.%, the maximum tensile strength and electrical conductivity are 270 MPa and 26.4% IACS, respectively. The wear mechanism of zinc alloy is a mixture of adhesive wear and abrasive wear, and the adhesive wear is dominant.
- Open Access
- 1 January 2020
- Published by IOP Publishing in IOP Conference Series: Materials Science and Engineering
- Vol. 746 (1)
Effect of Al Content on Microstructure and Properties of Zn-Cu-Al Alloy
Zn-Cu-Al zinc alloy was prepared by metal mould casting. The effects of Al addition on the microstructure, electrical conductivity and wear resistance of Zn-Cu-Al alloy were studied. The results show that the structure of Zn-Cu-Al alloy is composed of Zn solid solution containing Cu and Al (η phase), eutectic phase (α+η) and CuZn5 (ε phase); Al0.4Zn0.6 phase appeared when Al addition content exceeded 2.0wt.%; With the increase of Al addition content, eutectic phase (α+η) content increased and η phase grain refined. Meanwhile, the hardness and electrical conductivity of the alloy increase with the increase of Al addition content. When the addition of Al is 5.0 wt.%, the hardness and electrical conductivity of the alloy reach the maximum, 151HV and 26.4% IACS, respectively. The wear mechanism of the alloy is mainly plastic deformation with a mixture mode of plastic deformation and adhesion.
- 1 January 2020
- Published by IOP Publishing in IOP Conference Series: Materials Science and Engineering
- Vol. 746 (1)
Open AccessEffect of Al Content on Microstructure and Properties of Zn-Cu-Al Alloy
Zn-Cu-Al zinc alloy was prepared by metal mould casting. The effects of Al addition on the microstructure, electrical conductivity and wear resistance of Zn-Cu-Al alloy were studied. The results show that the structure of Zn-Cu-Al alloy is composed of Zn solid solution containing Cu and Al (η phase), eutectic phase (α+η) and CuZn5 (ε phase); Al0.4Zn0.6 phase appeared when Al addition content exceeded 2.0wt.%; With the increase of Al addition content, eutectic phase (α+η) content increased and η phase grain refined. Meanwhile, the hardness and electrical conductivity of the alloy increase with the increase of Al addition content. When the addition of Al is 5.0 wt.%, the hardness and electrical conductivity of the alloy reach the maximum, 151HV and 26.4% IACS, respectively. The wear mechanism of the alloy is mainly plastic deformation with a mixture mode of plastic deformation and adhesion.