Latest Publications

  • Open Access

    Feasibility Of Making Concrete Using Lignite Coal Bottom Ash As Fine Aggregate

    by T. S. Thandavamoorthy

    Concrete is generally produced using materials such as crushed stone and river sand to the extent of about 80-90% combined with cement and water. These materials are quarried from natural sources. Their depletion will cause strain on the environment. To prevent this, bottom ash produced at thermal power plants by burning of coal has been utilized in this investigation into making concrete. The experimental investigation presents the development of concrete containing lignite coal bottom ash as fine aggregate in various percentages of 25, 50, and 100. Compressive, split tensile, and flexural strength as part of mechanical properties; acid, sulphate attack, and sustainability under elevated temperature as part of durability properties, were determined. These properties were compared with that of normal concrete. It was concluded from this investigation that bottom ash to an extent of 25% can be substituted in place of river sand in the production of concrete.


  • Wood waste as coarse aggregate in the production of concrete

    by T.S. Thandavamoorthy

    An attempt was made in this experimental investigation to recycle wood waste. Concrete-containing wood aggregate in percentages of 0, 15, 20 and 25 in place of crushed stone was developed with a characteristic compressive strength of 25 MPa, with a mix proportion of 1:1.26:2.76 and with water/cement ratio of .45. One hundred and twenty specimens were cast and tested to evaluate the strength and durability properties of concrete. The performance of wood aggregate concrete was compared with control concrete that contained only crushed stone aggregate. The compressive strength of control concrete was 31.40 MPa and that of wood aggregate concrete with 15% replacement level was 32.36 MPa which is 3.06% above the control concrete. Split tensile strength of 15% replaced wood aggregate concrete was 2.25 MPa as against a value of 2.05 MPa for control concrete registering an increase of 9.75%. The flexural strength of control concrete was 2.49 MPa and that of concrete containing 15% wood aggregate was 2.51 MPa which was .80% higher than the control concrete. The weight loss of wood aggregate concrete with 15% replacement level under acid attack was 30.38% greater than the control concrete. Under alkaline attack, the weight loss of wood aggregate concrete with 15% replacement level registered an increase of 9.72% over control concrete. Therefore, wood aggregate can be used in the production of concrete, and the optimum replacement was found to be 15% from all considerations.


  • Open Access

    Load-Deflection Characteristics Of Steel, Polypropylene And Hybrid Fiber Reinforced Concrete Beams

    by M. Tamil Selvi, T. S. Thandavamoorthy

    Concrete is the most widely used construction material because of its specialty of being cast into any desired shape. The main requirements of earthquake resistant structures are good ductility and energy absorption capacity. Fiber reinforced concrete possesses high flexural and tensile strength, improved ductility, and high energy absorption over the conventional concrete in sustaining dynamic loads. The aim of this paper is to compare the properties of concrete beams in which three types of fibers are added individually. Steel fibers, polypropylene fibers and hybrid fibers were added to concrete in the weight ratio of four percentages in the preparation of four beam specimens. The fourth specimen did not contain fibers and acted as a control specimen. The dimensions of the beam specimens were 150 mm × 150 mm × 700 mm. The reinforced concrete beams of M30 grade concrete were prepared for casting and testing. Various parameters such as load carrying capacity, stiffness degradation, ductility characteristics and energy absorption capacity of FRC beams were compared with that of RC beams. The companion specimens were cast and tested to study strength properties and then the results were compared. All the beams were tested under three point bending under Universal Testing Machine (UTM). The results were evaluated with respect to modulus of elasticity, first crack load, ultimate load, and ultimate deflection. The test result shows that use of hybrid fiber improves the flexural performance of the reinforced concrete beams. The flexural behavior and stiffness of the tested beams were calculated, and compared with respect to their load carrying capacities. Comparison was also made with theoretical calculations in order to determine the load-deflection curves of the tested beams. Results of the experimental programme were compared with theoretical predictions. Based on the results of the experimental programme, it can be concluded that the addition of steel, polypropylene and hybrid fibers by 4% by weight of cement (but 2.14 % by volume of cement) had the best effect on the stiffness and energy absorption capacity of the beams.