A. G. Kanevskii
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
A. G. Kanevskii has a total of 3 co-authors. Here are the top co-authors by number of shared publications:
- Aleksandr A. Aleksandrov
Baikov Institute of Metallurgy and Materials Science, Russian Academy of Sciences
1 shared publication - L. I. Leont’ev
National University of Science and Technology “MISIS”; Institute of Metallurgy, UB RAS; Scientific Council on Metallurgy and Metal Science of Russian Academy of Sciences
1 shared publication - V. Ya. Dashevskii
Baikov Institute of Metallurgy and Materials Science, Russian Academy of Sciences, Moscow, Russia
1 shared publication
Latest Publications
- 1 September 2014
- Published by Pleiades Publishing Ltd in Inorganic Materials: Applied Research
- Vol. 5 (5) , 432-436
Solubility of oxygen in zirconium-containing iron-nickel melts
The oxygen solubility in zirconium-containing Fe-Ni melts is for the first time studied experimentally at 1873 K using the Fe-40% Ni alloy as an example. It is shown that the deoxidizing ability of zirconium in this melt is very high, but it is slightly lower than pure iron. This is due to the fact that, when the nickel content in the melt increases, the bond strengths of zirconium with the melt base (γ Zr(Fe) ∘ = 0.043; (γ Zr(Ni) ∘ = 0.00007) rise to a considerably greater degree than the bond strengths of oxygen weaken (γ O(Fe) ∘ = 0.0105; (γ O(Ni) ∘ = 0.357). The equilibrium constant of interaction of zirconium and oxygen dissolved in the Fe-40% Ni melt (K (Fe-40% Ni) = 6.011 × 10−7) and the interaction parameters characterizing these solutions (e Zr O = −7.16; e O Zr = −1.25; e Zr Zr = 2.16) were determined.
- 1 September 2014
- Published by Pleiades Publishing Ltd in Inorganic Materials: Applied Research
- Vol. 5 (5) , 432-436
Solubility of oxygen in zirconium-containing iron-nickel melts
The oxygen solubility in zirconium-containing Fe-Ni melts is for the first time studied experimentally at 1873 K using the Fe-40% Ni alloy as an example. It is shown that the deoxidizing ability of zirconium in this melt is very high, but it is slightly lower than pure iron. This is due to the fact that, when the nickel content in the melt increases, the bond strengths of zirconium with the melt base (γ Zr(Fe) ∘ = 0.043; (γ Zr(Ni) ∘ = 0.00007) rise to a considerably greater degree than the bond strengths of oxygen weaken (γ O(Fe) ∘ = 0.0105; (γ O(Ni) ∘ = 0.357). The equilibrium constant of interaction of zirconium and oxygen dissolved in the Fe-40% Ni melt (K (Fe-40% Ni) = 6.011 × 10−7) and the interaction parameters characterizing these solutions (e Zr O = −7.16; e O Zr = −1.25; e Zr Zr = 2.16) were determined.