Alireza Kohandehghan
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Alireza Kohandehghan has a total of 5 co-authors. Here are the top co-authors by number of shared publications:
- David Mitlin
University of Alberta Department of Chemical and Materials Engineering, 9107 116th Street, Edmonton, AB, Canada
1 shared publication Elmira Memarzadeh
University of Alberta Department of Chemical and Materials Engineering, 9107 116th Street, Edmonton, AB, Canada
1 shared publicationKai Cui
National Institute for Nanotechnology (NINT), NRC, 11421 Saskatchewan Dr, Edmonton, AB, Canada
1 shared publicationMartin Kupsta
National Institute for Nanotechnology (NINT), NRC, 11421 Saskatchewan Dr, Edmonton, AB, Canada
1 shared publicationPeter Kalisvaart
University of Alberta Department of Chemical and Materials Engineering, 9107 116th Street, Edmonton, AB, Canada
1 shared publication
Latest Publications
- 28 May 2014
- Published by Royal Society of Chemistry (RSC) in Journal of Materials Chemistry A
- Vol. 2 (29) , 11261-11279
Nanometer-scale Sn coatings improve the performance of silicon nanowire LIB anodes
We demonstrate that a thin partially dewetted coating of Sn will improve the cycling performance of silicon nanowire (SiNWs) lithium ion battery (LIB) anodes. The optimum architecture 3Sn/SiNWs (i.e. a Sn layer with an average film thickness of a 3 nm covering the nanowire) maintained a reversible capacity of 1865 mA h g−1 after 100 cycles at a rate of 0.1 C. This is almost double of the baseline uncoated SiNWs, where the reversible capacity after 100 cycles was 1046 mA h g−1 (∼78% improvement). The 1Sn/SiNWs and 3Sn/SiNWs electrodes demonstrated much improved cycling coulombic efficiency, with >99% vs. 94–98% for the baseline. At a high current density of 5 C, these nanocomposite offered 2× the capacity retention of bare SiNWs (∼20 vs. ∼10% of 0.1 C capacity). It is demonstrated that the Sn coating both lithiates and delithiates at a higher voltage than Si and thus imparts a compressive stress around the nanowires. This confines their radial expansion in favor of longitudinal, and reduces the well-known failure mode by lithiation-induced nanowire stranding and fracture. TOF-SIMS analysis on the post-cycled delithiated specimens shows enhanced Li signal near the current collector due to accelerated SEI formation at the interface. FIB demonstrates concurrent en-masse delamination of SEI agglomerated sections of the nanowires from the current collector. Both of these deleterious effects are lessened by the presence of the Sn coatings.
- 28 May 2014
- Published by Royal Society of Chemistry (RSC) in Journal of Materials Chemistry A
- Vol. 2 (29) , 11261-11279
Nanometer-scale Sn coatings improve the performance of silicon nanowire LIB anodes
We demonstrate that a thin partially dewetted coating of Sn will improve the cycling performance of silicon nanowire (SiNWs) lithium ion battery (LIB) anodes. The optimum architecture 3Sn/SiNWs (i.e. a Sn layer with an average film thickness of a 3 nm covering the nanowire) maintained a reversible capacity of 1865 mA h g−1 after 100 cycles at a rate of 0.1 C. This is almost double of the baseline uncoated SiNWs, where the reversible capacity after 100 cycles was 1046 mA h g−1 (∼78% improvement). The 1Sn/SiNWs and 3Sn/SiNWs electrodes demonstrated much improved cycling coulombic efficiency, with >99% vs. 94–98% for the baseline. At a high current density of 5 C, these nanocomposite offered 2× the capacity retention of bare SiNWs (∼20 vs. ∼10% of 0.1 C capacity). It is demonstrated that the Sn coating both lithiates and delithiates at a higher voltage than Si and thus imparts a compressive stress around the nanowires. This confines their radial expansion in favor of longitudinal, and reduces the well-known failure mode by lithiation-induced nanowire stranding and fracture. TOF-SIMS analysis on the post-cycled delithiated specimens shows enhanced Li signal near the current collector due to accelerated SEI formation at the interface. FIB demonstrates concurrent en-masse delamination of SEI agglomerated sections of the nanowires from the current collector. Both of these deleterious effects are lessened by the presence of the Sn coatings.