Arife Dogan
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Research Interests
Arife Dogan has a total of 8 co-authors. Here are the top co-authors by number of shared publications:
Orhan Murat Dogan
Department of Prosthodontics , Cumhuriyet University , Sivas , Turkey
3 shared publicationsSelda Keskin
Department of Prosthodontics , Cumhuriyet University , Sivas , Turkey
2 shared publicationsAli Usanmaz
Department of Chemistry, Middle East Technical University
1 shared publicationArzu Zeynep Yildirim Bicer
Department of Prosthodontics, Faculty of Dentistry , Gazi University , Ankara , Turkey
1 shared publicationGiray Bolayir
Department of Prosthodontics, Faculty of Dentistry, Cumhuriyet University
1 shared publicationHakan Demir
Department of Prosthodontics, Faculty of Dentistry, Cumhuriyet University
1 shared publication
Latest Publications
- 20 March 2013
- Published by Taylor & Francis in The Journal of Adhesion
- Vol. 89 (7) , 594-610
Effect of Argon Plasma Pretreatment on Tensile Bond Strength of a Silicone Soft Liner to Denture Base Polymers
This study evaluated the effect of argon plasma treatment on tensile bonding of heat-cured and auto-polymerized acrylic resins prior to the processing of a silicone soft liner. Both types of polymethylmethacrylate (PMMA) resins were treated with argon plasma for 1 min or 10 min (n = 5). A control group, including untreated resin specimens, was also formed. After processing of the soft liner, the specimens were deflasked and stored dry for 24 h, and they were then subjected to tensile bond strength testing. In order to see the plasma effect on the resin surface chemistry, representative specimens were analysed by XPS. Highest tensile bond strengths were observed in the 1-min exposure group for each resin, and 10-min exposure yielded the lowest bond strength likely due to the damaging effect of the plasma treatment. XPS analysis showed that the O/C ratios increased greatly in treated samples and that the binding energy values were not significantly changed.
- 20 March 2013
- Published by Taylor & Francis in The Journal of Adhesion
- Vol. 89 (7) , 594-610
Effect of Argon Plasma Pretreatment on Tensile Bond Strength of a Silicone Soft Liner to Denture Base Polymers
This study evaluated the effect of argon plasma treatment on tensile bonding of heat-cured and auto-polymerized acrylic resins prior to the processing of a silicone soft liner. Both types of polymethylmethacrylate (PMMA) resins were treated with argon plasma for 1 min or 10 min (n = 5). A control group, including untreated resin specimens, was also formed. After processing of the soft liner, the specimens were deflasked and stored dry for 24 h, and they were then subjected to tensile bond strength testing. In order to see the plasma effect on the resin surface chemistry, representative specimens were analysed by XPS. Highest tensile bond strengths were observed in the 1-min exposure group for each resin, and 10-min exposure yielded the lowest bond strength likely due to the damaging effect of the plasma treatment. XPS analysis showed that the O/C ratios increased greatly in treated samples and that the binding energy values were not significantly changed.
- Open Access
- 1 January 2009
- Published by Japanese Society for Dental Materials and Devices in Dental Materials Journal
- Vol. 28 (3) , 253-260
Temperature rise induced by various light curing units through human dentin
This study investigated temperature rises caused by different light curing units (LCUs) in dentin of different thicknesses. The different LCUs tested in this study were namely: quartz-tungsten-halogen (QTH) (Heliolux DLX) LCU, plasma arc (PAC) (Apollo 95E Elite) LCU, and light emitting diode (LED) (Mini LED) in standard curing mode as well as pulse and soft-start modes. One hundred and forty dentin disks of 0.5, 1, 1.5, and 2 mm thickness were prepared from mandibular molars (n=7). Temperatures were recorded using a L-type thermocouple in direct contact with the light guide tip. For all curing units/modes, dentin thickness was inversely proportional to temperature rise and that QTH light gave significantly higher values compared to PAC and LED in all the test conditions. The highest temperature rise was observed under 0.5-mm-thick dentin disk with QTH, whereas the lowest temperature rise was registered with LED light in pulse mode under 2-mm-thick dentin.
- 1 January 2009
- Published by Japanese Society for Dental Materials and Devices in Dental Materials Journal
- Vol. 28 (3) , 253-260
Open AccessTemperature rise induced by various light curing units through human dentin
This study investigated temperature rises caused by different light curing units (LCUs) in dentin of different thicknesses. The different LCUs tested in this study were namely: quartz-tungsten-halogen (QTH) (Heliolux DLX) LCU, plasma arc (PAC) (Apollo 95E Elite) LCU, and light emitting diode (LED) (Mini LED) in standard curing mode as well as pulse and soft-start modes. One hundred and forty dentin disks of 0.5, 1, 1.5, and 2 mm thickness were prepared from mandibular molars (n=7). Temperatures were recorded using a L-type thermocouple in direct contact with the light guide tip. For all curing units/modes, dentin thickness was inversely proportional to temperature rise and that QTH light gave significantly higher values compared to PAC and LED in all the test conditions. The highest temperature rise was observed under 0.5-mm-thick dentin disk with QTH, whereas the lowest temperature rise was registered with LED light in pulse mode under 2-mm-thick dentin.
- 1 January 2007
- Published by Japanese Society for Dental Materials and Devices in Dental Materials Journal
- Vol. 26 (3) , 329-334
Structure-property Relation of a Soft Liner Material Used in Denture Applications
With a view to understanding the structure-property relation of a silicone-based soft lining denture material after polymerization, its chemical composition and viscoelastic properties were investigated. Chemical compositions of the cured and uncured polymers of a commercial silicone permanent soft liner were determined by infrared spectroscopic analysis, nuclear magnetic resonance (NMR), and X-ray photoelectron spectroscopy. Dynamic mechanical analysis (DMA) method was used to investigate the viscoelastic behavior of the cured polymer of liner. Spectroscopic analysis showed that the main component of soft liner was vinyl-terminated poly(dimethylsiloxane), and the adhesive was 3-methacryloxypropyltrimethoxy silane. NMR results revealed that other components included benzoyl peroxide as initiator for polymerization and also silicilic acid. Surface analysis by XPS provided interesting insights about the nature of adhesive bonding, as well as diffusion of silicilic acid through the matrix of the processed material and leaching-out. DMA results showed a two-phase character, and that the cured polymer was highly elastic.
- 1 January 2007
- Published by Japanese Society for Dental Materials and Devices in Dental Materials Journal
- Vol. 26 (3) , 329-334
Structure-property Relation of a Soft Liner Material Used in Denture Applications
With a view to understanding the structure-property relation of a silicone-based soft lining denture material after polymerization, its chemical composition and viscoelastic properties were investigated. Chemical compositions of the cured and uncured polymers of a commercial silicone permanent soft liner were determined by infrared spectroscopic analysis, nuclear magnetic resonance (NMR), and X-ray photoelectron spectroscopy. Dynamic mechanical analysis (DMA) method was used to investigate the viscoelastic behavior of the cured polymer of liner. Spectroscopic analysis showed that the main component of soft liner was vinyl-terminated poly(dimethylsiloxane), and the adhesive was 3-methacryloxypropyltrimethoxy silane. NMR results revealed that other components included benzoyl peroxide as initiator for polymerization and also silicilic acid. Surface analysis by XPS provided interesting insights about the nature of adhesive bonding, as well as diffusion of silicilic acid through the matrix of the processed material and leaching-out. DMA results showed a two-phase character, and that the cured polymer was highly elastic.