Lynda Amichi
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Lynda Amichi has a total of 121 co-authors. Here are the top co-authors by number of shared publications:
- Catherine Bougerol
Université Grenoble Alpes, CNRS, Institut Néel, 38000 Grenoble, France
6 shared publications Adeline Grenier
Université Grenoble Alpes, CEA, LETI 2 , F-38000 Grenoble, France
5 shared publications- David A. Cullen
Oak Ridge National Laboratory
3 shared publications - David Cooper
LETI, University Grenoble Alpes, CEA 1 , F-38000 Grenoble
3 shared publications - Eva Monroy
Univ. Grenoble-Alpes, CEA, Grenoble INP, IRIG, PHELIQS 4 , 17 av. des Martyrs, Grenoble 38000
3 shared publications Haoran Yu
Center for Nanophase Materials Sciences Oak Ridge National Laboratory Oak Ridge TN 37930 United States
3 shared publications
Latest Publications
- 6 October 2026
- Published by The Electrochemical Society in Journal of the Electrochemical Society
- Vol. 173 (19) , 194502
Ellagic Acid as a Molecular Additive to Unlock Activity and Durability in Platinum Fuel Cell Catalysts
Polymer electrolyte membrane fuel cells (PEMFCs) is promising for heavy-duty transportation sector, yet the high cost of platinum catalysts remains a major barrier to widespread adoption. Here, we report the use of a polyphenolic additive, ellagic acid (EA), to simultaneously enhance the activity and durability of carbon supported platinum (Pt/C) catalysts. Incorporation of EA into the catalyst layer increases the performance at 0.9 V by up to 30%, with improvements directly attributed to the extent of platinum–EA interaction. For catalysts containing platinum within carbon pores, optimizing the ink solvent may enables EA penetration into the pores and further increases mass activity. Durability testing reveals that EA reduces sulfonate anion adsorption, leading to significantly improved catalyst stability under operating conditions. This molecular-level strategy demonstrates how tailored additives can unlock higher activity and resilience in Pt/C catalysts, providing a cost-effective route to advancing PEMFC technology for heavy-duty transport applications.
- 6 October 2026
- Published by The Electrochemical Society in Journal of the Electrochemical Society
- Vol. 173 (19) , 194502
Ellagic Acid as a Molecular Additive to Unlock Activity and Durability in Platinum Fuel Cell Catalysts
Polymer electrolyte membrane fuel cells (PEMFCs) is promising for heavy-duty transportation sector, yet the high cost of platinum catalysts remains a major barrier to widespread adoption. Here, we report the use of a polyphenolic additive, ellagic acid (EA), to simultaneously enhance the activity and durability of carbon supported platinum (Pt/C) catalysts. Incorporation of EA into the catalyst layer increases the performance at 0.9 V by up to 30%, with improvements directly attributed to the extent of platinum–EA interaction. For catalysts containing platinum within carbon pores, optimizing the ink solvent may enables EA penetration into the pores and further increases mass activity. Durability testing reveals that EA reduces sulfonate anion adsorption, leading to significantly improved catalyst stability under operating conditions. This molecular-level strategy demonstrates how tailored additives can unlock higher activity and resilience in Pt/C catalysts, providing a cost-effective route to advancing PEMFC technology for heavy-duty transport applications.
- Open Access
- 12 August 2026
- Published by Wiley in Advanced Materials
- Vol. 38 (57) , e74561
Adsorption‐Engineered Hydrocarbon Ionomers for Durable Proton‐Exchange Membrane Fuel Cells
Reducing reliance on perfluoroalkyl substances (PFAS) in proton‐exchange membrane fuel cells requires hydrocarbon ionomers that combine high performance with long‐term durability, a persistent challenge in catalyst‐layer design. Here, we identify oxidation‐driven ionomer‐catalyst interfacial degradation as a dominant failure pathway in hydrocarbon ionomer‐bonded cathodes and introduce an adsorption‐engineering strategy to overcome this limitation. The comparison of a commercial sulfonated poly(phenylene) (Pemion) with structurally engineered sulfonated poly(fluorene)s demonstrated that electrode durability is governed by the interplay between ionomer adsorption strength and resistance to oxidative degradation on carbon‐supported Pt catalysts. A poly(fluorene) ionomer with mobile alkyl sulfonic acid groups forms resilient interfaces, delivering 1.28 A cm − 2 at 0.65 V under fully humidified H 2 /air conditions (80°C and 150 kPa abs ), comparable to Pemion. After 90,000 accelerated potential cycles, the poly(fluorene)‐bonded cathode exhibits significantly improved durability, with only 29% performance loss compared to 58% for Pemion; further molecular refinement reduces the loss to 17%, approaching that of Nafion‐bonded cathodes (14%). These findings establish adsorption‐engineered ionomer design that decouples interfacial anchoring from oxidative degradation as a general strategy for achieving durable, high‐performance PFAS‐free PEM fuel cell electrodes.
- 12 August 2026
- Published by Wiley in Advanced Materials
- Vol. 38 (57) , e74561
Open AccessAdsorption‐Engineered Hydrocarbon Ionomers for Durable Proton‐Exchange Membrane Fuel Cells
Reducing reliance on perfluoroalkyl substances (PFAS) in proton‐exchange membrane fuel cells requires hydrocarbon ionomers that combine high performance with long‐term durability, a persistent challenge in catalyst‐layer design. Here, we identify oxidation‐driven ionomer‐catalyst interfacial degradation as a dominant failure pathway in hydrocarbon ionomer‐bonded cathodes and introduce an adsorption‐engineering strategy to overcome this limitation. The comparison of a commercial sulfonated poly(phenylene) (Pemion) with structurally engineered sulfonated poly(fluorene)s demonstrated that electrode durability is governed by the interplay between ionomer adsorption strength and resistance to oxidative degradation on carbon‐supported Pt catalysts. A poly(fluorene) ionomer with mobile alkyl sulfonic acid groups forms resilient interfaces, delivering 1.28 A cm − 2 at 0.65 V under fully humidified H 2 /air conditions (80°C and 150 kPa abs ), comparable to Pemion. After 90,000 accelerated potential cycles, the poly(fluorene)‐bonded cathode exhibits significantly improved durability, with only 29% performance loss compared to 58% for Pemion; further molecular refinement reduces the loss to 17%, approaching that of Nafion‐bonded cathodes (14%). These findings establish adsorption‐engineered ionomer design that decouples interfacial anchoring from oxidative degradation as a general strategy for achieving durable, high‐performance PFAS‐free PEM fuel cell electrodes.
- 23 September 2024
- Published by Wiley in Advanced Energy Materials
- Vol. 14 (43)
A Three–Dimensional Nanoscale View of Electrocatalyst Degradation in Hydrogen Fuel Cells
The loss of platinum (Pt) electrochemically active surface area (ECSA) is a critical degradation mode that often becomes a limiting factor for heavy‐duty proton exchange membrane fuel cell vehicles. High surface area carbon supports have been shown to improve Pt dispersion and limit detrimental ionomer‐electrocatalyst interactions due to their large interior pore volume. In this work, using automated scanning transmission electron tomography, the degradation of nanoparticles located on the interior versus exterior surfaces of the carbon support is compared following a catalyst‐specific accelerated stress test (AST) of 90,000 voltage cycles between 0.6 V to 0.95 V. The results reveal a notable increase in median particle size for both interior and exterior Pt catalyst particles, with a slightly higher increase in particle size distribution and loss of specific surface area for the particles located on the exterior carbon surface. The fraction of Pt nanoparticles that reside within the interior of the carbon support also increased following the AST test, accompanied by evidence of an increase in average carbon mesopore size. The results shed light on the degradation mechanisms affecting electrochemical properties and the enhanced particle accessibility at lower relative humidity.
- 23 September 2024
- Published by Wiley in Advanced Energy Materials
- Vol. 14 (43)
A Three–Dimensional Nanoscale View of Electrocatalyst Degradation in Hydrogen Fuel Cells
The loss of platinum (Pt) electrochemically active surface area (ECSA) is a critical degradation mode that often becomes a limiting factor for heavy‐duty proton exchange membrane fuel cell vehicles. High surface area carbon supports have been shown to improve Pt dispersion and limit detrimental ionomer‐electrocatalyst interactions due to their large interior pore volume. In this work, using automated scanning transmission electron tomography, the degradation of nanoparticles located on the interior versus exterior surfaces of the carbon support is compared following a catalyst‐specific accelerated stress test (AST) of 90,000 voltage cycles between 0.6 V to 0.95 V. The results reveal a notable increase in median particle size for both interior and exterior Pt catalyst particles, with a slightly higher increase in particle size distribution and loss of specific surface area for the particles located on the exterior carbon surface. The fraction of Pt nanoparticles that reside within the interior of the carbon support also increased following the AST test, accompanied by evidence of an increase in average carbon mesopore size. The results shed light on the degradation mechanisms affecting electrochemical properties and the enhanced particle accessibility at lower relative humidity.
- Open Access
- 24 July 2024
- Published by Oxford University Press (OUP) in Microscopy and Microanalysis
- Vol. 30 (Supplement)
Stability of Carbon-Supported Nanoparticles in Hydrogen Fuel Cells Resolved by Automated Electron Tomography
Proton exchange membrane fuel cells (PEMFC) offer great promise for hydrogen powered heavy duty trucks requiring a higher density of energy, fast refueling and additional range. Nevertheless, durability remains a significant challenge, primarily stemming from catalyst degradation in the cathode. Addressing these performance losses necessitates a deeper comprehension of degradation mechanisms under accelerated stress tests (ASTs) through structural characterization and localization. Electron tomography emerges as a key tool for linking the degradation rate and mechanism of Pt-based nanoparticles relative to their location on or within the porous carbon support [ 1, 2].
- 24 July 2024
- Published by Oxford University Press (OUP) in Microscopy and Microanalysis
- Vol. 30 (Supplement)
Open AccessStability of Carbon-Supported Nanoparticles in Hydrogen Fuel Cells Resolved by Automated Electron Tomography
Proton exchange membrane fuel cells (PEMFC) offer great promise for hydrogen powered heavy duty trucks requiring a higher density of energy, fast refueling and additional range. Nevertheless, durability remains a significant challenge, primarily stemming from catalyst degradation in the cathode. Addressing these performance losses necessitates a deeper comprehension of degradation mechanisms under accelerated stress tests (ASTs) through structural characterization and localization. Electron tomography emerges as a key tool for linking the degradation rate and mechanism of Pt-based nanoparticles relative to their location on or within the porous carbon support [ 1, 2].
- Open Access
- 22 November 2023
- Published by Springer Nature in Nature Communications
- Vol. 14 (1) , 1-11
A scalable membrane electrode assembly architecture for efficient electrochemical conversion of CO2 to formic acid
The electrochemical reduction of carbon dioxide to formic acid is a promising pathway to improve CO2 utilization and has potential applications as a hydrogen storage medium. In this work, a zero-gap membrane electrode assembly architecture is developed for the direct electrochemical synthesis of formic acid from carbon dioxide. The key technological advancement is a perforated cation exchange membrane, which, when utilized in a forward bias bipolar membrane configuration, allows formic acid generated at the membrane interface to exit through the anode flow field at concentrations up to 0.25 M. Having no additional interlayer components between the anode and cathode this concept is positioned to leverage currently available materials and stack designs ubiquitous in fuel cell and H2 electrolysis, enabling a more rapid transition to scale and commercialization. The perforated cation exchange membrane configuration can achieve >75% Faradaic efficiency to formic acid at 2 in a 25 cm2 cell. More critically, a 55-hour stability test at 200 mA/cm2 shows stable Faradaic efficiency and cell voltage. Technoeconomic analysis is utilized to illustrate a path towards achieving cost parity with current formic acid production methods.
- 22 November 2023
- Published by Springer Nature in Nature Communications
- Vol. 14 (1) , 1-11
Open AccessA scalable membrane electrode assembly architecture for efficient electrochemical conversion of CO2 to formic acid
The electrochemical reduction of carbon dioxide to formic acid is a promising pathway to improve CO2 utilization and has potential applications as a hydrogen storage medium. In this work, a zero-gap membrane electrode assembly architecture is developed for the direct electrochemical synthesis of formic acid from carbon dioxide. The key technological advancement is a perforated cation exchange membrane, which, when utilized in a forward bias bipolar membrane configuration, allows formic acid generated at the membrane interface to exit through the anode flow field at concentrations up to 0.25 M. Having no additional interlayer components between the anode and cathode this concept is positioned to leverage currently available materials and stack designs ubiquitous in fuel cell and H2 electrolysis, enabling a more rapid transition to scale and commercialization. The perforated cation exchange membrane configuration can achieve >75% Faradaic efficiency to formic acid at 2 in a 25 cm2 cell. More critically, a 55-hour stability test at 200 mA/cm2 shows stable Faradaic efficiency and cell voltage. Technoeconomic analysis is utilized to illustrate a path towards achieving cost parity with current formic acid production methods.
- Open Access
- 22 July 2023
- Published by Oxford University Press (OUP) in Microscopy and Microanalysis
- Vol. 29 (Supplement) , 1742-1743
Investigation of Nanoparticle Degradation in Hydrogen Fuel Cell Systems through Automated Electron Microscopy
Proton exchange membrane fuel cells (PEMFC) are promising devices for the deployment of hydrogen-powered heavy-duty vehicles, providing a higher efficiency and similar driving range and fueling time compared to internal combustion engine vehicles. However, PEMFCs still encounter durability challenges, mainly due to catalyst degradation in the cathode. Mitigating these performance losses requires a better understanding of the degradation mechanisms under heavy-duty accelerated stress tests (ASTs) [ 1]. Scanning transmission electron microscopy (STEM) combined with energy dispersive X-ray spectroscopy (EDS) is a key tool for analysis of Pt and PtCo nanoparticle size, spatial distribution, and composition [ 2]. In addition, electron tomography can be used to determine the rate and type of catalyst nanoparticle degradation as a function of position on the carbon support [ 3].
- 22 July 2023
- Published by Oxford University Press (OUP) in Microscopy and Microanalysis
- Vol. 29 (Supplement) , 1742-1743
Open AccessInvestigation of Nanoparticle Degradation in Hydrogen Fuel Cell Systems through Automated Electron Microscopy
Proton exchange membrane fuel cells (PEMFC) are promising devices for the deployment of hydrogen-powered heavy-duty vehicles, providing a higher efficiency and similar driving range and fueling time compared to internal combustion engine vehicles. However, PEMFCs still encounter durability challenges, mainly due to catalyst degradation in the cathode. Mitigating these performance losses requires a better understanding of the degradation mechanisms under heavy-duty accelerated stress tests (ASTs) [ 1]. Scanning transmission electron microscopy (STEM) combined with energy dispersive X-ray spectroscopy (EDS) is a key tool for analysis of Pt and PtCo nanoparticle size, spatial distribution, and composition [ 2]. In addition, electron tomography can be used to determine the rate and type of catalyst nanoparticle degradation as a function of position on the carbon support [ 3].
- 13 July 2021
- Published by AIP Publishing in Journal of Applied Physics
- Vol. 130 (2) , 025704
Mapping of the electrostatic potentials in MOCVD and hybrid GaN tunnel junctions for InGaN/GaN blue emitting light emitting diodes by off-axis electron holography correlated with structural, chemical, and optoelectronic characterization
Off-axis electron holography has been used to measure the width of the depletion region in a series of tunnel junction GaN light emitting diodes that have been prepared using different growth processes for blue emission. The total measured potentials are combinations of the mean inner potential, dopant potential, and piezoelectric contributions. The dopant potential has been unmixed from the mean inner potential such that the width of the tunnel junctions in the different diodes can be measured. The experimental results are then compared to secondary ion mass spectrometry, simulations, and opto-electronic testing. We find that the measured tunnel junction widths are consistent with simulations as well as the current density and voltage characteristics. As such, off-axis electron holography has been demonstrated as a unique technique that can be used to reproducibly measure the electrostatic potentials in tunnel junctions with nm-scale resolution in real III–V device specimens.
- 13 July 2021
- Published by AIP Publishing in Journal of Applied Physics
- Vol. 130 (2) , 025704
Mapping of the electrostatic potentials in MOCVD and hybrid GaN tunnel junctions for InGaN/GaN blue emitting light emitting diodes by off-axis electron holography correlated with structural, chemical, and optoelectronic characterization
Off-axis electron holography has been used to measure the width of the depletion region in a series of tunnel junction GaN light emitting diodes that have been prepared using different growth processes for blue emission. The total measured potentials are combinations of the mean inner potential, dopant potential, and piezoelectric contributions. The dopant potential has been unmixed from the mean inner potential such that the width of the tunnel junctions in the different diodes can be measured. The experimental results are then compared to secondary ion mass spectrometry, simulations, and opto-electronic testing. We find that the measured tunnel junction widths are consistent with simulations as well as the current density and voltage characteristics. As such, off-axis electron holography has been demonstrated as a unique technique that can be used to reproducibly measure the electrostatic potentials in tunnel junctions with nm-scale resolution in real III–V device specimens.
- 10 February 2020
- Published by AIP Publishing in Journal of Applied Physics
- Vol. 127 (6) , 065702
Three-dimensional measurement of Mg dopant distribution and electrical activity in GaN by correlative atom probe tomography and off-axis electron holography
The distribution and electrical activity of p-type doping (Mg) in gallium nitride (GaN) grown by metal organic chemical vapor deposition was investigated by correlating atom probe tomography (APT) and off-axis electron holography. APT results revealed that high Mg concentrations promote the formation of Mg-rich clusters. This is associated with the formation of pyramidal inversion domains (PIDs). The direct measurement of the doping concentration outside the clusters provided by APT suggests a saturation in the p-type electrical activity for Mg concentrations above 7 × 1019 cm−3. Maps of the electrostatic potential provided by off-axis electron holography confirm that the highest carrier concentration was achieved in the regions with the highest dopant concentration of 2 × 1020 cm−3, despite the presence of a high density of Mg-rich clusters revealed by APT. The correlation of these techniques suggests that PIDs are not the major cause of the reduction in electrostatic potential.
- 10 February 2020
- Published by AIP Publishing in Journal of Applied Physics
- Vol. 127 (6) , 065702
Three-dimensional measurement of Mg dopant distribution and electrical activity in GaN by correlative atom probe tomography and off-axis electron holography
The distribution and electrical activity of p-type doping (Mg) in gallium nitride (GaN) grown by metal organic chemical vapor deposition was investigated by correlating atom probe tomography (APT) and off-axis electron holography. APT results revealed that high Mg concentrations promote the formation of Mg-rich clusters. This is associated with the formation of pyramidal inversion domains (PIDs). The direct measurement of the doping concentration outside the clusters provided by APT suggests a saturation in the p-type electrical activity for Mg concentrations above 7 × 1019 cm−3. Maps of the electrostatic potential provided by off-axis electron holography confirm that the highest carrier concentration was achieved in the regions with the highest dopant concentration of 2 × 1020 cm−3, despite the presence of a high density of Mg-rich clusters revealed by APT. The correlation of these techniques suggests that PIDs are not the major cause of the reduction in electrostatic potential.
- Open Access
- 25 October 2019
- Published by IOP Publishing in Nanotechnology
- Vol. 31 (4) , 045702
Correlative investigation of Mg doping in GaN layers grown at different temperatures by atom probe tomography and off-axis electron holography
Correlation between off-axis electron holography and atom probe tomography (APT) provides morphological, chemical and electrical information about Mg doping (p-type) in gallium nitride (GaN) layers that have been grown at different temperatures at a nanometric scale. APT allows access to the three-dimensional distribution of atoms and their chemical nature. In particular, this technique allows visualisation of the Mg-rich clusters observed in p-doped GaN layers grown by metal-organic chemical vapour deposition. As the layer growth temperature increases, the cluster density decreases but their size indicted by the number of atoms increases. Moreover, APT reveals that threading dislocations are decorated with Mg atoms. Off-axis electron holography provides complementary information about the electrical activity of the Mg doping. As only a small fraction of dopant atoms are ionised at room temperature, this fraction is increased by annealing the specimen to 400 °C in situ in a transmission electron microscope (TEM). A strong reduction of the dopant electrical activity is observed for increases in the layer growth temperature. The correlation of APT with TEM-based techniques was shown to be a unique approach in order to investigate how the growth temperature affects both the chemical distribution and electrical activity of Mg dopant atoms.
- 25 October 2019
- Published by IOP Publishing in Nanotechnology
- Vol. 31 (4) , 045702
Open AccessCorrelative investigation of Mg doping in GaN layers grown at different temperatures by atom probe tomography and off-axis electron holography
Correlation between off-axis electron holography and atom probe tomography (APT) provides morphological, chemical and electrical information about Mg doping (p-type) in gallium nitride (GaN) layers that have been grown at different temperatures at a nanometric scale. APT allows access to the three-dimensional distribution of atoms and their chemical nature. In particular, this technique allows visualisation of the Mg-rich clusters observed in p-doped GaN layers grown by metal-organic chemical vapour deposition. As the layer growth temperature increases, the cluster density decreases but their size indicted by the number of atoms increases. Moreover, APT reveals that threading dislocations are decorated with Mg atoms. Off-axis electron holography provides complementary information about the electrical activity of the Mg doping. As only a small fraction of dopant atoms are ionised at room temperature, this fraction is increased by annealing the specimen to 400 °C in situ in a transmission electron microscope (TEM). A strong reduction of the dopant electrical activity is observed for increases in the layer growth temperature. The correlation of APT with TEM-based techniques was shown to be a unique approach in order to investigate how the growth temperature affects both the chemical distribution and electrical activity of Mg dopant atoms.
- 1 June 2019
- Published by Institute of Electrical and Electronics Engineers (IEEE)
- p. 1-5
Doping of GaN grown on silicon via ion implantation
- 1 June 2019
- Published by Institute of Electrical and Electronics Engineers (IEEE)
- p. 1-5
Doping of GaN grown on silicon via ion implantation