Joong Eun Jung
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Joong Eun Jung has a total of 16 co-authors. Here are the top co-authors by number of shared publications:
- Baig-Gyu Choi
High Temperature Materials Department, Korea Institute of Materials Science, Changwon 51508, Korea
1 shared publication - Deok Hyun Jo
Department of Materials Science and Engineering, Dong-A University, Busan 49315, Republic of Korea
1 shared publication - Deuk Hyun Son
School of Materials Science and Engineering, Pusan National University, Busan 46241, Republic of Korea
1 shared publication - Durim Eo
Korea Additive Manufacturing Innovation Center, Korea Institute of Industrial Technology, Siheung, Republic of Korea
1 shared publication - Hee Pyeong Yang
Department of Materials Science and Engineering, Dong-A University, Busan 49315, Republic of Korea
1 shared publication - Hyub Lee
Customized Manufacturing R&D Department, Korea Institute of Industrial Technology (KITECH), Siheung, Republic of Korea
1 shared publication
Latest Publications
- Open Access
Microstructure and Mechanical Properties of Wire Laser Additive Manufactured Deposits and Their Tungsten Inert Gas Welds
Ti-6Al-4V (Ti64) alloy is widely utilized in the aerospace industry due to its high strength, fatigue resistance, corrosion resistance, and cryogenic properties. However, its high raw material costs and machining difficulties necessitate the development of efficient manufacturing processes. This study evaluates the mechanical reliability and microstructure of Ti64 components fabricated using wire laser additive manufacturing (WLAM) and subsequently joined via tungsten inert gas (TIG) welding. The WLAM process produces refined microstructures with superior mechanical properties by minimizing defects; however, insufficient process optimization may result in a lack of fusion (LOF) and porosity. Microstructural analysis revealed that the WLAM deposits exhibited a fine basket-weave α structure with an average α-lath width of 1.27 ± 0.69 μm, while the TIG-welded region exhibited a coarsened α-lath, reaching 3.02 ± 2.06 μm, which led to a reduction in ductility. Tensile testing demonstrated that the WLAM deposits exhibited superior mechanical properties, with a yield strength of 910 MPa, ultimate tensile strength of 1015 MPa, and elongation of 12.8%, outperforming conventional wrought Ti64 alloys. Conversely, the TIG-welded joints exhibited reduced mechanical properties, with a yield strength of 812 MPa, ultimate tensile strength of 917 MPa, and elongation of 7.5%, primarily attributed to microstructural coarsening in the weld region. The findings of this study confirm that WLAM enhances the mechanical properties of Ti64, whereas TIG welding may introduce structural weaknesses. This research provides insight into the microstructural evolution and mechanical behavior of WLAM-fabricated Ti64 components, with valuable implications for their application in aerospace structures.
Open AccessMicrostructure and Mechanical Properties of Wire Laser Additive Manufactured Deposits and Their Tungsten Inert Gas Welds
Ti-6Al-4V (Ti64) alloy is widely utilized in the aerospace industry due to its high strength, fatigue resistance, corrosion resistance, and cryogenic properties. However, its high raw material costs and machining difficulties necessitate the development of efficient manufacturing processes. This study evaluates the mechanical reliability and microstructure of Ti64 components fabricated using wire laser additive manufacturing (WLAM) and subsequently joined via tungsten inert gas (TIG) welding. The WLAM process produces refined microstructures with superior mechanical properties by minimizing defects; however, insufficient process optimization may result in a lack of fusion (LOF) and porosity. Microstructural analysis revealed that the WLAM deposits exhibited a fine basket-weave α structure with an average α-lath width of 1.27 ± 0.69 μm, while the TIG-welded region exhibited a coarsened α-lath, reaching 3.02 ± 2.06 μm, which led to a reduction in ductility. Tensile testing demonstrated that the WLAM deposits exhibited superior mechanical properties, with a yield strength of 910 MPa, ultimate tensile strength of 1015 MPa, and elongation of 12.8%, outperforming conventional wrought Ti64 alloys. Conversely, the TIG-welded joints exhibited reduced mechanical properties, with a yield strength of 812 MPa, ultimate tensile strength of 917 MPa, and elongation of 7.5%, primarily attributed to microstructural coarsening in the weld region. The findings of this study confirm that WLAM enhances the mechanical properties of Ti64, whereas TIG welding may introduce structural weaknesses. This research provides insight into the microstructural evolution and mechanical behavior of WLAM-fabricated Ti64 components, with valuable implications for their application in aerospace structures.
- Open Access
Effect of Laser Power on the Recrystallization Temperature of an Additively Manufactured IN718
Over the past few decades, there has been much research on additive manufacturing in both the academic and the industrial spheres to overcome the limitations of conventional manufacturing methods, thereby enabling the production of complex designs for improved performance. To achieve this purpose, it is crucial to meticulously set suitable laser parameters within the context of microstructural characteristics, including type and fraction of defects, texture development, residual stress, and grain size, etc. In the present study, we focused on recrystallization behavior, a type of relaxation process for accumulated thermal stress during the L-PBF process, as a function of laser power applied on the L-PBF process. The laser power has significant effects on the amount of recrystallized grain, directly related to the recrystallization temperature. Within the range of laser power used in this study, a downward trend was observed in the recrystallization temperature as the laser power increased from 370 W to 390 W. This trend suggests that higher laser power leads to a faster cooling rate, influenced by the volume of melt pool as well as the amount of heat dissipation from the melt pool, resulting in higher thermal stress during the process.
Open AccessEffect of Laser Power on the Recrystallization Temperature of an Additively Manufactured IN718
Over the past few decades, there has been much research on additive manufacturing in both the academic and the industrial spheres to overcome the limitations of conventional manufacturing methods, thereby enabling the production of complex designs for improved performance. To achieve this purpose, it is crucial to meticulously set suitable laser parameters within the context of microstructural characteristics, including type and fraction of defects, texture development, residual stress, and grain size, etc. In the present study, we focused on recrystallization behavior, a type of relaxation process for accumulated thermal stress during the L-PBF process, as a function of laser power applied on the L-PBF process. The laser power has significant effects on the amount of recrystallized grain, directly related to the recrystallization temperature. Within the range of laser power used in this study, a downward trend was observed in the recrystallization temperature as the laser power increased from 370 W to 390 W. This trend suggests that higher laser power leads to a faster cooling rate, influenced by the volume of melt pool as well as the amount of heat dissipation from the melt pool, resulting in higher thermal stress during the process.