Eafanti
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Eafanti has a total of 4 co-authors. Here are the top co-authors by number of shared publications:
- Jared Tracy
National Institute of Standards and Technology,Gaithersburg,MD,United States
1 shared publication - Nick Bosco
National Renewable Energy Laboratory, Golden, CO, USA
1 shared publication - Reinhold Horst Dauskardt
Stanford University
1 shared publication - Sarah Kurtz
University of California, Merced, CA, USA
1 shared publication
Latest Publications
- Open Access
- 4 October 2017
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Journal of Photovoltaics
- Vol. 7 (6) , 1536-1540
Defining Threshold Values of Encapsulant and Backsheet Adhesion for PV Module Reliability
The width-tapered cantilever beam method is used to quantify the debond energy (adhesion) of encapsulant and backsheet structures of 32 modules collected from the field. The collected population of modules contains both those that have remained intact and those with instances of either or both encapsulant and backsheet delamination. From this survey, initial threshold values (an adhesion value above which a module should remain intact throughout its lifetime) for encapsulant and backsheet interfaces are proposed. For encapsulants this value is ∼$160\,{\text{J}\text{/}\text{m}}^{2}$ and for backsheets ∼$10\,{\text{J}\text{/}\text{m}}^{2}$. It is expected that these values will continue to be refined and evolve as the width-tapered cantilever beam method gets adopted by the PV industry, and that they may aid in the future improvement of accelerated lifetime tests and the development of new, low-cost materials.
- 4 October 2017
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Journal of Photovoltaics
- Vol. 7 (6) , 1536-1540
Open AccessDefining Threshold Values of Encapsulant and Backsheet Adhesion for PV Module Reliability
The width-tapered cantilever beam method is used to quantify the debond energy (adhesion) of encapsulant and backsheet structures of 32 modules collected from the field. The collected population of modules contains both those that have remained intact and those with instances of either or both encapsulant and backsheet delamination. From this survey, initial threshold values (an adhesion value above which a module should remain intact throughout its lifetime) for encapsulant and backsheet interfaces are proposed. For encapsulants this value is ∼$160\,{\text{J}\text{/}\text{m}}^{2}$ and for backsheets ∼$10\,{\text{J}\text{/}\text{m}}^{2}$. It is expected that these values will continue to be refined and evolve as the width-tapered cantilever beam method gets adopted by the PV industry, and that they may aid in the future improvement of accelerated lifetime tests and the development of new, low-cost materials.