MAMaman Kartaman Ajiriyanto

Maman Kartaman Ajiriyanto

*This is an algorithmically generated author record based on publicly available information.

Current Organizations / Institutes

The organizations/institutes from the scholar's latest article


Maman Kartaman Ajiriyanto has a total of 6 co-authors. Here are the top co-authors by number of shared publications:

  • A S D Putri

    Center for Nuclear Fuel Technology – National Nuclear Energy Agency of Indonesia BATAN, Kawasan PUSPIPTEK Gd. 20, Tangerang Selatan, Banten, 15310, Indonesia

    1 shared publication
  • Dian Anggraini

    Pusat Teknologi Bahan Bakar Nuklir-BATAN

    1 shared publication
  • E Nurlaily

    Center for Nuclear Fuel Technology – National Nuclear Energy Agency of Indonesia BATAN, Kawasan PUSPIPTEK Gd. 20, Tangerang Selatan, Banten, 15310, Indonesia

    1 shared publication
  • J Cs Sihotang

    Center for Nuclear Fuel Technology – National Nuclear Energy Agency of Indonesia BATAN, Kawasan PUSPIPTEK Gd. 20, Tangerang Selatan, Banten, 15310, Indonesia

    1 shared publication
  • N A Kundari

    Polytechnic Institute of Nuclear Technology - National Nuclear Energy Agency (BATAN), Yogyakarta, Indonesia

    1 shared publication
  • Rosika Kriswarini

    Pusat Teknologi Bahan Bakar Nuklir-BATAN

    1 shared publication

Latest Publications

  • Open Access

    Corrosion analysis of post-heat treatment and post-weld SS316 with electrokinetic reactivation and cyclic polarization method

    by M Kartaman A, E Nurlaily, A S D Putri, J Cs Sihotang, N A Kundari

    Austenitic stainless steel 316 has very high mechanical properties and corrosion resistance. This type of steel is widely used both in the nuclear and non-nuclear industries. In the nuclear industry, SS316 is used as a cladding material for uranium fuel due to its good corrosion and mechanical properties, and also low neutron absorption cross-section. In the Center for Nuclear Fuel Technology (PTBBN BATAN), it is used as material for the container of nuclear waste that is to be stored on Temporary Storage Installation of Spent Fuel (KHIPSB3 BATAN). SS316 is used as material for can to contain high-activity solid waste from the testing activity in Radiometallurgy Installation (IRM BATAN). The lid of the container is sealed with the GTAW welding process in order to tightly contain the solid waste. The main problem with the heat treatment and welding process of austenitic stainless steel is the occurrence of sensitization in a temperature range of 500-800°C. Therefore fully electrochemical analysis of SS316 stainless steel in various mediums has been conducted. SS 316 specimen was heat-treated to simulate the heat generated by the welding process. Sensitization analysis was conducted with qualitative and quantitative methods by EIS and EPR, and pitting corrosion resistance was by cyclic polarization method. The solution used for EIS and cyclic polarization test was 0 − 3.5% concentration of NaCl, and for EPR test was a mixture of H2SO4and KSCN. Material characterization before and after corrosion testing was microstructure examination. The result of the corrosion test showed that heat treatment on the temperature range of 500-800°C caused sensitization. The corrosion test curve result showed that a heat treatment temperature of 650°C for 1 hour had the highest activation current. The lowest Rp value for SS316 specimen post heat treatment in 675°C was 69.410 ohm. The welded SS316 specimen had a higher corrosion current than that of the unwelded specimen. The microstructure of the welded specimen showed that there was intergranular corrosion particularly in the HAZ region. The effect of NaCl concentration on the cyclic polarization test showed that the higher the NaCl concentration, the more easily the pitting corrosion. The indication of pitting corrosion occurrence was evaluated by considering the Epitand Erpvalues. The lower Epitvalue meant that pitting corrosion was more easily to occur.


  • Open Access

    Analisis Korosi Paduan ZIRLO-Mo Dalam Media NaCl Menggunakan Metode Polarisasi

    by Maman Kartaman Ajiriyanto, Dian Anggraini, Rosika Kriswarini

    Paduan zirlo-Mo merupakan jenis paduan logam zirkonium yang dapat dikembangkan menjadi bahan kelongsong reaktor pendingin air ringan. Parameter penting yang harus diketahui sebagai bahan kelongsong adalah sifat ketahanan korosi. Tujuan penelitian ini adalah untuk mengetahui ketahanan korosi paduan zirlo-Mo dalam media NaCl dengan variasi konsentrasi 0,03; 0,3 dan 3 % dan dibandingkan dengan ketahanan korosi paduan zircaloy-2 dan zircaloy-4 pada media yang sama. Sampel uji dibuat berbentuk disk kemudian dimounting dan dipreparasi metalografi meliputi pengamplasan menggunakan kertas SiC dengan ukuran 500 sampai 1200 grit secara bertahap. Laju korosi zirlo-Mo dianalisis menggunakan metode polarisasi menggunakan alat Potensiostat. Keunggulan metode tahanan polarisasi adalah waktu pengujian korosi relatif lebih cepat dibandingkan dengan metode perubahan berat, selain itu metode ini dapat menentukan laju korosi yang sangat rendah yaitu kurang dari 0,1 mpy. Pengujian lain yang dilakukan untuk mendukung analisis laju korosi adalah pengujian kekerasan mikro dengan Microhardness Tester dan pengamatan mikrostruktur mengunakan Mikroskop optik. Hasil pengujian menunjukkan bahwa paduan zirlo-Mo, zircaloy-2 dan zircaloy-4 secara keseluruhan memiliki laju korosi sangat rendah yaitu kurang dari 1 mpy. Laju korosi paduan zircaloy-2 dan zircaloy-4 dan zirlo-Mo pada media NaCl 3 % berturut-turut adalah 0,006; 0,007 and 0,590 mpy. Laju korosi paduan zirlo-Mo adalah relatif paling tinggi, hal ini disebabkan karena paduan zirlo-Mo mempunyai struktur lath martensit atau accicular yang memiliki kekerasan tinggi. Struktur lath martensit dan kekerasan tinggi sangat rentan terhadap korosi. Nilai kekerasan paduan zircaloy-2, zircaloy-4 dan zirlo-Mo berturut-turut adalah 194,79; 227,95 and 360,05 HV. Adanya larutan padat Mo dan matrik Zr-α serta struktur martensite atau accicular pada paduan zirlo-Mo mengakibatkan kekerasan paduan menjadi tinggi. Kata kunci: laju korosi, tahanan polarisasi, paduan zirlo-Mo, mikrostruktur, kekerasan mikro