Merve Aksit
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Merve Aksit has a total of 10 co-authors. Here are the top co-authors by number of shared publications:
- Volker Altstädt
Polymer Engineering, University of Bayreuth, Bayreuth, Germany
4 shared publications - Alper Aksit
Department of Polymer Engineering, University of Bayreuth, Universitätsstraße 30, 95447 Bayreuth, Germany
3 shared publications - Hans-Werner Schmidt
Macromolecular Chemistry and Bavarian Polymer Institute, University of Bayreuth, Universitätsstraße 30, 95447 Bayreuth, Germany
2 shared publications - Klaus Kreger
Macromolecular Chemistry and Bavarian Polymer Institute, University of Bayreuth, Universitätsstraße 30, 95447 Bayreuth, Germany
2 shared publications - Bastian Klose
Macromolecular Chemistry I, University of Bayreuth, Universitaetsstrasse 30, 95447 Bayreuth, Germany
1 shared publication - Chunjing Zhao
Depatment of Polymer Engineering, University Bayreuth, Universitätsstraße 30, 95447 Bayreuth, Germany
1 shared publication
Latest Publications
- Open Access
Low-Density Polybutylene Terephthalate Foams with Enhanced Compressive Strength via a Reactive-Extrusion Process
Due to their appealing properties such as high-temperature dimensional stability, chemical resistance, compressive strength and recyclability, new-generation foams based on engineering thermoplastics such as polyethylene terephthalate (PET) and polybutylene terephthalate (PBT) have been gaining significant attention. Achieving low-density foams without sacrificing the mechanical properties is of vital importance for applications in the field of transportation and construction, where sufficient compressive strength is desired. In contrast to numerous research studies on PET foams, only a limited number of studies on PBT foams and in particular, on extruded PBT foams are known. Here we present a novel route to extruded PBT foams with densities as low as 80 kg/m3 and simultaneously with improved compressive properties manufactured by a tandem reactive-extrusion process. Improved rheological properties and therefore process stability were achieved using two selected 1,3,5-benzene-trisamides (BTA1 and BTA2), which are able to form supramolecular nanofibers in the PBT melt upon cooling. With only 0.08 wt % of BTA1 and 0.02 wt % of BTA2 the normalized compressive strength was increased by 28% and 15%, respectively. This improvement is assigned to the intrinsic reinforcing effect of BTA fibers in the cell walls and struts.
Open AccessLow-Density Polybutylene Terephthalate Foams with Enhanced Compressive Strength via a Reactive-Extrusion Process
Due to their appealing properties such as high-temperature dimensional stability, chemical resistance, compressive strength and recyclability, new-generation foams based on engineering thermoplastics such as polyethylene terephthalate (PET) and polybutylene terephthalate (PBT) have been gaining significant attention. Achieving low-density foams without sacrificing the mechanical properties is of vital importance for applications in the field of transportation and construction, where sufficient compressive strength is desired. In contrast to numerous research studies on PET foams, only a limited number of studies on PBT foams and in particular, on extruded PBT foams are known. Here we present a novel route to extruded PBT foams with densities as low as 80 kg/m3 and simultaneously with improved compressive properties manufactured by a tandem reactive-extrusion process. Improved rheological properties and therefore process stability were achieved using two selected 1,3,5-benzene-trisamides (BTA1 and BTA2), which are able to form supramolecular nanofibers in the PBT melt upon cooling. With only 0.08 wt % of BTA1 and 0.02 wt % of BTA2 the normalized compressive strength was increased by 28% and 15%, respectively. This improvement is assigned to the intrinsic reinforcing effect of BTA fibers in the cell walls and struts.
- Open Access
Properties of Styrene-Maleic Anhydride Copolymer Compatibilized Polyamide 66/Poly (Phenylene Ether) Blends: Effect of Blend Ratio and Compatibilizer Content
Two different blend ratios of polyamide 66 (PA66) and poly (2,6-dimethyl-1,4-phenylene ether) (PPE) (60/40 and 40/60 w/w) were produced via melt mixing. A styrene–maleic anhydride copolymer (SMA) was utilized at various contents from 2.5–15 wt% to compatibilize the immiscible blend system. The influence of SMA content and blend ratio was investigated based on (thermo-) mechanical and morphological properties of the PA66/PPE blends. Correlations between the interaction of SMA with the blend partners were established. For 60/40 blends, a droplet-sea morphology was visualized by transmission electron microscopy, wherein no major changes were seen upon SMA addition. In the case of 40/60 blends, strong coalescence was found in the binary blend. Up to 5 wt% SMA, the coalescence was inhibited by the interfacial activity of SMA, whereas 10 wt% SMA initiated a disperse-to-co-continuous transition, which was completed at 15 wt% SMA. An enhancement of tensile properties was achieved for all blends possessing SMA, where the maximum concentration of 15 wt% resulted in the highest elongation at break and tensile strength values. The relative improvement of the tensile properties was higher with the PPE-rich blend (40/60) which was attributed to a partial emulsification of the PPE phases forming a bimodal PPE domain size distribution with nano-droplets in the range of 60–160 nm.
Open AccessProperties of Styrene-Maleic Anhydride Copolymer Compatibilized Polyamide 66/Poly (Phenylene Ether) Blends: Effect of Blend Ratio and Compatibilizer Content
Two different blend ratios of polyamide 66 (PA66) and poly (2,6-dimethyl-1,4-phenylene ether) (PPE) (60/40 and 40/60 w/w) were produced via melt mixing. A styrene–maleic anhydride copolymer (SMA) was utilized at various contents from 2.5–15 wt% to compatibilize the immiscible blend system. The influence of SMA content and blend ratio was investigated based on (thermo-) mechanical and morphological properties of the PA66/PPE blends. Correlations between the interaction of SMA with the blend partners were established. For 60/40 blends, a droplet-sea morphology was visualized by transmission electron microscopy, wherein no major changes were seen upon SMA addition. In the case of 40/60 blends, strong coalescence was found in the binary blend. Up to 5 wt% SMA, the coalescence was inhibited by the interfacial activity of SMA, whereas 10 wt% SMA initiated a disperse-to-co-continuous transition, which was completed at 15 wt% SMA. An enhancement of tensile properties was achieved for all blends possessing SMA, where the maximum concentration of 15 wt% resulted in the highest elongation at break and tensile strength values. The relative improvement of the tensile properties was higher with the PPE-rich blend (40/60) which was attributed to a partial emulsification of the PPE phases forming a bimodal PPE domain size distribution with nano-droplets in the range of 60–160 nm.
- Open Access
Properties of Styrene–Maleic Anhydride Copolymer Compatibilized Polyamide 66/Poly (Phenylene Ether) Blends: Effect of Maleic Anhydride Concentration and Copolymer Content
Polyamide 66 (PA66)/poly (2,6-dimethyl-1,4-phenylene ether) (PPE) blends with a ratio of 50/50 (w/w) were produced by a twin-screw compounder. The immiscible blends were compatibilized using two different styrene–maleic anhydride copolymers (SMA) with a low (SMAlow) and a high (SMAhigh) maleic anhydride (MA) concentration of 8 and 25 wt%, respectively. Furthermore, the SMA content was varied from 0 to 10 wt%. The influence of MA concentration and SMA content on the morphological and thermomechanical properties of PA66/PPE blends was investigated. Herein, we established correlations between the interfacial activity of the SMA with blend morphology and corresponding tensile properties. A droplet-sea to co-continuous morphology transition was shown by scanning electron microscopy to occur between 1.25 and 5 wt% in the case of SMAhigh. For SMAlow, the transition started from 7.5 wt% and was still ongoing at 10 wt%. It was found that SMAlow with 10 wt% content enhanced the tensile strength (10%) and elongation at break (70%) of PA66/PPE blends. This improvement can be explained by the strong interfacial interaction of SMAlow within the blend system, which features the formation of nanoemulsion morphology, as shown by transmission electron microscopy. Very small interdomain distances hinder matrix deformations, which forces debonding and cohesive failure of the PPE phase as a “weaker” main deformation mechanism. Due to a lack of interfacial activity, the mechanical properties of the blends with SMAhigh were not improved.
Open AccessProperties of Styrene–Maleic Anhydride Copolymer Compatibilized Polyamide 66/Poly (Phenylene Ether) Blends: Effect of Maleic Anhydride Concentration and Copolymer Content
Polyamide 66 (PA66)/poly (2,6-dimethyl-1,4-phenylene ether) (PPE) blends with a ratio of 50/50 (w/w) were produced by a twin-screw compounder. The immiscible blends were compatibilized using two different styrene–maleic anhydride copolymers (SMA) with a low (SMAlow) and a high (SMAhigh) maleic anhydride (MA) concentration of 8 and 25 wt%, respectively. Furthermore, the SMA content was varied from 0 to 10 wt%. The influence of MA concentration and SMA content on the morphological and thermomechanical properties of PA66/PPE blends was investigated. Herein, we established correlations between the interfacial activity of the SMA with blend morphology and corresponding tensile properties. A droplet-sea to co-continuous morphology transition was shown by scanning electron microscopy to occur between 1.25 and 5 wt% in the case of SMAhigh. For SMAlow, the transition started from 7.5 wt% and was still ongoing at 10 wt%. It was found that SMAlow with 10 wt% content enhanced the tensile strength (10%) and elongation at break (70%) of PA66/PPE blends. This improvement can be explained by the strong interfacial interaction of SMAlow within the blend system, which features the formation of nanoemulsion morphology, as shown by transmission electron microscopy. Very small interdomain distances hinder matrix deformations, which forces debonding and cohesive failure of the PPE phase as a “weaker” main deformation mechanism. Due to a lack of interfacial activity, the mechanical properties of the blends with SMAhigh were not improved.
- Open Access
Extruded Polystyrene Foams with Enhanced Insulation and Mechanical Properties by a Benzene-Trisamide-Based Additive
Low thermal conductivity and adequate mechanical strength are desired for extruded polystyrene foams when they are applied as insulation materials. In this study, we improved the thermal insulation behavior and mechanical properties of extruded polystyrene foams through morphology control with the foam nucleating agent 1,3,5-benzene-trisamide. Furthermore, the structure–property relationships of extruded polystyrene foams were established. Extruded polystyrene foams with selected concentrations of benzene-trisamide were used to evaluate the influence of cell size and foam density on the thermal conductivity. It was shown that the addition of benzene-trisamide reduces the thermal conductivity by up to 17%. An increase in foam density led to a higher compression modulus of the foams. With 0.2 wt % benzene-trisamide, the compression modulus increased by a factor of 4 from 11.7 ± 2.7 MPa for the neat polystyrene (PS) to 46.3 ± 4.3 MPa with 0.2 wt % benzene-trisamide. The increase in modulus was found to follow a power law relationship with respect to the foam density. Furthermore, the compression moduli were normalized by the foam density in order to evaluate the effect of benzene-trisamide alone. A 0.2 wt % benzene-trisamide increased the normalized compression modulus by about 23%, which could be attributed to the additional stress contribution of nanofibers, and might also retard the face stretching and edge bending of the foams.
Open AccessExtruded Polystyrene Foams with Enhanced Insulation and Mechanical Properties by a Benzene-Trisamide-Based Additive
Low thermal conductivity and adequate mechanical strength are desired for extruded polystyrene foams when they are applied as insulation materials. In this study, we improved the thermal insulation behavior and mechanical properties of extruded polystyrene foams through morphology control with the foam nucleating agent 1,3,5-benzene-trisamide. Furthermore, the structure–property relationships of extruded polystyrene foams were established. Extruded polystyrene foams with selected concentrations of benzene-trisamide were used to evaluate the influence of cell size and foam density on the thermal conductivity. It was shown that the addition of benzene-trisamide reduces the thermal conductivity by up to 17%. An increase in foam density led to a higher compression modulus of the foams. With 0.2 wt % benzene-trisamide, the compression modulus increased by a factor of 4 from 11.7 ± 2.7 MPa for the neat polystyrene (PS) to 46.3 ± 4.3 MPa with 0.2 wt % benzene-trisamide. The increase in modulus was found to follow a power law relationship with respect to the foam density. Furthermore, the compression moduli were normalized by the foam density in order to evaluate the effect of benzene-trisamide alone. A 0.2 wt % benzene-trisamide increased the normalized compression modulus by about 23%, which could be attributed to the additional stress contribution of nanofibers, and might also retard the face stretching and edge bending of the foams.