Ibrahim Mohamed El-Kattan
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Ibrahim Mohamed El-Kattan has a total of 16 co-authors. Here are the top co-authors by number of shared publications:
- Mohamed Abuelseoud Abdelzaher
Environmental Science and Industrial Development Department, Faculty of Postgraduate Studies for Advanced Sciences, Beni-suef University, Beni-Suef, Egypt
2 shared publications A A Farghali
Material Sciences and Nano Technology Department, Faculty of Postgraduate Studies for Advanced Sciences, Beni-Suef University, Beni-Suef 62511, Egypt
1 shared publicationA S Faried
Department of Civil Engineering, Faculty of Engineering, Fayoum University, Fayoum, Egypt
1 shared publicationAhmed Baher
Environmental Science and Industrial Development Department, Faculty of Postgraduate Studies for Advanced Sciences, Beni-Suef University, Beni-Suef 62511, Egypt
1 shared publicationAhmed H. Elgendy
1 shared publication- Asmaa Sayed Hamouda
Environmental Sciences and Industrial Development Department, Faculty of Postgraduate Studies for Advanced Sciences, Beni-Suef University, Beni-Suef, Egypt
1 shared publication
Latest Publications
- 16 September 2021
- Published by Egyptian Knowledge Bank in Egyptian Journal of Chemistry
- Vol. 65 (3) , 1-2
Laboratory Study for Accelerating the CKD Mineral Carbonation
Mineral carbonation is one of the typical carbon capture, utilization, and storage technologies, to obtain synthetic carbonates from metal oxide and CO2. However, the technology is known to be extremely challenging to achieve economic feasibility because expensive chemical solvents used the account for most of the cost. To overcome this limitation, we conducted a pilot laboratory study to secure the economic viability of the technology by replacing these chemical solvents with costless metallic carbon dioxide cylinders. For the current study, we implement cement kiln dust (CKD), which is an alkali industrial by-product, together with mineral CO2 gas. In this research paper, we attained CO2 storage and CaCO3 yield, which is comparable in both quantitative and qualitative respects to the existing studies. With a steady flow rate of 0.9 L/m of carbon dioxide furthermore fixed time, the carbonation of CKD could increase dramatically, reaching 35% calcium carbonate at 550°C and 27% calcium carbonate at 450°C respectively. It was also found that CO2 flow rate is one component, which can elute Ca from CKD, and had significant effects on carbonation efficiency. The solid to liquid ratio was the most influential factor in the Ca elution process. the microstructure, morphology, and thermal traits of the designed patches are characterized using scanning electron microscopy (SEM) to indicate phases composition, X-Ray Diffraction (XRD), and Fourier-transform infrared spectroscopy (FTIR) measurements.
- 16 September 2021
- Published by Egyptian Knowledge Bank in Egyptian Journal of Chemistry
- Vol. 65 (3) , 1-2
Laboratory Study for Accelerating the CKD Mineral Carbonation
Mineral carbonation is one of the typical carbon capture, utilization, and storage technologies, to obtain synthetic carbonates from metal oxide and CO2. However, the technology is known to be extremely challenging to achieve economic feasibility because expensive chemical solvents used the account for most of the cost. To overcome this limitation, we conducted a pilot laboratory study to secure the economic viability of the technology by replacing these chemical solvents with costless metallic carbon dioxide cylinders. For the current study, we implement cement kiln dust (CKD), which is an alkali industrial by-product, together with mineral CO2 gas. In this research paper, we attained CO2 storage and CaCO3 yield, which is comparable in both quantitative and qualitative respects to the existing studies. With a steady flow rate of 0.9 L/m of carbon dioxide furthermore fixed time, the carbonation of CKD could increase dramatically, reaching 35% calcium carbonate at 550°C and 27% calcium carbonate at 450°C respectively. It was also found that CO2 flow rate is one component, which can elute Ca from CKD, and had significant effects on carbonation efficiency. The solid to liquid ratio was the most influential factor in the Ca elution process. the microstructure, morphology, and thermal traits of the designed patches are characterized using scanning electron microscopy (SEM) to indicate phases composition, X-Ray Diffraction (XRD), and Fourier-transform infrared spectroscopy (FTIR) measurements.
- Open Access
- 1 February 2021
- Published by IOP Publishing in IOP Conference Series: Materials Science and Engineering
- Vol. 1046 (1) , 012002
Influence of nanosilica, metakaolin and Polypropylene Fiber on dynamic and physicomechanical properties of Portland cement mortar
This study presents an experimental research conducted to inspect the impact of partial substitution through the usage of nano silica (NS) and metakaolin (MK) on cement mortars (CMs). Besides to, the effect of the additive usage such as polypropylene (PP) on the dynamic and physicomechanical properties of CMs as single and combined effect. CM was formed through the usage of different substitution ratios of nano silica varying from 2 to 6% and metakaolin varying from 10 to 30 wt %, by cement weight, where the considered content for PP fiber was at 0.2%. Scanning electron microscopy (SEM), ultrasonic pulse velocity (UPV), flexural strength, and Compressive strength analysis are demonstrated in this paper. Results illustrated that, physicomechanical and dynamic properties of CMs positively enhanced as a result of using a mixture of PP, nano silica, and metakaolin. The CMs that included 0.2% PP, 4% NS, and 20% MK, showed the highest impact on physicomechanical properties compared to other mortar specimens.
- 1 February 2021
- Published by IOP Publishing in IOP Conference Series: Materials Science and Engineering
- Vol. 1046 (1) , 012002
Open AccessInfluence of nanosilica, metakaolin and Polypropylene Fiber on dynamic and physicomechanical properties of Portland cement mortar
This study presents an experimental research conducted to inspect the impact of partial substitution through the usage of nano silica (NS) and metakaolin (MK) on cement mortars (CMs). Besides to, the effect of the additive usage such as polypropylene (PP) on the dynamic and physicomechanical properties of CMs as single and combined effect. CM was formed through the usage of different substitution ratios of nano silica varying from 2 to 6% and metakaolin varying from 10 to 30 wt %, by cement weight, where the considered content for PP fiber was at 0.2%. Scanning electron microscopy (SEM), ultrasonic pulse velocity (UPV), flexural strength, and Compressive strength analysis are demonstrated in this paper. Results illustrated that, physicomechanical and dynamic properties of CMs positively enhanced as a result of using a mixture of PP, nano silica, and metakaolin. The CMs that included 0.2% PP, 4% NS, and 20% MK, showed the highest impact on physicomechanical properties compared to other mortar specimens.
- Open Access
- 1 February 2021
- Published by IOP Publishing in IOP Conference Series: Materials Science and Engineering
- Vol. 1046 (1) , 012024
Single and combined impact of silica fumes with Functionalized multi-walled carbon Nanotubes and nano silica on performance of cement mortars composites
This present work aims to study the impact of single and combined effects of silica fumes (SF) with nano silica (NS) and functionalized multi walled carbon Nanotubes (MWCNTs) on physicomechanical and dynamic properties of cement mortars (CMs). The Portland cement (PC) was partially substituted with different ratios of SF, MWCNTs and NS which, firstly was individually substituted but Secondly, were added together. PC was individually substituted with 2, 4, 6, 8, 10 wt. % of SF then combined with 0.2, 0.4, 0.6, 0.8 and 1.0 wt. % of MWCNTs and 2, 4, 6, 8, 10 wt. % of NS which mixing together. The physicomechanical and dynamic properties such as compressive strength, bending strength, water consistency; both initial and final setting times were measured. The phases of hydration products of some selected samples were additionally investigated by using XRD analyses, the morphology of hardened samples was studied by SEM techniques and TEM showed the particle size of nanoparticles. The results illustrated that, the compressive strength of cement mortars (CM) which containing SF increasing by 27% at 28 days and 11 % for bending strength at early ages comparing to control sample. In combination with functionalized MWCNTS, the compressive and bending strengths increased by 36 and 17 % in case of CMs that containing 0.4 Wt.,% functionalized MWCNTs and 8 Wt.,% SF. additionally, the combination of SF with NS showed increment in compressive strength by 28 % at 8 Wt.,% SF and 8 Wt.,% NS, respectively. SEM-photos showed that CMs containing 0.4 Wt., % functionalized MWCNTs and 8 Wt., % SF had more compacting microstructure than control sample due to bridging effect of MWCNTs and pozzolanic effect of SF.
- 1 February 2021
- Published by IOP Publishing in IOP Conference Series: Materials Science and Engineering
- Vol. 1046 (1) , 012024
Open AccessSingle and combined impact of silica fumes with Functionalized multi-walled carbon Nanotubes and nano silica on performance of cement mortars composites
This present work aims to study the impact of single and combined effects of silica fumes (SF) with nano silica (NS) and functionalized multi walled carbon Nanotubes (MWCNTs) on physicomechanical and dynamic properties of cement mortars (CMs). The Portland cement (PC) was partially substituted with different ratios of SF, MWCNTs and NS which, firstly was individually substituted but Secondly, were added together. PC was individually substituted with 2, 4, 6, 8, 10 wt. % of SF then combined with 0.2, 0.4, 0.6, 0.8 and 1.0 wt. % of MWCNTs and 2, 4, 6, 8, 10 wt. % of NS which mixing together. The physicomechanical and dynamic properties such as compressive strength, bending strength, water consistency; both initial and final setting times were measured. The phases of hydration products of some selected samples were additionally investigated by using XRD analyses, the morphology of hardened samples was studied by SEM techniques and TEM showed the particle size of nanoparticles. The results illustrated that, the compressive strength of cement mortars (CM) which containing SF increasing by 27% at 28 days and 11 % for bending strength at early ages comparing to control sample. In combination with functionalized MWCNTS, the compressive and bending strengths increased by 36 and 17 % in case of CMs that containing 0.4 Wt.,% functionalized MWCNTs and 8 Wt.,% SF. additionally, the combination of SF with NS showed increment in compressive strength by 28 % at 8 Wt.,% SF and 8 Wt.,% NS, respectively. SEM-photos showed that CMs containing 0.4 Wt., % functionalized MWCNTs and 8 Wt., % SF had more compacting microstructure than control sample due to bridging effect of MWCNTs and pozzolanic effect of SF.