Yong Zhang
Research Subjects
Yong Zhang has a total of 20 co-authors. Here are the top co-authors by number of shared publications:
- Liangshun Huang
School of Mechanical Engineering, Jiangxi Polytechnic University, Jiujiang, People’s Republic of China
2 shared publications Bin Zhang
1 shared publicationChen-Kai Yu
1 shared publicationCheng-Xing Wu
1 shared publicationFumin Xu
1 shared publicationGanhua Liu
1 shared publication
Latest Publications
- Open Access
- 13 September 2026
- Published by Elsevier in SSRN Electronic Journal
Simultaneous Enhancement of Strength and Thermal Conductivity in,Mg-Zn-Gd-Zr Alloys: Modulation of Precipitates, Dislocations, and Texture
Magnesium alloy sheets for 3C device covers require a balanced combination of high strength, high thermal conductivity and room-temperature formability, but alloying and deformation commonly degrade heat transport. This work aims to develop an industrially scalable thermo-mechanical route for Mg-Zn-Gd-Zr thin sheets and to clarify the coupled effects of precipitates, dislocations and texture. Mg-6.14Zn-6.07Gd-0.54Zr (wt.%) extruded plates were processed by multidirectional multipass hot rolling to 0.65 mm and then aged at 170 °C for 1 h. The aged sheet achieved a yield strength of 293 MPa, a thermal conductivity of 120.2 W/(m·K), and an Erichsen index (I.E.) of 4.18 mm. Rolling increased the yield strength mainly through dislocation storage and Orowan strengthening by approximately 50–60 nm precipitates, but decreased the thermal conductivity from 129.6 to 109.2 W/(m·K) because of increased solute content, phase-interface thermal resistance and dislocation scattering. Short-time aging restored the thermal conductivity by approximately 11 W/(m·K) through partial dislocation rearrangement/annihilation while maintaining high strength. Texture modification and recrystallization reduced tensile anisotropy and retained useful stretch formability. These results define a practical process window for high-thermal-conductivity Mg alloy sheets for heat-dissipation covers.
- 13 September 2026
- Published by Elsevier in SSRN Electronic Journal
Open AccessSimultaneous Enhancement of Strength and Thermal Conductivity in,Mg-Zn-Gd-Zr Alloys: Modulation of Precipitates, Dislocations, and Texture
Magnesium alloy sheets for 3C device covers require a balanced combination of high strength, high thermal conductivity and room-temperature formability, but alloying and deformation commonly degrade heat transport. This work aims to develop an industrially scalable thermo-mechanical route for Mg-Zn-Gd-Zr thin sheets and to clarify the coupled effects of precipitates, dislocations and texture. Mg-6.14Zn-6.07Gd-0.54Zr (wt.%) extruded plates were processed by multidirectional multipass hot rolling to 0.65 mm and then aged at 170 °C for 1 h. The aged sheet achieved a yield strength of 293 MPa, a thermal conductivity of 120.2 W/(m·K), and an Erichsen index (I.E.) of 4.18 mm. Rolling increased the yield strength mainly through dislocation storage and Orowan strengthening by approximately 50–60 nm precipitates, but decreased the thermal conductivity from 129.6 to 109.2 W/(m·K) because of increased solute content, phase-interface thermal resistance and dislocation scattering. Short-time aging restored the thermal conductivity by approximately 11 W/(m·K) through partial dislocation rearrangement/annihilation while maintaining high strength. Texture modification and recrystallization reduced tensile anisotropy and retained useful stretch formability. These results define a practical process window for high-thermal-conductivity Mg alloy sheets for heat-dissipation covers.
- 10 August 2025
- Published by Wiley in Advanced Engineering Materials
- Vol. 27 (18)
Fabrication of Gradient Microstructure for Enhancing Wear Resistance of Mg‐1.9Mn‐0.3Ce Alloy via Ultrasonic Surface Rolling Process
The strengthening mechanism on wear behavior of Mg‐1.9Mn‐0.3Ce alloy subjected to surface rolling process (USRP) under different sliding speeds and applied loads is investigated in this study. The wear rates and coefficient of friction (COF) values of Mg‐1.9Mn‐0.3Ce alloy after USRP are both reduced. In particular, at a sliding speed of 0.02 m s−1 and 10 N load, the COF and wear rate of the USRP‐treated sample are ≈19% and 74% lower than those of the untreated sample. At a low sliding speed (0.02 m s−1), the wear behavior of untreated samples transitioned from fatigue wear to a mix of abrasive and delamination wear with increasing applied load. In contrast, the worn surface of samples treated by USRP retained fatigue wear characteristics while showing milder delamination and abrasive wear at higher applied loads. At a high sliding speed (0.2 m s−1), the wear resistance of Mg‐1.9Mn‐0.3Ce alloy is also improved with varying applied loads, although the wear mechanism is not significantly changed compared to the untreated sample. The improved wear behavior of Mg‐1.9Mn‐0.3Ce alloy after USRP is primarily attributed to the strengthening effect by the modified microstructure and the inhibiting effect of crack initiation and propagation enabled by the gradient microstructure.
- 10 August 2025
- Published by Wiley in Advanced Engineering Materials
- Vol. 27 (18)
Fabrication of Gradient Microstructure for Enhancing Wear Resistance of Mg‐1.9Mn‐0.3Ce Alloy via Ultrasonic Surface Rolling Process
The strengthening mechanism on wear behavior of Mg‐1.9Mn‐0.3Ce alloy subjected to surface rolling process (USRP) under different sliding speeds and applied loads is investigated in this study. The wear rates and coefficient of friction (COF) values of Mg‐1.9Mn‐0.3Ce alloy after USRP are both reduced. In particular, at a sliding speed of 0.02 m s−1 and 10 N load, the COF and wear rate of the USRP‐treated sample are ≈19% and 74% lower than those of the untreated sample. At a low sliding speed (0.02 m s−1), the wear behavior of untreated samples transitioned from fatigue wear to a mix of abrasive and delamination wear with increasing applied load. In contrast, the worn surface of samples treated by USRP retained fatigue wear characteristics while showing milder delamination and abrasive wear at higher applied loads. At a high sliding speed (0.2 m s−1), the wear resistance of Mg‐1.9Mn‐0.3Ce alloy is also improved with varying applied loads, although the wear mechanism is not significantly changed compared to the untreated sample. The improved wear behavior of Mg‐1.9Mn‐0.3Ce alloy after USRP is primarily attributed to the strengthening effect by the modified microstructure and the inhibiting effect of crack initiation and propagation enabled by the gradient microstructure.
- 23 March 2024
- Published by Elsevier in Materials Letters
- Vol. 364
The microstructural characterization and wear behavior of Mg-Zn-Ce alloy with trace Ca addition
- 23 March 2024
- Published by Elsevier in Materials Letters
- Vol. 364
The microstructural characterization and wear behavior of Mg-Zn-Ce alloy with trace Ca addition