Zhe Lyu
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Zhe Lyu has a total of 16 co-authors. Here are the top co-authors by number of shared publications:
- Leijun Li
Department of Chemical and Materials Engineering, University of Alberta, Edmonton, Canada
5 shared publications Leijun Li
2 shared publicationsAmerican Welding Society
1 shared publicationBenjamin E. Long
Optomec Inc, Albuquerque, NM USA
1 shared publication- Jing Li
Department of Chemical and Materials Engineering, University of Alberta, Edmonton, AB T6G 2V4, Canada
1 shared publication - Nitin Saini
Department of Chemical and Materials Engineering, University of Alberta, Edmonton, Canada
1 shared publication
Latest Publications
- Open Access
- 19 April 2025
- Published by Elsevier in Journal of Materials Research and Technology
- Vol. 36, 5128-5143
A mechanistic study of retained δ-ferrite in additively-manufactured Grade 91 steel
- 19 April 2025
- Published by Elsevier in Journal of Materials Research and Technology
- Vol. 36, 5128-5143
Open AccessA mechanistic study of retained δ-ferrite in additively-manufactured Grade 91 steel
- Open Access
- 8 March 2025
- Published by Elsevier in Materials Science and Engineering: A
- Vol. 930
Crystal plasticity analysis of instrumented indentation on a service-aged Cr–Mo steel
- 8 March 2025
- Published by Elsevier in Materials Science and Engineering: A
- Vol. 930
Open AccessCrystal plasticity analysis of instrumented indentation on a service-aged Cr–Mo steel
- 1 August 2024
- Published by American Welding Society in Welding Journal
- Vol. 103 (12) , 372-377
Effects of Preheating on the Microstructure of Laser-DED AISI 420
AISI 420 stainless steel (420 SS) is a martensitic type known for its high strength and abrasion resistance, and it is extensively used in hard-facing applications (Refs. 1, 2). However, Type 420 SS contains untempered martensite in the as-welded condition and is generally considered to have poor weldability. Successful arc welding of 420 SS requires proper preheating, post-weld heat treatment, and strict adherence to low hydrogen practices. Direct energy deposition (DED) is a fusion-based additive manufacturing (AM) process that melts metal powders to produce complex shapes and can be used for surfacing or hard-facing operations. However, as small-volume AM deposits undergo self-quenching, the cooling rate can be much faster than in welding. Consequently, the phase transformations in the AM deposit deviate further from equilibrium relative to traditional welding processes, resulting in heterogeneous microstructures and mechanical properties, potentially limiting the direct use of AM components without post-AM heat treatment (Ref. 3). Our prior work with laser-DED (L-DED) hard-facing 420 SS powder without preheat combined experiments, characterization, and kinetic modeling to rationalize the presence of remnant δ-ferrite and austenite quantitatively in room temperature microstructures. This study aimed to quantify the effects of preheating above the Ms temperature on the extent of solidification segregation and microstructures for a wall build for L-DED processing of the same heat of 420 powder. The results of the current work are contrasted with our prior study, which allows for a greater understanding of L-DED opportunities with 420 SS.
- 1 August 2024
- Published by American Welding Society in Welding Journal
- Vol. 103 (12) , 372-377
Effects of Preheating on the Microstructure of Laser-DED AISI 420
AISI 420 stainless steel (420 SS) is a martensitic type known for its high strength and abrasion resistance, and it is extensively used in hard-facing applications (Refs. 1, 2). However, Type 420 SS contains untempered martensite in the as-welded condition and is generally considered to have poor weldability. Successful arc welding of 420 SS requires proper preheating, post-weld heat treatment, and strict adherence to low hydrogen practices. Direct energy deposition (DED) is a fusion-based additive manufacturing (AM) process that melts metal powders to produce complex shapes and can be used for surfacing or hard-facing operations. However, as small-volume AM deposits undergo self-quenching, the cooling rate can be much faster than in welding. Consequently, the phase transformations in the AM deposit deviate further from equilibrium relative to traditional welding processes, resulting in heterogeneous microstructures and mechanical properties, potentially limiting the direct use of AM components without post-AM heat treatment (Ref. 3). Our prior work with laser-DED (L-DED) hard-facing 420 SS powder without preheat combined experiments, characterization, and kinetic modeling to rationalize the presence of remnant δ-ferrite and austenite quantitatively in room temperature microstructures. This study aimed to quantify the effects of preheating above the Ms temperature on the extent of solidification segregation and microstructures for a wall build for L-DED processing of the same heat of 420 powder. The results of the current work are contrasted with our prior study, which allows for a greater understanding of L-DED opportunities with 420 SS.
- Open Access
- 9 July 2024
- Published by Elsevier in Journal of Materials Research and Technology
- Vol. 31, 2762-2773
Quantification of δ-ferrite and austenite retention in laser-deposited martensitic stainless steel
- 9 July 2024
- Published by Elsevier in Journal of Materials Research and Technology
- Vol. 31, 2762-2773
Open AccessQuantification of δ-ferrite and austenite retention in laser-deposited martensitic stainless steel
- Open Access
Effect of Fusion Boundary Microstructure on Flow-Accelerated Corrosion Cracking
Flow-accelerated corrosion (FAC) preferentially attacks the downstream heat-affected zone of the root-pass weld in steam pipe systems. A detailed characterization identifies the fusion boundary as the initiation location for the attack. Alloying elements are found depleted along the weld fusion boundary, and multiple welding thermal cycles and repetitive austenite-to-ferrite phase transformations result in an increased proportion of grains with Goss {110} texture along the fusion boundary. The synergistic effects of chemical segregation and the Schmid factor may contribute to the preferential initiation of FAC cracks along the root weld fusion boundary, making it the weakest link for FAC attack in steam pipe girth welds.
Open AccessEffect of Fusion Boundary Microstructure on Flow-Accelerated Corrosion Cracking
Flow-accelerated corrosion (FAC) preferentially attacks the downstream heat-affected zone of the root-pass weld in steam pipe systems. A detailed characterization identifies the fusion boundary as the initiation location for the attack. Alloying elements are found depleted along the weld fusion boundary, and multiple welding thermal cycles and repetitive austenite-to-ferrite phase transformations result in an increased proportion of grains with Goss {110} texture along the fusion boundary. The synergistic effects of chemical segregation and the Schmid factor may contribute to the preferential initiation of FAC cracks along the root weld fusion boundary, making it the weakest link for FAC attack in steam pipe girth welds.
- Open Access
- 12 March 2024
- Published by Elsevier in Materials Science and Engineering: A
- Vol. 898
Degradation of a Cr-Mo steel by carbide precipitation over long-term service
- 12 March 2024
- Published by Elsevier in Materials Science and Engineering: A
- Vol. 898
Open AccessDegradation of a Cr-Mo steel by carbide precipitation over long-term service
- 21 August 2023
- Published by Elsevier in Engineering Failure Analysis
- Vol. 153
Failure analysis of blowholes in welded boiler water walls
- 21 August 2023
- Published by Elsevier in Engineering Failure Analysis
- Vol. 153
Failure analysis of blowholes in welded boiler water walls