KRKh. Ri

Kh. Ri

*This is an algorithmically generated author record based on publicly available information.

Current Organizations / Institutes

The organizations/institutes from the scholar's latest article


Kh. Ri has a total of 6 co-authors. Here are the top co-authors by number of shared publications:


Latest Publications

  • Open Access

    Effects of quenching temperature on the structure, segregation, and properties of the AM4.5Kd + 0.2 wt.% La alloy after artificial aging

    by N. A. Slavinskaya, H. Ri, E. H. Ri, A. S. Zhivetev

    The identification of structural components in the AM4.5Kd + 0.2 wt.% La alloy, subjected to quenching at different temperatures (535–605 °C) and artificial aging at 155 °C for 4 h, was conducted through electron microscopy and XRD. An increase in the quenching temperature from 535 to 605 °C promotes the enlargement of structural components, including the α-solid solution, various aluminides, and eutectics. We observed that the base metal is not homogeneous in its chemical composition, consisting of two types of solid solutions: α1 and α2. The Cu and Mn solubility in the α2-solid solution is higher than in the α1-solid solution. As the quenching temperature increases to tq = 605 °C, the copper content in the α1-solid solution decreases. In contrast, the copper content in the α2-solid solution follows a curve with two maxima at 545 °С (4.5 at.%) and 585 °С (8.7 at.%). The Mn content in the α1-solid solution decreases sharply to the 545 °С quenching temperature and remains relatively constant up to tq = 605 °С (0.2 at.%). The Mn content in the α2-solid solution follows a curve with its maximum at tq = 545 °С (4.3 at.% Mn). Subsequent temperature rise results in a sharp drop in Mn content from 1.0 at.% at t = 565 °С to 0.3 at.% at 605 °С. Hence, the max solubility of Cu and Mn in the α2-solid solution occurs at 545 °C. At 585 °С, only an elevated Cu content (~8.7 at.%) was observed. Aluminides of alloying elements with different stoichiometries crystallize at different quenching temperatures, with complex AlxTiyLazCuvCdw and AlxCuyMnzCdv alloyed aluminides being most commonly found. ncreasing the quenching temperature to 535–545 °С results in higher hardness of the AM4.5Kd + 0.2 wt.% of La alloy, reaching 98–104 HB, with subsequent decrease to 60 HB as the quenching temperature reaches 605 °С. The hardness of the unhardened alloy is 60 HB. The optimal quenching temperature for the AM4.5Kd + 0.2 wt.% of La alloy is in the range of 535–545 °С. This temperature corresponds to the highest hardness of the alloy and the microhardness of the aluminide.

  • Features of formation of the Al–Ni–Zr system alloy structure obtained by reducing oxide compounds by aluminothermy using SHS metallurgy

    by Kh. Ri, E. Kh. Ri, M. A. Ermakov, E. D. Kim, Х. Ри

    This work is focused on establishing the regularity of the effect of zirconium (2.21; 3.29; 3.69 and 6.92 wt.% Zr) on structure formation, the nature of distribution of elements and the microhardness of structural components in the Al–Ni–Zr system alloys obtained by aluminothermy using the SHS metallurgy. Regularities of the formation of structural components and their microhardness depending on the content of zirconium in Al–Ni alloys (50 wt.%) have been identified and scientifically substantiated. Structural components were identified by the methods of electromicroscopic studies and X-ray microanalysis of elements. The structure of the initial alloy consists of Al3Ni2 (β′-phase) and Al3Ni nickel aluminides. Zirconium doping of the alloy in the amount of 2.21 wt.% leads to crystallization of zirconium nickel aluminide Al2(Ni,Zr). With further increase in the content of zirconium (more than 2.21 wt.% Zr), complex alloyed intermetallic compounds crystallize – Zr, W, Si aluminides and Ni zirconides. A regularity was established in the decrease of the solubility of nickel in nickel aluminides Al3Ni2 and Al3Ni and their microhardness as the zirconium content increases in the Al–Ni–Zr alloys from 2.21 to 6.92 wt.%. In nickel aluminide with zirconium Al2(Ni,Zr), this contributes to a decrease in the solubility of Ni, Al and increase in the concentration of Si and Zr. Zirconium doping of the Al–Ni alloy in the amount over 2.21 wt.% contributes to an increase in hardness (HRA), despite a decrease in the microhardness of the metal base (Al3Ni2, Al3Ni and Al2(Ni,Zr)). The main reason for increasing the hardness of the Al–Ni–Zr alloys is the crystallization of complex-alloyed intermetallides – Zr, W, Si aluminides and nickel zirconide, which probably have an increased microhardness. Thus, zirconium doping of the Al–Ni alloy makes it possible to obtain a plastic metal base from nickel aluminides Al3Ni2, Al3Ni and Al2(Ni,Zr) and complex-alloyed intermetallides with high hardness.