Chueh-Lin Wu
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Chueh-Lin Wu has a total of 7 co-authors. Here are the top co-authors by number of shared publications:
- Chia-Chin Chiang
Department of Mechanical Engineering, National Kaohsiung University of Science and Technology, Kaohsiung, TAIWAN
1 shared publication - Shih-Hung Lin
Department of Electronic Engineering, National Yunlin University of Science and Technology, Douliou, Taiwan
1 shared publication - Sin-Liang Ou
Bachelor Program for Design and Materials for Medical Equipment and Devices, Da-Yeh University, Changhua 51591, Taiwan
1 shared publication - Wen-Jen Liu
Department of Materials Science and Engineering, I-Shou University, Kaohsiung 84001, Taiwan
1 shared publication - Yu-Zhi Wang
Graduate School of Materials Science, National Yunlin University of Science and Technology, 123 University Road, Section 3, Douliou, Yunlin 64002, Taiwan
1 shared publication - Yuan-Tsung Chen
Graduate School of Materials Science, National Yunlin University of Science and Technology, Douliou, Taiwan, R.O.C.
1 shared publication
Latest Publications
- Open Access
Thickness, Annealing, and Surface Roughness Effect on Magnetic and Significant Properties of Co40Fe40B10Dy10 Thin Films
In this study, Co40Fe40B10Dy10 thin films were deposited using a direct current (DC) magnetron sputtering technique. The films were deposited on glass substrates with thicknesses of 10, 20, 30, 40, and 50 nm, and heat-treated in a vacuum annealing furnace at 100, 200, and 300 °C. Various instruments were used to examine and analyze the effects of roughness on the magnetic, adhesive, and mechanical properties. From the low frequency alternating current magnetic susceptibility (χac) results, the optimum resonance frequency is 50 Hz, and the maximum χac value tends to increase with the increase in the thicknesses and annealing temperatures. The maximum χac value is 0.18 at a film thickness of 50 nm and an annealing temperature of 300 °C. From the four-point probe, it is found that the resistivity and sheet resistance values decrease with the increase in film deposition thicknesses and higher annealing temperatures. From the magnetic force microscopy (MFM), the stripe-like magnetic domain distribution is more obvious with the increase in annealing temperature. According to the contact angle data, at the same annealing temperature, the contact angle decreases as the thickness increases due to changes in surface morphology. The maximal surface energy value at 300 °C is 34.71 mJ/mm2. The transmittance decreases with increasing film thickness, while the absorption intensity is inversely proportional to the transmittance, implying that the thickness effect suppresses the photon signal. Smoother roughness has less domain pinning, more carrier conductivity, and less light scattering, resulting in superior magnetic, electrical, adhesive, and optical performance.
Open AccessThickness, Annealing, and Surface Roughness Effect on Magnetic and Significant Properties of Co40Fe40B10Dy10 Thin Films
In this study, Co40Fe40B10Dy10 thin films were deposited using a direct current (DC) magnetron sputtering technique. The films were deposited on glass substrates with thicknesses of 10, 20, 30, 40, and 50 nm, and heat-treated in a vacuum annealing furnace at 100, 200, and 300 °C. Various instruments were used to examine and analyze the effects of roughness on the magnetic, adhesive, and mechanical properties. From the low frequency alternating current magnetic susceptibility (χac) results, the optimum resonance frequency is 50 Hz, and the maximum χac value tends to increase with the increase in the thicknesses and annealing temperatures. The maximum χac value is 0.18 at a film thickness of 50 nm and an annealing temperature of 300 °C. From the four-point probe, it is found that the resistivity and sheet resistance values decrease with the increase in film deposition thicknesses and higher annealing temperatures. From the magnetic force microscopy (MFM), the stripe-like magnetic domain distribution is more obvious with the increase in annealing temperature. According to the contact angle data, at the same annealing temperature, the contact angle decreases as the thickness increases due to changes in surface morphology. The maximal surface energy value at 300 °C is 34.71 mJ/mm2. The transmittance decreases with increasing film thickness, while the absorption intensity is inversely proportional to the transmittance, implying that the thickness effect suppresses the photon signal. Smoother roughness has less domain pinning, more carrier conductivity, and less light scattering, resulting in superior magnetic, electrical, adhesive, and optical performance.