  • Analytical and experimental study on the behavior of self‐compacting geopolymer concrete with nanosilica

    by Vigneshkumar Alagarsamy, C. Freeda Christy, M. Muthukannan, U. Johnson Alengaram

    This study investigates the effects of nanosilica (NS) addition on self‐compacting geopolymer concrete (SCGC), focusing on mechanical properties, microstructure, durability, and flexural behavior of the beam. Optimizing the dosage of NS and its impact on SCGC's performance is cardinal in advancing sustainable and resilient concrete construction practices. Fly ash and ground granulated blast furnace slag were used as primary binders, with NS incorporated at replacement levels of 0%–6% (by weight of binder) at 1% intervals. Tests were conducted on fresh properties (slump flow, V‐funnel, and L‐box), mechanical properties (compressive, split tensile, and flexural strength), durability (water absorption, sorptivity, rapid chloride penetration, acid and sulfate resistance), and microstructural characteristics (scanning electron microscope [SEM], x‐ray diffraction [XRD], and Fourier transform infrared [FTIR]). The structural performance of beam specimens was also compared with ANSYS finite element analysis. The results indicate that up to 3% NS addition leads to enhanced compressive, split tensile, and flexural strengths, attributed to microstructure refinement. However, beyond the 3% addition, the mechanical properties decline due to the NS agglomeration. NS‐3% samples exhibit reduced water absorption rates, improved resistance to chloride ion penetration, and minimal deterioration against acid and sulfate attacks. SEM analysis confirms a denser microstructure in NS‐3% samples, while XRD and FTIR analysis indicate optimal particle dispersion and enhanced chemical bonding. The experimental values were slightly higher with deviations of 3.44%–5.74% for load and 1.94%–5.3% for deflection, indicating a strong correlation. Overall, integrating NS up to 3% enhances SCGC's mechanical properties, microstructure densification, and chemical bonding, promising improved durability and long‐term performance.


  • Open Access

    Fresh, hardened properties and microstructural analysis on the effect of NaOH molarities of industrial by-products based self-compacting geopolymer concrete

    by Vigneshkumar A, C. Freeda Christy, M. Muthukannan, U. Johnson Alengaram

    The sodium hydroxide (NaOH) molarity in Self-compacting geopolymer concrete (SCGC) is essential for activating the precursor and aggregate to develop strength, workability, and microstructure. In this study, SCGC mixes prepared with 50% fly ash (FA) and 50% ground granulated blast furnace slag (GGBS) to investigate fresh and hardened properties with NaOH molarities (M) ranges from 8 to 16, the ratio of Na2SiO3 to NaOH kept constant at 2.5 and ratio of alkaline solution to the binder at 0.45 with 2% SP for the polymerization process. SCGC workability studies indicate the NaOH concentration increased, the slump flow decreased, and 14 M was the optimum molarity. The compressive, split tensile, and flexural strength results showed 39.4 MPa, 4.72 MPa, and 5.91 MPa at 28 days. The C–S–H gel enhanced the strength qualities studied from Fourier transform infrared spectroscopy. The scanning electron microscope showed microstructural densification of the entire system, which improved with the NaOH concentration, and the strength increased with the degree of polymerization and polycondensation. Hence, based on workability, the optimized NaOH concentration is 14 M with binder contents of FA (50%) and GGBS (50%). This study helps to improve the microstructure and strength properties with potential cost implications of SCGC.


  • Open Access

    Investigation of superplasticizer influence on rheological and strength properties of self-compacting geopolymer concrete

    by Vigneshkumar Alagarsamy, Clementz Edwardraj Freeda Christy, Muthukannan Muthiah, Ubagaram Johnson Alengaram

    Self-compacting concrete plays a crucial role in the concrete industry due to the increasing demand for rapid infrastructure development to accommodate the growing population. However, traditional concrete requires a large amount of cement, leading to significant CO₂ emissions during production. To address this issue, an innovative self-compacting geopolymer concrete (SCGC) has been developed, eliminating the need for cement while maintaining key self-compacting properties such as flowability, passing ability, and filling ability, along with desirable hardened characteristics.The self-compacting behavior of SCGC is influenced by the dosage of superplasticizers (SP), which significantly improves its workability. Four SCGC mixes were prepared with varying SP dosages at 2% intervals (ranging from 0% to 6%), using 450 kg/m³ of fly ash and a Na₂SiO₃ to NaOH ratio of 1:2.5. The alkali solution-to-binder ratio was maintained at 0.45, with additional water at 54 kg/m³. The effect of SP dosage on workability and mechanical strength was analyzed in the SCGC mixes. The results indicate that an SP dosage of 2% was optimal at a NaOH molarity of 12, yielding the best rheological and strength properties. Based on these findings, it is recommended that the SP dosage in SCGC be optimized at 2%.


  • Open Access

    Influence of Alkaline Binders on the Workability and Strength of Self Compacting Geopolymer Concrete

    by Vigneshkumar Alagarsamy, Freeda Christy Clementz Edwardraj, Muthukannan Muthiah, Johnson Alengaram Ubagaram

    Self-compacting geopolymer concrete (SCGC) has emerged as a promising alternative to traditional concrete due to its environmental benefits. In SCGC, alkaline binders, such as sodium hydroxide (NaOH) and sodium silicate (Na₂SiO₃), play a crucial role in influencing both workability and strength. Notably, the ratio of alkaline binders significantly impacts the overall performance of SCGC. This study investigated five SCGC mixes with varying alkaline binder (A/B) ratios ranging from 0.40 to 0.60, incorporating 50% fly ash (FA) and 50% ground granulated blast furnace slag (GGBS). The mixes included 14 M NaOH, a superplasticizer (9 kg/m³), and extra water (54 kg/m³) to evaluate the effect of the A/B ratio on workability and mechanical strength properties. The results revealed that the fresh properties of SCGC with A/B ratios of 0.4, 0.45, and 0.5 complied with EFNARC guidelines, as assessed by the slump flow test, with the lowest T50cm slump flow recorded at 696 mm. The mix with an A/B ratio of 0.5 exhibited the best mechanical performance, achieving a compressive strength (CS) of 38.3 MPa, a splitting tensile strength (STS) of 4.63 MPa, and a flexural strength (FS) of 5.85 MPa. These findings suggest that an SCGC mix with a 0.5 A/B ratio optimizes rheological and mechanical properties at a 14 M NaOH concentration.


  • Open Access

    Study of silicon dioxide nanoparticles on the rheological and mechanical behaviors of self-compacting geopolymer concrete

    by Vigneshkumar A, C. Freeda Christy, M. Muthukannan, U. Johnson Alengaram, M. Maheswaran, Nittin Johnson Jeyaraj

    Geopolymer concrete (GPC) is a rising eco-conscious substitute for traditional cement-based concrete, bringing the construction industry closer to sustainability. Self-compacting geopolymer concrete (SCGC) enhances the concrete flowability and fills the congested reinforced areas without vibrators in concrete structures such as bridges, tunnels and canals. This study aims to analyze the impact of silicon dioxide nanoparticles (NS) on the rheological and mechanical properties of SCGC to optimize the dosage of NS in SCGC. For this purpose, NS (0–6%) blended in partially distributed binders of fly ash and ground granulated blast furnace slag (50:50) with 0.5 alkaline binder ratio, 2% superplasticizers (9 kg m−3) (MasterGlenium SKY 8233) and 12% extra water (54 kg m−3). Sodium silicate solution and sodium hydroxide ratio of 2.5 was used for this study. It is observed that SCGC with 3% NS replacement complied with the guidelines of EFNARC. According to the T50cm slump flow test, V-funnel test, and L-box test results meet the guidelines of up to 4% NS replacement, and 3% NS addition offers excellent mechanical properties in SCGC. This study concluded that the replacement of 3% of NS improved the fresh and hardened properties of SCGC, which can apply to construction.


  • Open Access

    Parametric study on the performance of industrial byproducts based geopolymer concrete blended with rice husk ash & nano silica

    by M. Maheswaran, C. Freeda Christy, M. Muthukannan, K. Arunkumar, A. Vigneshkumar

    In this study, Geopolymer concrete (GPC) blended with fly ash (FA), ground granulated blast furnace slag (GGBS), rice husk ash (RHA), and nano-silica (NS) developed and investigated in three aspects: In the first aspect of GPC (FA+GGBS), FA varied from 0-100% of GGBS at 10 % intervals to determine the optimum proportion of FA-GGBS. In the second aspect of GPC (FA+GGBS+RHA), RHA varied from 0-25% of FA at 5% intervals with a constant of 30% GGBS attained from the first aspect of the study. In the third aspect of GPC (FA+GGBS+RHA+NS), NS was replaced with 1, 3, and 5% with the optimum proportions of GGBS (30%) and RHA (15%) obtained from the first and second aspects of the study. The fresh and hardened properties of GPC were obtained at 7 and 28 days under ambient curing. The compressive strength improved while FA was replaced by GGBS (0-100%) from 27.75 to 45 MPa. Meanwhile, workability has decreased to 0.81 from 0.97. Hence, the optimized proportion of FA and GGBS was obtained as 70:30 from the workability aspect. RHA replacement provided compressive strength increment up to 15% (39.5 MPa), but workability gradually decreased (0.92 to 0.84) from 0 to 25%. So, the optimum proportion of RHA was achieved by 15% from the second aspect. In the third aspect, the workability increased from 0.89 to 0.92 while NS replacement (0-3%) with FA. Also, compressive strength has improved from 39.52 to 41.95 MPa. Thus, the optimized NS proportion gained at 3% of NS. Overall, this study provides a view of industrial by-product utilization as part of GPC in optimal proportions.