SDSemih Duran

Semih Duran

*This is an algorithmically generated author record based on publicly available information.

Current Organizations / Institutes

The organizations/institutes from the scholar's latest article


Semih Duran has a total of 15 co-authors. Here are the top co-authors by number of shared publications:


Latest Publications

  • Open Access

    Effects of infill pattern, infill ratio and print orientation on the mechanical and vibration response of PLA structures

    by Gökhan Haydarlar, Mehmet Alper Sofuoğlu, Tevfik Oğuzhan Ergüder, Semih Duran

    This study examined the combined effects of infill pattern, infill ratio, and pattern orientation on the tensile and vibration behavior of PLA structures produced by fused filament fabrication (FFF). Despite extensive studies on individual FFF parameters, the combined tensile and vibration behavior of honeycomb, tetrahedral, and Hilbert curve infills has not yet been systematically evaluated under a common structural parameter set. To address this gap, PLA specimens were manufactured using a Taguchi L9 design and evaluated by tensile testing and impact-based modal analysis. Pattern orientation governed the tensile response, accounting for about 60% of the variation in elastic modulus, 75% in tensile strength, and 67% in elongation. The highest elastic modulus was obtained in H45 (945.1 MPa), while T45 showed the highest tensile strength (40.3 MPa) and elongation (5.5%). In contrast, infill pattern was the main factor governing vibration behavior, accounting for about 59% of the stiffness variation and 80% of the damping ratio variation. Specifically, the Hilbert curve pattern showed the highest stiffness, while the tetrahedral pattern showed the highest damping ratio. Natural frequency was governed primarily by pattern orientation, which accounted for about 45% of the variation, while infill pattern had a secondary effect, contributing about 35%. HC45 exhibited the highest stiffness (450,000 N/m), T15 the highest damping ratio (0.128%), and T45 the highest natural frequency (195 Hz). These findings showed that mechanical strength and vibration response were controlled by different properties of internal architecture, providing a practical route for tailoring lightweight FFF components for engineering applications.

  • Open Access

    Structural and tribological properties of TiWAlSiCuN films annealed at different temperatures

    by Semih Duran

    This work focuses on evaluating the influence of post-deposition annealing temperature on the structural characteristics and tribological behavior of TiWAlSiCuN films. The films were produced on AISI M2 tool steel substrates using RF magnetron sputtering and then heat-treated at 600, 700, 800, and 900 °C for 90 min in a controlled atmosphere. Structural phase evolution was investigated by X-ray diffraction, whereas elemental distribution was characterized through scanning electron microscopy coupled with energy-dispersive spectroscopy. Furthermore, hardness, surface roughness, coefficient of friction, and wear rate measurements were carried out to assess the performance of the films after annealing. The experimental results demonstrated that annealing temperature played a critical role in determining both the microstructural and tribological properties of the films. Among all films examined, the film treated at 800 °C showed the most favorable performance, achieving a hardness of 24.5±0.9 GPa, a friction coefficient of 0.37, a surface roughness of 0.07 µm, and a wear rate of 1.97×10-6 mm3/(N·m). The superior performance obtained at 800 °C was attributed to the enhanced microstructural stability of the TiN-containing film structure, which preserved film integrity during sliding and limited tribo-oxidative damage.

  • Microstructural evolution and thermal stability of magnetron-sputtered TiAlNiVN HEA films deposited on Al2024

    by Ahmet Melik Yılmaz, Semih Duran, Hikmet Çiçek

    In this study, TiAlNiVN HEA films were deposited on Al2024 substrates by magnetron sputtering using different Al and V target currents in order to investigate the influence of composition on microstructural evolution and thermal stability. The deposited films, named A1, A2, and A3, were subsequently subjected to thermal treatment at 300, 400, and 500 °C, followed by rapid cooling to room temperature. Structural, chemical, and surface-related changes associated with the thermal treatment were systematically examined using X-ray diffraction (XRD), scanning electron microscopy (SEM), energy-dispersive spectroscopy (EDS), and 3D profilometer. Cross-sectional SEM analyses revealed a gradual increase in film thickness with increasing target currents, confirming the strong dependence of deposition rate on sputtering conditions. As-deposited films exhibited an amorphous or weakly crystalline structure, while thermal treatment up to 400 °C preserved this structural state with only limited surface oxidation. In contrast, thermal treatment at 500 °C led to pronounced phase evolution, including the formation of oxide- and intermetallic-related phases, accompanied by a significant increase in oxygen content. These changes were further reflected in surface morphology, where severe roughening, local blistering, and loss of surface continuity were observed. Indentation-induced crack analyses indicated that the films retained stable crack behavior after 300 and 400 °C treatments, whereas extensive crack initiation and propagation occurred after exposure to 500 °C. Overall, the results demonstrate that TiAlNiVN films maintain structural and surface stability up to 400 °C, while 500 °C represents a critical thermal threshold leading to accelerated degradation.

  • Effect of process parameters and annealing treatment on mechanical and surface properties of PLA samples

    by Gökhan Haydarlar, Tevfik Oğuzhan Ergüder, Semih Duran

    Context— Fused Deposition Modeling (FDM) has become a commonly adopted additive manufacturing method because it offers economical production, geometric versatility, and broad material availability. Among the thermoplastics used in FDM, polylactic acid (PLA) is widely preferred due to its environmentally friendly nature and favorable processing characteristics. Nevertheless, the mechanical properties and surface finish of PLA parts produced by FDM are highly sensitive to both manufacturing parameters and post-processing practices. Although previous research has reported the separate effects of factors such as layer thickness, infill density, and annealing, studies that systematically evaluate their combined impact are still scarce.Objective— This research focused on examining how variations in layer thickness, infill density, and annealing temperature affect the tensile performance and surface characteristics of PLA parts produced by FDM. In particular, the study aimed to determine which processing parameters most strongly influence tensile strength, elastic modulus, elongation, specific tensile strength, and surface roughness, as well as to explain their role in balancing stiffness and ductility in printed PLA parts.Method— An L9 Taguchi orthogonal array was implemented to assess the influence of layer thickness set at 0.12, 0.16, and 0.20 mm, infill density levels of 20, 40, and 60 percent, and annealing states consisting of as-printed, 60 °C, and 90 °C. Tensile samples made of PLA were fabricated using an FDM-based 3D printing system under controlled processing conditions. Mechanical characterization was carried out through tensile testing to obtain tensile strength, elastic modulus, and elongation values, whereas specific tensile strength was determined by incorporating sample mass measurements. Surface quality was evaluated by measuring the average surface roughness (Ra) with a three-dimensional optical profilometer. The effects and relative significance of the selected parameters were statistically analyzed using signal-to-noise ratios and analysis of variance techniques.Results— The results showed that infill density was the most important factor affecting tensile strength, with a contribution ratio of 87.76%, and maximum strengths of approximately 43–45 MPa obtained at 60% infill. Layer thickness was identified as the dominant parameter controlling elastic modulus (48.17%) and elongation (71.64%), its critical role in the stiffness–ductility balance. Surface roughness increased as thicker layers formed more pronounced and visible layer-step structures. Surface roughness increased as thicker layers produced more pronounced and visible layer-step structures. The overall effect of layer thickness on surface roughness was 84.73%.Conclusion— This work presents an integrated assessment of how multiple processing parameters influence the mechanical behavior and surface characteristics of PLA components. The results support the optimization of strength, ductility, weight efficiency, and surface finish, and contribute practical insight for the engineering design of PLA parts manufactured by FDM.

  • Magnetron sıçratma yöntemiyle biriktirilen TiWSiN ince filmlerin yapısal ve tribolojik özelliklerine farklı azot akış hızlarının etkisinin araştırılması

    by Semih Duran, Ahmet Melik Yılmaz, Hikmet Çiçek

    TiWSiN ince filmler magnetron sıçratma yöntemiyle farklı azot akış hızlarında biriktirilerek üretilmiştir. Taramalı elektron mikroskobu (SEM) ile üretilen filmlerin kalınlıkları 1.71 µm ve 1.39 µm olarak ölçülmüştür. Artan azot akış miktarının, film kalınlıklarında belirgin bir azalmaya yol açtığı gözlemlenmiştir. X-ışını kırınım (XRD) cihazı ile TiWSiN ince filmlerde farklı açı ve düzlemlerde sadece TiN kristallerinin oluştuğu belirlenmiştir. Enerji dağılımlı spektroskopi (EDS) cihazı ile filmlerin kimyasal kompozisyonlarını oluşturan Ti, W, Si ve N elementlerinin atomik oranları belirlenmiştir. TiWSiN ince filmlerin sertlik değerlerinin tespit edilmesi için mikro sertlik ölçümleri yapılmıştır. En yüksek sertlik değeri 6.8 GPa ile N-40 filminde ölçülmüştür. Filmin mikro yapısında baskın olan TiN (111) fazının varlığı, N-40 filminde sertliğin artmasına katkıda bulunmuştur. TiWSiN ince filmlerin tribolojik testleri aşınma cihazı ve 3D profilometre cihazı kullanılarak araştırılmıştır. Yapılan aşınma testlerinde, N-40 filminin aşınma hızı 1.81×10-5 (mm3/(N.m)) ve N-50 filminin aşınma hızı ise 9.98×10-5 (mm3/(N.m)) olarak hesaplanmıştır. Sonuçlar incelendiğinde, 4 sccm azot akış hızında biriktirilen N-40 filminin aşınma direncinin N-50 filmine kıyasla yaklaşık 5.5 kat daha yüksek olduğu tespit edilmiştir. Tribotest sonuçları, N-40 filminin aşınma derinlik profilinin filmin taban malzeme üzerinde varlığını sürdürdüğünü açıkça ortaya koymuştur. Bu bulgular, N-40 filminin tribolojik performansının daha yüksek olduğunu göstermektedir. Sonuç olarak, azot akış hızının kontrolünün TiWSiN filmlerin performansını doğrudan etkilediği belirlenmiştir.


  • Effect of post-annealing on structural, tribological, and adhesion properties of TiW/TiWSi/TiWSiN graded composite films

    by Ahmet Sami İnAnç, Ahmet Melik Yılmaz, Semih Duran, Gökhan Gülten, Hikmet Çiçek


  • Open Access

    Production of TiNi/Ti 2 AlN Multilayer Films with Different Numbers of Layers and Evolution of Tribological and Adhesion Properties

    by Semih Duran, Hikmet Çiçek, Ahmet Melik Yılmaz, İhsan Efeoğlu

    TiNi/Ti 2 AlN multilayer films are deposited on AISI M2 steel and Inconel 718 substrates using the magnetron sputtering technique. After heat treatment at 750 °C, TiNi and Ti 2 AlN MAX phase crystal structures are obtained in these films. The effects of different layer numbers on the structural, mechanical, tribological, adhesion, and fatigue properties of TiNi/Ti 2 AlN multilayer films are investigated. All films’ thickness is measured to be ≈2 μm. The 20 layers film deposited on Inconel 718 exhibited the best mechanical properties, with a hardness of 30.6 GPa and an elastic modulus of 407 GPa. A significant improvement in the tribological performance of the films is observed with an increasing number of layers. The lowest wear rate, calculated as 1.96 × 10 −5 (mm 3 (N·m) −1 ), is observed for the 20 layers film deposited on Inconel 718 at room temperature. At high temperatures, the friction coefficients of the 16 and 20 layers films deposited on Inconel 718 decreased to 0.25. In terms of adhesion properties, the 10 layers films deposited on AISI M2 steel demonstrated the best performance with a critical load value of 45 N. The results of the multipass scratch test clearly showed that the 20 layers film deposited on Inconel 718 exhibited the best fatigue behavior among all films.


  • Open Access

    Application of honeycomb pattern to Ti2AlN MAX phase films by plasma etching

    by Semih Duran, Hikmet Çiçek, İsmail Hakkı Korkmaz, İhsan Efeoğlu

    The honeycomb pattern possesses a distinctive hexagonal structure capable of seamless repetition on a flat surface, leaving no gaps. Moreover, all arm thicknesses and angles are equal to one another. This remarkable configuration is deemed biomimetic, with numerous examples found in nature. Notably, it exhibits remarkably low density and exceptional mechanical strength. MAX phase films have gathered significant attention due to their exceptional capacity to amalgamate the essential properties of both metals and ceramics. Additionally, they possess the unique ability to effectively mend surface cracks that may arise as a result of friction-wear, restoring the material to a certain degree of integrity. In this study, Ti2AlN MAX phase thin films were deposited on M2 steel substrates by a closed field unbalanced magnetron sputtering system (CFUBMS). 750 °C heat treatment was applied to obtain the produced films in crystalline form. In addition, plasma etching parameters suitable for the phase structure of the deposited film were determined. With the inductive coupling plasma etching (ICP) process, the honeycomb pattern was given to the Ti2AlN MAX phase films with a continuous and smooth geometry at a depth of 2 μm. This study gives ideas for the development of multi-coating systems in which patterns of different geometries are included in a single layer.