V. A. Razzhivin
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
V. A. Razzhivin has a total of 22 co-authors. Here are the top co-authors by number of shared publications:
- Yaroslav A. Erisov
Samara National Research University (Samara University), Samara, Russia
7 shared publications - Alexander I. Khaimovich
Department of Engine Production Technology, Samara National Research University, Moskovskoye shosse 34, 443086 Samara, Russia
3 shared publications - Anton Vasilevich Agapovichev
Engine Production Technology Department, Samara National Research University, 34 Moskovskoye Shosse, 443086 Samara, Russia
3 shared publications - Fedor Vasilievich Grechnikov
Samara Scientific Center, Russian Academy of Sciences, Samara, Russia
3 shared publications - Surudin Sergei Viktorovich
Samara National Research University
3 shared publications - Vitaly Genadievich Smelov
Engine Production Technology Department, Samara National Research University, 34 Moskovskoye Shosse, 443086 Samara, Russia
3 shared publications
Latest Publications
- Open Access
- 10 October 2024
- Published by Altai State Technical University in Ползуновский вестник
- No. 3,p. 181-190
ИССЛЕДОВАНИЕ КРИСТАЛЛОГРАФИЧЕСКОЙ ТЕКСТУРЫ ТОНКИХ ЛЕНТ ИЗ АЛЮМИНИЕВЫХ СПЛАВОВ АД0, АМЦ и Д16
Уменьшение толщины листовых алюминиевых сплавов позволяет получать облегчённые конструкции и слоистые композиты. Однако при уменьшении толщину образцов менее 0,5 мм существенно изменяются механические и технологические свойства сплавов. Одной из причин такого поведения является кристаллографическая текстура. Для изучения её особенностей методом холодной прокатки получены тонкие ленты из сплавов АД0, АМц и Д16 толщиной 0,4 и 0,2 м, проведён отжиг. Представлены прямы и обратные полюсные фигуры, зависимости полюсной плотности от толщины образцов и марки сплава. Установлено, что в сплаве Д16 после холодной прокатки и отжига в образцах толщиной 0,4 и 0,2 мм текстурные компоненты сохраняются, изменяется их полюсная плотность. В техническом алюминии АД0 отдельные текстурные компоненты, такие как {110}, {4-16}<-121>, {-3-5-1}, {110} сохраняются, компоненты {213} и {311}<-112> присутствуют только в образцах толщиной 0,4 мм, а компоненты {1-31} и {-101} присутствуют только в образцах толщиной 0,2 мм. В сплаве АМц велика бестекстурная составляющая, которая представляет собой набор различных компонент, которые не встречаются в большинстве алюминиевых сплавов, в том числе в тех, которые представлены в этом исследовании. Механические свойства тонких лент из исследуемых сплавов связаны с кристаллографической текстурой. Постоянство текстурных компонент в образцах из сплава Д16 приводит к снижению механических свойств с уменьшением толщины от 0,4 до 0,2 мм. Бестекстурное состояние, которое наблюдается в сплаве АМц, вызывает снижение прочностных показателей и повышение пластичности, а смешанное состояние кристаллографической текстуры в техническом алюминии АД0 вызывает увеличение прочностных показателей и снижение относительного удлинения.
- 10 October 2024
- Published by Altai State Technical University in Ползуновский вестник
- No. 3,p. 181-190
Open AccessИССЛЕДОВАНИЕ КРИСТАЛЛОГРАФИЧЕСКОЙ ТЕКСТУРЫ ТОНКИХ ЛЕНТ ИЗ АЛЮМИНИЕВЫХ СПЛАВОВ АД0, АМЦ и Д16
Уменьшение толщины листовых алюминиевых сплавов позволяет получать облегчённые конструкции и слоистые композиты. Однако при уменьшении толщину образцов менее 0,5 мм существенно изменяются механические и технологические свойства сплавов. Одной из причин такого поведения является кристаллографическая текстура. Для изучения её особенностей методом холодной прокатки получены тонкие ленты из сплавов АД0, АМц и Д16 толщиной 0,4 и 0,2 м, проведён отжиг. Представлены прямы и обратные полюсные фигуры, зависимости полюсной плотности от толщины образцов и марки сплава. Установлено, что в сплаве Д16 после холодной прокатки и отжига в образцах толщиной 0,4 и 0,2 мм текстурные компоненты сохраняются, изменяется их полюсная плотность. В техническом алюминии АД0 отдельные текстурные компоненты, такие как {110}, {4-16}<-121>, {-3-5-1}, {110} сохраняются, компоненты {213} и {311}<-112> присутствуют только в образцах толщиной 0,4 мм, а компоненты {1-31} и {-101} присутствуют только в образцах толщиной 0,2 мм. В сплаве АМц велика бестекстурная составляющая, которая представляет собой набор различных компонент, которые не встречаются в большинстве алюминиевых сплавов, в том числе в тех, которые представлены в этом исследовании. Механические свойства тонких лент из исследуемых сплавов связаны с кристаллографической текстурой. Постоянство текстурных компонент в образцах из сплава Д16 приводит к снижению механических свойств с уменьшением толщины от 0,4 до 0,2 мм. Бестекстурное состояние, которое наблюдается в сплаве АМц, вызывает снижение прочностных показателей и повышение пластичности, а смешанное состояние кристаллографической текстуры в техническом алюминии АД0 вызывает увеличение прочностных показателей и снижение относительного удлинения.
- Open Access
Evaluating the Effectiveness of Magnetic-Pulse Treatment for Healing Continuity Defects in the Metal of Oil and Gas Pipelines
This research paper addresses the issues in evaluating the effectiveness of magnetic-pulse treatment for healing continuity defects in the metal of oil and gas pipelines. A theoretical analysis of the magnetic-pulse action mechanism on continuity defects in the metal was carried out. The results of experimental studies of the effect of magnetic-pulse action on continuity defects of thick-walled samples, cut from used gas pipelines containing microcracks with different geometries, are also presented. The samples were processed under two different technological operating modes of the magnetic-pulse unit: the applied energy was 10 kJ for the first mode and 20 kJ for the second mode. The state of the cracks’ microstructure before and after the magnetic pulse treatment was studied using an optical microscope. As a result of the studies, it was found that magnetic-pulse treatment led to local heating of the crack tips, which was confirmed by the formation of a heat-affected zone in the vicinity of the crack tips. The temperature at the crack tips reached the metal’s melting point at the applied energy of 20 kJ, whereas at the energy of 10 kJ, signs of metal melting were not noted. In the course of the conducted experiments, it was found that the cracks were not completely eliminated after magnetic-pulse treatment; however, the edges of the crack tips melted, with subsequent filling by molten material. Magnetic-pulse treatment resulted in blunting of the crack tips, as their shape became smoother. It was established that the geometry and shape of the crack tip have significant influences on the effectiveness of this technology, as a narrow and sharp crack tip required less energy to reach the metal’s melting point compared to smoother one. The effect of magnetic pulse treatment on the microstructure of pipeline metal and its strength characteristics was also studied. It was found that this treatment leads to structural changes in the area of the crack tip in the form of grain refinement and subsequent strengthening of the pipeline metal.
Open AccessEvaluating the Effectiveness of Magnetic-Pulse Treatment for Healing Continuity Defects in the Metal of Oil and Gas Pipelines
This research paper addresses the issues in evaluating the effectiveness of magnetic-pulse treatment for healing continuity defects in the metal of oil and gas pipelines. A theoretical analysis of the magnetic-pulse action mechanism on continuity defects in the metal was carried out. The results of experimental studies of the effect of magnetic-pulse action on continuity defects of thick-walled samples, cut from used gas pipelines containing microcracks with different geometries, are also presented. The samples were processed under two different technological operating modes of the magnetic-pulse unit: the applied energy was 10 kJ for the first mode and 20 kJ for the second mode. The state of the cracks’ microstructure before and after the magnetic pulse treatment was studied using an optical microscope. As a result of the studies, it was found that magnetic-pulse treatment led to local heating of the crack tips, which was confirmed by the formation of a heat-affected zone in the vicinity of the crack tips. The temperature at the crack tips reached the metal’s melting point at the applied energy of 20 kJ, whereas at the energy of 10 kJ, signs of metal melting were not noted. In the course of the conducted experiments, it was found that the cracks were not completely eliminated after magnetic-pulse treatment; however, the edges of the crack tips melted, with subsequent filling by molten material. Magnetic-pulse treatment resulted in blunting of the crack tips, as their shape became smoother. It was established that the geometry and shape of the crack tip have significant influences on the effectiveness of this technology, as a narrow and sharp crack tip required less energy to reach the metal’s melting point compared to smoother one. The effect of magnetic pulse treatment on the microstructure of pipeline metal and its strength characteristics was also studied. It was found that this treatment leads to structural changes in the area of the crack tip in the form of grain refinement and subsequent strengthening of the pipeline metal.
- Open Access
- 30 September 2023
- Published by Altai State Technical University in Фундаментальные проблемы современного материаловедения
- Vol. 20 (3) , 390-397
ВЛИЯНИЕ ПОЛОЖЕНИЯ ЗАГОТОВКИ НА ПАЛЛЕТЕ ПРИ ЛАЗЕРНОМ РАСКРОЕ НА ФОРМИРОВАНИЕ ЗОНЫ ТЕРМИЧЕСКОГО ВЛИЯНИЯ
В данной работе выполнены исследования свойств и структуры материала зоны термического влияния, возникающей при лазерном раскрое металла, в зависимости от расположения заготовки на паллете: над выступом и между выступами паллеты. Показаны существенные отличия свойств и структуры на этих участках. Даны рекомендации по расположению заготовки относительно выступов паллеты. Свойства материала в зоне реза над выступом паллеты и между выступами существенно отличаются. Значения микротвердости в зоне над выступами паллеты на краю примерно на 50 % меньше, чем в зоне между выступами. По мере движения вглубь образца разница уменьшается. Содержание магния почти в два раза ниже в зоне над выступами, чем между выступами. В поверхностных слоях заготовки в зоне над выступами размеры включений по величине больше, чем в глубине. Это вызвано дополнительным закаливанием металла заготовки находящегося между выступами, и более длительным контактом с ванной жидкого металла из-за затруднения его удаления при резке на выступе паллеты. Удаление дефектного слоя методом фрезерования на глубину 0,5 мм нивелирует разницу свойств металла в зоне над выступом паллеты, между выступами и в глубине.
- 30 September 2023
- Published by Altai State Technical University in Фундаментальные проблемы современного материаловедения
- Vol. 20 (3) , 390-397
Open AccessВЛИЯНИЕ ПОЛОЖЕНИЯ ЗАГОТОВКИ НА ПАЛЛЕТЕ ПРИ ЛАЗЕРНОМ РАСКРОЕ НА ФОРМИРОВАНИЕ ЗОНЫ ТЕРМИЧЕСКОГО ВЛИЯНИЯ
В данной работе выполнены исследования свойств и структуры материала зоны термического влияния, возникающей при лазерном раскрое металла, в зависимости от расположения заготовки на паллете: над выступом и между выступами паллеты. Показаны существенные отличия свойств и структуры на этих участках. Даны рекомендации по расположению заготовки относительно выступов паллеты. Свойства материала в зоне реза над выступом паллеты и между выступами существенно отличаются. Значения микротвердости в зоне над выступами паллеты на краю примерно на 50 % меньше, чем в зоне между выступами. По мере движения вглубь образца разница уменьшается. Содержание магния почти в два раза ниже в зоне над выступами, чем между выступами. В поверхностных слоях заготовки в зоне над выступами размеры включений по величине больше, чем в глубине. Это вызвано дополнительным закаливанием металла заготовки находящегося между выступами, и более длительным контактом с ванной жидкого металла из-за затруднения его удаления при резке на выступе паллеты. Удаление дефектного слоя методом фрезерования на глубину 0,5 мм нивелирует разницу свойств металла в зоне над выступом паллеты, между выступами и в глубине.
- 1 January 2023
- Published by Pleiades Publishing Ltd in Physics of the Solid State
- Vol. 65 (1) , 12-16
Impact of Workpiece Position on Pallet during Laser Cutting on Heat-Affected Zone Formation
The study in this work focuses on the properties and structure of the material in the heat-affected zone that occurs during laser metal cutting, depending on the positioning of the workpiece on the pallet: above the protrusion and between the protrusions of the pallet. Significant differences in properties and structure in these areas are demonstrated. Recommendations on the positioning of the workpiece relative to the pallet protrusions are given. Material properties in the cutting zone above the pallet protrusion and between the protrusions differ significantly. Microhardness values in the zone above the pallet protrusions at the edge are approximately 50% lower than in the zone between the protrusions. As the analysis moves deeper into the sample, the difference decreases. The magnesium concentration is nearly two times lower in the zone above the protrusions than between the protrusions. In the surface layers of the workpiece above the protrusions, the sizes of inclusions are larger than in the depth. This is due to additional quenching of the metal in the workpiece located between the protrusions and prolonged contact with the bath of liquid metal due to difficulties in its removal during cutting on the pallet protrusion. Removing the defective layer by milling to a depth of 0.5 mm neutralizes the difference in the material properties in the zone above the pallet protrusion, between the protrusions, and in the depth.
- 1 January 2023
- Published by Pleiades Publishing Ltd in Physics of the Solid State
- Vol. 65 (1) , 12-16
Impact of Workpiece Position on Pallet during Laser Cutting on Heat-Affected Zone Formation
The study in this work focuses on the properties and structure of the material in the heat-affected zone that occurs during laser metal cutting, depending on the positioning of the workpiece on the pallet: above the protrusion and between the protrusions of the pallet. Significant differences in properties and structure in these areas are demonstrated. Recommendations on the positioning of the workpiece relative to the pallet protrusions are given. Material properties in the cutting zone above the pallet protrusion and between the protrusions differ significantly. Microhardness values in the zone above the pallet protrusions at the edge are approximately 50% lower than in the zone between the protrusions. As the analysis moves deeper into the sample, the difference decreases. The magnesium concentration is nearly two times lower in the zone above the protrusions than between the protrusions. In the surface layers of the workpiece above the protrusions, the sizes of inclusions are larger than in the depth. This is due to additional quenching of the metal in the workpiece located between the protrusions and prolonged contact with the bath of liquid metal due to difficulties in its removal during cutting on the pallet protrusion. Removing the defective layer by milling to a depth of 0.5 mm neutralizes the difference in the material properties in the zone above the pallet protrusion, between the protrusions, and in the depth.
- Open Access
Research on Cracked Conditions in Nickel Chrome Alloy Ni50Cr33W4.5Mo2.8TiAlNb, Obtained by Direct Laser Deposition
Nowadays, additive manufacturing (AM) is a powerful way to make complex-shaped components for airspace engineering from nickel-based superalloys. So, while nickel-based superalloys could easily be we L-DED in sheet-metal thicknesses, they suffered from strain-age cracking and solidification during AM or in the post-weld aging treatment. This is attributed to the fact that besides the limitation of γ′- phase forming elements (Al and Ti), as they form by AM very rapidly and reduce ductility, the majority of the superalloys contain carbide-forming elements such as Cr, Mo, and W. The precipitation of carbides, which is very effective in strengthening, develops cracks in the heat-affected zone (HAZ) during AM. The difference in isochoric heat capacities and the thermal expansion coefficient (TEC) at the phase boundary leads to the appearance of dangerous local destruction energy. If the area of the interfacial interface is sufficiently extended, then the accumulation of this energy reaches a level sufficient for a crack formation. We have proposed a crack initiation criterion (CIC) for assessing the dangerous level of fracture energy. The CIC was derived from an estimate of the local energy balance from the heat transfer equation for the two-phase area. Practical approbation of the criterion was carried out after L-DED of samples from Ni50Cr33W4.5Mo2.8TiAlNb (EP648) alloy powder with an increased carbon content based on the study of the chemical composition near the crack formed during solidification. Using the proposed criterion provides an opportunity to give the rank to carbide-forming elements according to the degree of their influence on the fracture energy. Thus, the release of aluminum carbide turned out to be 5.48 times more dangerous than the release of titanium carbide and more than 5 times more dangerous than the release of tungsten carbide and molybdenum.
Open AccessResearch on Cracked Conditions in Nickel Chrome Alloy Ni50Cr33W4.5Mo2.8TiAlNb, Obtained by Direct Laser Deposition
Nowadays, additive manufacturing (AM) is a powerful way to make complex-shaped components for airspace engineering from nickel-based superalloys. So, while nickel-based superalloys could easily be we L-DED in sheet-metal thicknesses, they suffered from strain-age cracking and solidification during AM or in the post-weld aging treatment. This is attributed to the fact that besides the limitation of γ′- phase forming elements (Al and Ti), as they form by AM very rapidly and reduce ductility, the majority of the superalloys contain carbide-forming elements such as Cr, Mo, and W. The precipitation of carbides, which is very effective in strengthening, develops cracks in the heat-affected zone (HAZ) during AM. The difference in isochoric heat capacities and the thermal expansion coefficient (TEC) at the phase boundary leads to the appearance of dangerous local destruction energy. If the area of the interfacial interface is sufficiently extended, then the accumulation of this energy reaches a level sufficient for a crack formation. We have proposed a crack initiation criterion (CIC) for assessing the dangerous level of fracture energy. The CIC was derived from an estimate of the local energy balance from the heat transfer equation for the two-phase area. Practical approbation of the criterion was carried out after L-DED of samples from Ni50Cr33W4.5Mo2.8TiAlNb (EP648) alloy powder with an increased carbon content based on the study of the chemical composition near the crack formed during solidification. Using the proposed criterion provides an opportunity to give the rank to carbide-forming elements according to the degree of their influence on the fracture energy. Thus, the release of aluminum carbide turned out to be 5.48 times more dangerous than the release of titanium carbide and more than 5 times more dangerous than the release of tungsten carbide and molybdenum.
- 22 October 2022
- Published by Allerton Press in Russian Journal of Non-Ferrous Metals
- Vol. 63 (5) , 544-550
Influence of the Cold Rolling Reduction Ratio and the Final Annealing Temperature on the Properties and Microstructure of Al–Mg–Sc Alloy Sheets
The effect of the cold rolling reduction ratio (εh) on the microstructure and the complex of mechanical and technological properties of cold-rolled sh
- 22 October 2022
- Published by Allerton Press in Russian Journal of Non-Ferrous Metals
- Vol. 63 (5) , 544-550
Influence of the Cold Rolling Reduction Ratio and the Final Annealing Temperature on the Properties and Microstructure of Al–Mg–Sc Alloy Sheets
The effect of the cold rolling reduction ratio (εh) on the microstructure and the complex of mechanical and technological properties of cold-rolled sh
- Open Access
- 19 August 2022
- Published by National University of Science and Technology MISiS in Izvestiya Vuzov. Tsvetnaya Metallurgiya (Proceedings of Higher Schools. Nonferrous Metallurgy)
- Vol. 28 (4) , 75-83
Effect of reduction ratio during cold rolling and final annealing temperature on the properties and microstructure of Al–Mg–Sc alloy sheets
Исследовано влияние степени обжатия при холодной прокатке (εh), а также температуры окончательного отжига листов, прокатанных с различной степенью обжатия, на микроструктуру и комплекс механических и технологических свойств холоднокатаных листов из алюминиевого сплава В-1579 системы Al–Mg–Sc. Установлено, что с ростом значений εh характер пластической анизотропии изменяется слабо, наблюдается увеличение пределов прочности и текучести и уменьшение относительного удлинения. При этом анизотропия пределов прочности и текучести практически отсутствует. С повышением степени обжатия до 30–40 % анизотропия относительного удлинения увеличивается – его значение в направлении прокатки уменьшается более интенсивно. Однако после прокатки с εh > 50 % анизотропия относительного удлинения практически исчезает. Независимо от температуры отжига образцы, прокатанные с большей степенью обжатия, имеют более высокие прочностные характеристики. Установлено, что с ростом температуры отжига пределы прочности и текучести снижаются, а относительное удлинение возрастает. При этом разупрочнение при повышении температуры термообработки происходит более интенсивно для образцов, прокатанных с меньшим обжатием. После отжига для всех анализируемых режимов характер распределения показателей анизотропии в плоскости листа не уменьшается и соответствует деформационному типу текстур. Более того, значение коэффициента плоскостной анизотропии уменьшается по сравнению с холоднокатаным образцом. При этом технологические свойства образцов, прокатанных с большей степенью деформации, после отжига выше, чем у образцов, прокатанных с меньшим обжатием, независимо от температуры отжига.
- 19 August 2022
- Published by National University of Science and Technology MISiS in Izvestiya Vuzov. Tsvetnaya Metallurgiya (Proceedings of Higher Schools. Nonferrous Metallurgy)
- Vol. 28 (4) , 75-83
Open AccessEffect of reduction ratio during cold rolling and final annealing temperature on the properties and microstructure of Al–Mg–Sc alloy sheets
Исследовано влияние степени обжатия при холодной прокатке (εh), а также температуры окончательного отжига листов, прокатанных с различной степенью обжатия, на микроструктуру и комплекс механических и технологических свойств холоднокатаных листов из алюминиевого сплава В-1579 системы Al–Mg–Sc. Установлено, что с ростом значений εh характер пластической анизотропии изменяется слабо, наблюдается увеличение пределов прочности и текучести и уменьшение относительного удлинения. При этом анизотропия пределов прочности и текучести практически отсутствует. С повышением степени обжатия до 30–40 % анизотропия относительного удлинения увеличивается – его значение в направлении прокатки уменьшается более интенсивно. Однако после прокатки с εh > 50 % анизотропия относительного удлинения практически исчезает. Независимо от температуры отжига образцы, прокатанные с большей степенью обжатия, имеют более высокие прочностные характеристики. Установлено, что с ростом температуры отжига пределы прочности и текучести снижаются, а относительное удлинение возрастает. При этом разупрочнение при повышении температуры термообработки происходит более интенсивно для образцов, прокатанных с меньшим обжатием. После отжига для всех анализируемых режимов характер распределения показателей анизотропии в плоскости листа не уменьшается и соответствует деформационному типу текстур. Более того, значение коэффициента плоскостной анизотропии уменьшается по сравнению с холоднокатаным образцом. При этом технологические свойства образцов, прокатанных с большей степенью деформации, после отжига выше, чем у образцов, прокатанных с меньшим обжатием, независимо от температуры отжига.
- Open Access
Practical Approbation of Thermodynamic Criteria for the Consolidation of Bimetallic and Functionally Gradient Materials
This study concerns the key problem of determining the conditions for the consolidation or fracture of bimetallic compounds and high-gradient materials with different coefficients of thermal expansion. The well-known approach to determining the strength is based on the assessment of the critical energy release rates during fracture, depending on the conditions of loading (the portion of shear loading). Unfortunately, most of the experimental results cannot be used directly to select suitable fracture toughness criteria before such a connection is made. This especially applies to the region of interphase interaction, when it is required to estimate the internal energy of destruction accumulated during the preparation of the joint in the adhesion layer within the range of 20–50 μm. Hence, criteria for the adhesive consolidation of bimetallic compound layers were obtained on the basis of the thermodynamics of nonequilibrium processes. The analysis of the quality of the joint using the obtained criteria was carried out on the basis of the calculation of isochoric and isobaric heat capacities and coefficients of thermal expansion of multiphase layers. The applicability of the criteria for the qualitative assessment of the adhesion of layers is demonstrated in the example of bimetallic joints of steel 316L—aluminum alloy AlSi10Mg obtained by the SLM method at various fusion modes.
Open AccessPractical Approbation of Thermodynamic Criteria for the Consolidation of Bimetallic and Functionally Gradient Materials
This study concerns the key problem of determining the conditions for the consolidation or fracture of bimetallic compounds and high-gradient materials with different coefficients of thermal expansion. The well-known approach to determining the strength is based on the assessment of the critical energy release rates during fracture, depending on the conditions of loading (the portion of shear loading). Unfortunately, most of the experimental results cannot be used directly to select suitable fracture toughness criteria before such a connection is made. This especially applies to the region of interphase interaction, when it is required to estimate the internal energy of destruction accumulated during the preparation of the joint in the adhesion layer within the range of 20–50 μm. Hence, criteria for the adhesive consolidation of bimetallic compound layers were obtained on the basis of the thermodynamics of nonequilibrium processes. The analysis of the quality of the joint using the obtained criteria was carried out on the basis of the calculation of isochoric and isobaric heat capacities and coefficients of thermal expansion of multiphase layers. The applicability of the criteria for the qualitative assessment of the adhesion of layers is demonstrated in the example of bimetallic joints of steel 316L—aluminum alloy AlSi10Mg obtained by the SLM method at various fusion modes.
- Open Access
Interface Quality Indices of Al–10Si–Mg Aluminum Alloy and Cr18–Ni10–Ti Stainless-Steel Bimetal Fabricated via Selective Laser Melting
Bimetallic materials are important in many industries (aerospace, medicine, etc.) since they allow the creation of constructions that combine specific functional properties, for example, low density (aluminum alloy) and high corrosion resistance (stainless steel), due to layering fabrication of the bimetallic joint. On the other hand, the difference in thermophysical properties of the dissimilar material layers leads to residual stresses, which cause deformation and destruction of such a bimetallic joint produced via the methods of surfacing or additive technologies. This article discusses the methods based on the gray relational analysis and generalized desirability function for the quality assessment of Al–10Si–Mg aluminum alloy and Cr18–Ni10–Ti stainless-steel bimetal fabricated via selective laser melting (SLM). There are four main parameters (quality indices) of the quality generalized assessment, which determine the degree of Al penetration into the steel substrate and Fe into the deposited layer, the difference in microhardness values on both sides of the interface boundary, and the resistance to mechanical destruction of the bimetallic joint. According to the results obtained, the best set of quality indices corresponds to the SLM technological modes with an energy density of 105 and 147 J/mm3. The greatest functionality of the bimetals is determined by the quality index associated with its strength. Therefore, methods of gray relational analysis and desirability function make it possible to form a generalized assessment for the bimetallic joint quality and, consequently, to select the best technological mode.
Open AccessInterface Quality Indices of Al–10Si–Mg Aluminum Alloy and Cr18–Ni10–Ti Stainless-Steel Bimetal Fabricated via Selective Laser Melting
Bimetallic materials are important in many industries (aerospace, medicine, etc.) since they allow the creation of constructions that combine specific functional properties, for example, low density (aluminum alloy) and high corrosion resistance (stainless steel), due to layering fabrication of the bimetallic joint. On the other hand, the difference in thermophysical properties of the dissimilar material layers leads to residual stresses, which cause deformation and destruction of such a bimetallic joint produced via the methods of surfacing or additive technologies. This article discusses the methods based on the gray relational analysis and generalized desirability function for the quality assessment of Al–10Si–Mg aluminum alloy and Cr18–Ni10–Ti stainless-steel bimetal fabricated via selective laser melting (SLM). There are four main parameters (quality indices) of the quality generalized assessment, which determine the degree of Al penetration into the steel substrate and Fe into the deposited layer, the difference in microhardness values on both sides of the interface boundary, and the resistance to mechanical destruction of the bimetallic joint. According to the results obtained, the best set of quality indices corresponds to the SLM technological modes with an energy density of 105 and 147 J/mm3. The greatest functionality of the bimetals is determined by the quality index associated with its strength. Therefore, methods of gray relational analysis and desirability function make it possible to form a generalized assessment for the bimetallic joint quality and, consequently, to select the best technological mode.
- 1 January 2021
- Published by Allerton Press in Russian Journal of Non-Ferrous Metals
- Vol. 62 (1) , 48-53
Development of a Rheological Model of Hot Deformation as Exemplified by 1424 and В-1461 Aluminum Lithium Alloys
A variant of a rheological model of hot deformation is proposed: the law of hyperbolic sine, which, as opposed to standard law, accounts not only for the r
- 1 January 2021
- Published by Allerton Press in Russian Journal of Non-Ferrous Metals
- Vol. 62 (1) , 48-53
Development of a Rheological Model of Hot Deformation as Exemplified by 1424 and В-1461 Aluminum Lithium Alloys
A variant of a rheological model of hot deformation is proposed: the law of hyperbolic sine, which, as opposed to standard law, accounts not only for the r