Ryo Morita
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Ryo Morita has a total of 49 co-authors. Here are the top co-authors by number of shared publications:
- Kimitoshi Yoneda
Central Research Institute of Electric Power Industry , Yokosuka, JAPAN
5 shared publications Fumio Inada
Central Research Institute of Electric Power Industry
4 shared publications- Aboulaye Traoré
Department of Applied Physics, Institute of Pure and Applied Sciences, University of Tsukuba 2 , Tsukuba, Ibaraki 305-8573, Japan
3 shared publications - Kenichi Tezuka
Department of Tissue and Organ Development, Gifu University Graduate School of Medicine, 1-1 Yanagido, Gifu City, Gifu 501-1194, Japan
3 shared publications - Koichi Yonezawa
Osaka University Graduate School of Engineering Science
3 shared publications - Takeaki Sakurai
Graduate School of Pure and Applied Sciences, University of Tsukuba, 1-1-1 Tennodai, Tsukuba, Ibaraki 305-8573, Japan
3 shared publications
Latest Publications
- 26 August 2024
- Published by AIP Publishing in Applied Physics Letters
- Vol. 125 (9)
Investigation of interface traps in β-(AlGa)2O3/Ga2O3 heterostructures by dynamic capacitance dispersion technique
In this work, interface traps in β-(AlGa)2O3/Ga2O3 modulation-doped field effect transistor (MODFET) were investigated qualitatively and quantitatively by means of dynamic capacitance dispersion technique. The fabricated β-(AlGa)2O3/Ga2O3 MODFET showed drain current modulation demonstrating the transistor behavior. The existence of two-dimensional electron gas was confirmed by the plateau region in the capacitance–voltage (C–V) characteristics. The difference in capacitance profile dispersion at multifrequency C–V measurement suggested the loss mechanism due to trapping and de-trapping effects of carriers. An interface analysis of β-(AlGa)2O3/Ga2O3 heterostructures estimated the interface states with density of trap states and time constants of 0.56×1012–5.92×1012 cm−2 eV−1 and 59–27 μs, respectively.
- 26 August 2024
- Published by AIP Publishing in Applied Physics Letters
- Vol. 125 (9)
Investigation of interface traps in β-(AlGa)2O3/Ga2O3 heterostructures by dynamic capacitance dispersion technique
In this work, interface traps in β-(AlGa)2O3/Ga2O3 modulation-doped field effect transistor (MODFET) were investigated qualitatively and quantitatively by means of dynamic capacitance dispersion technique. The fabricated β-(AlGa)2O3/Ga2O3 MODFET showed drain current modulation demonstrating the transistor behavior. The existence of two-dimensional electron gas was confirmed by the plateau region in the capacitance–voltage (C–V) characteristics. The difference in capacitance profile dispersion at multifrequency C–V measurement suggested the loss mechanism due to trapping and de-trapping effects of carriers. An interface analysis of β-(AlGa)2O3/Ga2O3 heterostructures estimated the interface states with density of trap states and time constants of 0.56×1012–5.92×1012 cm−2 eV−1 and 59–27 μs, respectively.
- 12 August 2024
- Published by AIP Publishing in Applied Physics Letters
- Vol. 125 (7)
Deep-level transient spectroscopy of defect states at p-type oxide/β-Ga2O3 heterojunctions
Defects in p-type oxide/β-Ga2O3 heterojunction diodes were investigated using p-type Cu2O as a case study. Diodes with polycrystalline and epitaxial Cu2O films were analyzed using deep-level transient spectroscopy. For both diodes, two electron bulk defects were detected, including a minority defect at 0.23 eV below EC within Cu2O and a majority defect at 0.53 eV below EC within β-Ga2O3. Furthermore, a high-density interface state of 4.5 × 1012 cm−2/eV was observed in the polycrystalline Cu2O/β-Ga2O3 diode. The presence of a high density of interface states helped reduce the turn-on voltage owing to the interface recombination current. However, it also enabled electron carriers to tunnel through the interface to β-Ga2O3, followed by variable range hopping through the bulk defect in the β-Ga2O3 layer, ultimately causing undesirable premature breakdown. The results of this study underscore the critical role of optimizing the crystal structure during p-type oxide growth for desired defect characteristics, particularly concerning interface states, in β-Ga2O3 bipolar devices for different applications, offering insights for high-performance power rectifier development.
- 12 August 2024
- Published by AIP Publishing in Applied Physics Letters
- Vol. 125 (7)
Deep-level transient spectroscopy of defect states at p-type oxide/β-Ga2O3 heterojunctions
Defects in p-type oxide/β-Ga2O3 heterojunction diodes were investigated using p-type Cu2O as a case study. Diodes with polycrystalline and epitaxial Cu2O films were analyzed using deep-level transient spectroscopy. For both diodes, two electron bulk defects were detected, including a minority defect at 0.23 eV below EC within Cu2O and a majority defect at 0.53 eV below EC within β-Ga2O3. Furthermore, a high-density interface state of 4.5 × 1012 cm−2/eV was observed in the polycrystalline Cu2O/β-Ga2O3 diode. The presence of a high density of interface states helped reduce the turn-on voltage owing to the interface recombination current. However, it also enabled electron carriers to tunnel through the interface to β-Ga2O3, followed by variable range hopping through the bulk defect in the β-Ga2O3 layer, ultimately causing undesirable premature breakdown. The results of this study underscore the critical role of optimizing the crystal structure during p-type oxide growth for desired defect characteristics, particularly concerning interface states, in β-Ga2O3 bipolar devices for different applications, offering insights for high-performance power rectifier development.
- Open Access
- 1 October 2023
- Published by AIP Publishing in AIP Advances
- Vol. 13 (10)
Electrical properties of vertical Cu2O/β-Ga2O3 (001) p–n diodes
In this work, p-type cuprous oxide (Cu2O) films grown on beta gallium oxide (β-Ga2O3) substrates by magnetron sputtering were reported. The resulting vertical Cu2O/β-Ga2O3 heterojunction p–n diodes demonstrated superior performance compared to devices fabricated with polycrystalline Cu2O thin films. Meanwhile, analysis of the discrepancies between the built-in potential and turn-on voltage revealed diverse carrier transport mechanisms in the fabricated devices. Numerical fitting of the forward J–V characteristics further discerned that distinct carrier transport mechanisms dominated under various bias voltages or temperature conditions. At 300 K, trap-assisted tunneling dominates the regime because of the presence of defects in β-Ga2O3 or Cu2O. While the bias voltage is low, the polycrystalline nature of the films formed at room temperature leads to the prevalence of grain boundaries as the primary source of interface-type defects at the Cu2O/β-Ga2O3 interface. Consequently, the dominant mechanism governing carrier transport is interface recombination. As the temperature increases, however, thermionic emission becomes more important. This study presents an opportunity for further investigation into the epitaxial growth of Cu2O and provides insights into the carrier transport mechanism of β-Ga2O3-based heterojunctions.
- 1 October 2023
- Published by AIP Publishing in AIP Advances
- Vol. 13 (10)
Open AccessElectrical properties of vertical Cu2O/β-Ga2O3 (001) p–n diodes
In this work, p-type cuprous oxide (Cu2O) films grown on beta gallium oxide (β-Ga2O3) substrates by magnetron sputtering were reported. The resulting vertical Cu2O/β-Ga2O3 heterojunction p–n diodes demonstrated superior performance compared to devices fabricated with polycrystalline Cu2O thin films. Meanwhile, analysis of the discrepancies between the built-in potential and turn-on voltage revealed diverse carrier transport mechanisms in the fabricated devices. Numerical fitting of the forward J–V characteristics further discerned that distinct carrier transport mechanisms dominated under various bias voltages or temperature conditions. At 300 K, trap-assisted tunneling dominates the regime because of the presence of defects in β-Ga2O3 or Cu2O. While the bias voltage is low, the polycrystalline nature of the films formed at room temperature leads to the prevalence of grain boundaries as the primary source of interface-type defects at the Cu2O/β-Ga2O3 interface. Consequently, the dominant mechanism governing carrier transport is interface recombination. As the temperature increases, however, thermionic emission becomes more important. This study presents an opportunity for further investigation into the epitaxial growth of Cu2O and provides insights into the carrier transport mechanism of β-Ga2O3-based heterojunctions.
- 16 July 2023
- Published by ASME International
Development of Prediction Tool for Flow-Accelerated Corrosion: (2) Evaluation of Geometry Factor for Various Pipe Components
Pipe wall thinning is an important issue in the maintenance of power plants. In particular, flow-accelerated corrosion (FAC) in carbon steel pipelines requires continuous monitoring because of its potential to cause catastrophic pipe rupture. In Japan, management rules for pipe wall thinning in power plants were established after the Mihama accident in 2004 based on pipe wall thickness measurements. However, this monitoring may lead to a large number of measurements for each outage in the power plants. In addition, because this approach assumes constant operating condition, some issues may occur when the plant operating conditions change and a decrease or increase in the FAC rate is expected. For the future improvement of pipe wall thinning management in Japanese power plants, the introduction of prediction methods or prediction codes for thinning rate and residual lifetime evaluation is expected, as already introduced in many other countries. Therefore, the authors conducted research to develop prediction methods for pipe wall thinning management for use in domestic power plants. In this study, to easily apply the FAC prediction model under single-phase water conditions to the actual piping system of nuclear power plants in Japan, we evaluated the geometry effect and the piping layout effect for the various piping components based on CFD parameter analysis. From the CFD results, the influence of the mass transfer coefficient on the parameters of the piping components such as the beta ratio of the orifice was evaluated. An original correlation was developed to enable prediction for the piping system of the actual plants, which consists of the various piping components.
- 16 July 2023
- Published by ASME International
Development of Prediction Tool for Flow-Accelerated Corrosion: (2) Evaluation of Geometry Factor for Various Pipe Components
Pipe wall thinning is an important issue in the maintenance of power plants. In particular, flow-accelerated corrosion (FAC) in carbon steel pipelines requires continuous monitoring because of its potential to cause catastrophic pipe rupture. In Japan, management rules for pipe wall thinning in power plants were established after the Mihama accident in 2004 based on pipe wall thickness measurements. However, this monitoring may lead to a large number of measurements for each outage in the power plants. In addition, because this approach assumes constant operating condition, some issues may occur when the plant operating conditions change and a decrease or increase in the FAC rate is expected. For the future improvement of pipe wall thinning management in Japanese power plants, the introduction of prediction methods or prediction codes for thinning rate and residual lifetime evaluation is expected, as already introduced in many other countries. Therefore, the authors conducted research to develop prediction methods for pipe wall thinning management for use in domestic power plants. In this study, to easily apply the FAC prediction model under single-phase water conditions to the actual piping system of nuclear power plants in Japan, we evaluated the geometry effect and the piping layout effect for the various piping components based on CFD parameter analysis. From the CFD results, the influence of the mass transfer coefficient on the parameters of the piping components such as the beta ratio of the orifice was evaluated. An original correlation was developed to enable prediction for the piping system of the actual plants, which consists of the various piping components.
- 16 July 2023
- Published by ASME International
Development of Prediction Tool for Flow-Accelerated Corrosion (4) Development and Validation of Prediction Software “FALSET” With Water Single-Phase FAC Data Obtained in Japanese PWR Plants
Pipe wall thinning is one of the important issues to be managed in the maintenance of power plants. In Japan, as utilities manage wall thinning on the basis of pipe wall thickness measurements, a large number of wall thickness measurements are necessary for each outage in power plants. Therefore, the authors have developed a wall thinning prediction software, “FALSET”, for the improvement of wall thinning management. This report describes details of FALSET, and its validation and modification using Japanese PWR plant data with high-pH operation and all secondary system temperature conditions. The results show that FALSET can evaluate the wall thinning rate that is close to the measured thinning rate of actual Japanese plant, thereby improving the reliability of FALSET.
- 16 July 2023
- Published by ASME International
Development of Prediction Tool for Flow-Accelerated Corrosion (4) Development and Validation of Prediction Software “FALSET” With Water Single-Phase FAC Data Obtained in Japanese PWR Plants
Pipe wall thinning is one of the important issues to be managed in the maintenance of power plants. In Japan, as utilities manage wall thinning on the basis of pipe wall thickness measurements, a large number of wall thickness measurements are necessary for each outage in power plants. Therefore, the authors have developed a wall thinning prediction software, “FALSET”, for the improvement of wall thinning management. This report describes details of FALSET, and its validation and modification using Japanese PWR plant data with high-pH operation and all secondary system temperature conditions. The results show that FALSET can evaluate the wall thinning rate that is close to the measured thinning rate of actual Japanese plant, thereby improving the reliability of FALSET.
- 16 July 2023
- Published by ASME International
Development of Prediction Tool for Flow-Accelerated Corrosion: (3) Development and Validation of Prediction Software “FALSET” With Water Single-Phase FAC Data Obtained in Japanese BWR Plants
The current management of the pipe wall thinning of Japanese nuclear power plants is based on the thinning rate and residual lifetime evaluated using the measured pipe wall thickness. For the improvement of the current management in Japan, we have developed an original prediction software for pipe wall thinning named FALSET. FALSET can predict the maximum thinning rate in each pipe component in one-dimensional pipelines by using our simplified prediction models for the local thinning rate of flow-accelerated corrosion (FAC) and liquid droplet impingement erosion (LDI). In this report, we describe the validation and improvement of FALSET using water single-phase FAC data on feedwater and condensate lines in Japanese boiling water reactors (BWRs) under a neutral pH 7.0 condition with dissolved oxygen. The results show that FALSET has high predictive performance for water single-phase FAC data obtained in Japanese BWR plants.
- 16 July 2023
- Published by ASME International
Development of Prediction Tool for Flow-Accelerated Corrosion: (3) Development and Validation of Prediction Software “FALSET” With Water Single-Phase FAC Data Obtained in Japanese BWR Plants
The current management of the pipe wall thinning of Japanese nuclear power plants is based on the thinning rate and residual lifetime evaluated using the measured pipe wall thickness. For the improvement of the current management in Japan, we have developed an original prediction software for pipe wall thinning named FALSET. FALSET can predict the maximum thinning rate in each pipe component in one-dimensional pipelines by using our simplified prediction models for the local thinning rate of flow-accelerated corrosion (FAC) and liquid droplet impingement erosion (LDI). In this report, we describe the validation and improvement of FALSET using water single-phase FAC data on feedwater and condensate lines in Japanese boiling water reactors (BWRs) under a neutral pH 7.0 condition with dissolved oxygen. The results show that FALSET has high predictive performance for water single-phase FAC data obtained in Japanese BWR plants.
- 1 January 2019
- Published by Japan Society of Mechanical Engineers in The Proceedings of the National Symposium on Power and Energy Systems
- Vol. 2019.24, D213
Validity of ASME Allowable Vibration Velocity Code and Its Application to Pipe Fatigue Evaluation
ASME OM 2012 specifies a maximum vibration velocity of piping systems, which will not cause fatigue damage. An analytical study using ABAQUS was performed on various piping configurations to clarify the derivation process and application range of this rule. As a result, it was suggested that this rule was reasonable and that it covered many of the piping configurations. A seismic indicator that can evaluate the cumulative fatigue damage value is suggested to be derived using the rule by applying a portion of 103 times or less of the fatigue strength diagram.
- 1 January 2019
- Published by Japan Society of Mechanical Engineers in The Proceedings of the National Symposium on Power and Energy Systems
- Vol. 2019.24, D213
Validity of ASME Allowable Vibration Velocity Code and Its Application to Pipe Fatigue Evaluation
ASME OM 2012 specifies a maximum vibration velocity of piping systems, which will not cause fatigue damage. An analytical study using ABAQUS was performed on various piping configurations to clarify the derivation process and application range of this rule. As a result, it was suggested that this rule was reasonable and that it covered many of the piping configurations. A seismic indicator that can evaluate the cumulative fatigue damage value is suggested to be derived using the rule by applying a portion of 103 times or less of the fatigue strength diagram.
- 1 January 2018
- Published by Japan Society of Mechanical Engineers in The Proceedings of the National Symposium on Power and Energy Systems
- Vol. 2018.23, D224
Research for Pipe Wall Thinning Management Improvement (Part 4)
As one of the major activities of the JSME research committee for the improvement of pipe wall thinning management, latest knowledge concerning pipe wall thinning phenomena and state of the inspection technologies of wall thickness have been surveyed and reviewed. Although a complete management of pipe wall wastage consists of prediction, inspection, and evaluation, survey of the evaluation part has been running late compared to the prediction and inspection parts. On the other hand, many overseas countries adopt local thinning criteria that calculate minimum thickness according to the thinning area because pipe wall thinning phenomena caused by flow accelerated corrosion (FAC) and liquid drop impingement (LDI) decrease pipe wall thickness locally. Additionally,“Risk-Informed In-service Inspection (RI-ISI)” has been introduced and developed by the Electric Power Research Institute (EPRI) , etc. in the USA. This paper focuses on the study of domestic and overseas codes that adopt local thinning criteria, the examples of local thinning analysis applying these codes and the risk assessment procedure which was developed by EPRI. In EPRI’s RI-ISI procedure, leakage risk due to pipe failure is evaluated by consequence categories and pipe failure potential. Finally, future issues are discussed in order to adopt local thinning criteria and risk management in Japan.
- 1 January 2018
- Published by Japan Society of Mechanical Engineers in The Proceedings of the National Symposium on Power and Energy Systems
- Vol. 2018.23, D224
Research for Pipe Wall Thinning Management Improvement (Part 4)
As one of the major activities of the JSME research committee for the improvement of pipe wall thinning management, latest knowledge concerning pipe wall thinning phenomena and state of the inspection technologies of wall thickness have been surveyed and reviewed. Although a complete management of pipe wall wastage consists of prediction, inspection, and evaluation, survey of the evaluation part has been running late compared to the prediction and inspection parts. On the other hand, many overseas countries adopt local thinning criteria that calculate minimum thickness according to the thinning area because pipe wall thinning phenomena caused by flow accelerated corrosion (FAC) and liquid drop impingement (LDI) decrease pipe wall thickness locally. Additionally,“Risk-Informed In-service Inspection (RI-ISI)” has been introduced and developed by the Electric Power Research Institute (EPRI) , etc. in the USA. This paper focuses on the study of domestic and overseas codes that adopt local thinning criteria, the examples of local thinning analysis applying these codes and the risk assessment procedure which was developed by EPRI. In EPRI’s RI-ISI procedure, leakage risk due to pipe failure is evaluated by consequence categories and pipe failure potential. Finally, future issues are discussed in order to adopt local thinning criteria and risk management in Japan.
- 19 July 2015
- Published by ASME International
Experimental Investigation for Acoustic Resonance in Tandem Branches Under Each Dry and Wet Steam Flow
Flow-induced acoustic resonances of piping system containing closed side-branches are sometimes encountered in power plants. In the United States, the steam dryer in boiling water reactor had been damaged by high cycle fatigue due to acoustic-induced vibration under a power uprating condition. The steam piping systems of current power plants often have nearly saturated wet steam condition. The side-branches of current power plants vary in their configuration (single, tandem, and coaxial), number, and so on. Therefore, many types of flow-induced acoustic resonance at branch piping have been investigated by many researchers. However, most of previous studies were under air flow condition and there were few previous experiments under wet steam flow. In this study, some types of the acoustic resonance at branch piping are investigated by conducting experiments under each dry and wet steam conditions. As a result, it is clarified that influence of branch configurations (single or tandem) on resonance amplitude and frequency under steam flow. In addition, their differences between dry and wet steam are discussed.
- 19 July 2015
- Published by ASME International
Experimental Investigation for Acoustic Resonance in Tandem Branches Under Each Dry and Wet Steam Flow
Flow-induced acoustic resonances of piping system containing closed side-branches are sometimes encountered in power plants. In the United States, the steam dryer in boiling water reactor had been damaged by high cycle fatigue due to acoustic-induced vibration under a power uprating condition. The steam piping systems of current power plants often have nearly saturated wet steam condition. The side-branches of current power plants vary in their configuration (single, tandem, and coaxial), number, and so on. Therefore, many types of flow-induced acoustic resonance at branch piping have been investigated by many researchers. However, most of previous studies were under air flow condition and there were few previous experiments under wet steam flow. In this study, some types of the acoustic resonance at branch piping are investigated by conducting experiments under each dry and wet steam conditions. As a result, it is clarified that influence of branch configurations (single or tandem) on resonance amplitude and frequency under steam flow. In addition, their differences between dry and wet steam are discussed.