Dalibor Novák
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Dalibor Novák has a total of 4 co-authors. Here are the top co-authors by number of shared publications:
- Dalibor Matýsek
Department of Geological Engineering, Faculty of Mining and Geology VŠB—Technical University of Ostrava Ostrava‐Poruba Czechia
2 shared publications - Lenka Řeháčková
Faculty of Materials Science and Technology VSB‐Technical University of Ostrava Ostrava‐Poruba Czech Republic
2 shared publications - Pavlína Peikertová
Nanotechnology Centre, CEET, VSB–Technical University of Ostrava
2 shared publications - Vlastimil Novák
Department of Chemistry and Physico-Chemical Processes, Faculty of Materials Science and Technology, VSB-Technical University of Ostrava
2 shared publications
Latest Publications
- Open Access
Influence of B2O3 on Reactive and Non-Reactive Wetting Behavior of CaO-SiO2-MgO-Al2O3-B2O3 System
Boron oxide is introduced into slag as a flux, significantly lowering the liquidus temperature; however, this advantage is accompanied by several undesirable consequences. This study aims to evaluate the impact of boron oxide addition on the wetting reactivity of the CaO-SiO2-MgO-Al2O3-B2O3 slag system, particularly on platinum and graphite substrates, which are commonly utilized for wettability investigations of such systems. The slag system was modified to incorporate varying concentrations of B2O3, reaching up to 30 wt%, with the addition of this oxide at the expense of CaO and SiO2 in a constant ratio, while the contents of Al2O3 and MgO remained unchanged. High-temperature wettability tests were conducted at temperatures up to 1550 °C under a flow of high-purity argon atmosphere (99.9999%). For the platinum substrate, the results indicated non-reactive wetting, characterized by a decrease in wetting angles with increasing temperature and boron oxide content. Conversely, for the graphite substrate, the nature of wetting varied, resulting in either reactive or non-reactive behavior depending on the B2O3 content. Following the high-temperature experiments, additional analyses were performed using scanning electron microscopy (SEM) and energy-dispersive spectrometry (EDS). Furthermore, the powdered oxide systems underwent characterization through Fourier transform infrared spectroscopy (FTIR) and X-ray powder diffraction (XRPD).
Open AccessInfluence of B2O3 on Reactive and Non-Reactive Wetting Behavior of CaO-SiO2-MgO-Al2O3-B2O3 System
Boron oxide is introduced into slag as a flux, significantly lowering the liquidus temperature; however, this advantage is accompanied by several undesirable consequences. This study aims to evaluate the impact of boron oxide addition on the wetting reactivity of the CaO-SiO2-MgO-Al2O3-B2O3 slag system, particularly on platinum and graphite substrates, which are commonly utilized for wettability investigations of such systems. The slag system was modified to incorporate varying concentrations of B2O3, reaching up to 30 wt%, with the addition of this oxide at the expense of CaO and SiO2 in a constant ratio, while the contents of Al2O3 and MgO remained unchanged. High-temperature wettability tests were conducted at temperatures up to 1550 °C under a flow of high-purity argon atmosphere (99.9999%). For the platinum substrate, the results indicated non-reactive wetting, characterized by a decrease in wetting angles with increasing temperature and boron oxide content. Conversely, for the graphite substrate, the nature of wetting varied, resulting in either reactive or non-reactive behavior depending on the B2O3 content. Following the high-temperature experiments, additional analyses were performed using scanning electron microscopy (SEM) and energy-dispersive spectrometry (EDS). Furthermore, the powdered oxide systems underwent characterization through Fourier transform infrared spectroscopy (FTIR) and X-ray powder diffraction (XRPD).
- Open Access
Wetting of Graphite and Platinum Substrate by Oxide System with Graded B2O3 Content
This work focuses on wetting two types of substrates (a platinum substrate and a polished graphite substrate) by molten polycomponent oxide system CaO–MgO–SiO2–Al2O3–B2O3 to test the level of interaction at high temperatures. The tested systems were subjected to high-temperature wetting tests in the temperature range from liquidus temperature to 1550 °C using the sessile drop method. A total of four oxide systems were tested with graded boron oxide contents ranging from 0 to 30 wt%. The experiments were conducted in a CLASIC high-temperature resistance observation furnace and an inert atmosphere of high-purity argon. Droplet silhouettes were obtained with a CANON EOS 550D high-resolution camera during heat treatment, with reactive and non-reactive wetting occurring depending on the substrate type. The dependence of the average wetting angles on temperature and time was evaluated, and it was found that boron oxide decreased the average wetting angles of molten oxide droplets. The analyses were accompanied by the SEM/EDX analysis of the substrate and FTIR analysis of the droplets after high-temperature experiments. The phase composition of the oxide systems was evaluated by XRD analysis.
Open AccessWetting of Graphite and Platinum Substrate by Oxide System with Graded B2O3 Content
This work focuses on wetting two types of substrates (a platinum substrate and a polished graphite substrate) by molten polycomponent oxide system CaO–MgO–SiO2–Al2O3–B2O3 to test the level of interaction at high temperatures. The tested systems were subjected to high-temperature wetting tests in the temperature range from liquidus temperature to 1550 °C using the sessile drop method. A total of four oxide systems were tested with graded boron oxide contents ranging from 0 to 30 wt%. The experiments were conducted in a CLASIC high-temperature resistance observation furnace and an inert atmosphere of high-purity argon. Droplet silhouettes were obtained with a CANON EOS 550D high-resolution camera during heat treatment, with reactive and non-reactive wetting occurring depending on the substrate type. The dependence of the average wetting angles on temperature and time was evaluated, and it was found that boron oxide decreased the average wetting angles of molten oxide droplets. The analyses were accompanied by the SEM/EDX analysis of the substrate and FTIR analysis of the droplets after high-temperature experiments. The phase composition of the oxide systems was evaluated by XRD analysis.