Ya. I. Sapuzhak
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Ya. I. Sapuzhak has a total of 11 co-authors. Here are the top co-authors by number of shared publications:
- O. Ya. Chepil
Karpenko Physico-Mechanical Institute, National Academy of Sciences of Ukraine, Lviv, Ukraine
5 shared publications - Oksana Hembara
Lviv Polytechnic National University, Lviv, Ukraine
5 shared publications - N. T. Hembara
Karpenko Physico-Mechanical Institute, National Academy of Sciences of Ukraine, Lviv, Ukraine
4 shared publications - Ivanna Soviak
Karpenko Physico-Mechanical Institute of the National Academy of Sciences of Ukraine, Lviv, Ukraine
3 shared publications - Andriy M. Syrotyuk
Karpenko Physico-Mechanical Institute of the National Academy of Sciences of Ukraine, Lviv, Ukraine
1 shared publication Karpenko Physico-Mechanical Institute of NAS of Ukraine
1 shared publication
Latest Publications
- 11 August 2025
- Published by National Academy of Sciences of Ukraine (Co. LTD Ukrinformnauka) (Publications) in Physicochemical Mechanics of Materials
- Vol. 61 (4) , 119-124
Mathematical modeling of local hydrogen concentration around defects
The mechanisms of hydrogen-induced failure and the processes of hydrogen transport in metals are considered. A mathematical model of hydrogen diffusion is proposed, which accounts for the interaction between local elastoplastic deformations and hydrogen diffusion. Using the finite element method, the distribution of hydrogen in the vicinity of crack-like defects on the inner surface of steel pipelines under internal pressure is analyzed. Analytical dependences are derived to assess the local hydrogen concentration near defects of various geometric shapes. It is established that with increasing internal pressure, the concentration of both diffusible and trapped hydrogen significantly increases, contributing to hydrogen embrittlement of the material. The obtained results can be used to predict service life of pipelines in hydrogen power applications.
- 11 August 2025
- Published by National Academy of Sciences of Ukraine (Co. LTD Ukrinformnauka) (Publications) in Physicochemical Mechanics of Materials
- Vol. 61 (4) , 119-124
Mathematical modeling of local hydrogen concentration around defects
The mechanisms of hydrogen-induced failure and the processes of hydrogen transport in metals are considered. A mathematical model of hydrogen diffusion is proposed, which accounts for the interaction between local elastoplastic deformations and hydrogen diffusion. Using the finite element method, the distribution of hydrogen in the vicinity of crack-like defects on the inner surface of steel pipelines under internal pressure is analyzed. Analytical dependences are derived to assess the local hydrogen concentration near defects of various geometric shapes. It is established that with increasing internal pressure, the concentration of both diffusible and trapped hydrogen significantly increases, contributing to hydrogen embrittlement of the material. The obtained results can be used to predict service life of pipelines in hydrogen power applications.
- 1 August 2025
- Published by Springer Nature in Materials Science
- Vol. 61 (4) , 550-557
Mathematical modeling of local hydrogen concentration around defects
- 1 August 2025
- Published by Springer Nature in Materials Science
- Vol. 61 (4) , 550-557
Mathematical modeling of local hydrogen concentration around defects
- 1 July 2025
- Published by Springer Nature in Materials Science
- Vol. 61 (1) , 120-128
Evaluation of the increased local trapped hydrogen concentration
- 1 July 2025
- Published by Springer Nature in Materials Science
- Vol. 61 (1) , 120-128
Evaluation of the increased local trapped hydrogen concentration
- 28 February 2025
- Published by National Academy of Sciences of Ukraine (Co. LTD Ukrinformnauka) (Publications) in Physicochemical Mechanics of Materials
- Vol. 61 (1) , 118-125
Evaluation of increased local trap hydrogen concentration
Mathematical models of hydrogenation of low-alloy steels, enabling the assessment of increased local hydrogen concentration near defects of various types were developed. Analytical dependences were established, and computational evaluations of the local distribution of trapped hydrogen near voids of different shapes and crack-like defects on the internal surface of a pipeline made of low-alloy steel were performed, depending on the internal pressure of the hydrogen-containing environment.
- 28 February 2025
- Published by National Academy of Sciences of Ukraine (Co. LTD Ukrinformnauka) (Publications) in Physicochemical Mechanics of Materials
- Vol. 61 (1) , 118-125
Evaluation of increased local trap hydrogen concentration
Mathematical models of hydrogenation of low-alloy steels, enabling the assessment of increased local hydrogen concentration near defects of various types were developed. Analytical dependences were established, and computational evaluations of the local distribution of trapped hydrogen near voids of different shapes and crack-like defects on the internal surface of a pipeline made of low-alloy steel were performed, depending on the internal pressure of the hydrogen-containing environment.
- 31 August 2023
- Published by National Academy of Sciences of Ukraine (Co. LTD Ukrinformnauka) (Publications) in Physicochemical Mechanics of Materials
- Vol. 59 (4) , 44-50
Analytical estimation of hydrogen concentration in a defective material
The problem of hydrogen diffusion in a metal with pores is formulated. Pores are sources of absorption (traps) of hydrogen. Traps were considered to be point-like, distributed uniformly over the entire volume of the metal. Solutions to the problem of diffusion in a defective body have been obtained. In particular, expressions for determining the concentration of both diffusion-moving and trapped hydrogen are obtained for the plate. We also obtained a ratio for determining the amount of hydrogen sorbed by a defective plate at an arbitrary moment of time during its hydrogenation. The amount of hydrogen sorbed by a defect-free plate and a plate with uniformly distributed traps was compared. A 2-3 time excess of hydrogen content in the defective plate compared to the defect-free plate was established.
- 31 August 2023
- Published by National Academy of Sciences of Ukraine (Co. LTD Ukrinformnauka) (Publications) in Physicochemical Mechanics of Materials
- Vol. 59 (4) , 44-50
Analytical estimation of hydrogen concentration in a defective material
The problem of hydrogen diffusion in a metal with pores is formulated. Pores are sources of absorption (traps) of hydrogen. Traps were considered to be point-like, distributed uniformly over the entire volume of the metal. Solutions to the problem of diffusion in a defective body have been obtained. In particular, expressions for determining the concentration of both diffusion-moving and trapped hydrogen are obtained for the plate. We also obtained a ratio for determining the amount of hydrogen sorbed by a defective plate at an arbitrary moment of time during its hydrogenation. The amount of hydrogen sorbed by a defect-free plate and a plate with uniformly distributed traps was compared. A 2-3 time excess of hydrogen content in the defective plate compared to the defect-free plate was established.
- 5 May 2023
- Published by National Academy of Sciences of Ukraine (Co. LTD Ukrinformnauka) (Publications) in Physicochemical Mechanics of Materials
- Vol. 59 (2) , 67-72
Assessing life time of a shaft with a crack in hydrogen
A theoretical-experimental approach for predicting the kinetics of fatigue crack growth and determining the lifetime of the responsible elements of structures in hydrogen is proposed. Based on the created calculation model of fatigue crack growth and experimentally constructed kinetic diagrams of fatigue failure of 35KhN3MFA steel, the residual life of the rotor shaft of the steam generator, weakened by a surface semi-elliptical crack in air and in gaseous hydrogen environment, is determined. It is established that hydrogen reduces the residual life of the rotor shaft by two orders of magnitude in hydrogen, compared to its residual lifee in air.
- 5 May 2023
- Published by National Academy of Sciences of Ukraine (Co. LTD Ukrinformnauka) (Publications) in Physicochemical Mechanics of Materials
- Vol. 59 (2) , 67-72
Assessing life time of a shaft with a crack in hydrogen
A theoretical-experimental approach for predicting the kinetics of fatigue crack growth and determining the lifetime of the responsible elements of structures in hydrogen is proposed. Based on the created calculation model of fatigue crack growth and experimentally constructed kinetic diagrams of fatigue failure of 35KhN3MFA steel, the residual life of the rotor shaft of the steam generator, weakened by a surface semi-elliptical crack in air and in gaseous hydrogen environment, is determined. It is established that hydrogen reduces the residual life of the rotor shaft by two orders of magnitude in hydrogen, compared to its residual lifee in air.
- 1 January 2023
- Published by National Academy of Sciences of Ukraine (Co. LTD Ukrinformnauka) (Publications)
- p. 204-207
Assessment of the Residual Lifetime of a Defective Pipeline at Different Hydrogen Concentrations in the Metal
The residual lifetime of a pipeline with an axial semi-elliptical crack on the outer surface was estimated. It was established that lifetime significantly decreases with an increase in the hydrogen concentrations in the metal of the pipeline. Similar tendencies are also visible with a change in the a/c relation (defect shape). That is, more elongated semi-elliptical cracks are more dangerous as compared to deeper defects. In general, of all the considered cases, the most dangerous is an elongated (a/c = 0.25) axial semi-elliptical crack on the outer surface of the pipe at a hydrogen concentration in the metal of the pipeline СH = 5.462 ppm.
- 1 January 2023
- Published by National Academy of Sciences of Ukraine (Co. LTD Ukrinformnauka) (Publications)
- p. 204-207
Assessment of the Residual Lifetime of a Defective Pipeline at Different Hydrogen Concentrations in the Metal
The residual lifetime of a pipeline with an axial semi-elliptical crack on the outer surface was estimated. It was established that lifetime significantly decreases with an increase in the hydrogen concentrations in the metal of the pipeline. Similar tendencies are also visible with a change in the a/c relation (defect shape). That is, more elongated semi-elliptical cracks are more dangerous as compared to deeper defects. In general, of all the considered cases, the most dangerous is an elongated (a/c = 0.25) axial semi-elliptical crack on the outer surface of the pipe at a hydrogen concentration in the metal of the pipeline СH = 5.462 ppm.