Saeid Akrami
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Saeid Akrami has a total of 13 co-authors. Here are the top co-authors by number of shared publications:
- Hiroshi Yamada
Department of Chemical Systems Engineering Graduate School of Engineering, Nagoya University, Furo‐cho, Chikusa‐ku Nagoya Japan
2 shared publications - Katawalamullage Kanishka Hansani De Silva
Surface Science Laboratory Toyota Technological Institute Nagoya Japan
2 shared publications - Katsutoshi Nagaoka
Department of Chemical Systems Engineering, Graduate School of Engineering, Nagoya University, Furo-cho, Chikusa-ku, Nagoya 464-8603, Japan
2 shared publications - Katsutoshi Sato
Department of Chemical Systems Engineering, Graduate School of Engineering, Nagoya University, Furo-cho, Chikusa-ku, Nagoya 464-8603, Japan
2 shared publications - Kohei Era
Department of Chemical Systems Engineering, Graduate School of Engineering, Nagoya University, Furo-cho, Chikusa-ku, Nagoya, 464-8603, Japan
2 shared publications - Koji Inazu
National Institute of Technology Numazu College 3600 Ooka Numazu Shizuoka 410‐8501 Japan
2 shared publications
Latest Publications
- Open Access
- 8 May 2024
- Published by Royal Society of Chemistry (RSC) in Sustainable Energy & Fuels
- Vol. 8 (12) , 2593-2600
Barium-doped iron nanoparticles supported on MgO as an efficient catalyst for ammonia synthesis under mild reaction conditions
A Ba-doped Fe/MgO catalyst pre-reduced at 700 °C, much higher than that of conventional Fe catalysts, forms an Fe0-core and BaO-shell structure. This enhances ammonia synthesis activity due to electron donation from BaO to N2via Fe0.
- 8 May 2024
- Published by Royal Society of Chemistry (RSC) in Sustainable Energy & Fuels
- Vol. 8 (12) , 2593-2600
Open AccessBarium-doped iron nanoparticles supported on MgO as an efficient catalyst for ammonia synthesis under mild reaction conditions
A Ba-doped Fe/MgO catalyst pre-reduced at 700 °C, much higher than that of conventional Fe catalysts, forms an Fe0-core and BaO-shell structure. This enhances ammonia synthesis activity due to electron donation from BaO to N2via Fe0.
- Open Access
- 14 November 2023
- Published by Wiley in ChemSusChem
- Vol. 16 (22) , e202300942
Catalytic Behavior of K‐doped Fe/MgO Catalysts for Ammonia Synthesis Under Mild Reaction Conditions
An important part of realizing a carbon‐neutral society using ammonia will be the development of an inexpensive yet efficient catalyst for ammonia synthesis under mild reaction conditions (via an impregnation method, as a highly active catalyst for ammonia synthesis under mild reaction conditions (350 °C, 1.0 MPa). At the mentioned conditions, the activity of Fe/K(3)/MgO (17.5 mmol h−1 gcat−1) was greater than that of a commercial fused iron catalyst (8.6 mmol h−1 gcat−1) currently used in the Haber‐Bosch process. K doping was found to increase the ratio of Fe0 on the surface and turnover frequency of Fe in our Fe/K(3)/MgO catalyst. In addition, increasing the pressure to 3.0 MPa at the same temperature led to a significant improvement of the ammonia synthesis rate to 29.6 mmol h−1 gcat−1, which was higher than that of two more expensive, benchmark Ru‐based catalysts, which are also potential alternative catalysts. A kinetics analysis revealed that the addition of K enhanced the ammonia synthesis activity at ≥300 °C by changing the main adsorbed species from NH to N which can accelerate dissociative adsorption of nitrogen as the rate limiting step in ammonia synthesis.
- 14 November 2023
- Published by Wiley in ChemSusChem
- Vol. 16 (22) , e202300942
Open AccessCatalytic Behavior of K‐doped Fe/MgO Catalysts for Ammonia Synthesis Under Mild Reaction Conditions
An important part of realizing a carbon‐neutral society using ammonia will be the development of an inexpensive yet efficient catalyst for ammonia synthesis under mild reaction conditions (via an impregnation method, as a highly active catalyst for ammonia synthesis under mild reaction conditions (350 °C, 1.0 MPa). At the mentioned conditions, the activity of Fe/K(3)/MgO (17.5 mmol h−1 gcat−1) was greater than that of a commercial fused iron catalyst (8.6 mmol h−1 gcat−1) currently used in the Haber‐Bosch process. K doping was found to increase the ratio of Fe0 on the surface and turnover frequency of Fe in our Fe/K(3)/MgO catalyst. In addition, increasing the pressure to 3.0 MPa at the same temperature led to a significant improvement of the ammonia synthesis rate to 29.6 mmol h−1 gcat−1, which was higher than that of two more expensive, benchmark Ru‐based catalysts, which are also potential alternative catalysts. A kinetics analysis revealed that the addition of K enhanced the ammonia synthesis activity at ≥300 °C by changing the main adsorbed species from NH to N which can accelerate dissociative adsorption of nitrogen as the rate limiting step in ammonia synthesis.