Hira Zaman
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Hira Zaman has a total of 14 co-authors. Here are the top co-authors by number of shared publications:
Muhammad Zahid Ishaque
Department of Physics, University of Sargodha, Sargodha, 40100, Pakistan
3 shared publications- Yasir Zaman
Department of Physics, University of Sargodha, Sargodha, Pakistan
3 shared publications - Abu Bakar Siddique
Institute of Chemistry, University of Sargodha, Sargodha, Pakistan
2 shared publications Alia Arif
Department of Physics, University of Sargodha, Sargodha, 40100, Pakistan
2 shared publicationsMuhammad Shahzad
Department of Physics, University of Sargodha, Sargodha, 40100, Pakistan
2 shared publications- Abu Bakar Siddique
Institute of Chemistry, University of Sargodha, Sargodha, Pakistan
1 shared publication
Latest Publications
- 29 December 2023
- Published by Springer Nature in Water, Air, & Soil Pollution
- Vol. 235 (1) , 1-18
Therapeutic Physical Properties, Photocatalytic, and Anti-bacterial Activities of Hydrothermally Fabricated Cu-doped ZnO NPs
- 29 December 2023
- Published by Springer Nature in Water, Air, & Soil Pollution
- Vol. 235 (1) , 1-18
Therapeutic Physical Properties, Photocatalytic, and Anti-bacterial Activities of Hydrothermally Fabricated Cu-doped ZnO NPs
- Open Access
- 18 October 2023
- Published by Royal Society of Chemistry (RSC) in RSC Advances
- Vol. 13 (44) , 30838-30854
Fabrication of ternary metal oxide (ZnO:NiO:CuO) nanocomposite heterojunctions for enhanced photocatalytic and antibacterial applications
In this article, ZnO:NiO:CuO nanocomposites (NCPs) were synthesized using a hydrothermal method, with different Zn : Ni : Cu molar ratios (1 : 1 : 1, 2 : 1 : 1, 1 : 2 : 1, and 1 : 1 : 1). The PXRD confirmed the formation of a NCP consisting of ZnO (hexagonal), NiO (cubic), and CuO (monoclinic) structures. The crystallite sizes of NCPs were calculated using Debye Scherrer and Williamson–Hall methods. The calculated crystalline sizes (Scherrer method) of the NCPs were determined to be 21, 27, 23, and 20 nm for the molar ratios 1 : 1 : 1, 2 : 1 : 1, 1 : 2 : 1, and 1 : 1 : 2, respectively. FTIR spectra confirmed the successful formation of heterojunction NCPs via the presence of metal–oxygen bonds. The UV-vis spectroscopy was used to calculate the bandgap of synthesized samples and was found in the range of 2.99–2.17 eV. SEM images showed the mixed morphology of NCPs i.e., irregular spherical and rod-like structures. The dielectric properties, including AC conductivity, dielectric constant, impedance, and dielectric loss parameters were measured using an LCR meter. The DC electrical measurements revealed that NCPs have a high electrical conductivity. All the NCPs were evaluated for the photocatalytic degradation of Methylene blue (MB), methyl orange (MO), and a mixture of both of these dyes. The NCPs with a molar ratio 1 : 1 : 2 (Zn : Ni : Cu) displayed outstanding photocatalytic activity under sunlight, achieving the degradation efficiency of 98% for methylene blue (MB), 92% for methyl orange (MO) and more than 87% in the case of a mixture of dyes within just 90 minutes of illumination. The antibacterial activity results showed the more noxious nature of NCPs against Gram-negative bacteria with a maximum zone of inhibition revealed by the NCPs of molar ratio 1 : 2 : 1 (Zn : Ni : Cu). On the basis of these observations, it can be anticipated that the NCPs can be successfully employed for the purification of contaminated water by the degradation of hazardous organic compounds and in antibacterial ointments.
- 18 October 2023
- Published by Royal Society of Chemistry (RSC) in RSC Advances
- Vol. 13 (44) , 30838-30854
Open AccessFabrication of ternary metal oxide (ZnO:NiO:CuO) nanocomposite heterojunctions for enhanced photocatalytic and antibacterial applications
In this article, ZnO:NiO:CuO nanocomposites (NCPs) were synthesized using a hydrothermal method, with different Zn : Ni : Cu molar ratios (1 : 1 : 1, 2 : 1 : 1, 1 : 2 : 1, and 1 : 1 : 1). The PXRD confirmed the formation of a NCP consisting of ZnO (hexagonal), NiO (cubic), and CuO (monoclinic) structures. The crystallite sizes of NCPs were calculated using Debye Scherrer and Williamson–Hall methods. The calculated crystalline sizes (Scherrer method) of the NCPs were determined to be 21, 27, 23, and 20 nm for the molar ratios 1 : 1 : 1, 2 : 1 : 1, 1 : 2 : 1, and 1 : 1 : 2, respectively. FTIR spectra confirmed the successful formation of heterojunction NCPs via the presence of metal–oxygen bonds. The UV-vis spectroscopy was used to calculate the bandgap of synthesized samples and was found in the range of 2.99–2.17 eV. SEM images showed the mixed morphology of NCPs i.e., irregular spherical and rod-like structures. The dielectric properties, including AC conductivity, dielectric constant, impedance, and dielectric loss parameters were measured using an LCR meter. The DC electrical measurements revealed that NCPs have a high electrical conductivity. All the NCPs were evaluated for the photocatalytic degradation of Methylene blue (MB), methyl orange (MO), and a mixture of both of these dyes. The NCPs with a molar ratio 1 : 1 : 2 (Zn : Ni : Cu) displayed outstanding photocatalytic activity under sunlight, achieving the degradation efficiency of 98% for methylene blue (MB), 92% for methyl orange (MO) and more than 87% in the case of a mixture of dyes within just 90 minutes of illumination. The antibacterial activity results showed the more noxious nature of NCPs against Gram-negative bacteria with a maximum zone of inhibition revealed by the NCPs of molar ratio 1 : 2 : 1 (Zn : Ni : Cu). On the basis of these observations, it can be anticipated that the NCPs can be successfully employed for the purification of contaminated water by the degradation of hazardous organic compounds and in antibacterial ointments.