Shaoming Zhang
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Shaoming Zhang has a total of 9 co-authors. Here are the top co-authors by number of shared publications:
- Guangbao Sun
Gaona Aero Material Co., Ltd., Beijing 100081, China
1 shared publication - Guohao Liu
Research Institute of Advanced Materials (Shenzhen) Co., Ltd., Shenzhen 518045, China
1 shared publication - Lianbo Wang
School of Material Science and Technology, Shanghai Institute of Technology, Shanghai 200240, China
1 shared publication - Peng Zhang
Central Iron & Steel Research Institute Co., Ltd., Beijing 100081, China
1 shared publication - Qiang Hu
Metal Powder Materials Industrial Technology Research Institute of GRINM, Beijing 101407, China
1 shared publication - Rui Wang
Gaona Aero Material Co., Ltd., Beijing 100081, China
1 shared publication
Latest Publications
- Open Access
Enhancement of Spreadability in Haynes 230 Powder via In Situ Micro-Oxidation Gas Atomization for Additive Manufacturing Process
The powder bed packing density of metal powders plays a crucial role in additive manufacturing as it directly affects the defect and mechanical properties of the fabricated parts. Powder bed packing density is related to powder flowability and spreadability. In this study, we introduced a new method to improve powder flowability and spreadability, where Haynes 230 powder with exceptional flowability was successfully produced using an in situ micro-oxidation gas atomization process. Compared to conventional gas atomization, the powder exhibited improved flowability and spreadability, measuring at 11.8 s/50 g. Additionally, the angle of repose was reduced by 25%, resulting in a powder bed packing density of 5.67 g/cm3, corresponding to 63.7% of the theoretical density. Notably, the oxygen content in the powder was only 180 ppm, as confirmed by XRD testing, and no oxide peaks were detected. Furthermore, the depth of the oxide layer on the particle surface increased by less than 20 nm. As a result, the in situ micro-oxidation process reduces the number of pores and cracks in the Haynes 230 alloy formed specimens and improves the relative density of the built specimens. This study highlights the potential of in situ micro-oxidation gas atomization as a promising method for producing powders with high flowability and spreadability for laser powder bed fusion (LPBF) processes.
Open AccessEnhancement of Spreadability in Haynes 230 Powder via In Situ Micro-Oxidation Gas Atomization for Additive Manufacturing Process
The powder bed packing density of metal powders plays a crucial role in additive manufacturing as it directly affects the defect and mechanical properties of the fabricated parts. Powder bed packing density is related to powder flowability and spreadability. In this study, we introduced a new method to improve powder flowability and spreadability, where Haynes 230 powder with exceptional flowability was successfully produced using an in situ micro-oxidation gas atomization process. Compared to conventional gas atomization, the powder exhibited improved flowability and spreadability, measuring at 11.8 s/50 g. Additionally, the angle of repose was reduced by 25%, resulting in a powder bed packing density of 5.67 g/cm3, corresponding to 63.7% of the theoretical density. Notably, the oxygen content in the powder was only 180 ppm, as confirmed by XRD testing, and no oxide peaks were detected. Furthermore, the depth of the oxide layer on the particle surface increased by less than 20 nm. As a result, the in situ micro-oxidation process reduces the number of pores and cracks in the Haynes 230 alloy formed specimens and improves the relative density of the built specimens. This study highlights the potential of in situ micro-oxidation gas atomization as a promising method for producing powders with high flowability and spreadability for laser powder bed fusion (LPBF) processes.
- Open Access
- 15 January 2024
- Published by MDPI AG in Applied Sciences
- Vol. 14 (2) , 721
Numerical Simulation of Liquid Film Characteristics during Atomization of Aluminum Alloy Powder
The process of atomizing aluminum alloy powder using a rotating disk was studied by numerical simulation and experimental verification. The motion characteristics of the molten metal thin liquid film and the evolution law of atomization into droplets were systematically studied with different disk shapes and speeds. The results showed that the slippage of the liquid film on the surface of the spherical disk was smaller, the liquid film spread more evenly, and the velocity distribution was more uniform. Under the same working condition, the boundary diameter of the continuous liquid film on the spherical disk was 21–29% larger, and the maximum liquid film velocity increased by approximately 19%. In other words, the liquid film obtained more energy at the same rotational speed, the energy utilization rate was higher, and the liquid filaments produced by the splitting region of the disk surface were finer and greater in number. The data showed that the average thickness of the liquid film on the surfaces of different disk shapes was more affected by the speed of the flat disk, and the thickness on the spherical disk was relatively stable and uniform, but the difference in thickness between the two disk shapes decreased from 4.2 μm to 0.3 μm when the speed increased from 10,000 rpm to 60,000 rpm. In particular, the influence of the disk shape on the liquid film thickness became smaller when the speed increased to a certain range. At the same time, the characteristics of the liquid film during the spreading movement of molten metal on the disk and the mechanisms of the primary and secondary breakage of the liquid film were obtained through this simulation study.
- 15 January 2024
- Published by MDPI AG in Applied Sciences
- Vol. 14 (2) , 721
Open AccessNumerical Simulation of Liquid Film Characteristics during Atomization of Aluminum Alloy Powder
The process of atomizing aluminum alloy powder using a rotating disk was studied by numerical simulation and experimental verification. The motion characteristics of the molten metal thin liquid film and the evolution law of atomization into droplets were systematically studied with different disk shapes and speeds. The results showed that the slippage of the liquid film on the surface of the spherical disk was smaller, the liquid film spread more evenly, and the velocity distribution was more uniform. Under the same working condition, the boundary diameter of the continuous liquid film on the spherical disk was 21–29% larger, and the maximum liquid film velocity increased by approximately 19%. In other words, the liquid film obtained more energy at the same rotational speed, the energy utilization rate was higher, and the liquid filaments produced by the splitting region of the disk surface were finer and greater in number. The data showed that the average thickness of the liquid film on the surfaces of different disk shapes was more affected by the speed of the flat disk, and the thickness on the spherical disk was relatively stable and uniform, but the difference in thickness between the two disk shapes decreased from 4.2 μm to 0.3 μm when the speed increased from 10,000 rpm to 60,000 rpm. In particular, the influence of the disk shape on the liquid film thickness became smaller when the speed increased to a certain range. At the same time, the characteristics of the liquid film during the spreading movement of molten metal on the disk and the mechanisms of the primary and secondary breakage of the liquid film were obtained through this simulation study.