Luan dos Santos Menezes
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Luan dos Santos Menezes has a total of 16 co-authors. Here are the top co-authors by number of shared publications:
- José Guilherme Neves
Department of Restorative Dentistry – Dental Materials Division, State University of Campinas, Piracicaba Dental School (FOP-UNICAMP), Brazil
4 shared publications Daniel Navarro da Rocha
Department of Bioengineering, R-Crio Criogenia S.A, Campinas, Brazil
3 shared publicationsLourenço Correr-Sobrinho
Department of Restorative Dentistry – Dental Materials Division, State University of Campinas, Piracicaba Dental School (FOP-UNICAMP), Brazil
3 shared publicationsAmérico Bortolazzo Correr
Department of Restorative Dentistry – Dental Materials Area, Piracicaba Dental School, State University of Campinas – UNICAMP, Piracicaba, Sao Paulo, Brazil
2 shared publicationsAna Rita Morales
Department of Materials Engineering, School of Chemical Engineering, Universidade de Campinas, Campinas, Brazil
2 shared publicationsAna Rosa Costa
Department of Restorative Dentistry – Dental Materials Area, Piracicaba Dental School, State University of Campinas – UNICAMP, Piracicaba, Sao Paulo, Brazil
2 shared publications
Latest Publications
- 12 February 2026
- Published by SAGE Publications in Proceedings of the Institution of Mechanical Engineers, Part H: Journal of Engineering in Medicine
- Vol. 240 (3) , 246-256
Treatment of dental implant surfaces with graphene oxide nanoparticles: Synthesis, characterization, and assessment of antimicrobial potential
This study assesses the synthesis and characterization of titanium implant surface nanocoating with graphene oxide (GO) at varying concentrations. Nanocoatings were applied using the dip coating technique, and GO nanoparticles were synthesized chemically. Physicochemical, morphological, and biological characterizations were conducted using scanning electron microscopy (SEM), transmission electron microscopy (TEM), Raman spectroscopy, in vitro bioactivity assay, cell viability, and colony-forming units per milliliter (CFU/mL). Cell viability data were subjected to two-way ANOVA, followed by Tukey’s test (α = 0.05). CFU/mL data were analyzed using the Kruskal-Wallis test, followed by Dunn’s test (α = 0.05). TEM revealed a sheet-like structure of GO nanoparticles. SEM showed the roughness of the nanocoated titanium surface. Raman spectroscopy indicated the presence of GO on the titanium surface, as evidenced by D and G bands. Higher apatite crystal deposition was observed on surfaces with greater GO concentrations at 7 and 14 days (bioactivity assay). The highest percentage of cell viability was noted in the 1.5% GO group after 48 h, compared to other groups at different time points ( p < 0.05). Surface treatment with varying GO concentrations induced greater cell viability compared to the acidic treatment ( p < 0.05). The 1.5% GO group showed the lowest antibacterial efficacy, as evidenced by the highest CFU/mL values ( p < 0.05). GO particles remained stable and chemically unchanged during the coating process. The GO-coated titanium surfaces showed no cytotoxicity and exhibited notable bioactive and antibacterial effects against Streptococcus mutans . These findings suggest that GO coatings may effectively enhance the biological and antimicrobial performance of titanium implants.
- 12 February 2026
- Published by SAGE Publications in Proceedings of the Institution of Mechanical Engineers, Part H: Journal of Engineering in Medicine
- Vol. 240 (3) , 246-256
Treatment of dental implant surfaces with graphene oxide nanoparticles: Synthesis, characterization, and assessment of antimicrobial potential
This study assesses the synthesis and characterization of titanium implant surface nanocoating with graphene oxide (GO) at varying concentrations. Nanocoatings were applied using the dip coating technique, and GO nanoparticles were synthesized chemically. Physicochemical, morphological, and biological characterizations were conducted using scanning electron microscopy (SEM), transmission electron microscopy (TEM), Raman spectroscopy, in vitro bioactivity assay, cell viability, and colony-forming units per milliliter (CFU/mL). Cell viability data were subjected to two-way ANOVA, followed by Tukey’s test (α = 0.05). CFU/mL data were analyzed using the Kruskal-Wallis test, followed by Dunn’s test (α = 0.05). TEM revealed a sheet-like structure of GO nanoparticles. SEM showed the roughness of the nanocoated titanium surface. Raman spectroscopy indicated the presence of GO on the titanium surface, as evidenced by D and G bands. Higher apatite crystal deposition was observed on surfaces with greater GO concentrations at 7 and 14 days (bioactivity assay). The highest percentage of cell viability was noted in the 1.5% GO group after 48 h, compared to other groups at different time points ( p < 0.05). Surface treatment with varying GO concentrations induced greater cell viability compared to the acidic treatment ( p < 0.05). The 1.5% GO group showed the lowest antibacterial efficacy, as evidenced by the highest CFU/mL values ( p < 0.05). GO particles remained stable and chemically unchanged during the coating process. The GO-coated titanium surfaces showed no cytotoxicity and exhibited notable bioactive and antibacterial effects against Streptococcus mutans . These findings suggest that GO coatings may effectively enhance the biological and antimicrobial performance of titanium implants.
- 20 June 2024
- Published by SAGE Publications in Proceedings of the Institution of Mechanical Engineers, Part H: Journal of Engineering in Medicine
- Vol. 238 (7) , 793-802
Cellulose acetate scaffold coated with a hydroxyapatite/graphene oxide nanocomposite for application in tissue engineering
The objective of this study was to synthesize and characterize porous Cellulose Acetate (CA) scaffolds using the electrospinning technique and functionalize the surface of the scaffolds obtained through the dip-coating method with a Hydroxyapatite (HA) nanocomposite and varying concentrations of graphene oxide (GO) for application in tissue engineering regeneration techniques. The scaffolds were divided into four distinct groups based on their composition: 1) CA scaffolds; 2) CAHAC scaffolds; 3) CAHAGOC 1.0% scaffolds; 4) CAHAGOC 1.5% scaffolds. Scaffold analyses were conducted using X-ray Diffraction (XRD), Fourier Transform Infrared Spectroscopy (FTIR), Raman Spectroscopy, Scanning Electron Microscopy with Energy Dispersive Spectroscopy (SEM/EDS), and in vitro cell viability assays (WST). For the biological test analysis, Variance (two-way) was used, followed by Tukey’s post-test (α = 0.05). The XRD results revealed the predominant presence of CaP phases in the CAHAC, CAHAGOC 1.0%, and CAHAGOC 1.5% groups, emphasizing the presence of HA in the scaffolds. FTIR demonstrated characteristics of cellulose and PO4 bands in the groups containing HA, confirming the presence of CaP in the synthesized materials, as also indicated by XRD. Raman spectroscopy showed the presence of D and G bands, consistent with GO, confirming the successful incorporation of the HAGO nanocomposite into the scaffolds. The micrographs displayed overlapping electrospun fibers, forming the three-dimensional structure in the produced scaffolds. It was possible to observe hydroxyapatite crystals filling some of these pores, creating a suitable structure for cell adhesion, proliferation, and nutrition, as corroborated by the results of in vitro tests. All scaffolds exhibited high cell viability, with significant cell proliferation. Even after 48 h, there was a slight reduction in the number of cells, but a noteworthy increase in cell proliferation was evident in the CAHAGOC 1.5% group after 48 h ( p < 0.05). In conclusion, it can be affirmed that the produced scaffolds demonstrated physical and biological characteristics and properties capable of promoting cell adhesion and proliferation. Therefore, they represent significant potential for application in tissue engineering, offering a new perspective regarding techniques and biomaterials applied in regenerative therapies.
- 20 June 2024
- Published by SAGE Publications in Proceedings of the Institution of Mechanical Engineers, Part H: Journal of Engineering in Medicine
- Vol. 238 (7) , 793-802
Cellulose acetate scaffold coated with a hydroxyapatite/graphene oxide nanocomposite for application in tissue engineering
The objective of this study was to synthesize and characterize porous Cellulose Acetate (CA) scaffolds using the electrospinning technique and functionalize the surface of the scaffolds obtained through the dip-coating method with a Hydroxyapatite (HA) nanocomposite and varying concentrations of graphene oxide (GO) for application in tissue engineering regeneration techniques. The scaffolds were divided into four distinct groups based on their composition: 1) CA scaffolds; 2) CAHAC scaffolds; 3) CAHAGOC 1.0% scaffolds; 4) CAHAGOC 1.5% scaffolds. Scaffold analyses were conducted using X-ray Diffraction (XRD), Fourier Transform Infrared Spectroscopy (FTIR), Raman Spectroscopy, Scanning Electron Microscopy with Energy Dispersive Spectroscopy (SEM/EDS), and in vitro cell viability assays (WST). For the biological test analysis, Variance (two-way) was used, followed by Tukey’s post-test (α = 0.05). The XRD results revealed the predominant presence of CaP phases in the CAHAC, CAHAGOC 1.0%, and CAHAGOC 1.5% groups, emphasizing the presence of HA in the scaffolds. FTIR demonstrated characteristics of cellulose and PO4 bands in the groups containing HA, confirming the presence of CaP in the synthesized materials, as also indicated by XRD. Raman spectroscopy showed the presence of D and G bands, consistent with GO, confirming the successful incorporation of the HAGO nanocomposite into the scaffolds. The micrographs displayed overlapping electrospun fibers, forming the three-dimensional structure in the produced scaffolds. It was possible to observe hydroxyapatite crystals filling some of these pores, creating a suitable structure for cell adhesion, proliferation, and nutrition, as corroborated by the results of in vitro tests. All scaffolds exhibited high cell viability, with significant cell proliferation. Even after 48 h, there was a slight reduction in the number of cells, but a noteworthy increase in cell proliferation was evident in the CAHAGOC 1.5% group after 48 h ( p < 0.05). In conclusion, it can be affirmed that the produced scaffolds demonstrated physical and biological characteristics and properties capable of promoting cell adhesion and proliferation. Therefore, they represent significant potential for application in tissue engineering, offering a new perspective regarding techniques and biomaterials applied in regenerative therapies.
- 16 February 2024
- Published by SAGE Publications in Journal of Bioactive and Compatible Polymers
- Vol. 39 (2) , 91-103
Cellulose acetate scaffold containing hydroxyapatite/graphene oxide nanocomposite by electrospinning for advanced regenerative therapies
The aim of this study was to synthesize and characterize Cellulose Acetate (CA) porous scaffolds using the electrospinning technique associated with Hydroxyapatite (HA) and different concentrations of graphene oxide (GO), for advanced regenerative therapies application. The scaffolds were categorized into four distinct groups based on their composition: (1) Pure CA scaffolds; (2) CAHA scaffolds; (3) CAHAGO 1.0% scaffolds; (4) CAHAGO 1.5% scaffolds. Transmission Electron Microscopy (TEM) was used for the characterization of the nanocomposite. The scaffolds were analyzed by X-Ray Diffraction (XRD), Fourier Transform Infrared Spectroscopy (FTIR), Raman Spectroscopy, Scanning Electron Microscopy with Energy Dispersive Spectroscopy (SEM/EDS), and in vitro cell viability assays (WST). For the biological test analysis of Variance (two-way) was used, followed by Tukey’s post-test (α = 0.05). The TEM analysis allowed for the visualization of the deposition of HA on the graphene sheets, confirming the synthesis of the nanocomposite. XRD revealed the predominant presence of CaP phases in the CAHA, CAHAGO 1.0%, and CAHAGO 1.5% groups, underscoring the inherent mineral composition of the scaffolds. FTIR demonstrated cellulose characteristics and PO4 bands in the groups containing HA, confirming the effective incorporation of this material. Raman spectroscopy revealed distinct peaks in the GO groups, conclusively verifying the successful integration of graphene into the scaffold matrix. The micrographs showcased irregular pores filling the entire surface, arising from the intricate overlapping of fibers during scaffold formation. Importantly, all scaffolds exhibited excellent cell viability in the conducted assays. A proliferation process was observed in CAHA and CAHAGO 1.5% groups after 48 h ( p < 0.05). In conclusion, the scaffolds synthesized hold significant promise in the realm of tissue engineering and provide a fresh perspective on the possibilities for regenerative therapies.
- 16 February 2024
- Published by SAGE Publications in Journal of Bioactive and Compatible Polymers
- Vol. 39 (2) , 91-103
Cellulose acetate scaffold containing hydroxyapatite/graphene oxide nanocomposite by electrospinning for advanced regenerative therapies
The aim of this study was to synthesize and characterize Cellulose Acetate (CA) porous scaffolds using the electrospinning technique associated with Hydroxyapatite (HA) and different concentrations of graphene oxide (GO), for advanced regenerative therapies application. The scaffolds were categorized into four distinct groups based on their composition: (1) Pure CA scaffolds; (2) CAHA scaffolds; (3) CAHAGO 1.0% scaffolds; (4) CAHAGO 1.5% scaffolds. Transmission Electron Microscopy (TEM) was used for the characterization of the nanocomposite. The scaffolds were analyzed by X-Ray Diffraction (XRD), Fourier Transform Infrared Spectroscopy (FTIR), Raman Spectroscopy, Scanning Electron Microscopy with Energy Dispersive Spectroscopy (SEM/EDS), and in vitro cell viability assays (WST). For the biological test analysis of Variance (two-way) was used, followed by Tukey’s post-test (α = 0.05). The TEM analysis allowed for the visualization of the deposition of HA on the graphene sheets, confirming the synthesis of the nanocomposite. XRD revealed the predominant presence of CaP phases in the CAHA, CAHAGO 1.0%, and CAHAGO 1.5% groups, underscoring the inherent mineral composition of the scaffolds. FTIR demonstrated cellulose characteristics and PO4 bands in the groups containing HA, confirming the effective incorporation of this material. Raman spectroscopy revealed distinct peaks in the GO groups, conclusively verifying the successful integration of graphene into the scaffold matrix. The micrographs showcased irregular pores filling the entire surface, arising from the intricate overlapping of fibers during scaffold formation. Importantly, all scaffolds exhibited excellent cell viability in the conducted assays. A proliferation process was observed in CAHA and CAHAGO 1.5% groups after 48 h ( p < 0.05). In conclusion, the scaffolds synthesized hold significant promise in the realm of tissue engineering and provide a fresh perspective on the possibilities for regenerative therapies.
- Open Access
- 10 September 2023
- Published by Archives of Health Investigation in ARCHIVES OF HEALTH INVESTIGATION
- Vol. 12 (9) , 1962-1968
Chemical, Morphological and Bacterial Adhesion Analysis of Orthodontic Wires Composed of Different Metallic Alloys
The purpose of this study was to evaluate the chemical, morphological and bacterial adhesion characteristics of orthodontic arches composed of different metal alloys. The wire segments (n=10) were allocated to the following groups: G1) Tru-Chrome- Rock Mountain Steel Wire (Colorado-USA); G2) NiTi- Rock Mountain Wire (Colorado-USA); G3) TiMb Rock Mountain Wire (Colored-USA); G4) NbTi Gummetal- Rock Mountain Wire (Colorado-USA). The orthodontic arches were segmented (20mm) and sterilized by means of ultraviolet light. Using Confocal Laser Microscopy (CLM), the roughness of archwires were investigated. The metallic alloys composition was analyzed by means of Scanning Electron Microscopy/Energy-dispersive Spectroscopy (SEM/EDS). The S. mutans biofilm growth was performed on the arches and analyzed by means of SEM and Spectrophotometry. Surface roughness and Spectrophotometry data were submitted to one-way ANOVA, followed by Tukey's test (α=0.05) and SEM/EDS data obtained by exploratory analysis. The NbTi arches showed higher surface roughness when compared to the other groups, followed by the NiTi and TiMb arches and the steel arches group (p<0.05). It was observed a lower adherence of S. mutans biofilm in steel arches when compared to the other groups. The absorbance results showed higher biofilm formation for the NbTi group, followed by Steel, NiTi and TiMb. (p<0.05). The results of EDS confirm the compositions proposed by the manufacturer. It was concluded that the alloy type in orthodontic arches has an effect on surface roughness. The chemical and morphological characteristics of the arches are related to the adhesion of S. mutans biofilm.
- 10 September 2023
- Published by Archives of Health Investigation in ARCHIVES OF HEALTH INVESTIGATION
- Vol. 12 (9) , 1962-1968
Open AccessChemical, Morphological and Bacterial Adhesion Analysis of Orthodontic Wires Composed of Different Metallic Alloys
The purpose of this study was to evaluate the chemical, morphological and bacterial adhesion characteristics of orthodontic arches composed of different metal alloys. The wire segments (n=10) were allocated to the following groups: G1) Tru-Chrome- Rock Mountain Steel Wire (Colorado-USA); G2) NiTi- Rock Mountain Wire (Colorado-USA); G3) TiMb Rock Mountain Wire (Colored-USA); G4) NbTi Gummetal- Rock Mountain Wire (Colorado-USA). The orthodontic arches were segmented (20mm) and sterilized by means of ultraviolet light. Using Confocal Laser Microscopy (CLM), the roughness of archwires were investigated. The metallic alloys composition was analyzed by means of Scanning Electron Microscopy/Energy-dispersive Spectroscopy (SEM/EDS). The S. mutans biofilm growth was performed on the arches and analyzed by means of SEM and Spectrophotometry. Surface roughness and Spectrophotometry data were submitted to one-way ANOVA, followed by Tukey's test (α=0.05) and SEM/EDS data obtained by exploratory analysis. The NbTi arches showed higher surface roughness when compared to the other groups, followed by the NiTi and TiMb arches and the steel arches group (p<0.05). It was observed a lower adherence of S. mutans biofilm in steel arches when compared to the other groups. The absorbance results showed higher biofilm formation for the NbTi group, followed by Steel, NiTi and TiMb. (p<0.05). The results of EDS confirm the compositions proposed by the manufacturer. It was concluded that the alloy type in orthodontic arches has an effect on surface roughness. The chemical and morphological characteristics of the arches are related to the adhesion of S. mutans biofilm.