Nazerke Muktanova
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Nazerke Muktanova has a total of 37 co-authors. Here are the top co-authors by number of shared publications:
- Bauyrzhan Rakhadilov
PlasmaScience LLP, Ust-Kamenogorsk 070018, Kazakhstan
9 shared publications - Dauir Kakimzhanov
PlasmaScience LLP, Ust-Kamenogorsk 070010, Kazakhstan
5 shared publications - Aidar Kengesbekov
D. Serikbayev East Kazakhstan state technical university
4 shared publications - Nurtoleu Magazov
D. Serikbayev East Kazakhstan state technical university
4 shared publications - Ainur Seitkhanova
Pavlodar Pedagogical University, Pavlodar 140000, Kazakhstan
2 shared publications - Daryn Baizhan
Research Center Surface Engineering and Tribology, Sarsen Amanzholov East Kazakhstan University, Ust-Kamenogorsk 070000, Kazakhstan
2 shared publications
Latest Publications
- Open Access
- 14 October 2026
- Published by al-Farabi Kazakh National University in Recent Contributions to Physics
- Vol. 99 (4) , 59-68
Impact Of Co–Cr, Ni, and NiCr binder systems on the microstructure and functional properties of WC coatings produced by detonation spraying
This study investigates the influence of metallic binder composition (Co–Cr, Ni, and NiCr) on the microstructure and performance characteristics of tungsten carbide-based coatings deposited by detonation spraying. A comprehensive characterization was carried out using scanning electron microscopy, EDS elemental mapping, microhardness testing, tribological evaluation, scratch testing, and electrochemical corrosion analysis. The results demonstrate that binder type significantly affects coating porosity, WC phase distribution, hardness, and tribological behavior. The WC–Co-Cr coating exhibited the most favorable combination of properties: the lowest coefficient of friction (0.515), the highest microhardness (1232.55 HV), the best scratch resistance, and superior corrosion resistance in 3.5 wt.% NaCl solution. The WC–Ni coating showed the lowest porosity (0.40%) due to the high fluidity of the nickel binder, while WC–NiCr demonstrated the highest porosity (2.78%) and the most pronounced susceptibility to cracking under progressive loading. The findings confirm the strong potential of detonation-sprayed WC–Co-Cr coatings for extending the service life of pipeline valves and other components operating under wear and corrosion conditions in the oil and gas industry.
- 14 October 2026
- Published by al-Farabi Kazakh National University in Recent Contributions to Physics
- Vol. 99 (4) , 59-68
Open AccessImpact Of Co–Cr, Ni, and NiCr binder systems on the microstructure and functional properties of WC coatings produced by detonation spraying
This study investigates the influence of metallic binder composition (Co–Cr, Ni, and NiCr) on the microstructure and performance characteristics of tungsten carbide-based coatings deposited by detonation spraying. A comprehensive characterization was carried out using scanning electron microscopy, EDS elemental mapping, microhardness testing, tribological evaluation, scratch testing, and electrochemical corrosion analysis. The results demonstrate that binder type significantly affects coating porosity, WC phase distribution, hardness, and tribological behavior. The WC–Co-Cr coating exhibited the most favorable combination of properties: the lowest coefficient of friction (0.515), the highest microhardness (1232.55 HV), the best scratch resistance, and superior corrosion resistance in 3.5 wt.% NaCl solution. The WC–Ni coating showed the lowest porosity (0.40%) due to the high fluidity of the nickel binder, while WC–NiCr demonstrated the highest porosity (2.78%) and the most pronounced susceptibility to cracking under progressive loading. The findings confirm the strong potential of detonation-sprayed WC–Co-Cr coatings for extending the service life of pipeline valves and other components operating under wear and corrosion conditions in the oil and gas industry.
- 30 September 2026
- Published by Toraighyrov University in Science and Technology of Kazakhstan
- No. 3,2026
СТРУКТУРНЫЙ И ФУНКЦИОНАЛЬНЫЙ АНАЛИЗ ПОКРЫТИЙ CRN И CR/CRN НА СПЛАВЕ E110
Цель работы заключалась в получении однослойных покрытий CrN и многослойных покрытий Cr/CrN на циркониевом сплаве E110 и в оценке влияния газового режима осаждения и многослойной архитектуры на их структурное состояние, механико-трибологические свойства и устойчивость к высокотемпературному паровому окислению. Покрытия получали реактивным магнетронным распылением хромовой мишени. Для однослойного CrN проверяли три газовых режима Ar/N2 : 90/30, 85/35 и 80/40 ст.см³/мин. Для Cr/CrN готовили покрытия из 2, 4 и 6 слоёв. Образцы исследовали методами СЭМ/EDS, XRD, GDOES, наноиндентирования, АСМ и испытаний на трение; отдельно проводили выдержку в водяном паре при 1100 °C в течение 2 ч. Установлено, что при Ar/N2 = 80/40 ст.см³/мин формируется наиболее ровный однослойный CrN: Ra = 0,114±0,006 мкм, а на рентгенограмме выражены линии кубического CrN. В серии Cr/CrN толщина увеличивалась с ростом числа слоёв; у 6-слойного образца она достигала около 4,18 мкм. Для этого покрытия получены H = 5,00±0,27 ГПа, E = 110±4 ГПа и скорость износа 2,26×10-4 мм³·Н-¹·м-¹ После парового окисления на поверхности покрытий регистрировался Cr2 O3 , а в 6-слойном образце сохранялись слабые линии CrN и Cr, что указывает на частичную сохранность внутренних слоёв. Практическая значимость работы состоит в обосновании перспективности многослойной архитектуры Cr/CrN как защитного барьерного покрытия для циркониевых оболочек ТВЭЛ нового поколения, устойчивых к аварийным режимам эксплуатации. Ключевые слова: циркониевый сплав E110, покрытия Cr/CrN, магнетронное распыление, высокотемпературное паровое окисление, многослойная структура, топливо, устойчивое к авариям.
- 30 September 2026
- Published by Toraighyrov University in Science and Technology of Kazakhstan
- No. 3,2026
СТРУКТУРНЫЙ И ФУНКЦИОНАЛЬНЫЙ АНАЛИЗ ПОКРЫТИЙ CRN И CR/CRN НА СПЛАВЕ E110
Цель работы заключалась в получении однослойных покрытий CrN и многослойных покрытий Cr/CrN на циркониевом сплаве E110 и в оценке влияния газового режима осаждения и многослойной архитектуры на их структурное состояние, механико-трибологические свойства и устойчивость к высокотемпературному паровому окислению. Покрытия получали реактивным магнетронным распылением хромовой мишени. Для однослойного CrN проверяли три газовых режима Ar/N2 : 90/30, 85/35 и 80/40 ст.см³/мин. Для Cr/CrN готовили покрытия из 2, 4 и 6 слоёв. Образцы исследовали методами СЭМ/EDS, XRD, GDOES, наноиндентирования, АСМ и испытаний на трение; отдельно проводили выдержку в водяном паре при 1100 °C в течение 2 ч. Установлено, что при Ar/N2 = 80/40 ст.см³/мин формируется наиболее ровный однослойный CrN: Ra = 0,114±0,006 мкм, а на рентгенограмме выражены линии кубического CrN. В серии Cr/CrN толщина увеличивалась с ростом числа слоёв; у 6-слойного образца она достигала около 4,18 мкм. Для этого покрытия получены H = 5,00±0,27 ГПа, E = 110±4 ГПа и скорость износа 2,26×10-4 мм³·Н-¹·м-¹ После парового окисления на поверхности покрытий регистрировался Cr2 O3 , а в 6-слойном образце сохранялись слабые линии CrN и Cr, что указывает на частичную сохранность внутренних слоёв. Практическая значимость работы состоит в обосновании перспективности многослойной архитектуры Cr/CrN как защитного барьерного покрытия для циркониевых оболочек ТВЭЛ нового поколения, устойчивых к аварийным режимам эксплуатации. Ключевые слова: циркониевый сплав E110, покрытия Cr/CrN, магнетронное распыление, высокотемпературное паровое окисление, многослойная структура, топливо, устойчивое к авариям.
- 29 March 2026
- Published by Karagandy University of the name of academician E.A. Buketov in Bulletin of the Karaganda University "Physics Series"
- Vol. 12131 (1)
Incorporating TiO2 Nanoparticles to Enhance Corrosion Resistance, Cytocompatibility of PEO Calcium–Phosphate Coatings on Titanium
Titanium and its alloys are widely used in biomedical implants due to their favorable mechanical properties and corrosion resistance; however, their natural surface lacks sufficient bioactivity. Micro-arc oxidation is a promising approach to producing bioactive coatings, and the incorporation of nanoparticles such as TiO2 may further improve their functionality. This study aimed to determine the optimal TiO2 nanoparticle concentration in the micro-arc oxidation electrolyte that ensures coating stability and biological safety. Calcium–phosphate coatings were fabricated on commercially pure titanium using micro-arc oxidation with two TiO2 concentrations: 0.5 wt.% (MAO 1) and 1 wt.% (MAO 2). Surface morphology, porosity, and phase composition were analyzed by scanning electron microscopy, energy-dispersive spectroscopy, and X-ray diffraction. Corrosion resistance was evaluated via potentiodynamic polarization in NaCl and Ringer’s solutions, while biocompatibility was assessed in vitro using HOS human osteosarcoma cells and MTT assays. Increasing the TiO2 content to 1 % decreased coating porosity (13.7 % vs. 26.3 % for MAO 1), enhanced corrosion protection, and reduced the friction coefficient compared to bare titanium. However, MAO 2 exhibited high cytotoxicity (81 % cell death) and partial structural degradation in the biological medium. MAO 1 maintained integrity and showed no toxic effects (3 % cell death). These results suggest that 0.5 % TiO2 is the optimal concentration, providing a balance between corrosion resistance, mechanical stability, and biocompatibility, supporting the development of safer implant coatings.
- 29 March 2026
- Published by Karagandy University of the name of academician E.A. Buketov in Bulletin of the Karaganda University "Physics Series"
- Vol. 12131 (1)
Incorporating TiO2 Nanoparticles to Enhance Corrosion Resistance, Cytocompatibility of PEO Calcium–Phosphate Coatings on Titanium
Titanium and its alloys are widely used in biomedical implants due to their favorable mechanical properties and corrosion resistance; however, their natural surface lacks sufficient bioactivity. Micro-arc oxidation is a promising approach to producing bioactive coatings, and the incorporation of nanoparticles such as TiO2 may further improve their functionality. This study aimed to determine the optimal TiO2 nanoparticle concentration in the micro-arc oxidation electrolyte that ensures coating stability and biological safety. Calcium–phosphate coatings were fabricated on commercially pure titanium using micro-arc oxidation with two TiO2 concentrations: 0.5 wt.% (MAO 1) and 1 wt.% (MAO 2). Surface morphology, porosity, and phase composition were analyzed by scanning electron microscopy, energy-dispersive spectroscopy, and X-ray diffraction. Corrosion resistance was evaluated via potentiodynamic polarization in NaCl and Ringer’s solutions, while biocompatibility was assessed in vitro using HOS human osteosarcoma cells and MTT assays. Increasing the TiO2 content to 1 % decreased coating porosity (13.7 % vs. 26.3 % for MAO 1), enhanced corrosion protection, and reduced the friction coefficient compared to bare titanium. However, MAO 2 exhibited high cytotoxicity (81 % cell death) and partial structural degradation in the biological medium. MAO 1 maintained integrity and showed no toxic effects (3 % cell death). These results suggest that 0.5 % TiO2 is the optimal concentration, providing a balance between corrosion resistance, mechanical stability, and biocompatibility, supporting the development of safer implant coatings.
- Open Access
Detonation Spraying of Functionally Graded Hydroxyapatite/Titanium Coatings on Ti–6Al–4V Alloy
In this work, two configurations of Ti/HAp functionally graded coatings were fabricated on Ti–6Al–4V alloy substrates using detonation spraying. The coatings differed in the number and sequence of Ti and hydroxyapatite (HAp) deposition cycles, resulting in distinct gradient architectures: Configuration 1 incorporated a sharper transition from the Ti-rich base to the HAp-rich surface, whereas Configuration 2 featured a smoother and more gradual compositional gradient. The microstructure and elemental distribution were examined by scanning electron microscopy (SEM) and energy-dispersive X-ray spectroscopy (EDS). Both configurations exhibited well-defined gradient layering, with titanium concentrated near the coating–substrate interface and an increased Ca and P content toward the upper bioceramic region. Raman spectroscopy confirmed the preservation of hydroxyapatite as the main phase, showing a characteristic 961 cm−1 band. Adhesion strength measured according to ASTM C633-13 was 45.78 ± 4.4 MPa for Configuration 1 and 52.32 ± 6.7 MPa for Configuration 2, both significantly exceeding the minimum required 15 MPa. The findings demonstrate that detonation-sprayed Ti/HAp gradient coatings provide strong adhesion and stable bioceramic surfaces, making them promising for metal implant applications.
Open AccessDetonation Spraying of Functionally Graded Hydroxyapatite/Titanium Coatings on Ti–6Al–4V Alloy
In this work, two configurations of Ti/HAp functionally graded coatings were fabricated on Ti–6Al–4V alloy substrates using detonation spraying. The coatings differed in the number and sequence of Ti and hydroxyapatite (HAp) deposition cycles, resulting in distinct gradient architectures: Configuration 1 incorporated a sharper transition from the Ti-rich base to the HAp-rich surface, whereas Configuration 2 featured a smoother and more gradual compositional gradient. The microstructure and elemental distribution were examined by scanning electron microscopy (SEM) and energy-dispersive X-ray spectroscopy (EDS). Both configurations exhibited well-defined gradient layering, with titanium concentrated near the coating–substrate interface and an increased Ca and P content toward the upper bioceramic region. Raman spectroscopy confirmed the preservation of hydroxyapatite as the main phase, showing a characteristic 961 cm−1 band. Adhesion strength measured according to ASTM C633-13 was 45.78 ± 4.4 MPa for Configuration 1 and 52.32 ± 6.7 MPa for Configuration 2, both significantly exceeding the minimum required 15 MPa. The findings demonstrate that detonation-sprayed Ti/HAp gradient coatings provide strong adhesion and stable bioceramic surfaces, making them promising for metal implant applications.
- Open Access
- 2 December 2025
- Published by MDPI AG in Applied Sciences
- Vol. 15 (23) , 12773
Effect of Multilayer Cr/CrN Coatings Deposited by Magnetron Sputtering on the Thermal Stability and High-Temperature Steam Oxidation Resistance of Zirconium Alloy E110
The effect of the multilayer structure of Cr/CrN coatings deposited by reactive magnetron sputtering on zirconium alloy E110 (Zr–1Nb) on their thermal stability and resistance to steam oxidation at 1100 °C was studied. Coatings with different numbers of alternating Cr and CrN sublayers (1, 2, 4, and 6) were fabricated using experimental methods of X-ray diffraction (XRD) and scanning electron microscopy with energy-dispersive analysis (SEM/EDS). It was shown that an increase in the number of alternating Cr and CrN sublayers leads to the preservation of the cubic phase of CrN, the formation of a dense structure, and a decrease in Cr–Zr interdiffusion. After testing, multilayer coatings retaining the internal structure and a sufficiently structurally dense Cr2O3 layer effectively ensured air penetration. The best thermal stability was demonstrated by a six-layer coating, ensuring minimal oxidation and preservation of the E110 substrate.
- 2 December 2025
- Published by MDPI AG in Applied Sciences
- Vol. 15 (23) , 12773
Open AccessEffect of Multilayer Cr/CrN Coatings Deposited by Magnetron Sputtering on the Thermal Stability and High-Temperature Steam Oxidation Resistance of Zirconium Alloy E110
The effect of the multilayer structure of Cr/CrN coatings deposited by reactive magnetron sputtering on zirconium alloy E110 (Zr–1Nb) on their thermal stability and resistance to steam oxidation at 1100 °C was studied. Coatings with different numbers of alternating Cr and CrN sublayers (1, 2, 4, and 6) were fabricated using experimental methods of X-ray diffraction (XRD) and scanning electron microscopy with energy-dispersive analysis (SEM/EDS). It was shown that an increase in the number of alternating Cr and CrN sublayers leads to the preservation of the cubic phase of CrN, the formation of a dense structure, and a decrease in Cr–Zr interdiffusion. After testing, multilayer coatings retaining the internal structure and a sufficiently structurally dense Cr2O3 layer effectively ensured air penetration. The best thermal stability was demonstrated by a six-layer coating, ensuring minimal oxidation and preservation of the E110 substrate.
- Open Access
Structural and Phase Characteristics and Properties of Multilayer Cr/CrN Coatings Obtained by Magnetron Sputtering
Multilayer Cr/CrN coatings with two-, four-, and six-layer architectures were deposited on E110 zirconium alloy substrates by reactive magnetron sputtering. The effect of layer number on structure, phase composition, and performance was systematically investigated. XRD revealed that the coatings consisted mainly of CrN and Cr phases, with an increase in the CrN fraction and texture intensity as the number of layers increased. Cross-sectional SEM and EDS analyses confirmed the formation of dense multilayer structures with clear Cr/CrN interfaces and strong adhesion to the substrate. Nanoindentation showed a progressive increase in hardness and Young’s modulus from 2.59 ± 0.09 GPa and 97 ± 2 GPa (two-layer) to 5.0 ± 0.27 GPa and 110 ± 4 GPa (six-layer), respectively. Tribological and scratch tests demonstrated that the 6-layer coating exhibited the lowest wear rate and highest adhesion strength (Lc ≈ 20.5 N).
Open AccessStructural and Phase Characteristics and Properties of Multilayer Cr/CrN Coatings Obtained by Magnetron Sputtering
Multilayer Cr/CrN coatings with two-, four-, and six-layer architectures were deposited on E110 zirconium alloy substrates by reactive magnetron sputtering. The effect of layer number on structure, phase composition, and performance was systematically investigated. XRD revealed that the coatings consisted mainly of CrN and Cr phases, with an increase in the CrN fraction and texture intensity as the number of layers increased. Cross-sectional SEM and EDS analyses confirmed the formation of dense multilayer structures with clear Cr/CrN interfaces and strong adhesion to the substrate. Nanoindentation showed a progressive increase in hardness and Young’s modulus from 2.59 ± 0.09 GPa and 97 ± 2 GPa (two-layer) to 5.0 ± 0.27 GPa and 110 ± 4 GPa (six-layer), respectively. Tribological and scratch tests demonstrated that the 6-layer coating exhibited the lowest wear rate and highest adhesion strength (Lc ≈ 20.5 N).
- Open Access
Use of Computational Fluid Dynamics (CFD) Methods to Analyze Combustion Chamber Processes at HVOF Spraying and Their Comparison with Experimental Data
This paper discusses the process of high-velocity oxygen fuel (HVOF) spraying with modeling of the gas flow parameters and behavior of WC-Co-Cr powder particles of different fractions (up to 20 µm, 21–35 μm and 36–45 μm). It was found that the temperature of the gas stream reaches a maximum of about 2700 °C, after which it gradually decreases, and the pressure in the combustion chamber (before the exit of gases through the nozzle) reaches maximum values, exceeding 400,000 Pa, and the pressure at the exit of the nozzle stabilizes at about 100,000 Pa, which corresponds to the standard atmospheric pressure. The gas velocity increases to 1300–1400 m/s and then decreases to 400 m/s at a distance of about 150 mm. It was determined that powder particles of the 21–35 µm fraction provide more stable parameters of velocity and temperature. Small particles (up to 20 µm) lose velocity and temperature faster as they advance, which deteriorates the coating quality, which was also experimentally confirmed. All results obtained from the HVOF process modeling fully align with the data from experimental studies.
Open AccessUse of Computational Fluid Dynamics (CFD) Methods to Analyze Combustion Chamber Processes at HVOF Spraying and Their Comparison with Experimental Data
This paper discusses the process of high-velocity oxygen fuel (HVOF) spraying with modeling of the gas flow parameters and behavior of WC-Co-Cr powder particles of different fractions (up to 20 µm, 21–35 μm and 36–45 μm). It was found that the temperature of the gas stream reaches a maximum of about 2700 °C, after which it gradually decreases, and the pressure in the combustion chamber (before the exit of gases through the nozzle) reaches maximum values, exceeding 400,000 Pa, and the pressure at the exit of the nozzle stabilizes at about 100,000 Pa, which corresponds to the standard atmospheric pressure. The gas velocity increases to 1300–1400 m/s and then decreases to 400 m/s at a distance of about 150 mm. It was determined that powder particles of the 21–35 µm fraction provide more stable parameters of velocity and temperature. Small particles (up to 20 µm) lose velocity and temperature faster as they advance, which deteriorates the coating quality, which was also experimentally confirmed. All results obtained from the HVOF process modeling fully align with the data from experimental studies.
- Open Access
- 1 January 2025
- Published by American Institute of Mathematical Sciences (AIMS) in AIMS Materials Science
- Vol. 12 (6) , 1215-1240
Influence of gas mixture on the mechanical and physical properties of CrN coatings obtained by magnetron sputtering method
This paper investigated the influence of the Ar/N2 working gas mixture composition on the morphological, structural, mechanical, and corrosion properties of single-layer CrN coatings obtained by reactive magnetron sputtering on E110 zirconium alloy substrates. It was shown that an increase in the N2 fraction in the working gas leads to a sequential compaction of the coating structure, an increase in the degree of nitride formation, and the formation of a more homogeneous cubic CrN phase (Fm-3m), which was confirmed by Grazing-Incidence X-Ray Diffraction data (GI-XRD). Scanning electron microscopy (SEM) analysis revealed a transition from a relatively loose morphology at 90/30 sccm to a denser and finer-grained structure at 80/40 sccm. It was established that an increase in the partial pressure of nitrogen contributes to a decrease in surface roughness (Ra from 0.152 to 0.114 μm) and an increase in nanohardness from 4.1 to 6.7 GPa, as well as Young's modulus from 97 to 110 GPa, associated with the formation of a denser and closer to stoichiometric CrN phase. Electrochemical tests in 3.5% NaCl showed a significant improvement in corrosion resistance; the corrosion current density decreased from 3.82 × 10-6 to 1.73 × 10-6 A/cm2, and the corrosion rate decreased from 0.054 to 0.0024 mm/year.
- 1 January 2025
- Published by American Institute of Mathematical Sciences (AIMS) in AIMS Materials Science
- Vol. 12 (6) , 1215-1240
Open AccessInfluence of gas mixture on the mechanical and physical properties of CrN coatings obtained by magnetron sputtering method
This paper investigated the influence of the Ar/N2 working gas mixture composition on the morphological, structural, mechanical, and corrosion properties of single-layer CrN coatings obtained by reactive magnetron sputtering on E110 zirconium alloy substrates. It was shown that an increase in the N2 fraction in the working gas leads to a sequential compaction of the coating structure, an increase in the degree of nitride formation, and the formation of a more homogeneous cubic CrN phase (Fm-3m), which was confirmed by Grazing-Incidence X-Ray Diffraction data (GI-XRD). Scanning electron microscopy (SEM) analysis revealed a transition from a relatively loose morphology at 90/30 sccm to a denser and finer-grained structure at 80/40 sccm. It was established that an increase in the partial pressure of nitrogen contributes to a decrease in surface roughness (Ra from 0.152 to 0.114 μm) and an increase in nanohardness from 4.1 to 6.7 GPa, as well as Young's modulus from 97 to 110 GPa, associated with the formation of a denser and closer to stoichiometric CrN phase. Electrochemical tests in 3.5% NaCl showed a significant improvement in corrosion resistance; the corrosion current density decreased from 3.82 × 10-6 to 1.73 × 10-6 A/cm2, and the corrosion rate decreased from 0.054 to 0.0024 mm/year.
- Open Access
Investigation of the Influence of the Oxygen Flow Rate on the Mechanical, Structural and Operational Properties of 86WC-10Co-4Cr Coatings, as Determined Using the High-Velocity Oxyfuel Spraying Method
The structural-phase composition and tribological and performance properties of coatings based on an 86WC-10Co-4Cr composition obtained by the HVOF method at varying (150 L/min, 170 L/min, 190 L/min) oxygen flow rates were studied. The results showed that the coefficient of friction of coatings in gear oil remained almost unchanged with the variation in oxygen flow rate. However, microhardness increased significantly with an increasing oxygen flow rate, reaching a maximum at 190 L/min. An increasing oxygen flow rate was also accompanied by an increase in roughness and coating thickness, with a decrease in porosity, particularly notable at 190 L/min. Adhesion strength reached the maximum values for the A2 and A3 coatings under high loads. The phase composition of the coatings included WC, W2C and CoO phases irrespective of the oxygen flow rate, and their microstructure was characterized by a more homogeneous and dense structure. Thus, this study confirmed that the optimal oxygen flow rate for achieving an improved performance and tribological characteristics of 86WC-10Co-4Cr coatings is 190 L/min.
Open AccessInvestigation of the Influence of the Oxygen Flow Rate on the Mechanical, Structural and Operational Properties of 86WC-10Co-4Cr Coatings, as Determined Using the High-Velocity Oxyfuel Spraying Method
The structural-phase composition and tribological and performance properties of coatings based on an 86WC-10Co-4Cr composition obtained by the HVOF method at varying (150 L/min, 170 L/min, 190 L/min) oxygen flow rates were studied. The results showed that the coefficient of friction of coatings in gear oil remained almost unchanged with the variation in oxygen flow rate. However, microhardness increased significantly with an increasing oxygen flow rate, reaching a maximum at 190 L/min. An increasing oxygen flow rate was also accompanied by an increase in roughness and coating thickness, with a decrease in porosity, particularly notable at 190 L/min. Adhesion strength reached the maximum values for the A2 and A3 coatings under high loads. The phase composition of the coatings included WC, W2C and CoO phases irrespective of the oxygen flow rate, and their microstructure was characterized by a more homogeneous and dense structure. Thus, this study confirmed that the optimal oxygen flow rate for achieving an improved performance and tribological characteristics of 86WC-10Co-4Cr coatings is 190 L/min.
- Open Access
- 30 September 2024
- Published by Republican State Enterprise "National Nuclear Center of the Republic of Kazakhstan" in NNC RK Bulletin
- No. 3,p. 91-104
INFLUENCE OF VARYING THE SPRAYING DISTANCE ON THE STRUCTURAL-PHASE STATE AND MECHANOTRIBOLOGICAL PROPERTIES OF 86WC-10Co-4Cr-BASED COATINGS OBTAINED BY THE HVOF METHOD
This paper presents the results of a metallographic and tribological study of 86WC-10Co-4Cr coatings obtained by the HVOF method on the Termika-3 unit at varying spraying distances. The influence of spraying distance on the coating microstructure, phase composition, as well as mechanical and tribological properties, was studied. The phase composition, microstructure and elemental distribution were analyzed using X-ray diffraction, scanning electron microscopy and energy dispersive spectroscopy techniques. The hardness was measured on a Vickers microhardness tester, the friction coefficient and wear rate were investigated using a tribometer. According to the results of the study, it was found that the optimum spraying distance for 86WC-10Co-4Cr coatings with improved wear resistance and hardness characteristics and low porosity is 300 mm.
- 30 September 2024
- Published by Republican State Enterprise "National Nuclear Center of the Republic of Kazakhstan" in NNC RK Bulletin
- No. 3,p. 91-104
Open AccessINFLUENCE OF VARYING THE SPRAYING DISTANCE ON THE STRUCTURAL-PHASE STATE AND MECHANOTRIBOLOGICAL PROPERTIES OF 86WC-10Co-4Cr-BASED COATINGS OBTAINED BY THE HVOF METHOD
This paper presents the results of a metallographic and tribological study of 86WC-10Co-4Cr coatings obtained by the HVOF method on the Termika-3 unit at varying spraying distances. The influence of spraying distance on the coating microstructure, phase composition, as well as mechanical and tribological properties, was studied. The phase composition, microstructure and elemental distribution were analyzed using X-ray diffraction, scanning electron microscopy and energy dispersive spectroscopy techniques. The hardness was measured on a Vickers microhardness tester, the friction coefficient and wear rate were investigated using a tribometer. According to the results of the study, it was found that the optimum spraying distance for 86WC-10Co-4Cr coatings with improved wear resistance and hardness characteristics and low porosity is 300 mm.