Shao-Quan Lu
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Shao-Quan Lu has a total of 4 co-authors. Here are the top co-authors by number of shared publications:
- Liu-Ho Chiu
Department of Mechanical and Materials Engineering, Tatung University, Taipei 104-327, Taiwan
4 shared publications - Chung-Kwei Lin
Research Center of Digital Oral Science and Technology, College of Oral Medicine, Taipei Medical University, Taipei 11031, Taiwan
2 shared publications - Pei-Jung Chang
Research Center of Digital Oral Science and Technology, College of Oral Medicine, Taipei Medical University, Taipei 110, Taiwan
2 shared publications - Hsueh-Hung Cheng
Department of Mechanical and Materials Engineering, Tatung University, Taipei 104-327, Taiwan
1 shared publication
Latest Publications
- Open Access
Effects of Prior Heat Treatment and Induction Hardening on the Properties of JIS SUJ3 Bearing Steel
Bearing steels are frequently used in highly loaded components, such as roller bearings, due to their excellent hardenability and wear resistance. Microstructure, hardness, and residual stress distribution of the bearings significantly affect the wear resistance of the parts. In the present study, experiments investigated the effects of austenitizing temperature (850, 900, and 950 °C), with or without cryogenic treatment, and induction hardening treatment (9 and 12 kW) on the microstructure, microhardness, the amount of retained austenite, surface residual stress, and wear behavior of JIS SUJ3 steel. The experimental results revealed that the austenitized specimens’ microstructure consisted of martensite, retained austenite, and dispersed granular alloy carbide exhibiting high hardness. After cryogenic or induction hardening treatment, the surface residual stress of austenitized specimens exhibited compressive stress rather than its original tensile stress state. The induction hardening treatment can significantly increase the microhardness of austenitized specimens, followed by quenching. Furthermore, the induction-hardened surface possessed less retained austenite. For practical industrial applications, a prior austenitizing heat treatment at 950 °C followed by hardening with an induction power of 12 kW was the optimal parameter for JIS SUJ3 bearing steel. The maximum microhardness and surface residual stress were 920 HV0.3 and −1083 MPa, respectively, while the lowest weight loss was 0.5 mg after the 10,000-revolution wear test.
Open AccessEffects of Prior Heat Treatment and Induction Hardening on the Properties of JIS SUJ3 Bearing Steel
Bearing steels are frequently used in highly loaded components, such as roller bearings, due to their excellent hardenability and wear resistance. Microstructure, hardness, and residual stress distribution of the bearings significantly affect the wear resistance of the parts. In the present study, experiments investigated the effects of austenitizing temperature (850, 900, and 950 °C), with or without cryogenic treatment, and induction hardening treatment (9 and 12 kW) on the microstructure, microhardness, the amount of retained austenite, surface residual stress, and wear behavior of JIS SUJ3 steel. The experimental results revealed that the austenitized specimens’ microstructure consisted of martensite, retained austenite, and dispersed granular alloy carbide exhibiting high hardness. After cryogenic or induction hardening treatment, the surface residual stress of austenitized specimens exhibited compressive stress rather than its original tensile stress state. The induction hardening treatment can significantly increase the microhardness of austenitized specimens, followed by quenching. Furthermore, the induction-hardened surface possessed less retained austenite. For practical industrial applications, a prior austenitizing heat treatment at 950 °C followed by hardening with an induction power of 12 kW was the optimal parameter for JIS SUJ3 bearing steel. The maximum microhardness and surface residual stress were 920 HV0.3 and −1083 MPa, respectively, while the lowest weight loss was 0.5 mg after the 10,000-revolution wear test.
- Open Access
Effects of Prior Microstructure on the Properties of Induction-Hardened JIS SCM440 Steel
JIS SCM440 steel is commonly used in precision parts after induction-hardening heat treatment. The fatigue behavior of induction-hardening parts largely depends on the combination of hardening depth and the magnitude and distribution of hardness and compressive residual stress. Therefore, it is necessary to determine the effects of different prior microstructures on the properties of JIS SCM440 steel after induction hardening. In the present study, the effects of prior microstructure (including spheroidized, annealed, normalized, and quenched and tempered) on the microhardness, hardening width, and residual stress of the induction-hardened specimens are investigated. The experimental results showed that the distribution behavior of residual stress in the hardened zone and heat-affected zone is due to the temperature gradient of the induction-hardening treatment. The hardened center appeared as compressive residual stress due to the martensitic transformation, which was accompanied by volume expansion. On the contrary, tensile residual stress will be generated in the heat-affected zone of incomplete phase transformation. The prior microstructure can affect the residual stress magnitude and distribution of microhardness and residual stresses due to the content of the cementite dissolved into the austenite at high temperatures. The difference in the carbon content of martensite after quenching will result in obvious differences in properties. The induction-hardened specimens with a normalized prior microstructure have the highest residual tensile stress in the heat-affected zone. The maximum residual tensile stress was 371 MPa in the heat-affected zone. The induction-hardened specimens with a quenched and tempered prior microstructure have the deepest hardening depth and widest residual compressive stress distribution range. The highest microhardness was 764 HV0.3, while the maximum residual compressive stress was −752 MPa.
Open AccessEffects of Prior Microstructure on the Properties of Induction-Hardened JIS SCM440 Steel
JIS SCM440 steel is commonly used in precision parts after induction-hardening heat treatment. The fatigue behavior of induction-hardening parts largely depends on the combination of hardening depth and the magnitude and distribution of hardness and compressive residual stress. Therefore, it is necessary to determine the effects of different prior microstructures on the properties of JIS SCM440 steel after induction hardening. In the present study, the effects of prior microstructure (including spheroidized, annealed, normalized, and quenched and tempered) on the microhardness, hardening width, and residual stress of the induction-hardened specimens are investigated. The experimental results showed that the distribution behavior of residual stress in the hardened zone and heat-affected zone is due to the temperature gradient of the induction-hardening treatment. The hardened center appeared as compressive residual stress due to the martensitic transformation, which was accompanied by volume expansion. On the contrary, tensile residual stress will be generated in the heat-affected zone of incomplete phase transformation. The prior microstructure can affect the residual stress magnitude and distribution of microhardness and residual stresses due to the content of the cementite dissolved into the austenite at high temperatures. The difference in the carbon content of martensite after quenching will result in obvious differences in properties. The induction-hardened specimens with a normalized prior microstructure have the highest residual tensile stress in the heat-affected zone. The maximum residual tensile stress was 371 MPa in the heat-affected zone. The induction-hardened specimens with a quenched and tempered prior microstructure have the deepest hardening depth and widest residual compressive stress distribution range. The highest microhardness was 764 HV0.3, while the maximum residual compressive stress was −752 MPa.
- Open Access
Effects of Shot Peening Pressure, Time, and Material on the Properties of Carburized Steel Shafts
Carburized steel shafts are commonly used in industry due to their good wear resistance and fatigue life. If the surface of carburized shafts exhibits an undesired tensile stress, shot peening treatment may be required to alter the stress condition on the surface. In the present study, the effects of shot peening pressure (3–5 kg/cm2), time (32–64 s), and material (stainless steel, carbon steel, and glass) on the residual stress, retained austenite, microhardness, and surface roughness of the carburized shafts were investigated. The experimental results showed that the surface residual tensile stress was changed into compressive stress after the shot peening treatment. The shot peening effects increased with the increasing peening pressure and time. In addition, a significant decrease in the amount of retained austenite in the subsurface region was observed. Peening with different materials can affect the peening effect. Using glass pellets exhibited the best shot peening effect but suffered massive pellet fracture during processing. In overall consideration, the optimal peening parameters for carburized steel shafts for practical industrial applications involved using the stainless-steel pellets with a peening pressure of 5 kg/cm2 and a peening time of 64 s. The maximum residual stress was −779 MPa at a depth of 0.02 mm, while the highest surface microhardness was 827 HV0.1.
Open AccessEffects of Shot Peening Pressure, Time, and Material on the Properties of Carburized Steel Shafts
Carburized steel shafts are commonly used in industry due to their good wear resistance and fatigue life. If the surface of carburized shafts exhibits an undesired tensile stress, shot peening treatment may be required to alter the stress condition on the surface. In the present study, the effects of shot peening pressure (3–5 kg/cm2), time (32–64 s), and material (stainless steel, carbon steel, and glass) on the residual stress, retained austenite, microhardness, and surface roughness of the carburized shafts were investigated. The experimental results showed that the surface residual tensile stress was changed into compressive stress after the shot peening treatment. The shot peening effects increased with the increasing peening pressure and time. In addition, a significant decrease in the amount of retained austenite in the subsurface region was observed. Peening with different materials can affect the peening effect. Using glass pellets exhibited the best shot peening effect but suffered massive pellet fracture during processing. In overall consideration, the optimal peening parameters for carburized steel shafts for practical industrial applications involved using the stainless-steel pellets with a peening pressure of 5 kg/cm2 and a peening time of 64 s. The maximum residual stress was −779 MPa at a depth of 0.02 mm, while the highest surface microhardness was 827 HV0.1.
- Open Access
Effect of Different Microstructures on Surface Residual Stress of Induction-Hardened Bearing Steel
JIS SUJ2 steel is most widely used in bearing steel. The advantages are good hardenability, excellent fatigue, wear resistance and comprehensive mechanical properties. The wear resistance and fatigue resistance of this steel are attracting more attention, and the residual stress state and its distribution on the surface of the heat affected zone are critical factors affecting the fatigue life and wear resistance of the parts. In this study, SUJ2 is used as a material by which to study the surface residual stress and retained austenite distribution of induction-hardened steel. Quenching and tempering treatments were used to obtain different microstructures and an induction method was used to re-quench the case region. After the heat treatment, the residual stress and retained austenite volume on the surface were analyzed by X-ray diffraction and analyses of the microstructure and the hardness were also conducted. The results show that the microstructure after heat treatment contains unsolved carbides, tempered martensite and retained austenite. In the induction-hardened area, the residual stress is all compressive, and the values are more than −750 MPa. In conclusion, the microstructures of the specimens before induction hardening have a significant impact on the effective case depth for the same output power condition and the surface residual stress changes from a tensile to a compressive state. In the induction-hardened area, the maximum of the residual compressive stress was increased as the austenitized temperature of quenching increased.
Open AccessEffect of Different Microstructures on Surface Residual Stress of Induction-Hardened Bearing Steel
JIS SUJ2 steel is most widely used in bearing steel. The advantages are good hardenability, excellent fatigue, wear resistance and comprehensive mechanical properties. The wear resistance and fatigue resistance of this steel are attracting more attention, and the residual stress state and its distribution on the surface of the heat affected zone are critical factors affecting the fatigue life and wear resistance of the parts. In this study, SUJ2 is used as a material by which to study the surface residual stress and retained austenite distribution of induction-hardened steel. Quenching and tempering treatments were used to obtain different microstructures and an induction method was used to re-quench the case region. After the heat treatment, the residual stress and retained austenite volume on the surface were analyzed by X-ray diffraction and analyses of the microstructure and the hardness were also conducted. The results show that the microstructure after heat treatment contains unsolved carbides, tempered martensite and retained austenite. In the induction-hardened area, the residual stress is all compressive, and the values are more than −750 MPa. In conclusion, the microstructures of the specimens before induction hardening have a significant impact on the effective case depth for the same output power condition and the surface residual stress changes from a tensile to a compressive state. In the induction-hardened area, the maximum of the residual compressive stress was increased as the austenitized temperature of quenching increased.