Qingfeng Duan
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Qingfeng Duan has a total of 18 co-authors. Here are the top co-authors by number of shared publications:
Dongfeng Cao
State Key Laboratory of Advanced Technology for Materials Synthesis and Processing Wuhan University of Technology Wuhan People's Republic of China
3 shared publicationsHaixiao Hu
State Key Laboratory of Advanced Technology for Materials Synthesis and Processing Wuhan University of Technology Wuhan People's Republic of China
3 shared publicationsWei Cai
State Key Laboratory of Advanced Technology for Materials Synthesis and Processing Wuhan University of Technology Wuhan People's Republic of China
3 shared publicationsJunkang Xia
State Key Laboratory of Advanced Technology for Materials Synthesis and Processing Wuhan University of Technology Wuhan People's Republic of China
2 shared publications- Shuxin Li
State Key Laboratory of Advanced Technology for Materials Synthesis and Processing, Wuhan University of Technology, Wuhan 430070, China
2 shared publications Yundong Ji
State Key Laboratory of Advanced Technology for Materials Synthesis and Processing Wuhan University of Technology Wuhan People's Republic of China
2 shared publications
Latest Publications
- 25 August 2025
- Published by Wiley in Polymer Composites
- Vol. 47 (3) , 2899-2914
Load‐Bearing Capacity and Failure Mode of L‐Shaped Laminates: The Role of Delamination Defect Location and Fiber Bridging
Delamination defects in the R‐zone of L‐shaped laminates, difficult to eliminate during manufacturing, compromise structural integrity and complicate performance evaluation. This study investigates the effect of delamination defect location on load‐bearing capacity and failure mechanisms of L‐shaped laminates using four‐point bending tests and a validated cohesive zone model with a modified traction‐separation law. Specimens with four typical defect locations were tested, with delamination initiation and propagation monitored by high‐speed imaging and load–displacement data recorded. Results show that load‐bearing capacity is significantly influenced by the defect location, and all delamination growth initiates from the defect site. While fiber bridging affects the failure mode, its impact on maximum capacity is limited due to a wide high‐stress region in the L‐shaped radius. An envelope diagram illustrates the relationship between defect location and load‐bearing capacity, providing critical insights for damage‐tolerant design of L‐shaped laminates.
- 25 August 2025
- Published by Wiley in Polymer Composites
- Vol. 47 (3) , 2899-2914
Load‐Bearing Capacity and Failure Mode of L‐Shaped Laminates: The Role of Delamination Defect Location and Fiber Bridging
Delamination defects in the R‐zone of L‐shaped laminates, difficult to eliminate during manufacturing, compromise structural integrity and complicate performance evaluation. This study investigates the effect of delamination defect location on load‐bearing capacity and failure mechanisms of L‐shaped laminates using four‐point bending tests and a validated cohesive zone model with a modified traction‐separation law. Specimens with four typical defect locations were tested, with delamination initiation and propagation monitored by high‐speed imaging and load–displacement data recorded. Results show that load‐bearing capacity is significantly influenced by the defect location, and all delamination growth initiates from the defect site. While fiber bridging affects the failure mode, its impact on maximum capacity is limited due to a wide high‐stress region in the L‐shaped radius. An envelope diagram illustrates the relationship between defect location and load‐bearing capacity, providing critical insights for damage‐tolerant design of L‐shaped laminates.
- Open Access
Experimental Investigation of Failure Behaviors of CFRP–Al Lap Joints with Various Configurations Under High- and Low-Temperature Conditions
The failure behaviors of CFR–aluminum lap joints with diverse configurations through quasi-static tensile tests were conducted at −40 °C, 25 °C, and 80 °C. Four specimen types were examined: CFRP–aluminum alloy two-bolt single-lap joints (TBSL), two-bolt double-lap joints (TBDL), two-bolt bonded–bolted hybrid single-lap joints (BBSL), and two-bolt bonded–bolted hybrid double-lap joints (BBDL). The analysis reveals that double-lap joints possess a markedly higher strength than single-lap joints. The ultimate loads of the TBSL (single-lap joints) at temperatures of −40 °C and 25 °C are 29.5% and 26.20% lower, respectively, than those of the TBDL (double-lap joints). Similarly, the ultimate loads of the BBSL (hybrid single-lap joints) at −40 °C, 25 °C, and 80 °C are 19.8%, 31.66%, and 40.05% lower, respectively, compared to the corresponding data of the TBDL. In bolted–bonded hybrid connections, the adhesive layer enhances the joint’s overall stiffness but exhibits significant temperature dependence. At room and low temperatures, the ultimate loads of the BBDL are 46.97 kN at −40 °C and 50.30 kN at 25 °C, which are significantly higher than those of the TBDL (42.24 kN and 44.63 kN, respectively). However, at high temperatures, the load–displacement curves of the BBDL and TBDL are nearly identical. This suggests that the adhesive layers are unable to provide a sufficient shear-bearing capacity due to their low modulus at elevated temperatures. This research provides valuable insights for designing composite–metal connections in aircraft structures, highlighting the impacts of different joint configurations and temperature conditions on failure modes and load-bearing capacities.
Open AccessExperimental Investigation of Failure Behaviors of CFRP–Al Lap Joints with Various Configurations Under High- and Low-Temperature Conditions
The failure behaviors of CFR–aluminum lap joints with diverse configurations through quasi-static tensile tests were conducted at −40 °C, 25 °C, and 80 °C. Four specimen types were examined: CFRP–aluminum alloy two-bolt single-lap joints (TBSL), two-bolt double-lap joints (TBDL), two-bolt bonded–bolted hybrid single-lap joints (BBSL), and two-bolt bonded–bolted hybrid double-lap joints (BBDL). The analysis reveals that double-lap joints possess a markedly higher strength than single-lap joints. The ultimate loads of the TBSL (single-lap joints) at temperatures of −40 °C and 25 °C are 29.5% and 26.20% lower, respectively, than those of the TBDL (double-lap joints). Similarly, the ultimate loads of the BBSL (hybrid single-lap joints) at −40 °C, 25 °C, and 80 °C are 19.8%, 31.66%, and 40.05% lower, respectively, compared to the corresponding data of the TBDL. In bolted–bonded hybrid connections, the adhesive layer enhances the joint’s overall stiffness but exhibits significant temperature dependence. At room and low temperatures, the ultimate loads of the BBDL are 46.97 kN at −40 °C and 50.30 kN at 25 °C, which are significantly higher than those of the TBDL (42.24 kN and 44.63 kN, respectively). However, at high temperatures, the load–displacement curves of the BBDL and TBDL are nearly identical. This suggests that the adhesive layers are unable to provide a sufficient shear-bearing capacity due to their low modulus at elevated temperatures. This research provides valuable insights for designing composite–metal connections in aircraft structures, highlighting the impacts of different joint configurations and temperature conditions on failure modes and load-bearing capacities.
- Top Cited Papers
- 21 January 2024
- Published by Elsevier in Composite Structures
- Vol. 332
A new mechanism based cohesive zone model for Mode I delamination coupled with fiber bridging of composite laminates
- 21 January 2024
- Published by Elsevier in Composite Structures
- Vol. 332
Top Cited PapersA new mechanism based cohesive zone model for Mode I delamination coupled with fiber bridging of composite laminates