Matúš Gavalec has a total of 16 co-authors. Here are the top co-authors by number of shared publications:
- Katarína Bártová
Faculty of Materials Science and Technology in Trnava, Slovak University of Technology in Bratislava, 811 07 Bratislava, Slovakia
2 shared publications - Marek Kudláč
Faculty of Materials Science and Technology in Trnava, Slovak University of Technology in Bratislava, 811 07 Bratislava, Slovakia
2 shared publications - Mária Dománková
Faculty of Materials Science and Technology in Trnava, Slovak University of Technology in Bratislava, 811 07 Bratislava, Slovakia
2 shared publications Alena Košinová
1 shared publication- David Slnek
Faculty of Materials Science and Technology in Trnava , Slovak University of Technology in Bratislava , J. Bottu 2781/25, 91724 Trnava , Slovakia
1 shared publication - Dragan Rajnovic
Department of Production Engineering, Faculty of Technical Science, University of Novi Sad, Trg Dositeja Obradovica 6, 21000 Novi Sad, Serbia
1 shared publication
Latest Publications
- Open Access
- 1 September 2025
- Published by Stowarzyszenie Menedzerow Jakosci i Produkcji in Production Engineering Archives
- Vol. 31 (3) , 376-385
Influence of high cutting speed turning on surface and corrosion properties of 08Ch18N10T austenitic stainless steel from the perspective of operational safety of primary circuit of a nuclear power plant
From the point of view of the safety of nuclear power plants, it is necessary to determine the properties of the manufactured material used. One of the possible risks is the use of inappropriate turning on the material, whose subsequent surface and thus corrosion properties in such an extreme environment are significantly stricken. In this work, high cutting speed (596 m⋅min −1 ) was used for turning austenitic stainless steel 08Ch18N10T using a CBN cutting tool. Such a high cutting speed significantly affected surface integrity and surface properties such as residual stresses, roughness, hardness and surface toughness (metallographically determined and analysed using X-ray tensometry and acoustic emission). The area that was turned contained deformed grains, which contained deformation twins and slip bands. All these factors can affect stress corrosion cracking susceptibility and corrosion resistance. For this reason, the sample was exposed in a MgCl2 solution according to the ASTM G36, while the surface crack density and the crack lengths or depths were determined. The effect of residual stresses on the direction and propagation of surface cracks has been proven. DL-EPR test recorded sensitization that did not occur at the grain boundaries but in the turning direction where pitting lines appeared. Exposure in a simulated primary circuit environment was performed in an autoclave, where no signs of stress corrosion cracking were confirmed.
- 1 September 2025
- Published by Stowarzyszenie Menedzerow Jakosci i Produkcji in Production Engineering Archives
- Vol. 31 (3) , 376-385
Open AccessInfluence of high cutting speed turning on surface and corrosion properties of 08Ch18N10T austenitic stainless steel from the perspective of operational safety of primary circuit of a nuclear power plant
From the point of view of the safety of nuclear power plants, it is necessary to determine the properties of the manufactured material used. One of the possible risks is the use of inappropriate turning on the material, whose subsequent surface and thus corrosion properties in such an extreme environment are significantly stricken. In this work, high cutting speed (596 m⋅min −1 ) was used for turning austenitic stainless steel 08Ch18N10T using a CBN cutting tool. Such a high cutting speed significantly affected surface integrity and surface properties such as residual stresses, roughness, hardness and surface toughness (metallographically determined and analysed using X-ray tensometry and acoustic emission). The area that was turned contained deformed grains, which contained deformation twins and slip bands. All these factors can affect stress corrosion cracking susceptibility and corrosion resistance. For this reason, the sample was exposed in a MgCl2 solution according to the ASTM G36, while the surface crack density and the crack lengths or depths were determined. The effect of residual stresses on the direction and propagation of surface cracks has been proven. DL-EPR test recorded sensitization that did not occur at the grain boundaries but in the turning direction where pitting lines appeared. Exposure in a simulated primary circuit environment was performed in an autoclave, where no signs of stress corrosion cracking were confirmed.
- Open Access
- 23 February 2024
- Published by Jan Evangelista Purkyne University in Usti nad Labem in Manufacturing Technology
- Vol. 24 (1) , 53-61
Research on FSW Welds of Al-Alloy Modified by Laser Shock Peening Process
The friction stir welding (FSW) method is classified as a so-called green or eco-friendly production technology in terms of its environmental impact. In the process of friction stir welding, there is no melting and the weld joint is formed by the movement of a rotating tool between the materials to be welded. The advantage of this technology is welding without the accompanying phenomena such as the release of harmful substances into the air, the emission of infrared, ultraviolet and visible radiation, and low energy consumption. In this work, friction stir welding tests of FSW and SR-FSW type were carried out, the butt welds themselves were performed on EN AW-6060 sheets of 5 mm thickness. The surfaces of the specimens that met the weld quality visually were treated with laser shock peening (LSP), which is based on a pulsed effect. In the process of experiments, the authors investigated the weld quality at different speeds and tool rotation visually, then the welds were subjected to microscopic analysis, microhardness analysis and nanohardness analysis.
- 23 February 2024
- Published by Jan Evangelista Purkyne University in Usti nad Labem in Manufacturing Technology
- Vol. 24 (1) , 53-61
Open AccessResearch on FSW Welds of Al-Alloy Modified by Laser Shock Peening Process
The friction stir welding (FSW) method is classified as a so-called green or eco-friendly production technology in terms of its environmental impact. In the process of friction stir welding, there is no melting and the weld joint is formed by the movement of a rotating tool between the materials to be welded. The advantage of this technology is welding without the accompanying phenomena such as the release of harmful substances into the air, the emission of infrared, ultraviolet and visible radiation, and low energy consumption. In this work, friction stir welding tests of FSW and SR-FSW type were carried out, the butt welds themselves were performed on EN AW-6060 sheets of 5 mm thickness. The surfaces of the specimens that met the weld quality visually were treated with laser shock peening (LSP), which is based on a pulsed effect. In the process of experiments, the authors investigated the weld quality at different speeds and tool rotation visually, then the welds were subjected to microscopic analysis, microhardness analysis and nanohardness analysis.
- Open Access
- 1 January 2024
- Published by University Library in Kragujevac in Applied Engineering Letters : Journal of Engineering and Applied Sciences
- Vol. 9 (2) , 76-84
ANALYSIS OF STRESS CORROSION CRACKING OF HETEROGENEOUS WELDED JOINTS IN SIMULATED PRIMARY WATER ENVIRONMENT
The paper deals with the stress corrosion cracking of heterogeneous welded joints. The welded joints were made of austenitic base metal (AISI 321) and ferritic weld metal by arc welding. Two methods were used to analyze the stress corrosion cracking of samples of this type of welded joint. The first method was a slow strain rate test (SSRT) using a tabletop device at a temperature of 60°C with a graded strain rate for three specimens (10−5, 10−6, and 10−7 1/s). The second method was exposure in a corrosion autoclave at a temperature of 270°C and pressure of 12.26 N/mm2, while prestressing devices were used to achieve the prestressing at the level of yield strength and 3% plastic deformation. One specimen was bent to 60°. Boric acid solutions were used as the medium, which was supposed to simulate the environment of the primary circuit of nuclear power plants, a type of water-water energetic reactor. The surface and the presence of corrosion products, cracks, fractures, or pits on specimens were monitored using scanning electron microscopy, stereomicroscopy, confocal microscopy, and light microscopy. A gravimetric analysis was performed, as well, to determine the corrosion rate after exposure to the autoclave.
- 1 January 2024
- Published by University Library in Kragujevac in Applied Engineering Letters : Journal of Engineering and Applied Sciences
- Vol. 9 (2) , 76-84
Open AccessANALYSIS OF STRESS CORROSION CRACKING OF HETEROGENEOUS WELDED JOINTS IN SIMULATED PRIMARY WATER ENVIRONMENT
The paper deals with the stress corrosion cracking of heterogeneous welded joints. The welded joints were made of austenitic base metal (AISI 321) and ferritic weld metal by arc welding. Two methods were used to analyze the stress corrosion cracking of samples of this type of welded joint. The first method was a slow strain rate test (SSRT) using a tabletop device at a temperature of 60°C with a graded strain rate for three specimens (10−5, 10−6, and 10−7 1/s). The second method was exposure in a corrosion autoclave at a temperature of 270°C and pressure of 12.26 N/mm2, while prestressing devices were used to achieve the prestressing at the level of yield strength and 3% plastic deformation. One specimen was bent to 60°. Boric acid solutions were used as the medium, which was supposed to simulate the environment of the primary circuit of nuclear power plants, a type of water-water energetic reactor. The surface and the presence of corrosion products, cracks, fractures, or pits on specimens were monitored using scanning electron microscopy, stereomicroscopy, confocal microscopy, and light microscopy. A gravimetric analysis was performed, as well, to determine the corrosion rate after exposure to the autoclave.